  • Purpose: The aim of this study was to evaluate the bone regeneration ability of 1% tetracycline (TC)-loaded silk fibroin membrane (SFM), in a rabbit calvarial defect model. Methods: Twenty New Zealand white rabbits were used for this study. Bilateral round defects were made on the rabbit parietal bone, using trephine bur with an 8 mm diameter. TC-loaded SFM or SFM was covered on the right parietal bone defect, and the left parietal bone defects were uncovered for the control. The animals were humanely sacrificed at 4 or 8 weeks postoperatively. A micro-computerized tomography (${\mu}$-CT) of each specimen was taken for analysis of bone regeneration. Hematoxylin and Eosin stain were done to observe histological findings. Results: From the ${\mu}$-CT results, regenerated bone volume ($mm^3$) of 1% TC-loaded SFM, SFM, and control were $7.80{\pm}5.87$, $8.79{\pm}3.44$, and $10.61{\pm}5.3$ at 4 weeks postoperatively, respectively (P>0.05). Regenerated bone volume ($mm^3$) of 1% TC-loaded SFM, SFM, and control were $36.56{\pm}8.50$, $25.86{\pm}8.17$, and $19.09{\pm}5.07$ at 8 weeks postoperatively, respectively (P<0.05). Conclusion: The 1% TC-loaded SFM showed more bone regeneration than the SFM and the uncovered control, in guided bone regeneration.

가토의 두개 결손부에서의 실크 단백질과 platelet-rich fibrin (PRF)의 골형성 효과 (The bone regenerative effect of silk fibroin mixed with platelet-rich fibrin (PRF) in the calvaria defect of rabbit)

  • 송지영;권해용;권광준;박영욱;김성곤
    • Journal of the Korean Association of Oral and Maxillofacial Surgeons
    • /
    • 제36권4호
    • /
    • pp.250-254
    • /
    • 2010
  • Introduction: This study evaluated the bone regenerative effect of silk fibroin mixed with platelet-rich fibrin (PRF) of a bone defect in rabbits. Materials and Methods: Ten New Zealand white rabbits were used for this study and bilateral round shaped defects were formed in the parietal bone (diameter: 8.0 mm). The silk fibroin mixed with PRF was grafted into the right parietal bone (experimental group). The left side (control group) was grafted only PRF. The animals were sacrificed at 4 weeks and 8 weeks. A micro-computerized tomography (${\mu}$CT) of each specimen was taken. Subsequently, the specimens were decalcified and stained for histological analysis. Results: The average value of plane film analysis was higher in the experimental group than in the control group at 4 weeks and 8weeks after surgery. However, the difference was not statistically significant.(P>0.05) The tissue mineral density (TMD) in the experimental group at 4 weeks after surgery was significantly higher than the control group.(P<0.05) Conclusion: Silk fibroin can be used as a scaffold of PRF for rabbit calvarial defect repair.

늑간근에 발생한 폐포성 횡문 근육종 1례 보고 (One Case of Alveolar Rhabdomyosareoma arising from Intercostal Muscle)

  • 김선한
    • Journal of Chest Surgery
    • /
    • 제25권6호
    • /
    • pp.598-604
    • /
    • 1992
  • Rhabdomyosarcoma is the most common soft tissue sarcoma in childhood and acounts for 6% to 15% of all cases of childhood cancer, Rhabdomyosarcoma in seventh most common form of childhood neoplasms, following acute leukemia, tumors of the central nervous system, lymphoma neuroblastoma, Wilm`s tumor, bone tumor. Rhabdomyosarcoma can arise anywhere in the body, but primary site in the thorax is relatively rare. We experienced a case of aveolar rhabdomyosarcoma arising from intercostal muscle, A 12 year-old woman was suffered from the intermittent left chest pain radiating to the scapular area and dyspnea, On physical examination, pulmonary friction rub was heard on the left upper lobe area. Qn adimission, the chest simple radiography revealed a 7 x 6, 5cm sized radio-opaque mass with pleural effusion in the superior mediastinum and the CT showed a well difined radio-opaque mass including the destructed 2nd rib and pleural effusion. The percutaneous tra-nsthoracic needle aspiration biopsy was likely to show blastoma. After the chemotherapy[vincristine, actinomycin-D, cyclophosphamde] was done to treat blastoma, the pleural effussion was subsided and the mass was slightly decreased by 4.5x 4. 5cm. For treatment and diagnosis, we performed en-bloc resection and the defected chest was reconstucted with Gortex patch. Grossly, the specimen was colored graysh-white and arised in between two ribs The microscopic findings showed that the tumor cells were small round with scant pinkish cytoplasm on the H-E stain and the tumor cell nests were grouped by reticulum fibers and showed alveolar pattern on the silver stain The electromicroscopic finding presented that the cytoplasm contained tangled fibrillar and flocculent materials. The histopathologic findings were compatable with laveolar rhabdomyosarcoma. She was discharged without any complication. After discharge, she has been treated with radiation theraphy and chemotheraphy, and not recurred untill last follow-up We report a case of alveolar rhabdomyosarcoma arising to intercostal muscle, developed in 12 year-old waman, with brief review of literatures.

