Nd2Fe14B Synthesis: Effect of Excess Neodymium on Phase Purity and Magnetic Property

  • Jadhav, Abhijit P.;Ma, Haoxuan;Kim, Dong Soo;Baek, Youn Kyung;Choi, Chul Jin;Kang, Young Soo
    • Bulletin of the Korean Chemical Society
    • /
    • v.35 no.3
    • /
    • pp.886-890
    • /
    • 2014
  • The properties of magnetic material of Nd-Fe-B are highly affected by various factors such as particle size, magnetic anisotropy, phase purity and crystal structure. Incorporation of excess neodymium was carried out in various percentages so that it will adjust the proportion of neodymium in the host crystal after reduction treatment and finally help to improve magnetic property of a material. The interdiffusion of Nd-Fe and boron was studied for various compositions and their effect on magnetic property was understood with theoretical concepts. The factors such as amount of hard and soft phase in the reduction treated product is also responsible for the possible exchange coupling between hard and soft phase magnets for better magnetic properties.

Effect of rolling parameters on soft-magnetic properties during hot rolling of Fe-based soft magnetic alloy powders (Fe계 연자성 합금 분말의 고온 압연시 자성특성에 미치는 압연인자들의 영향)

  • Kim, H.J.;H.Lee, J.;Lee, S.H.;Park, E.S.;Huh, M.Y.;Bae, J.C.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2009.05a
    • /
    • pp.266-269
    • /
    • 2009
  • Iron-based soft magnetic materials are widely used as cores, such as transformer transformers, motors, and generators. Reducing losses generated from soft magnetic materials of these applications results in improving energy conversion efficiency. Recently, the new P/M soft magnetic material realized an energy loss of 68 W/kg with a drive magnetic flux of 1 T, at a frequency of 1 kHz, rivaling general-purpose electromagnetic steel sheet in the low frequency range of 200 Hz to 1 kHz. In this research, the effect of rolling parameters on soft magnetic properties of Fe-based powder cores was investigated. The Fe-based soft magnetic plates were produced by the hot powder rolling process after both pure Fe and Fe-4%Si powders were canned, evacuated, and sealed in Cu can. The soft magnetic properties such as energy loss and coercive power were measured by B-H curve analyzer. The soft magnetic properties of rolled sheets were measured under conditions of a magnetic flux density of 1 T at a frequency of 200 kHz. It was found that rolling reduction ratio is the most effective parameter on reducing both energy loss and coercivity because of increasing aspect ratio with reduction ratio. By increasing aspect ratio from 1 to 9 through hot rolling of pure Fe powder, a significant loss reduction of one-third that of SPS sample was achieved.

  • PDF

Bulk Amorphous and/or Nanocrystalline Finemet Alloy Prepared by Super-high-pressure Consolidation

  • Lu, Wei;Yanb, Biao
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.788-789
    • /
    • 2006
  • Microstructure and soft magnetic properties of bulk amorphous and/or nanocrystalline $Fe_{73.5}Cu_1Nb_3Si_{13.5}B_9$ alloys prepared by consolidation at 5.5GPa were investigated. The relative density of the bulk sample 1 (from amorphous powders) was 98.5% and the grain sizes were about 10.6nm. While the relative density and grain sizes of bulk sample 2 (from nanocrystalline powders) are 98% and 20.1nm, respectively. Particularly, the bulk samples exhibited a good combined magnetic property: for Sample1, $M_s=125emu/g$ and $H_c=1.5Oe;$ for Sample2, $M_s=129emu/g$ and $H_c=3.3Oe$. The success of synthesizing the nanocrystalline Fe-based bulk alloys will be encouraging for the future development of bulk nanocrystalline soft magnetic alloys.

  • PDF

Microstructure and Soft Magnetic Properties of Fe-6.5 wt.%Si Sheets Fabricated by Powder Hot Rolling

  • Kim, Myung Shin;Kwon, Do Hun;Hong, Won Sik;Kim, Hwi Jun
    • Journal of Powder Materials
    • /
    • v.24 no.2
    • /
    • pp.122-127
    • /
    • 2017
  • Fe-6.5 wt.% Si alloys are widely known to have excellent soft magnetic properties such as high magnetic flux density, low coercivity, and low core loss at high frequency. In this work, disc-shaped preforms are prepared by spark plasma sintering at 1223 K after inert gas atomization of Fe-6.5 wt.% Si powders. Fe-6.5 wt.% Si sheets are rolled by a powder hot-rolling process without cracking, and their microstructure and soft magnetic properties are investigated. The microstructure and magnetic properties (saturation magnetization and core loss) of the hot-rolled Fe-6.5 wt.% Si sheets are examined by scanning electron microscopy, electron backscatter diffraction, vibration sample magnetometry, and AC B-H analysis. The Fe-6.5 wt.% Si sheet rolled at a total reduction ratio of 80% exhibits good soft magnetic properties such as a saturation magnetization of 1.74 T and core loss ($W_{5/1000}$) of 30.7 W/kg. This result is caused by an increase in the electrical resistivity resulting from an increased particle boundary density and the oxide layers between the primary particle boundaries.

