• 제목/요약/키워드: simulated body fluid

Search Result 123, Processing Time 0.026 seconds

Effects of Surface Modification on Biomimetic Deposition of Apatite in Zr-1Nb (표면변환이 Zr-1Nb합금의 아파타이트 석출에 미치는 효과)

  • Kim, Tae Ho;Cho, Kyu Jin;Hong, Sun Ig
    • Korean Journal of Metals and Materials
    • /
    • v.48 no.6
    • /
    • pp.575-580
    • /
    • 2010
  • Effects of the surface modification on the deposition behaviors of apatite crystals in Zr-1Nb plates were studied. Zr-1Nb alloy plates were polished with abrasive papers to have different roughness and some of them were treated in NaOH or coated with collagen before deposition of apatites in the simulated body fluid (SBF). The weight gain due to the deposition of apatite crystals increased as the surface roughness increased in Zr-1Nb. The size of granular apatite crystals were found to be smaller in Zr-1Nb roughened by $162{\mu}m$ abrasive paper than in Zr-1Nb roughened by $8.4{\mu}m$ paper, suggesting the nucleation rate increased with increase of surface roughness. After, 10 days immersion in a SBF, NaOH-treated Zr-1Nb was completely coated with apatite with the deposited apatite weight comparable to that in Ti-6Al-4V. The deposition rate of Zr-1Nb was not appreciably influenced by NaOH treatment unlike the significant influence of NaOHtreatment on the deposition rate of apatite in Ti-6Al-4V. One significant observation in this study is an appreciable increase of the apatite deposition rate after collagen coating both on Zr-1Nb and Ti-6Al-4V plate, which may be caused by the interaction between collagen and $Ca^{+2}$ ions.

Allergenicity and toxicity evaluation of the PAT protein expressed in herbicide-tolerant genetically modified Zoysia japonica (제초제저항성 GM 잔디에서 발현된 PAT 단백질의 알레르겐 유발 가능성 및 독성 평가)

  • Jeong, Hye-Rin;Sun, Hyeon-Jin;Kang, Ji-Nam;Kang, Hong-Gyu;Lee, Hyo-Yeon
    • Journal of Plant Biotechnology
    • /
    • v.47 no.4
    • /
    • pp.316-323
    • /
    • 2020
  • This study aimed to evaluate the potential allergenicity and oral toxicity of the phosphinothricin acetyltransferase (PAT) protein expressed in Zoysia japonica, a herbicide-tolerant genetically modified (GM) zoysiagrass. In silico analysis of PAT showed no similarities with any known allergenic or toxic proteins, with <35% amino acid sequence homology with known allergens across a length of 80 amino acids and no continuous eight amino acid identity with known allergens. The PAT protein expressed in Z. japonica degraded very rapidly in the simulated gastric fluid in the presence of pepsin, and, no glycosylation of PAT was observed. The oral toxicity test revealed no mortality or toxic effect in mice following PAT administration at 4,000 mg/kg body weight. Our findings indicate that the PAT protein expressed in Zoysia japonica does not exhibit allergenic or toxic properties.

Enhancement of bioactivity and osseointegration in Ti-6Al-4V orthodontic mini-screws coated with calcium phosphate on the TiO2 nanotube layer

