• 제목/요약/키워드: stainless steel substrate

검색결과 160건 처리시간 0.03초

음극 아크 증착으로 제조된 AlTiN 박막의 특성 (Properties of AlTiN Films Deposited by Cathodic Arc Deposition)

  • 양지훈;김성환;송민아;정재훈;정재인
    • 한국표면공학회지
    • /
    • 제49권3호
    • /
    • pp.307-315
    • /
    • 2016
  • The properties of AlTiN films by a cathodic arc deposition process have been studied. Oblique angle deposition has been applied to deposit AlTiN films. AlTiN films have been deposited on stainless steel (SUS304) and cemented carbide (WC) at a substrate temperature of $500^{\circ}C$. AlTiN films were analyzed by scanning electron microscopy, glow-discharge light spectroscopy, micro-vickers hardness, and nanoindenter. When applying a current of 50 A to the cathodic arc source, it showed that the density of macroparticle of AlTiN films was 5 lower than other deposition conditions. With the increase of the bias voltage applied to the substrate up to -150 V, the density of macroparticle was decreased. The change of the $N_2$ flow rate during coating process made no influence on the film properties. For the multi-layered films, the film prepared at oblique angle of $60^{\circ}$ showed the highest hardness of 28 GPa and $H^3/E^2$ index of 0.18. AlTiN films have been shown a good oxidation resistance up to $800^{\circ}C$.

치아/복합레진 수복부의 중합 수축시 검출된 음향방출의 통계적 검증 (Statistical Verification of Acoustic Emissions Detected during Polymerization Shrinkage of Resin Restoration in Dental Ring)

  • 구자욱;최낙삼
    • Composites Research
    • /
    • 제23권6호
    • /
    • pp.39-46
    • /
    • 2010
  • 치아의 와동에 수복된 치과용 복합레진을 광(LED) 조사를 통해 정화 수축시키면서 음향방출(acoustic emission, AE) 신호를 검출하였다. 비모수 통계법인 Mann-Whitney법과 Kruskal-Wallis법을 이용하여 시편의 재질과 계면의 접착조건에 따른 AE hit event 수와 최대진폭을 비교 평가하였다. PMMA와 치아시편으로부터 검출된 선호의 최대진폭은 정착조건에 따른 차이가 없었지만 스테인리스 시편으로부터 검출된 신호는 접착조건에 따라 최대 진폭의 차이가 있었다(p<0.05). AE hit event 수는 양호한 접착조건에서 시편의 재질에 따라 차이가 있었고(p<0.05), 세가지 재질의 시편 모두 접착조건이 양호한 실험에서 AE 신호가 적게 검출되었다. SEM을 이용하여 계면에 생성된 캡을 측정한 결과 AE가 많이 검출되고 검출된 신호의 최대 진폭이 큰 시편에서 갱의 폭이 넓고 형성 비율이 높았다.

전기화학법을 이용한 $\textrm{BaTiO}_3$박막의 제조 (Preparation of $\textrm{BaTiO}_3$ Thin Films by Electrochemical Method)

  • 공필구;유영성;이종국;김환;박순자
    • 한국재료학회지
    • /
    • 제7권2호
    • /
    • pp.114-120
    • /
    • 1997
  • $Ba(NO_{3})_{2}$$TiCl_{4}$의 혼합 수용액으로부터 전기화학법 중 음극혼원법(cathodic reduction method)을 이용하여 stainless steel기판 위에 $BaTiO_{3}$박막을 제조하였다. $BaTiO_{3}$전구체 박막은 혼합 수용액으로부터 반응초기에 $TiO_{2}{\cdot}nH_{2}O$M/형태로 우선적으로 형성되었으며, 일정 시간이 경과한 후에는 일정한 Ba/Ti몰비를 갖는 박막이 제조되었다. $BaTiO_{3}$박막 내 Ba/Ti조성비는 혼합 수용액 내에 존재하는 이온 조성비 $Ba^{2+}/Ti_{4+}$에 변화하였는데, 0.3M $Ba(NO_{3})_{2}$와 0.1M $TiCI_{4}$의 혼합 수용액과 $10mA/cm^2$의 전류를 흘려주는 조건에서 Ba/Ti의 조성비가 1에 가까운 박막을 얻을 수 있었다. 이러한 전구체 박막을 $500^{\circ}C$이상에서 열처리한 결고 페로브스카이트 상의 $BaTiO_{3}$박막이 제조되었다.