Soft Magnetic Property Depending on thickness of Free Layer in CoFe/Cu/CoFe/IrMn Spin Valve Film (CoFe/Cu/CoFe/IrMn 스핀밸브 박막의 자유층 두께 감소에 따른 연자성 자기저항 특성 연구)

  • Choi, Jong-Gu;Go, In-Suk;Gong, Yu-Mi;Kim, Min-Ho;Park, Young-Suk;Hwang, Do-Guwn;Lee, Sang-Suk
    • Journal of the Korean Magnetics Society
    • /
    • v.19 no.2
    • /
    • pp.52-56
    • /
    • 2009
  • Interlayer coupling field, coercivity, magnetoresitance ratio, and magnetic sensitivity depending on the thickness of free CoFe layer for the CoFe/Cu/CoFe/IrMn multilayer are investigated. In case of CoFe layer of $30\;{\AA}$ thickness for the CoFe(t)/Cu($25\;{\AA}$)/CoFe($60\;{\AA}$)/IrMn($80\;{\AA}$) multilayer with ferromagnet/non-magnet/ferromagnet structure induced by IrMn layer, the lowest coercivity and the highest magnetic sensitivity, which is contained soft magnetic property, are observed. On the other side, in case of CoFe layer of $90\;{\AA}$ thickness, there are the highest coercivity and the lowest magnetic sensitivity. The fabricated CoFe($30\;{\AA}$)/Cu($25\;{\AA}$)/CoFe($60\;{\AA}$)]/IrMn($80\;{\AA}$) spin valve device with $2{\times}8{\mu}m^2$ patterning size are measured by two probe method, which is selected the sensing current as the longitudinal direction and the easy axis as the transversal direction. The measuring magntoresistance ratio and magnetic sensitivity of GMR-SV device having the soft magnetic property are 3.0% and 0.3%/Oe, respectively.

Effect of Magnetic Property Modification on Current-Induced Magnetization Switching with Perpendicular Magnetic Layers and Polarization-Enhancement Layers

  • Kim, Woo-Jin;Lee, Kyung-Jin;Lee, Taek-Dong
    • Journal of Magnetics
    • /
    • v.14 no.3
    • /
    • pp.104-107
    • /
    • 2009
  • The effects of the magnetic property variation on current-induced magnetization switching in magnetic tunnel junction with perpendicular magnetic anistoropy (PMA) and the soft magnetic polarization-enhancement layers (PELs) inserted between the layers with PMA and the MgO layer was studied. A micromatnetic model was used to estimate the switching time of the free layer by different applied current densities, with changing saturation magnetization ($M_s$) of the PELs, interlayer exchange coupling between PMA layers and PELs. The switching time could be significantly reduced at low current densities, by increasing $M_s$ of PELs and decreasing interlayer exchange coupling.

Comparison of Soft Magnetic Properties of Permalloy and Conetic Thin Films (퍼멀로이와 코네틱 박막의 연자성 특성 비교)

  • Choi, Jong-Gu;Hwang, Do-Guwn;Lee, Sang-Suk;Rhee, Jang-Roh
    • Journal of the Korean Magnetics Society
    • /
    • v.19 no.4
    • /
    • pp.142-146
    • /
    • 2009
  • The soft magnetic property for the Corning glass/Ta(5 nm)/[Conetic, Permalloy)/Ta(3 nm) prepared by the ion beam deposition sputtering was investigated. The coercivity and saturation magnetic field of conetic (NiFeCuMo) and permalloy (NiFe) layer with easy and hard direction along to the applying magnetic field during deposition was compared with each other. The surface resistance of conetic film with a thickness of 10 nm was 2 times lower than one of permalloy film. The coercivity and the magnetic susceptibility of conetic film decreased and increased 3 times to one of permalloy film, respectively. These results suggest that a highly sensitive GMR-SV or MTJ using conetic film can be possible to develop the bio-device.