• 제목/요약/키워드: sigma ($\sigma$) phase

검색결과 264건 처리시간 0.035초

가공온도에 따라 다이업셋한 Nd-Fe-B-Cu 합금의 응력과 결정에 관한 연구 (A Study on the Stress and Crystal in Die-Upsetted Nd-Fe-B-Cu Alloys as a Function of Working Temperature)

  • 박정덕;양현수;곽창섭;정원용
    • 열처리공학회지
    • /
    • 제7권1호
    • /
    • pp.61-71
    • /
    • 1994
  • This study is to investigate the stress distributions, crystal orientations and magnetic properties during die-upsetting according to working temperature of Nd-Fe-B-Cu alloys. The stress distributions in the specimens during compressing process were calculated by a finite element method program(SPID). The calculated stresses were effective stress (${\sigma}_{eff}$), compression stress(${\sigma}_z$), radial direction stress(${\sigma}_r$) rotational direction stress(${\sigma}_e$) and shear stress(${\tau}_{rz}$). The stress distributions of ${\sigma}_z$, obtained by a computer simulation showed that the stress components causing the magnetic alignment during die-upsetting of the cast magnets were very high at the center-part of a specimen, and decreased toward the periphery-part of a specimen. In view of the above results the magnetic properties should be better at the center-part of a specimen than any other parts. But the measured magnetic properties were better at the mid-part. These results should be due to the fact that the specimens were casted. Normally the magnetic properties are affected by the casting process as well as by the stress levels. ${\sigma}_r$, ${\sigma}_e$ are thought to affect the liquid phase flowing and domain patterns, respectively. The influence of ${\tau}_{rz}$ was trivial, ${\sigma}_{eff}$ distributed similar throughout the specimen. The Nd-rich phase appeared at the peripheral of the specimen where the stress level of ${\sigma}_r$, ${\sigma}_z$, was low or the stress level of ${\sigma}_e$ was high. The Nd-rich phase was squeezed out during die-upsetting. This phase had an effect on the crystal orientation and grain growth. The stress distributions of alloy were irregular at the parts of the specimen where the die contacted with specimen.

  • PDF

SAF 2205 듀플렉스 스테인레스강의 미세조직 및 기계적 특성에 미치는 냉각속도의 영향 (Effect of Cooling Rate on Microstructural and Mechanical Properties of SAF 2205 Duplex Stainless Steel)

  • 오영주;양원존;이종훈;김두현;유위도;이재현
    • 열처리공학회지
    • /
    • 제26권1호
    • /
    • pp.14-20
    • /
    • 2013
  • Duplex stainless steel, which is a kind of stainless steel with a mixed microstructure of about equal proportions of austenite and ferrite, is generally known as a unique material with excellent corrosion resistance and high strength. However, toughness, strength, and corrosion resistance of the steel could be reduced due to precipitation of topologically closed packed phases such as sigma phase during cooling. In case of large forged products, they have strong possibility that ${\sigma}$-phase precipitates due to difference of cooling rate between surface and inner of the products. Investigation on sigma phase precipitation behavior of duplex stainless steel with change of cooling rate was carried out in this study. Forged SAF 2205 duplex stainless steel was used as specimens to examine the cooling rate effect. Dissolution behavior of sigma phase was also discussed through resolution test of duplex stainless steel containing lots of sigma phase. Experimental results revealed that impact energy was very sensitive to precipitation of small amount sigma phase. However, sigma phase could be removed by short term resolution treatment and impact resistance of the duplex stainless steel was restored.

텅스텐이 첨가된 슈퍼 2상 스테인리스강의 내부식성에 관한 연구 (Study of Corrosion Resistance in Super-Duplex, Tungsten-Containing Stainless Steel)

  • 최한글;박형균;정병호;한현성;배동수;강창룡
    • 한국해양공학회지
    • /
    • 제24권5호
    • /
    • pp.55-59
    • /
    • 2010
  • The effect of aging on the precipitation of the $\sigma$ phase and corrosion resistance in W-substituted, super-duplex stainless steel was investigated. The volume fraction of the $\sigma$ phase and the current density increased as the aging temperature increased up to $750^{\circ}C$, and, then, they decreased. As aging time increased, the volume fraction of the $\sigma$ phase and the current density also increased. The $\sigma$ phase considerably influenced to corrosion resistance. When Mo was substituted for W in super-duplex stainless steel, the volume fraction of the $\sigma$ phase and the current density both decreased markedly.

