아몰퍼스자성박막의 특성에 미치는 등방성 스트레인의 영향 (Effect of Isotropic Strain on Properties of Amorphous Magnetic films)

  • 신광호;김흥근;김영학;사공건
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 하계학술대회 논문집
    • /
    • pp.478-480
    • /
    • 2001
  • Fe-base amorphous films exhibit large saturation magnetostriction and soft magnetic Properties, which make them suitable for strain sensor applications. Most important material properties for the performance of these elements are the superior soft magnetic properties, such as high permeability and small coercive force, as well as magnetoelastic properties. It is well known that the strain generated in film deposition and/or post-heat treatment processes is one of important material properties, which effects on the soft magnetic properties of the film via magnetoelastic coupling. In this study, the effect of an isotropic strain in plane of magnetic films have been performed experimently. Amorphous films with the composition of (F $e_{90}$ $Co_{10}$)$_{78}$S $i_{l2}$ $B_{10}$ were employed in this study. The film with 5${\mu}{\textrm}{m}$ thick was deposed onto the polyimide substrate with 50${\mu}{\textrm}{m}$ thick by virtue of RF sputtering. The film was subject to post annealing with a static magnetic field with 500Oe magnetic field intensity at 35$0^{\circ}C$ for 1 hour. The polyimide substrate with the film was bonded with an adhesive on PZT piezoelectric substrate with 600${\mu}{\textrm}{m}$ thick in applying voltage of 500V. The change in MH loops of films due to the isotropic strain was measured by using VSM. The coercive force was evaluated from MH loops. It has shown in the results that M-H loops of films are subject to change considerably with a dc voltage, resulting of the magnetization rotation from normal to plane direction as the applied voltage is changed from 500V to 250V.50V.V.

  • PDF

템퍼링 및 자장열처리가 KM35F 합금의 연자성 특성에 미치는 영향 (Influence of the tempering and magnetic annealing on soft magnetic properties for the KM35F alloy)

  • 박병기;전용식;김동수
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2008년도 추계학술대회A
    • /
    • pp.1240-1243
    • /
    • 2008
  • The tempering and magnetic annealing are used to improve the soft magnetic properties such as initial permeability coercivity and core loss of the KM35F alloy. The first heat treatmentis performed at the temperature less than the curie temperature of the KM35F alloy to remove the thermal stress for few hours in nitrogen atmosphere. The second stage heat treatment is performed the magnetic annealing at $500{\sim}800^{\circ}C$ for few hours in nitrogen atmosphere, and then quenching to room temperature in absence of oxygen. Finally, magnetic properties of the thermally treated KM35F alloy are investigated for application as a soft magnetic material of the ISO solenoid valve core and plunger.

  • PDF

실란 및 분산제가 Epoxy와 연자성 금속 파우더 복합체의 Packing에 미치는 영향 (The Effect of Silane and Dispersant on the Packing in the Composite of Epoxy and Soft Magnetic Metal Powder)

  • 이창현;신효순;여동훈;남산
    • 한국전기전자재료학회논문지
    • /
    • 제30권12호
    • /
    • pp.751-756
    • /
    • 2017
  • A molding-type power inductor is an inductor that uses a hybrid material that is prepared by mixing a ferrite metal powder coated with an insulating layer and an epoxy resin, which is injected into a coil-embedded mold and heated and cured. The fabrication of molding-type inductors requires various techniques such as for coil formation and insertion, improving the magnetic properties of soft magnetic metal powder, coating an insulating film on the magnetic powder surface, and increasing the packing density by well dispersing the powder in the epoxy resin. Among these aspects, researches on additives that can disperse the metal soft magnetic powder having the greatest performance in the epoxy resin with high charge have not been reported yet. In this study, we investigated the effect of silanes, KBM-303 and KBM-403, and a commercial dispersant on the dispersion of metal soft magnetic powders in epoxy resin. The sedimentation height and viscosity were measured, and it was confirmed that the silane KBM-303 was suitable for dispersion. For this silane, the packing density was as high as about 72.49%. Moreover, when 1.2 wt% of dispersant BYK-103 was added, the packing density was about 80.5%.