  • Byeon, Seon-Mi;Kim, Hye-Ji;Lee, Min-Ho;Bae, Tae-Sung
    • The korean journal of orthodontics
    • /
    • v.52 no.6
    • /
    • pp.412-419
    • /
    • 2022
  • Objective: This study evaluated the effect of cyclic pre-calcification treatment on the improvement of bioactivity and osseointegration of Ti-6Al-4V mini-screws. Methods: The experimental groups were: an untreated group (UT), an anodized and heat-treated group (AH), and an anodized treatment followed by cyclic pre-calcification treatment group (ASPH). A bioactive material with calcium phosphate was coated on the mini-screws, and its effects on bioactivity and osseointegration were evaluated in in vitro and in vivo tests of following implantation in the rat tibia. Results: As a result of immersing the ASPH group in simulated body fluid for 2 days, protrusions appearing in the initial stage of hydroxyapatite precipitation were observed. On the 3rd day, the protrusions became denser, other protrusions overlapped and grew on it, and the calcium and phosphorus concentrations increased. The removal torque values increased significantly in the following order: UT group (2.08 ± 0.67 N·cm), AH group (4.10 ± 0.72 N·cm), and ASPH group (6.58 ± 0.66 N·cm) with the ASPH group showing the highest value (p < 0.05). In the ASPH group, new bone was observed that was connected to the threads, and it was confirmed that a bony bridge connected to the adjacent bone was formed. Conclusions: In conclusion, it was found that the surface treatment method used in the ASPH group improved the bioactivity and osseointegration of Ti-6Al-4V orthodontic mini-screws.

SURFACE CHARACTERISTICS AND BIOACTIVITY OF ANODICALLY OXIDIZED TITANIUM SURFACES (양극산화에 의한 티타늄 산화막의 표면 특성 및 생체 활성에 관한 연구)

  • Lee, Sang-Han;Cho, In-Ho
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.45 no.1
    • /
    • pp.85-97
    • /
    • 2007
  • Statement of problem: Recently, anodic oxidation of cp-titanium is a popular method for treatment of titanium implant surfaces. It is a relatively easy process, and the thickness, structure, composition, and the microstructure of the oxide layer can be variably modified. Moreover the biological properties of the oxide layer can be controlled. Purpose: In this study, the roughness, microstructure, crystal structure of the variously treated groups (current, voltage, frequency, electrolyte, thermal treatment) were evaluated. And the specimens were soaked in simulated body fluid (SBF) to evaluate the effects of the surface characteristics and the oxide layers on the bioactivity of the specimens which were directly related to bone formation and integration. Materials and methods: Surface treatments consisted of either anodization or anodization followed thermal treatment. Specimens were divided into seven groups, depending on their anodizing treatment conditions: constant current mode (350V for group 2), constant voltage mode (155V for group 3), 60 Hz pulse series (230V for group 4, 300V for group 5), and 1000 Hz pulse series (400V for group 6, 460V for group 7). Non-treated native surfaces were used as controls (group 1). In addition, for the purpose of evaluating the effects of thermal treatment, each group was heat treated by elevating the temperature by $5^{\circ}C$ per minute until $600^{\circ}C$ for 1 hour, and then bench cured. Using scanning electron microscope (SEM), porous oxide layers were observed on treated surfaces. The crystal structures and phases of titania were identified by thin-film x-ray diffractmeter (TF-XRD). Atomic force microscope (AFM) was used for roughness measurement (Sa, Sq). To evaluate bioactivity of modified titanium surfaces, each group was soaked in SBF for 168 hours (1 week), and then changed surface characteristics were analyzed by SEM and TF-XRD. Results: On basis of our findings, we concluded the following results. 1. Most groups showed morphologically porous structures. Except group 2, all groups showed fine to coarse convex structures, and the groups with superior quantity of oxide products showed superior morphology. 2. As a result of combined anodization and thermal treatment, there were no effects on composition of crystalline structure. But, heat treatment influenced the quantity of formation of the oxide products (rutile / anatase). 3. Roughness decreased in the order of groups 7,5,2,3,6,4,1 and there was statistical difference between group 7 and the others (p<0.05), but group 7 did not show any bioactivity within a week. 4. In groups that implanted ions (Ca/P) on the oxide layer through current and voltage control, showed superior morphology, and oxide products, but did not express any bioactivity within a week. 5. In group 3, the oxide layer was uniformly organized with rutile, with almost no titanium peak. And there were abnormally more [101] orientations of rutile crystalline structure, and bonelike apatite formation could be seen around these crystalline structures. Conclusion: As a result of control of various factors in anodization (current, voltage, frequency, electrolytes, thermal treatment), the surface morphology, micro-porosity, the 2nd phase formation, crystalline structure, thickness of the oxide layer could be modified. And even more, the bioactivity of the specimens in vitro could be induced. Thus anodic oxidation can be considered as an excellent surface treatment method that will able to not only control the physical properties but enhance the biological characteristics of the oxide layer. Furthermore, it is recommended in near future animal research to prove these results.

