Transactions on Electrical and Electronic Materials
/
v.9
no.4
/
pp.137-142
/
2008
The parasitic resistance is studied to silicon/metal contact junction for improving device performance and to lower contact/serial resistance silicide in natural sequence. In this paper constructs the stepwise Ni silicide process for parasitic resistance reduction for silicon/metal contact junction. We have investigated multi-step Ni silicide on SiGe substrate with stepwise annealing method as an alternative to compose more thermally reliable Ni silicide layer. Stepwise annealing for silicide formation is exposed to heating environment with $5^{\circ}C/sec$ for 10 seconds and a dwelling for both 10 and 30 seconds, and ramping-up and the dwelling was repeated until the final annealing temperature of $700\;^{\circ}C$ is achieved. Finally a direct comparison for single step and stepwise annealing process is obtained for 20 nm nickel silicide through stepwise annealing is $5.64\;{\Omega}/square$ at $600\;^{\circ}C$, and it is 42 % lower than that of as nickel sputtered. The proposed stepwise annealing for Ni silicidation can provide the least amount of NiSi at the interface of nickel silicide and silicon, and it provides lower resistance, higher thermal-stability, and superior morphology than other thermal treatment.
Kim, Zin-Sig;Ahn, Hokyun;Lim, Jong-Won;Nam, Eunsoo
Proceedings of the Korean Vacuum Society Conference
/
2014.02a
/
pp.292-292
/
2014
Wide band gap semiconductors, such as III-nitrides (GaN, AlN, InN, and their alloys), SiC, and diamond are expected to play an important role in the next-generation electronic devices. Specifically, GaN-based high electron mobility transistors (HEMTs) have been targeted for high power, high frequency, and high temperature operation electronic devices for mobile communication systems, radars, and power electronics because of their high critical breakdown fields, high saturation velocities, and high thermal conductivities. For the stable operation, high power, high frequency and high breakdown voltage and high current density, the fabrication methods have to be optimized with considerable attention. In this study, low ohmic contact resistance and smooth surface morphology to AlGaN/GaN on 2 inch c-plane sapphire substrate has been obtained with stepwise annealing at three different temperatures. The metallization was performed under deposition of a composite metal layer of Ti/Al/Ni/Au with thickness. After multi-layer metal stacking, rapid thermal annealing (RTA) process was applied with stepwise annealing temperature program profile. As results, we obtained a minimum specific contact resistance of $1.6{\times}10^{-7}{\Omega}cm2$.
The surface chemistry of D2O dosed Zircaloy-4 (Zry-4) surface followed by Ar-ion bombardment and annealing was studied by means of X-ray photoelectron spectroscopy (XPS) and Ultraviolet photoelectron spectroscopy (UPS). In the XPS study, Ar-ion bombardment caused decrease of the oxygen on the surface region of Zry-4 and therefore led to change the oxidation states of the zirconium from oxide to metallic form. In addition, oxidation states of zirconium were changed to lower oxidation states of zirconium due to depopulation of oxygen on the surface region by annealing. Up to about 787 K, the bulk oxygen diffused out to the subsurface region and after this temperature, the oxygen on the surface of Zry-4 was depopulated. UPS study showed that the valence band spectrum of the D2O exposed Zry-4 exhibited a dominant peak at around 13 eV and no clear Fermi edge was detected. After stepwise Ar+ sputtering processes, the decrease of the oxygen on the surface of Zry-4 led to suppress the dominant peak around 13 eV, the peak around 9 eV and develop a new peak of the metallic Zr 4d state (20.5-21.0 eV) at the Fermi level.
Park, Ju-Yun;Jung, Se-Won;Chun, Mi-Sun;Kang, Yong-Cheol
Bulletin of the Korean Chemical Society
/
v.30
no.6
/
pp.1349-1352
/
2009
We report the results of the surface chemistry of deuterized ethanol exposed Zircaloy-4 (Zry-4) surfaces with various amount of $C_2D_5$OD exposures at 190 K. This system was examined with Auger electron spectroscopy (AES) and temperature programmed desorption (TPD) techniques. In TPD study, $D_2$ was evolved at two different desorption temperature regions accompanying with broad desorption background. The lower temperature feature at around 520 K showed first-order desorption kinetics. The high temperature desorption peak at around 650 K shifted to lower desorption temperature as the exposure of $C_2D_5$OD increased. The Zr(MNV) Auger peak shifted about 2.5 eV from 147 eV to lower electron energy followed by 300 L of $C_2D_5$OD dosing. This implies metallic zirconium was oxidized by deuterized ethanol adsorption. After stepwise annealing of the oxidized Zry-4 sample up to 843 K, the shifted Zr(MNV) peak was gradually shifted back to metallic zirconium peak position. After the sample was heated to 843 K, the oxygen content near the Zry-4 surface was recovered to clean surface level. The concentration of carbon, however, was not recovered by annealing the sample.
