• Title/Summary/Keyword: silicon Carbide

Search Result 748, Processing Time 0.029 seconds

INTERNATIONAL COLLABORATION FOR SILICON CARBIDE MIRROR POLISHING AND DEVELOPMENT

  • HAN, JEONG-YEOL;CHO, MYUNG;POCZULP, GARY;NAH, JAKYUNG;SEO, HYUN-JOO;KIM, KYUNG-HWAN;TAHK, KYUNG-MO;KIM, DONG-KYUN;KIM, JINHO;SEO, MINHO;LEE, JONGGUN;HAN, SUNG-YEOP
    • Publications of The Korean Astronomical Society
    • /
    • v.30 no.2
    • /
    • pp.687-690
    • /
    • 2015
  • For research and development of Silicon Carbide (SiC) mirrors, the Korea Astronomy and Space Science Institute (KASI) and National Optical Astronomy Observatory (NOAO) have agreed to cooperate and share on polishing and measuring facilities, experience and human resources for two years (2014-2015). The main goals of the SiC mirror polishing are to achieve optical surface figures of less than 20 nm rms and optical surface roughness of less than 2 nm rms. In addition, Green Optics Co., Ltd (GO) has been interested in the SiC polishing and joined the partnership with KASI. KASI will be involved in the development of the SiC polishing and the optical surface measurement using three different kinds of SiC materials and manufacturing processes (POCO$^{TM}$, CoorsTek$^{TM}$ and SSG$^{TM}$ corporations) provided by NOAO. GO will polish the SiC substrate within requirements. Additionally, the requirements of the optical surface imperfections are given as: less than 40 um scratch and 500 um dig. In this paper, we introduce the international collaboration and interim results for SiC mirror polishing and development.

Thermal Conducting Behavior of Composites of Conjugated Short Fibrous-SiC Web with Different Filler Fraction (짧은 섬유상간의 접합을 가진 Silicon Carbide Web 복합재료의 분율별 열전도 거동)

  • Kim, Tae-Eon;Bae, Jin Chul;Cho, Kwang Yeon;Lee, Dong Jin;Shul, Yong-Gun
    • Journal of the Korean Ceramic Society
    • /
    • v.49 no.6
    • /
    • pp.549-555
    • /
    • 2012
  • Silicon carbide(SiC) exhibits many unique properties, such as high strength, corrosion resistance, and high temperature stability. In this study, a SiC-fiber web was prepared from polycarbosilane(PCS) solution by employing the electrospinning process. Then, the SiC-fiber web was pyrolyzed at $1800^{\circ}C$ in argon atmosphere after it was subjected to a thermal curing. The SiC-fiber web (ground web)/phenolic resin (resol) composite was fabricated by hot pressing after mixing the SiC-fiber web and the phenolic resin. The SiC-fiber web composition was controlled by changing the fraction of filler (filler/binder = 9:1, 8:2, 7:3, 6:4, 5:5). Thermal conductivity measurement indicates that at the filler content of 60%, the thermal conductivity was highest, at 6.6 W/mK, due to the resulting structure formed by the filler and binder being closed-packed. Finally, the microstructure of the composites of SiC-fiber web/resin was investigated by FE-SEM, EDS, and XRD.

Development of 200kW class electric vehicle traction motor driver based on SiC MOSFET (SiC MOSFET기반 200kW급 전기차 구동용 모터드라이버 개발)

  • Yeonwoo, Kim;Sehwan, Kim;Minjae, Kim;Uihyung, Yi;Sungwon, Lee
    • Journal of IKEEE
    • /
    • v.26 no.4
    • /
    • pp.671-680
    • /
    • 2022
  • In this paper, A 200kW traction motor driver that covers most of the traction motor specification of commercial electric vehicles (EV) is developed. In order to achieve high efficiency and high power density, a next-generation power semiconductors (Silicon carbide, SiC) are applied instead of power semiconductor(IGBT), which is Si based. Through hardware analysis for optimal use of SiC, expected efficiency and heat dissipation characteristics are obtained. A vector control algorithm for an IPMSM (Interior permanent magnet synchronous motor), which is mostly used in EV(Electric vehicle) traction motor, is implemented using DSP (Digital signal processor). In this paper, a prototype traction motor driver based SiC for EV is designed and manufactured, and its performance is verified through experiments.