손실 패턴에 따른 고속 스위치드 릴럭턴스 전동기의 SMC 분말을 이용한 효율 개선 (Strategic Utilization of Soft Magnetic Composite in a High-Speed Switched Reluctance Machine Depending on a Loss Pattern)

  • 이치우
    • 전기학회논문지
    • /
    • 제66권2호
    • /
    • pp.323-327
    • /
    • 2017
  • Soft magnetic composite (SMC) material has recently received a significant attention in the area of high-speed machines because of its unique properties such as good design flexibility and low eddy current loss. However, SMC's electromagnetic property is poor compared to silicon steel in terms of saturation, relative permeability, and hysteresis loss. This paper presents a technique for utilization of SMC in two strategic designs of a switched reluctance machine (SRM) depending on a loss pattern. To investigate the effect of SMC's merits and demerits, the stator material is changed from laminated steel to SMC.

FeCo의 결정성 및 조성 제어를 통한 자기 특성 향상 (Enhanced magnetic properties of FeCo alloys by engineering crystallinity and composition)

  • 김단비;김지원;엄누시아;박성흠;임재홍
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2018년도 춘계학술대회 논문집
    • /
    • pp.32.1-32.1
    • /
    • 2018
  • Novel soft magnetic materials can be achieved by altering material properties such as morphology, composition, crystallinity, and grain size of soft magnetic alloys. Especially, magnetic properties (i.e., saturation magnetization, coarcivity) of soft magnetics are significantly affected by grain boundaries which act as a control of magnetic domain wall movement. Thus, we herein develop a two-step electroless plating method to control morphology and grain size of FeCo films for excellent magnetic properties. Accordingly, the chemical composition to control the degree of polarization of FeCo alloys was altered by electroless deposition parameters; for example, electrolyte concentration and temperature. The grain size and crystallinity of FeCo alloys was dramatically affected by the reaction temperature because the grain growth mechanism dominantly occurs at $90^{\circ}C$ where as the neucleation only happens at $50^{\circ}C$. By simply controlling the temperature, the micron-sized FeCo grains embedded FeCo film was synthesized where the large grains allow high magnetization originated from larger magnetic domain with low corecivity and the nano-sized grains allow excellent soft magnetic properties due to the magnetic correlation length.

  • PDF

$Fe_{80}B_{12}Si_8$ 비정질 합금의 자구 및 자왜와 자기적 성질에 미치는 Mo 첨가와 자장 열처리 효과 (The effect of Mo addion and Magnetic field annealing on the magnetic properties, Magnetostriction and Domain structures of $Fe_{80}B_{12}Si_8$ amorphous alloy.)

  • 고창진;강계명;송진태
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1989년도 춘계학술대회 논문집
    • /
    • pp.49-51
    • /
    • 1989
  • The effect of Mo elenent and annealing condition on the magnetic properties were investigated in Fe$_{80}$B$_{12}$Si$_{8}$ amorphous alloy. With increasing Mo contents, soft magnetic properties were improved by decreasing coercive force and increasing maximum permeability. These improvements were attributed to the decreasing of magnetostriction by Mo addition. The annealing treatment also improved the soft magnetic properties of (Fe$_{1-x}$ Mo$_{x}$)$_{80}$ B$_{12}$ Si$_{8}$ amorphous alloys. It could be thought that these improvements were ascribed to the relaxation of internal stress.nal stress.ess.

  • PDF

Mn-Zn-Fe-O 금속타깃을 이용한 수직자기기록디스크의 하지연자성층용 Mn-Zn ferrite 박막제작 (Preparation for Mn-Zn Ferrite Soft Magnetic Underlayer Perpendicular Magnetic Recording Disk using Mn-Zn-Fe-O Metal Target)

  • 공석현;김경환
    • 한국전기전자재료학회논문지
    • /
    • 제19권9호
    • /
    • pp.883-887
    • /
    • 2006
  • In order to attain high-rate deposition of Mn-Zn ferrite thin film for soft magnetic underlayer in perpendicular magnetic recording media, a reactive sputtering using powder-metal targets under the mixture gas of Ar and $O_{2}$ was performed. It was succeeded that Mn-Zn ferrite films with (111) crystal orientation were deposited on Pt(111) underlayer without any annealing process. The film revealed 3.4 kG of 4 ${\pi}Ms$, 70 Oe of coercivity. The deposition rate of the new method was 16 times as high as that of the conventional method using ferrite target.

