Single Lap Riveted Joint의 베어링 거동 연구 (Study on Bearing Response of Single Lap Riveted Joint)

  • 허광수;윤성호;정종철;이상진;김정석
    • 한국철도학회:학술대회논문집
    • /
    • 한국철도학회 2005년도 춘계학술대회 논문집
    • /
    • pp.326-331
    • /
    • 2005
  • In this study, bearing response in single lap riveted joint is investigated by menas of single lap shear specimens with different types of adherend and fastener. Single lap shear specimen consists of adherend of SUS403 and carbon fabric/epoxy composite. Rivet of Avdel 2691 with 9.6mm diameter is used. Two types of fastener in single lap riveted joint are considered. One is a single lap shear specimen with single fastener, and the other is a single lap shear specimen with double fasteners. Especially, in case of single lap shear specimen with single fastener, the width of the specimen is varied as 2D, 3D, 4D, 6D at a fixed edge distance of 3D. Also the edge distance of the specimen is varied as 1.0D, 1.5D, 2.0D, 2.5D, 3.0D at a fixed width of 4D. In case of single lap shear specimen with double fasteners, two types of specimen are considered. One is a specimen with the width of 6D and edge distance of 3D. The other is a specimen with the width of 4D and edge distance of 2D. Here D designates the hole diameter for riveted joint.

  • PDF

단면 겹치기 이음 시험에 의한 경량구조물용 접착 이음강도의 평가 (Strength Evaluation of Adhesive Bonded Joint for Light Weight Structure by Single-Lab Joint Test)

  • 이강용;김준범;최홍섭;우형표
    • 한국자동차공학회논문집
    • /
    • 제5권2호
    • /
    • pp.87-93
    • /
    • 1997
  • The bonding strength evaluation of light weight materials for electrical vehicle applications has been performed through single lap joint tests in which the design parameters such as fillet, joint style, adherend, bonding overlap length,bonding thickness, and environmental condition(soaking time in $25^{\circ}C$ water) are considered. It is experimentally oberved that lap shear strength of joint increases for higher fillet height, longer overlap length, and thinner bonding layer thickness. Al-Al adherend combination shows much higher lap shear strength than AL-FRP and FRP-FRP adherend combinations. Riveting at adhesive bonded joint of AL-AL adherend combination makes lap shear strength decrease. Effect of soaking time on lap shear strength is negligible.

  • PDF

튜브형 단면겹치기 접착조인트의 비선형 반복연산해에 관한 연구 (Nonlinear Iterative Solution for Adhesively Bonded Tubular Single Lap Joints with Nonlinear Shear Properties)

  • 이수정;이대길
    • 대한기계학회논문집
    • /
    • 제19권7호
    • /
    • pp.1651-1656
    • /
    • 1995
  • The adhesively bonded tubular single lap joint shows large nonlinear behavior in the loaddisplacement relation, because structural adhesives for the joint are usually rubber toughened, which endows adhesives with nonlinear shear properties. since the majority of load transfer of the adhesively bonded tubular single lap joint is accomplished by the nonlinear behavior of the adhesive, its torque transmission capability should be calculated incorporating nonlinear shear properties. However, both the analytic and numerical analyses become complicated if the nonlinear shear properties of the adhesive are included during the calculation of torque transmission capabilities. In this paper, in order to obtain the torque transmission capabilities easily, an iterative solution which includes the nonlinear shear properties of the adhesive was derived using the analytic solution with the linear shear properties of the adhesive. Since the iterative solution can be obtained very fast due to its simplicity, it has been found that it can be used in the design of the adhesively bonded tubular single lap joint.

AI합금 단순겹치기 접착이음의 인장-전단강도 평가 (The Evaluation of Tensile-shear Strength on the Al-Alloy Single-lap Adhesive Joints)

  • 오승규;유영철;정의섭;이원
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1997년도 춘계학술대회 논문집
    • /
    • pp.567-571
    • /
    • 1997
  • Recently, automobile industry has led to increasing use of aluminum alloy for weight reduction. Automobile made of aluminum alloy can be given lighter, stronger and a harder surface by anodizing than one made of steel-alloy. In this paper, we investigate the influence of lap length, adherend thickness and adhesive thickness on adhesive strength of single-lap adhesive joints by conducting tensile-shear tests. Single-lap adhesive joints of aluminum was calculated using joint factor by using adhesive length, adherend thickness of specimen.

  • PDF

단일겹치기이음시험을 이용한 합금화용융아연코팅강판의 코팅층 접합강도 평가 (Estimations of the Adhesion Strength of Galvannealed Coatings on Coated Sheet Using Single Lap-Shear Test)

  • 이정민;이찬주;고대철;이선봉;김병민
    • 대한기계학회논문집A
    • /
    • 제33권6호
    • /
    • pp.560-567
    • /
    • 2009
  • This paper was designed to estimate the adhesion strength of galvannealed coatings on steel sheets. The adhesion strength were evaluated using single lap - shear tests where the lap joint was bonded by structural adhesive. Tests were performed for overlap length of 5mm, 10mm and 15 mm and three directions (0, 45, 90) of steel sheets used as the adherend of the overlap joint. After the tests, FE simulations of the single lap-shear test were also carried out to observe the stress distribution in the interface between the adhesive and the coated sheet. The results showed that the joint failure loads obtained from the tensile tests of bonded single lap-joints were the same, regardless of overlap lengths and directions of steel sheets. Also, the failure of galvannealed coatings greatly depended on shear stress distribution in the interface and the value was about 30MPa.