A Comparative Study on the Effect of Tamping Materials on the Impact Efficiency at Blasting Work (발파작업 시 충전매질에 따른 발파효과 비교 연구)

  • Bae, Sang-Soo;Han, Woo-Jin;Jang, Seung-Yup;Bang, Myung-Seok
    • Journal of the Korean Geosynthetics Society
    • /
    • v.21 no.2
    • /
    • pp.57-65
    • /
    • 2022
  • This study simulated the shock wave propagation through the tamping material between explosives and hole wall at blasting works and verified the effect of tamping materials. The Arbitrary Lagrangian-Eulerian(ALE) method was selected to model the mixture of solid (Lagrangian) and fluid (Eulerian). The time series analysis was carried out during blasting process time. Explosives and tamping materials (air or water) were modeled with finite element mesh and the hole wall was assumed as a rigid body that can determine the propagation velocity and shock force hitting the hole wall from starting point (explosives). The numerical simulation results show that the propagation velocity and shock force in case of water were larger than those in case of air. In addition, the real site at blasting work was modeled and simulated. The rock was treated as elasto-plastic material. The results demonstrate that the instantaneous shock force was larger and the demolished block size was smaller in water than in air. On the contrary, the impact in the back side of explosives hole was smaller in water, because considerable amount of shock energy was used to demolish the rock, but the propagation of compression through solid becomes smaller due to the damping effect by rock demolition. Therefore, It can be proven that the water as the tamping media was more profitable than air.

Evaluate the Suitability of MC3T3 Cells to Antibacterial Ag-30CaO·70SiO2 Gel (항균성 Ag-30CaO·70SiO2 Gel의 MC3T3 세포적합성에 관한 연구)

  • Yoon, Geum-Jae;Ryu, Jae-Kyung;An, Eung-Mo;Kim, Yun-Jong;Kim, Taik-Nam;Noh, In-Sup;Cho, Sung-Beck
    • Korean Journal of Materials Research
    • /
    • v.24 no.12
    • /
    • pp.671-676
    • /
    • 2014
  • It is known that bones get damaged by accidents and aging. Since the discovery of Bioglass, various kinds of ceramics have been also found to bond to living bone; some of these ceramics are already being clinically used as bone-repairing materials. In the present study, antibacterial calcium silicate gel ($Ag-30CaO{\cdot}70SiO_2$ gel) was prepared by sol-gel method in order to control the microstructure, which is related to the dissolution rate and induction period of apatite formation in body environment. In addition, biological $Ag-30CaO{\cdot}70SiO_2$ is tested. This was done to impart antimicrobial activity to the $30CaO{\cdot}70SiO_2$. Ag ion was added during sol-gel synthesis to replace the $H_2O$ added during the making of the $30CaO{\cdot}70SiO_2$ gel, which has silver solutions of various concentration. After the sol-gel process, 1N-$HNO_3$ solution was used to wash the gel when synthesizing the gel, in order to maintain the porous structure and remove PEG, water soluble polymers. Then, the apatite forming ability of the sol-gel derived CaO-$SiO_2$ gels was investigated using simulated body fluid (SBF), which had almost the same ion concentration as that of human blood plasma. The gels were analyzed by FT-IR spectroscopy, SEM observation, XRD, and fluorescent microscopy. The apatite was successfully created even after washing the gel; apatite is present in an amorphous state, and was found to affect the concentration of the Ag ion in cells in MC3T3 live & dead assay results. From these results, it is suggested that a good material that can be used to repair defects of nature bone is $Ag-30CaO{\cdot}70SiO_2$ gel.