When polyethylene terephthalate(PET) film specimen were stepwise elongated under tension with various speeds of about 0.5~500 mm/min, the necking area, consisted of transparent and opaque bands, was formed during plastic deformation. Stress oscillation was apparently obtained in the stress-strain curve of above specimen. However, stress oscillation was not obtained in the stress-strain curve of annealing specimen. Microstructure was examined dynamically using an optical microscopy and thermal analysis was carried out in a differential scanning calorimeter at a heating rate of 10${\circ}$/min. Also, orientation and crystallization were examined using monochromatic-pinhole technique and elastic modulus was measured by a dynamic mechanical analyzer in the temperature range of -150~70 ${\circ}$ with the frequency of 1 Hz. Transparent PET products were fabricated by use of the PET pellets annealed at 83${\circ}$ for 30 min in an electric furnace.
We demonstrated a high speed liquid crystal (LC) display mode based on a nonchiral smectic C LC in an antiparallel planar geometry. In this antiparallel planar nonchiral smectic C (APNSC) LC mode, analog gray scales and wide viewing properties are achieved using a stepwise thermal annealing process (STAP). Because of an initially stable LC alignment in large area through the STAP, the APNSC LC mode exhibits the characteristics of fast response and high contrast ratio. This new APNSC mode is suitable for processing the dynamic image at a video rate in the next-generation LCDs.
The ratio of trivalent to divalent copper has been determined by the redox titration for two superconducting phases of $YBa_2Cu^{3+}_{2x}Cu^{2+}_{3-2x}O_{6.5+x}$ with the onset temp. of 60K (x = 0.23 ${\pm}$ 0.01) and 90K (x = 0.35 ${\pm}$ 0.02), and for the insulating one (x ${\cong}$ 0) which was kept in an ambient atmosphere for 72 hrs. It is found that $T_c$, and the ratio of $Cu^{3+}/Cu^{2+}$ depend strongly on the annealing temperature and time. A typical orthorhombic phase can easily be obtained by a slow cooling or stepwise cooling at $PO_2$ = 1 atm, and shows a high Tc (ca. 90K) superconductivity.
The composites in the system aluminium titanate-mullite were synthesized by stepwise alkoxide hydrolysis of tetraethylorthosilicate, Si(OCLH5), and titaniumtetraethoxide, $Ti(OC_{2}H_{5})_4$ in $Al_{2}O_{3}$ ethanolic colloidal solution. All particles produced by sol-gel-process were amorphous, monodispesed and had a narrow particle size distribution. Sintered bodies at $1600 ^{\circ}C$ for 2h were subjected to prolonged durability tests-on the one hand annealing at the critical decomposition temperature of $1100 ^{\circ}C$ for lOOh and on the other cyclic thermal shock between 750 and $1400 ^{\circ}C$ for 100h. The best thermal durability was achieved by a composition containing 70 and 80 vol% aluminium titanate, which showed little change in microstructure and thermal expansion cycles during the tests. The microstructural degradation of samples studied using scanning electron microscopy, X-ray diffraction, and dilatometry, was presented here. The study was conducted in order to predict the service life of aluminium titanate-mullite ceramics formed by this processing route.
The oxidation of NiAl(110) was investigated in the temperature regime between 300K and 1300 K using LEED (low energy electron diffraction), TPD (temperature programmed desorption) and HREELS (high resolution electron energy loss spectroscopy). The adsorption of N2O and O2 up to reconstructions. Stepwise annealing of the oxygen-saturated sample from 600 K to 1300K in UHV (ultra-high vacuum,) results in firstly the onset of randomly oriented then finally fairly well-ordered. 5 ${\AA}$ Al2O3 film with quasi-hexagonal periodicity. Ordered thicker oxide films of 18-30 ${\AA}$ seem to be grown on this interfacial oxide layer by direct oxidation of sample at elevated temperature between 1150 and 1300 K because of the LEED pattern consisting of new broad hexagonal spots and the previous 5 ${\AA}$ spots. Although the periodicity of surface oxygen arrays shows no significant change from an hexagonal close-packing, the O-O distance changes from ∼3.0 ${\AA}$ film to ∼2.9 ${\AA}$ for thicker oxides. with the appearance of Auger parameter, for the 5${\AA}$ film can be described better as an interfacial oxide layer. The observation of three symmetric phonon peaks can be also a supporting evidence for this phase assignment since thicker oxide films on the Same Ni2Al3(110) show somewhat different phonon structure much closer to that of the ${\gamma}$-Al2O3. The adsorption/desorption of methanol further proves the preparation of less-defective and/or oxygen-terminated Al2O3 films showing ordered phase transitions with the change of oxide thickness between 5 ${\AA}$ to 30 ${\AA}$.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.