접착제로 접합된 복합재료 구동축의 토크 전달특성에 관한 연구 (A Study on the Torque Transmission Characteristics of Adhesively Bonded Composite Drive Shafts)

  • 김원태;김기수;이대길
    • 대한기계학회논문집
    • /
    • 제17권8호
    • /
    • pp.1980-2000
    • /
    • 1993
  • The stresses and torque transmission capabilities of adhesively bonded circular, hexagonal and elliptical lap joints were analyzed by the finite element and compared with the experimental results. The adherends of the joints were composed of carbon fiber/epoxy composite shafts and steel shafts. In calculating the torque transmission capabilities, the linear laminate properties of the composite material and the nonlinear shear properties of the adhesive were used. Using this method, the torque transmission capabilities of adhesively bonded lap joints could be obtained within 10% error compared to the experimental results except some single lap joints. The experiments revealed that the hexagonal joint had the best torque transmission capability from the single lap joints and the double lap joint had better torque transmission than the single lap joint.

사용환경온도에 따른 접착이음의 인장전단강도 변화 (Variation of fracture strength of adhesive joint according to the operating temperature)

  • 김재영;이찬주;이상곤;박근환;정병훈;;김병민
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2008년도 춘계학술대회 논문집
    • /
    • pp.517-520
    • /
    • 2008
  • Recently, use of adhesive bonding technology is increased to achieve the multi-material design for lightweight structure in automobile industry. In this paper, the fracture strength of adhesive has been studied with the single lap shear test conducted at different temperatures. The joint specimens are made from Al 5052 and SPRC 440 bonded with structural epoxy adhesive. The operating temperature has been considered up to $150[^{\circ}C]$ and the single lap shear test has been conducted with 5mm/min tensile rate. Fracture strength of adhesive bonded joint has been decreased with increase of operating temperature. The fracture strength at the $100[^{\circ}C]$ was shown about half of that at room temperature.

  • PDF

End mismatch를 갖는 접착이음의 강도 평가 (Stress Analysis Crack of Double-lap Joint with an End Mismatch)

  • 현철승;허성필;양원호;류명해
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2001년도 춘계학술대회논문집A
    • /
    • pp.465-470
    • /
    • 2001
  • The adhesively-bonded joints considered in this investigation include single-lap joint and double-lap joint. For an adhesively bonded double-lap joint, end mismatch between the two cuter adherends(upper, lower) can not removed completely although it can be controlled within a manufacturing tolerance. This paper shows that the end mismatch introduces local bending and end mismatch affects the shear and peel stresses in the adhesive. The double-lap joint with an end mismatch is affected of adhesive thickness, material properties of adhesive and adherend etc. Also, we concluded that there are critical value of an end mismatch to provoke the interface fracture.

  • PDF

접착제 접합 이음부 접합강도 평가에 대한 실험적 연구 (Experimental Study on Evaluation of Bonding Strength of Adhesively Bonded Joints by Adhesive)

  • 강기엽;이제명
    • Journal of Welding and Joining
    • /
    • 제30권6호
    • /
    • pp.62-67
    • /
    • 2012
  • In this study, the bonding strengths of adhesively bonded joints are experimentally investigated. A series of lap-shear tests are conducted using single lap type adhesive joints. In order to analyse the joint fabrication factors that affected the bonding strength, the parametric tests are conducted with various thickness of adhesive, surface roughness and fillet of adhesive. In addition, for the comparative study with the welded joint, lap-shear tests using specimens with 2 welded sides and 4 welded sides are also carried out. The quantitative results of the strength analysis are summarized, and some proposals are made on setting up testing standards for adhesively bonded joints.

단일겹침 접착제 접합부의 응력분포와 강도평가 (Stress Distribution and Strength Evaluation of Adhesive Bonded Single-lap Joints)

  • 이중삼;임재규;김연직
    • Journal of Welding and Joining
    • /
    • 제19권3호
    • /
    • pp.342-347
    • /
    • 2001
  • Recently, adhesive-bonding technique is wifely used in manufacturing structures. Stress and strain analysis of joints are essential to design adhesive-bonded joints structure. The single-lap adhesive joint is the design dominating the range of adhesive joints. In this study, single-lap specimens with different joint dimensions were used for the tensile-shear test and finite element calculation in of order to investigate the effect of overlap length and adhesive-bonding thickness on adhesive strength and stress distribution of the joints. Consequently, it was found that overlap lap size and thickness can be important parameters of structure joints using adhesive bonding, which is effected on adhesive strength.