SDSS (Super Duplex Stainless Steel) 강관의 미세조직 및 부식특성에 미치는 열처리 온도의 영향 (The Influence of Heat Treatment Temperature on Microstructure and Corrosion Behavior of SDSS Tube)

  • 이인섭;천창석;임태홍;한윤호;이면학
    • 한국표면공학회지
    • /
    • 제48권6호
    • /
    • pp.329-334
    • /
    • 2015
  • The aim of this paper is to determine the proper heat treatment temperature for SDSS tube production without ${\sigma}$-phase precipitation. When Mother steel tube was heat treated at $800^{\circ}C$ temperature, relatively a large amount of ${\sigma}$-phase precipitated and grain refinement of ferrite phase occurred simultaneously. However, in Pilgered and Drawn steel tubes, grain refinement of the ferrite phase did not occur and a small amount of ${\sigma}$-phase precipitated. For all three types of steel tubes, the pitting potential was reduced to 2/5 or less compared with the untreated one and corrosion also occurred in the salt spray test due to the precipitation of ${\sigma}$-phase. When heat treatment temperature was $900^{\circ}C$, grain refinement of the ferrite phase occurred and very little ${\sigma}$-phase precipitated in Pilgered and Drawn steel tubes. But when heat treatment was done at $1,000^{\circ}C$ temperature, all three types of steel tubes had a similar corrosion properties of that of untreated one and also corrosion did not occur in the salt spray test, as ${\sigma}$-phase did not precipitate. Therefore, the optimum heat treatment temperature range is determined to be more than $1000^{\circ}C$ for the SDSS at which corrosion does not occur.

슈퍼 듀플렉스 스테인리스강 UNS S32750의 FCA 용접 후 열처리가 공식에 미치는 영향 (Heat Treatment Effect on Pitting Corrosion of Super Duplex Stainless Steel UNS S32750 FCA Welds)

  • 장복수;문인준;김세철;고진현
    • Journal of Welding and Joining
    • /
    • 제31권5호
    • /
    • pp.20-25
    • /
    • 2013
  • This study was carried out to investigate the influence of a sigma phase precipitation on the pitting corrosion resistance and microstructural change of super duplex stainless steels(UNS S32750). The welds made by FCAW (Flux Cored Arc Welding) were heat treated ($930^{\circ}C$, $1080^{\circ}C$, $1230^{\circ}C$) and quenched. Based on the microstructural examination, it was found that the ${\sigma}$ phase was formed in base metals and welds heat treated at $930^{\circ}C$ while there were little ${\sigma}$phases formed in base metals and weld metal experienced the relatively fast cooling from $1080^{\circ}C$ and $1230^{\circ}C$. On the other hand, the most weight loss due to pitting corrosion occurred in base and weld metals heat treated at $930^{\circ}C$. It was confirmed that the pitting corrosion occurred in the phase boundaries of ferrite/sigma and austenite/sigma. The pitting corrosion resistance decreased owing to an increase in Cr, Mo depleted areas adjacent to the intermetallic phases such as ${\sigma}$phases. The hardness was greatly increased due to the precipitation ${\sigma}$phases.

Fractional-N 방식의 주파수 합성기 설계 (A design of fractional-N phase lock loop)

  • 김민아;최영식
    • 한국정보통신학회논문지
    • /
    • 제11권8호
    • /
    • pp.1558-1563
    • /
    • 2007
  • 논문은 fractional-N 방식의 주파수 합성기(PLL)를 낮은 차수의 ${\Delta}{\Sigma}$변조기로 더욱 높은 성능의 PLL로 설계하기 위하여 대역폭 가변 방식의 PLL과 ${\Delta}{\Sigma}$방식의 fractional-N PLL의 구조를 합성한 새로운 방식의 PLL을 제안한다. Matla으로 대역폭 가변을 이용한 ${\Delta}{\Sigma}$방식의 fractional-N PLL의 시뮬레이션을 수행하여 제안된 구조의 특성을 관찰하였다. 본 논문의 대역폭 가변 PLL은 HSPICE 0.35um CMOS 공정을 이용하여 시뮬레이션 하였고, 그 결과 제안된 PLL은 빠른 록이 가능하고 fractional spur를 20dB 정도 낮출 수 있었다.