Wavefront Compensation Using a Silicon Carbide Deformable Mirror with 37 Actuators for Adaptive Optics (적응광학계용 37채널 SiC 변형거울을 이용한 파면 보상)

  • Ahn, Kyohoon;Rhee, Hyug-Gyo;Lee, Ho-Jae;Lee, Jun-Ho;Yang, Ho-Soon;Kihm, Hagyong
    • Korean Journal of Optics and Photonics
    • /
    • v.27 no.3
    • /
    • pp.106-113
    • /
    • 2016
  • In this paper, we deal with the wavefront compensation capability of a silicon carbide (SiC) deformable mirror (DM) with 37 actuators for adaptive optics. The wavefront compensation capability of the SiC DM is predicted by computer simulation and examined by actual experiments with a closed-loop adaptive optics system consistsing of a light source, a phase plate, a SiC DM, a high speed Shack-Hartmann sensor, and a control computer. Distortion of wavefront is caused by the phase plate in the closed-loop adaptive optics system. The distorted wavefront has a peak-to-valley (PV) wavefront error of $0.3{\mu}m{\sim}0.9{\mu}m$ and root-mean-square (RMS) error of $0.06{\mu}m{\sim}0.25{\mu}m$. The high-speed Shack-Hartmann sensor measures the wavefront error of the distortion caused by the phase plate, and the SiC DM compensates for the distorted wavefront. The compensated wavefront has residual errors lower than $0.1{\mu}m$ PV and $0.03{\mu}m$ RMS. Consequently, we conclude that we can compensate for the distorted wavefront using the SiC DM in the closed-loop adaptive optics system with an operating frequency speed of 500 Hz.

A Study on the Possibility of Using Fire-Retardant Working Cloth Made from Silicon Carbide (SiC) Composite Spun Yarns (Silicon Carbide (SiC) 복합방적사로부터 제조된 원단의 방화복 활용 가능성에 관한 연구)

  • Kang, Hyun-Ju;Kang, Gun-Woong;Kwon, Oh-Hoon;Kwon, Hyeon-Myoung;Hwang, Ye-Eun;Jeon, Hye-Ji;Joo, Jong-Hyun;Park, Yong-Wan
    • Science of Emotion and Sensibility
    • /
    • v.24 no.4
    • /
    • pp.149-156
    • /
    • 2021
  • The mechanical properties of a woven fabric made of SiC (silicon carbide) fibers were determined in this study using the KES-FB system. The woven fabric is used in high heat settings above 1500℃. Composite spun yarns were used to create SiC fibers. By analyzing the wearing properties, we studied the prospect of using the textiles as fire-retardant work clothes. Mechanical properties determine the wearing attributes. Therefore, the tensile linearity (LT), tensile resilience (RT), and shear stiffness (G) values of the fabric varied according to the yarn type (filament or spun yarn). The thickness, weight per square meter, and density of the fabric were found to have an effect on the shear hysteresis (2HG) and compression resilience (RC) values. In terms of wearable clothing qualities, the fabric qualities of the SiC composite yarn demonstrated the highest ratio of compressive energy to thickness (WC/T), which indicates bulkiness. The fabric manufactured from SiC composite yarns passed the KFI criteria for carbonation length and cumulative flame time in the flame-retardant test. Therefore, we discovered that the material can be used as a fire-resistant work cloth.