  • PDF

PECVD를 이용한 금속 스탬프용 점착방지막 형성과 특성 평가 (Fabrication and Characterization of an Antistiction Layer by PECVD (plasma enhanced chemical vapor deposition) for Metal Stamps)

  • 차남구;박창화;조민수;김규채;박진구;정준호;이응숙
    • 한국재료학회지
    • /
    • 제16권4호
    • /
    • pp.225-230
    • /
    • 2006
  • Nanoimprint lithography (NIL) is a novel method of fabricating nanometer scale patterns. It is a simple process with low cost, high throughput and resolution. NIL creates patterns by mechanical deformation of an imprint resist and physical contact process. The imprint resist is typically a monomer or polymer formulation that is cured by heat or UV light during the imprinting process. Stiction between the resist and the stamp is resulted from this physical contact process. Stiction issue is more important in the stamps including narrow pattern size and wide area. Therefore, the antistiction layer coating is very effective to prevent this problem and ensure successful NIL. In this paper, an antistiction layer was deposited and characterized by PECVD (plasma enhanced chemical vapor deposition) method for metal stamps. Deposition rates of an antistiction layer on Si and Ni substrates were in proportion to deposited time and 3.4 nm/min and 2.5 nm/min, respectively. A 50 nm thick antistiction layer showed 90% relative transmittance at 365 nm wavelength. Contact angle result showed good hydrophobicity over 105 degree. $CF_2$ and $CF_3$ peaks were founded in ATR-FTIR analysis. The thicknesses and the contact angle of a 50 nm thick antistiction film were slightly changed during chemical resistance test using acetone and sulfuric acid. To evaluate the deposited antistiction layer, a 50 nm thick film was coated on a stainless steel stamp made by wet etching process. A PMMA substrate was successfully imprinting without pattern degradations by the stainless steel stamp with an antistiction layer. The test result shows that antistiction layer coating is very effective for NIL.

자동차용 사이드 몰딩과 엠블럼 적용을 위한 UV 경화형 아크릴 점착 테이프의 점착물성 (Adhesion Properties of UV-curable Acrylic PSA Tape for Automotive Sidemolding and Emblem)

  • 박지원;이승우;김현중;원동복;김동복;이강신;우항수;김언아
    • 접착 및 계면
    • /
    • 제12권3호
    • /
    • pp.81-87
    • /
    • 2011
  • 본 연구에서는 자동차 조립공정에 적용 할 수 있는 아크릴폼테이프를 합성하기 위하여 UV 중합 및 가교 공정을 도입하였다. 중합된 점착제를 폼에 합지하고 폼의 두께를 변화시켜 가며 시험편을 제조하였다. 기본물성을 측정하기 위해 stainless steel 표면에서의 강도를 측정하였으며 이때 peel, dynamic shear and t-block을 사용하였다. 일반적인 점착제에 비해 우수한 결과를 보여 주었으며 외부 요인 - 두께, 젖음시간 - 등에 의해 물성이 크게 변화하는 것을 확인 할 수 있었다. 본 연구에 활용된 아크릴폼점착제의 자동차 공정 활용성을 평가하기 위해 다양한 플라스틱 피착제에서 물성 측정을 진행하였다. 저표면에너지그룹으로 분류되는 PP와 PE에서는 그 물성이 전혀 발현되지 못했으나 기작 차이에 의해 dynamic shear 시험에서는 일부 물성이 발현됨을 확인 할 수 있었다.