$Fe_{87}Zr_{7}B_{5}Ag_{1}$(at%) 비정질 합금의 연자기 특성 (The Soft Magnetic Properties of $Fe_{87}Zr_{7}B_{5}Ag_{1}$ Amorphous Alloy)

  • 김현식;오영우;김병걸;정순종;김기욱
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1994년도 춘계학술대회 논문집
    • /
    • pp.120-122
    • /
    • 1994
  • We examined the magnetic properties as a function of annealing temperature of the as-quenched $Fe_{87}Zr_{7}B_{5}Ag_{1}$ amorphous alloy. The values of $H_{c}$=30m0e, $B_{a}$=0.44T and ${\mu}$i=146000 at $300^{\circ}C$ annealing treatment are obtained. The excel lent soft magnetic properties seem to result from the annihilation of quenching-Induced internal stress by the heat treatment and the change of microstructure due to the different relaxation behavior owing to adding insoluble element such as Ag. Therefore, the $Fe_{87}Zr_{7}B_{5}Ag_{1}$ amorphous alloy is quite promising for practical use as a core material in various transformers of high transformers of high frequency.

  • PDF

Bulk Amorphous and/or Nanocrystalline Finemet Alloy Prepared by Super-high-pressure Consolidation

  • Lu, Wei;Yanb, Biao
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.788-789
    • /
    • 2006
  • Microstructure and soft magnetic properties of bulk amorphous and/or nanocrystalline $Fe_{73.5}Cu_1Nb_3Si_{13.5}B_9$ alloys prepared by consolidation at 5.5GPa were investigated. The relative density of the bulk sample 1 (from amorphous powders) was 98.5% and the grain sizes were about 10.6nm. While the relative density and grain sizes of bulk sample 2 (from nanocrystalline powders) are 98% and 20.1nm, respectively. Particularly, the bulk samples exhibited a good combined magnetic property: for Sample1, $M_s=125emu/g$ and $H_c=1.5Oe;$ for Sample2, $M_s=129emu/g$ and $H_c=3.3Oe$. The success of synthesizing the nanocrystalline Fe-based bulk alloys will be encouraging for the future development of bulk nanocrystalline soft magnetic alloys.

  • PDF

나노 결정립 Fe-Al-O 산화막의 미세구조 변화에 따른 연자기적 특성 분석 (Soft Magnetic Property Analysis of Nanocrystalline Fe-Al-O Film with the Change of Microstructure)

  • 이영우;박범찬;김종오;문지현;최용대
    • 한국자기학회지
    • /
    • 제14권2호
    • /
    • pp.59-64
    • /
    • 2004
  • 나노 결정립 구조를 갖는 Fe-Al-O 연자성 산화막을 이온빔 에칭법으로 에칭하면서 연자기적 특성의 변화를 조사하였다. 두께가 감소할수록 보자력과 각형비가 증가하고 AFM 으로 조사한 표면굴곡도 증가하는 것으로 보아 결정립의 크기가 증가하는 것으로 판단된다. 이러한 현상은 비정질을 열처리한 나노결정립 연자성 재료와 다르게 성막하는 과정의 온도 상승에 의한 결정성장이 원인으로 판단된다. 따라서 우수한 연자성 박막을 제조하기 위해서는 두께 및 성막시간 등 최적 제조조건을 찾아야 한다. 마그네트론 스퍼터링법으로 제조된 Fe-Al-O 산화막의 경우 900 nm 이상에서 보자력이 1 Oe 이하인 연자성 박막을 얻을 수 있었다.