Tribological Properties of Sputtered Boron Carbide Coating and the Effect of ${CH}_4$ Reactive Component of Processing Gas

  • Cuong, Pham-Duc;Ahn, Hyo-Sok;Kim, Jong-Hee;Shin, Kyung-Ho
    • KSTLE International Journal
    • /
    • v.4 no.2
    • /
    • pp.56-59
    • /
    • 2003
  • Boron carbide thin coatings were deposited on silicon wafers by DC magnetron sputtering using a ${B}_4$C target with Ar as processing gas. Various amounts of methane gas (${CH}_4$) were added in the deposition process to better understand their influence on tribological properties of the coatings. Reciprocating wear tests employing an oscillating friction wear tester were performed to investigate the tribological behaviors of the coatings in ambient environment. The chemical characteristics of the coatings and worn surfaces were studied using X-ray Photoelectron Spectroscopy (XPS) and Auger Electron Spectroscopy (AES). It revealed that ${CH}_4$addition to Ar processing gas strongly affected the tribologcal properties of sputtered boron carbide coating. The coefficient of friction was reduced approximately from 0.4 to 0.1, and wear resistance was improved considerably by increasing the ratio of ${CH}_4$gas component from 0 to 1.2 vol %. By adding a sufficient amount of ${CH}_4$(1.2 %) in the deposition process, the boron carbide coating exhibited lowest friction and highest wear resistance.

Tribological properties of sputtered boron carbide coating and the effect of $CH_4$ reactive component of processing gas

  • Cuong Pham Duc;Ahn Hyo-Sok;Kim Jong-Hee;Shin Kyung-Ho
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 2003.11a
    • /
    • pp.78-84
    • /
    • 2003
  • Boron carbide thin coatings were deposited on silicon wafers by DC magnetron sputtering using a $B_4C$ target with As as processing gas. Various amounts of methane gas $(CH_4)$ were added in the deposition process to better understand their influence on tribological properties of the coatings. Reciprocating wear tests employing an oscillating friction wear tester were performed to investigate the tribological behaviors of the coatings in ambient environment. The chemical characteristics of the coatings and worn surfaces were studied using X-ray Photoelectron Spectroscopy (XPS) and Auger Electron Spectroscopy (AES). It revealed that $CH_4$ addition to As processing gas strongly affected the tribologcal properties of sputtered boron carbide coating. The coefficient of friction was reduced approximately from 0.4 to 0.1, and wear resistance was improved considerably by increasing the ratio of $CH_4$, gas component from 0 to $1.2\;vol\;\%$. By adding a sufficient amount of $CH_4\;(1.2\%)$ in the deposition process, the boron carbide coating exhibited lowest friction and highest wear resistance.

  • PDF

Changes in Mechanical Properties of WC-Co by Ultrasonic Nanocrystal Surface Modification Technique (UNSM 기술을 이용한 초경의 기계적 특성변화)

  • Lee, Seung-Chul;Kim, Jun-Hyong;Kim, Hak-Doo;Choi, Gab-Su;Amanov, Auezhan;Pyun, Young-Sik
    • Tribology and Lubricants
    • /
    • v.31 no.4
    • /
    • pp.157-162
    • /
    • 2015
  • In this study, an ultrasonic nanocrystalline surface modification (UNSM) technique is applied to tungsten carbide-cobalt (WC-Co) to extend the service life of carbide parts used in press mold. The UNSM technique modifies the structure, reduces the surface roughness, increases the surface hardness, induces the compressive residual stress, and increases the wear resistance of materials by introducing severe plastic deformation. The surface roughness, hardness, and compressive residual stress of WC after UNSM treatment improve by about 42, 10, and 71%, respectively. A wear test under dry conditions is used to assess the effectiveness of the UNSM technique on the friction and wear behavior of WC. The UNSM technique is found to reduce the WC friction coefficient by approximately 21% and enhance the wear resistance by approximately 85%. The improved friction and wear behavior of WC may be mainly attributed to the increased hardness and compressive residual stress. Moreover, the WC specimen is treated by UNSM technique using three different WC, silicon nitride (Si3N4) and stainless steel (STS304) balls. The surface treated by WC balls shows the highest hardness when compared with treatment by stainless steel and silicon nitride balls. According to the obtained results, the UNSM technique is believed to increase the durability of the carbide component by improving the friction and wear behavior.