팔라듐 합금 복합막 제조를 위한 Intermediate Layer 연구 (A Study on Intermediate Layer for Palladium-Based Alloy Composite Membrane Fabrication)

  • 황용묵;김광제;소원욱;문상진;이관영
    • 공업화학
    • /
    • 제17권5호
    • /
    • pp.458-464
    • /
    • 2006
  • 팔라듐 합금 복합막의 제조는 니켈 분말과 무기화합물의 혼합물로 개질된 튜브형 다공성 스테인레스 스틸 지지체 표면 위에 무전해 도금법(elctroless plating technique)에 의해 팔라듐 - 니켈 - 은을 박막으로 도금하는 형태로 이루어졌다. 일반적인 다공성 금속 지지체는 기공이 크기 때문에 그 자체로서 도금에 적합한 지지층이 되기가 어렵고, 결함이 없는 팔라듐 복합막의 제조가 쉽지 않아 본 연구에서는 금속 지지체와 팔라듐 사이에 중간층(intermediate layer)을 형성하여 이와 같은 문제점을 극복하고자 하였다. 중간층의 소재인 실리카 졸, 알루미나 졸, 이산화티타늄 졸 등의 무기화합물과 니켈 분말의 혼합물로 다공성 금속 지지체 위에 코팅하여 박막을 형성하고 제조 조건에 따른 질소 투과도를 측정하고 비교하였다. SEM 분석법에 의해 니켈과 무기화합물 혼합물의 표면층의 형성 모습도 측정하였다. 제조된 중간층 가운데 이산화티타늄 졸과 니켈의 혼합물이 가장 낮은 질소 투과도와 치밀한 표면층을 나타내었다. 최종적으로 니켈과 실리카의 혼합 중간층으로 이루어진 팔라듐-니켈-은 합금 복합막을 제조하고 수소와 질소의 투과도를 측정하였다. 1기압 이하에서 질소에 대한 수소 선택도는 무한대였으며 수소투과 속도는 1 기압, $500^{\circ}C$에서 $1.39{\times}10^{-2}mol/m^2{\cdot}s$의 값을 나타냈다.

미세금형 가공을 위한 전기화학식각 공정의 유한요소 해석 및 실험결과 비교 (Finite Element Simulation and Experimental Study on the Electrochemical Etching Process for Fabrication of Micro Metal Mold)

  • 류헌열;임현승;조시형;황병준;이성호;박진구
    • 한국재료학회지
    • /
    • 제22권9호
    • /
    • pp.482-488
    • /
    • 2012
  • To fabricate a precise micro metal mold, the electrochemical etching process has been researched. We investigated the electrochemical etching process numerically and experimentally to determine the etching tendency of the process, focusing on the current density, which is a major parameter of the process. The finite element method, a kind of numerical analysis, was used to determine the current density distribution on the workpiece. Stainless steel(SS304) substrate with various sized square and circular array patterns as an anode and copper(Cu) plate as a cathode were used for the electrochemical experiments. A mixture of $H_2SO_4$, $H_3PO_4$, and DIW was used as an electrolyte. In this paper, comparison of the results from the experiment and the numerical simulation is presented, including the current density distribution and line profile from the simulation, and the etching profile and surface morphology from the experiment. Etching profile and surface morphology were characterized using a 3D-profiler and FE-SEM measurement. From a comparison of the data, it was confirmed that the current density distribution and the line profile of the simulation were similar to the surface morphology and the etching profile of the experiment, respectively. The current density is more concentrated at the vertex of the square pattern and circumference of the circular pattern. And, the depth of the etched area is proportional to the current density.