The effect of calcium metaphosphate bone graft materials on bone regeneration (생분해성 Calcium Metaphosphate골이식재의 골조직재생효과에 관한 연구)

  • Chae, Han-seung;Lee, Yong-Moo;Yang, Seung-Min;Chun, Sung-Soo;Kim, Suk-Young;Ku, Young;Choung, Chong-Pyoung;Han, Soo-Boo;Choi, Sang-Mook;Rhyu, In-Chul
    • Journal of Periodontal and Implant Science
    • /
    • v.33 no.1
    • /
    • pp.13-26
    • /
    • 2003
  • Periodontal regeneration therapy with bone-substituting materials has gained favorable clinical efficacy by enhancing osseous regeneration in periodontal bony defect. As bone-substituting materials, bone powder, calcium phosphate ceramic, modified forms of hydroxyapatite, and hard tissue replacement polymer have demonstrated their periodontal bony regenerative potency. Bone-substituting materials should fulfill several requirements such as biocompatibility, osteogenecity, malleability, biodegradability. The purpose of this study was to investigate biocompatibility, osteo-conduction capacity and biodegradability of $Na_2O$, $K_2O$ added calcium metaphosphate(CMP). Beta CMP was obtained by thermal treatment of anhydrous $Ca_2(H_2PO_4)_2$. $Na_2O$ and $K_2O$ were added to CMP. The change of weight of pure CMP, $Na_2O$-CMP, and $K_2O$-CMP in Tris-buffer solution and simulated body fluid for 30 days was measured. Twenty four Newzealand white rabbits were used in negative control, positive control(Bio-Oss), pure CMP group, 5% $Na_2$-CMP group, 10% $Na_2O$-CMP goup, and 5% $K_2O$-CMP group. In each group, graft materials were placed in right and left parietal bone defects(diameter 10mm) of rabbit. The animals were sacrificed at 3 months and 6 months after implantation of the graft materials. Degree of biodegradability of $K_2O$ or $Na_2O$ added CMP was greater than that of pure CMP in experimental condition. All experimental sites were healed with no clinical evidence of inflammatory response to all CMP implants. Histologic observations revealed that all CMP grafts were very biocompatible and osseous conductive, and that in $K_2O$-CMP or $Na_2O$-CMP implanted sites, there was biodegradable pattern, and that in site of new bone formation, there was no significant difference between all CMP group and DPBB(Bio-Oss) group. From this result, it was suggested that all experimental CMP group graft materials were able to use as an available bone substitution.

Development and Evaluation of Natural Hydroxyapatite Ceramics Produced by the Heat Treatment of Pig Bones

  • Lim, Ki-Taek;Kim, Jin-Woo;Kim, Jangho;Chung, Jong Hoon
    • Journal of Biosystems Engineering
    • /
    • v.39 no.3
    • /
    • pp.227-234
    • /
    • 2014
  • Purpose: The aim of this research was to develop and evaluate natural hydroxyapatite (HA) ceramics produced from the heat treatment of pig bones. Methods: The properties of natural HA ceramics produced from pig bones were assessed in two parts. Firstly, the raw materials were characterized. A temperature of $1,200^{\circ}C$ was chosen as the calcination temperature. Fine bone powders (BPs) were produced via calcinations and a milling process. Sintered BPs were then characterized using field emission scanning electron microscopy (FE-SEM), X-ray diffraction (XRD), X-ray fluorescence spectroscopy (XRF), energy dispersive X-ray spectroscopy (EDX), Fourier transform infrared (FTIR) spectroscopy, and a 2-year in vitro degradability test. Secondly, an indirect cytotoxicity test was conducted on human osteoblast-like cells, MG63, treated with the BPs. Results: The average particle size of the BPs was $20{\pm}5{\mu}m$. FE-SEM showed a non-uniform distribution of the particle size. The phase obtained from XRD analysis confirmed the structure of HA. Elemental analysis using XRF detected phosphorus (P) and calcium (Ca) with the Ca/P ratio of 1.6. Functional groups examined by FTIR detected phosphate ($PO{_4}^{3-}$), hydroxyl ($OH^-$), and carbonate ($CO{_3}^{2-}$). The EDX, XRF, and FTIR analysis of BPs indicated the absence of organic compounds, which were completely removed after annealing at $1,200^{\circ}C$. The BPs were mostly stable in a simulated body fluid (SBF) solution for 2 years. An indirect cytotoxicity test on natural HA ceramics showed no threat to the cells. Conclusions: In conclusion, the sintering temperature of $1,200^{\circ}C$ affected the microstructure, phase, and biological characteristics of natural HA ceramics consisting of calcium phosphate. The Ca-P-based natural ceramics are bioactive materials with good biocompatibility; our results indicate that the prepared HA ceramics have great potential for agricultural and biological applications.