A STUDY ON THE REMOVAL OF DENTINAL SMEAR LAYER BY DENTIN CONDITIONER (상아질처리제(象牙質處理劑)에 의(依)한 상아질(象牙質) 표면(表面) 도말층(塗抹層)의 제거(除去)에 관(關)한 연구(硏究))

  • Ahn, Hyun-Mi;Son, Ho-Hyun
    • Restorative Dentistry and Endodontics
    • /
    • v.14 no.2
    • /
    • pp.65-76
    • /
    • 1989
  • The purpose of this study was to observe the effect on the removal of dentinal smear layer and morphological changes of reduced dentin surfaces by various dentin surface conditioners. Thirty-two healthy human premolars extracted due to periodontal or orthodontic reasons were used. The teeth were cross-sectioned to expose dentin at the middle portion of the crown with diamond rotary saw. The specimens were then divided into 8 groups. The sectioned dentin surfaces in group 1 to 4 were grinded with No. 400 grit silicone abrasive paper and those in group 5 to 8 were cut with #700 carbide bur under air-water spray. The grinded or cut dentin surfaces were conditioned with 3% $H_2O$, Dentin Conditioner(GC Inter. Corp., Japan), and Scotchprep(3M Dent Prod., U.S.A) according to manufacturer's directions. All the specimens were dried in room temperature for 48 hours, and gold-coated with Eiko ion coater(Eik-engineering Co.), and observed in Hitachi S-450 Scanning electron microscope at 15-25 KV. The following results were obtained; 1. The dentin surfaces grinded with the silicon abrasive paper were rougher in texture and heavier in amount of smear layer than those cut with the carbide bur. 2. Scrubbing of 3% $H_2O_2$ was not effective in removing dentinal smear layer. 3. 20-second conditioning of Dentin Conditioner (GC Inter. Corp) resulted in the removal of a significant amount of the smear layer without removing the tubular plugs and dissolving the peritubular dentin. 4. Scotchprep removed the smear layer very effectively. But at the same time it dissolved the peritubular dentin. 5. Irrespective of the uses of the silicon carbide abrasive paper or the carbide bur the morphological changes of dentin surfaces treated with the same conditioning agents were similar.

  • PDF

A STUDY ON SHEAR BOND STRENGTH OF COMPOSITE RESIN TO DENTIN FOLLOWING SURFACE TREATMENTS (표면처리에 따른 상아질과 콤포짓드 레진간의 전단결합강도에 관한 연구)

  • Noh, Eun-Hee;Park, Sang-Jin
    • Restorative Dentistry and Endodontics
    • /
    • v.16 no.1
    • /
    • pp.200-208
    • /
    • 1991
  • The purpose of this study was to observe shear bond strength of composite resin to dentin following surface treatment. Freshly extracted forty-eight sound human molars were used in this study. They were stored at $4^{\circ}C$ physiologic saline solution before experiment. The teeth was then mounted with self curing acrylic resin in brass mold. The buccal surfaces of the teeth were grinding approximately 1.5mm by means of water-irrigated grinding wheel to expose the flattened fresh dentin surfaces. The specimens were divided into 6 groups according to preparation and treatment procedures on dentin surfaces; Group 1: Untreated after preparation with No.301 diamond point Group 2: Treated with primer for 60 seconds after preparation with No.301 diamond point Group 3: Untreated after preparation with No.700 fissure carbide bur Group 4: Treated with primer for 60 seconds after preparation with No.700 fissure carbide bur Group 5: Untreated after grinding with 600 grit silicon carbide paper Group 6: Treated with primer for 60 seconds after grinding with 600 grit silicon carbide paper Light cure dental adhesive was applicated to each specimen. Silux plus(3M) was inserted then into polyethylene tube of 3mm diameter and 3mm height, and polymerized to dentin surface. All of the specimens were stored in distilled water at $35.6^{\circ}C$ for 24 hours prior to testing. The shear bond strength was measured using an Instron Universal Testing Machine. The results obtained from this study were as follows: 1. The shear bond strength to dentin was the highest in group II. 2. The shear bond strength to dentin was the lowest in group III. 3. There was no significant difference in shear bond strength to dentin according to preparation instrument. 4. The primer treatment group showed significantly greater shear bond strength than untreated group.