Full Color Top Emission AMOLED Displays on Flexible Metal Foil

  • Hack, Michael;Hewitt, Richard;Urbanik, Ken;Chwang, Anna;Brown, Julie J.;Lu, Jeng Ping;Shih, Chinwen;Ho, Jackson;Street, Bob;Ramos, Teresa;Rutherford, Nicole;Tognoni, Keith;Anderson, Bob;Huffman, Dave
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2006년도 6th International Meeting on Information Display
    • /
    • pp.305-308
    • /
    • 2006
  • Advanced mobile communication devices require a bright, high information content display in a small, light-weight, low power consumption package. For portable applications flexible (or conformable) and rugged displays will be the future. In this paper we outline our progress towards developing such a low power consumption active-matrix flexible OLED $(FOLED^{TM})$ display. We demonstrate full color 100 ppi QVGA active matrix OLED displays on flexible stainless steel substrates. Our work in this area is focused on integrating three critical enabling technologies. The first technology component is based on UDC's high efficiency long-lived phosphorescent OLED $(PHOLED^{TM})$ device technology, which has now been commercially demonstrated as meeting the low power consumption performance requirements for mobile display applications. Secondly, is the development of flexible active-matrix backplanes, and for this our team are employing PARC's Excimer Laser Annealed (ELA) poly-Si TFTs formed on metal foil substrates as this approach represents an attractive alternative to fabricating poly-Si TFTs on plastic for the realization of first generation flexible active matrix OLED displays. Unlike most plastics, metal foil substrates can withstand a large thermal load and do not require a moisture and oxygen permeation barrier. Thirdly, the key to reliable operation is to ensure that the organic materials are fully encapsulated in a package designed for repetitive flexing, and in this device we employ a multilayer thin film Barix encapsulation technology in collaboration with Vitex systems. Drive electronics and mechanical packaging are provided by L3 Displays.

  • PDF

적층제조된 스테인레스 316L에 대한 초음파나노표면개질에 따른 표면특성 및 부식성에 관한 연구 (Surface Quality and Corrosion of Additively Manufactured STS316L Treated by Ultrasonic Nanocrystal Surface Modification)

  • 김준호;오영택;박한별;이동호;김화정;김의준;심도식
    • 한국기계가공학회지
    • /
    • 제19권8호
    • /
    • pp.94-103
    • /
    • 2020
  • This study investigated the effects of ultrasonic nanocrystal surface modification (UNSM) on the deteriorated surface of AISI SUS316L additively manufactured (AM) using the powder bed fusion (PBF) technique. Specifically, the effects of UNSM conditions on surface topology, hardness, and anti-corrosion were examined. Before UNSM treatment, the stainless steel 316L powder was processed via the PBF machine to prepare a substrate. We observed surface changes due to UNSM treatments in PBF SUS316L substrates and examined the correlation between topology changes, roughness, hardness, and anti-corrosion. After UNSM treatment, the coarse as-built surface was refined, and a regular micro-profile was implemented. Compared to the non-treated PBF sample, the waviness and roughness of the surfaces after UNSM treatment decreased by up to 56.0% and 94.5%, respectively, and decreased further as the interval decreased. The hardness improved by up to 63.0% at a maximum depth of 500 ㎛ from top surface by the UNSM treatment. The results of the corrosion test showed that the corrosion resistance of the UNSM specimens was moderately improved compared to that of the untreated surface. This study confirmed that UNSM is an effective post-processing technique for additively manufactured parts.

Dual Fuel 엔진용 이중관 벨로우즈 제작 공정의 최적화에 관한 연구 II - 용접공정의 최적화 - (A study on the optimization of manufacturing processes of double wall bellows for dual fuel engine II - Optimization of welding process -)

  • 김평수;김종도;송무근
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제40권6호
    • /
    • pp.504-509
    • /
    • 2016
  • 이중관 벨로우즈는 우수한 성형성과 내식성을 고려하여 오스테나이트계 스테인리스강인 STS 316L 소재를 사용하여 2겹으로 내부 및 외부 벨로우즈를 각각 제작한 후 다양한 조건과 용접 방법을 적용하여 이중관 벨로우즈를 제작한다. 하지만 제품의 성형 또는 사용시 균열이나 파단에 가장 취약한 부분이 용접부이기 때문에 제품의 신뢰성을 획득하기 위하여 각각의 용접부에 대한 미세조직을 관찰하여 결함 발생 여부를 측정해야 한다. 본 연구에서는 다양한 용접 공정을 거쳐 제작된 벨로우즈의 용접부를 검사하고 미세조직을 분석하여 최적의 용접 조건을 도출하였다. 또한 용접부의 경도 측정을 통해 모재와 용접부 그리고 열영향부 등 용접영역의 기계적 특성을 평가하였다.