25Cr-7Ni-2Mo-4W 슈퍼 2상 스테인리스강의 기계적 성질에 미치는 R상의 영향 (Effect of R Phase Formation on the Mechanical Properties of 25Cr-7Ni-2Mo-4W Super Duplex Stainless Steel)

  • 이병찬;강창룡
    • 한국재료학회지
    • /
    • 제24권8호
    • /
    • pp.401-406
    • /
    • 2014
  • In this study, we investigated the precipitation behavior of the R-phase precipitated at the initial stage of aging and its effects on the mechanical properties of 25%Cr-7%Ni-2%Mo-4%W super duplex stainless steel. The R-phase was mainly precipitated at the interface of ferrite/austenite phases and inside of the ferrite phase during the initial stage of aging. It was transformed into the ${\sigma}$-phase with an increase of the aging time. The ferrite phase was decomposed into a new austenite(${\gamma}_2$)phase and the ${\sigma}$-phase by an aging treatment. The R phase was an intermetallic compound showing higher molybdenum and tungsten concentrations than the matrix and also showed higher molybdenum and tungsten concentrations than the ${\sigma}$ phase. In the initial stage of aging, precipitation of the R-phase did not change the hardness, the strength and the elongation. The hardness and the strength increased upon a longer aging time, but the elongation rapidly decreased. These results show that the R-phase did not significantly affect the hardness and the strength, though it did influence the elongation.

Delta-Sigma Modulator를 이용한 무선이동통신용 Fractional-N 주파수합성기 설계 (Design of Fractional-N Frequency Synthesizer with Delta-Sigma Modulator for Wireless Mobile Communications)

  • 박병하
    • 전기전자학회논문지
    • /
    • 제3권1호
    • /
    • pp.39-49
    • /
    • 1999
  • This paper describes a 1 GHz, low-phase-noise CMOS fractional-N frequency synthesizer with an integrated LC VCO. The proposed frequency synthesizer, which uses a high-order delta-sigma modulator to suppress the fractional spurious tones at all multiples of the fractional frequency resolution offset, has 64 programmable frequency channels with frequency resolution of $f_ref/64$. The measured phase noise is as low as -110 dBc/Hz at a 200 KHz offset frequency from a carrier frequency of 980 MHz. The reference sideband spurs are -73.5 dBc. The prototype is implemented in a $0.5{\mu}m$ CMOS process with triple metal layers. The active chip area is about $4mm^2$ and the prototype consumes 43 mW, including the VCO buffer power consumption, from a 3.3 V supply voltage.

  • PDF

스테인리스강 용접부의 기계적 성질에 미치는 후열처리의 영향 (The influence of post weld heat treatment on mechanical properties of stainless steel weldment)

  • 한종만;한기형;이은배;허만주;한용섭
    • Journal of Welding and Joining
    • /
    • 제14권3호
    • /
    • pp.75-85
    • /
    • 1996
  • In this paper the influence of postweld heat treatment on mechanical properties of SMAW and FCAW stainless steel weldments was examined and the obtained results are as follows ; (1) The amount of $\delta$-ferrite formed by SMAW and FCAW process decreased with increasing holding temperature and time in post weld heat treatment(PWHT), and it was found that the reduced ferrite was transformed into sigma phase after $800^{circ}C{\times}50hr$ PWHT. This sigma phase, even though it was very small, resulted in brittleness of dissimilar weldment between carbon steel and stainless steel in bending test, however in similar weldment between stainless steel and stainless steel was not occured. (2) The chemical composition of sigma phase was measured to 28-30%Cr, 7-9%Mo, 4-6Ni in 316L weldment, and also 35-37%Cr, 0.9-1.0Mo, 6-8%Ni in 309L weldment by EDS analysis.

  • PDF