Preparation of Nanocrystalline ZrO2 Film by Using a Zirconium Naphthenate and Evaluation of Calcium Phosphate Forming Ability (지르코늄 나프테네이트를 이용한 나노결정질 ZrO2 박막의 제조와 칼슘 포스페이트 형성 능력의 평가)

  • Oh, Jeong-Sun;Ahn, Jun-Hyung;Yun, Yeon-Hum;Kang, Bo-An;Kim, Sang-Bok;Hwang, Kyu-Seog;Shim, Yeon-A
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.9
    • /
    • pp.884-889
    • /
    • 2002
  • In order to investigate the calcium phosphate forming ability of nanocrystalline $ZrO_2$ film, we prepared $ZrO_2/Si$ structure by using a chemical solution deposition with a zirconium naphthenate as a starting material. Precursor sol was spin-coated onto the (100)Si substrate and prefired at 500$^{\circ}C$ for 10 min in air, followed by final annealing at 800$^{\circ}C$ for 30 min in air. Crystallinity of the annealed film was examined by X-ray diffraction analysis. Surface morphology and surface roughness of the film were characterized by field emission-scanning electron microscope and atomic force microscope. After annealing, nanocrystalline $ZrO_2$ grains were obtained on the surface of the film with a homogeneous interface between the film and substrate. After immersion for 1 or 5 days in a simulated body fluid, formation of calcium phosphate was observed on $ZrO_2$ film annealed at 800$^{\circ}C$ by energy dispersive X-ray spectrometer. The fourier transform infrared spectroscopy revealed that carbonate was substituted into the calcium phosphate.

Effect of Addition of β-TCP on Bioactivity and Mechanical Properties of Biodegradable PLA/β-TCP Composites (β-TCP 첨가량에 따른 생분해성 PLA/β-TCP 복합체의 생체활성과 기계적 특성 평가)

  • Moon, Hee-Jung;Kim, Seol-Ak;Kim, Dong-Ae
    • The Journal of the Korea Contents Association
    • /
    • v.21 no.3
    • /
    • pp.609-615
    • /
    • 2021
  • The aim of the present study was to investigate the mechanical properties of melt-injected poly lactic acid (PLA) composites with β-tricalcium phosphate (β-TCP). The PLA mixed with calcined PLA/β-TCP powder to be contents of 0, 10, 30, 50 wt%, respectively, was dissolved in chloroform solvent under stirring for 24 h. Then the liquid mixtures were dropped into ethanol to extract solvent. After drying, the well-dispersed PLA/β-TCP composites were granulated and melt-injected to prepare specimens for various mechanical testing. PLA/β-TCP induced the precipitation of an apatite bone-mineral phase on the surface after immersion in a human simulated body fluid (SBF) for 90 days, showing in bioactivity. Mean various mechanical properties PLA/β-TCP composite were increased up to 10-30 wt% with significantly in part and composite were decreased 50 wt% of showing in mechanical properties. In conclusion, Over 30 wt% addition of β-TCP to PLA may be not advisable to improve the mechanical properties of melt-injected polymeric composites. Results indicated that β-TCP can be used considered as potential reinforcing agent for increasing mechanical properties for PLA. Therefore, it was suggest that the additional effects of β-TCP and research on a wide range of substances.