  • PDF

교정용 와이어의 표면특성에 미치는 TiN 및 ZrN 코팅영향 (Effects of TiN and ZrN Coating on Surface Characteristics of Orthodontic Wire)

  • 김원기;김도영;최한철
    • 한국표면공학회지
    • /
    • 제41권4호
    • /
    • pp.147-155
    • /
    • 2008
  • The dental orthodontic wire provides a good combination of strength, corrosion resistance and moderate cost. The purpose of this study was to investigate the effects of TiN and ZrN coating on corrosion resistance and physical property of orthodontic wire using various instruments. Wires(round type and rectangular type) were used, respectively, for experiment. Ion plating was carried out for wire using Ti and Zr coating materials with nitrogen gas. Ion plated surface of each specimen was observed with field emission scanning electron microscopy(FE-SEM), energy dispersive X-ray spectroscopy(EDS), atomic force microscopy(AFM), vickers hardness tester, and electrochemical tester. The surface of TiN and ZrN coated wire was more smooth than that of other kinds of non-coated wire. TiN and ZrN coated surface showed higher hardness than that of non-coated surface. The corrosion potential of the TiN coated wire was comparatively high. The current density of TiN coated wire was smaller than that of non-coated wire in 0.9% NaCl solution. Pit nucleated at scratch of wire. The pitting corrosion resistance $|E_{pit}-E_{rep}|$ increased in the order of ZrN coated(300 mV), TiN coated(120 mV) and non-coated wire(0 mV).

The BMPs expression and histomorphometric study of ${\beta}-TCP$ / rhBMP-2 Grafting on the rabbit cranial bone defects

  • Lim, Byung-Sup;Jeon, Jae-Yoon;Park, Chang-Joo;Im, Jae-Jung;Hwang, Kyung-Gyun;Shim, Kwang-Sup
    • Journal of the Korean Association of Oral and Maxillofacial Surgeons
    • /
    • 제34권1호
    • /
    • pp.49-58
    • /
    • 2008
  • Objective: The Purpose of the study was to investigate the bone morphogenic protein expression of rhBMP-2(recombinant human bone morphogenic protein-2) as singnaling molecule and ${\beta}-TCP$(Tricalcium phosphate) as a bone substitute and carrier medium of rhBMP-2. Materials and Methods: 16 rabbits divided into 2 group of each 8 rabbit. Two standardized bone defect, round bilateral defect was made in the cranium of the 8 rabbit of first group, and was grafted with $150{\sim}500{\mu}m$ diameter ${\beta}-TCP$ 0.25g in one side, which was soaked with rhBMP-2, and autogenous bone was grafted on another side as a positive control. Second group of 8 rabbit, only ${\beta}-TCP$ was grafted with same size and same manner. After 2, 4, 8, and 12 weeks, specimen was taken for microscopic immunohiostochemical and histomorphometric analysis. Result: Grafting ${\beta}-TCP$ with rhBMP show the early formation of the bone regenerative factor (BMP-4) and more quantity of new bone formation than only use of ${\beta}-TCP$ (8,12 week), even show less new bone formation than autogenous bone. Conclusion : The experimental study result that ${\beta}-TCP$ graft combination with rhBMP-2 as a delivery system is an effective with osteoinductive capacity and biodegradable properties, so that provide clinical availibility of composite use in reconstruction of bony defect.

염모제 종류와 시술 순서에 따른 모발의 물리적 형태와 색의 변화 (A Study on Variations in Physical Properties and Color of Hair depending on Dye Type and Perm, Hair Coloring Treatment Procedure)

  • 박용;권수애
    • 한국생활과학회지
    • /
    • 제16권5호
    • /
    • pp.1051-1059
    • /
    • 2007
  • This study intends to find out possible variations in physical properties and color of hair depending on dye type(acidic and alkalic) and permanent treatment/hair dyeing procedure. To meet the goals, healthy hair samples were taken from 5 women's hair speciment in 20's without experiencing in any harmful substance via long-term medications. and beauty care using chemicals. To get possible findings depending upon hair dye type and treatment procedure, both acidic and alkalic hair dye were applied on some specimens after permanent treatment, while on other specimens before permanent treatment. In order to determine scale damage, this study used SEM(Hitachi S-2500C) both hair thickness and tensile strength were measured with optical microscope(Nikon, MM-60/L3T) and Instron (4482-standard). Wave configuration was measured transverse and longitudinal round diameter. The chromaticity of each specimen was measured using a spectrocolorimeter(Color Techno System, JP/JX-777) with visual $C/2^{\circ}$ (at $2^{\circ}$ with C light source) monitor fixed to determine Lab and CMYK values. As a result, it was found that hair specimens were more significantly damaged with alkalic hair dye treatment than with acidic hair dye treatment, while hair specimens were more effectively dyed with the former hair dye type than with the latter one. For possible results depending on treatment procedure, it was found that hair specimens were less damaged but more effectively dyed with permanent treatment followed by hair dyeing than vice versa. Therefore, it was concluded that permanent treatment followed by acidic hair dyeing would be more effective in reducing hair damages.

전기저항 측정법을 이용한 탄소나노튜브/폴리프로필렌 나노복합재료의 내부 손상 예측 (Electrical Resistance Measurement in Characterizing the Internal Damage of Carbon Nanotube/Polypropylene Nanocomposites)

  • 김학수;권동준;왕작가;구가영;김대식;이춘수;박종만
    • Composites Research
    • /
    • 제26권3호
    • /
    • pp.201-206
    • /
    • 2013
  • 전기저항 측정법을 이용하여 전도성을 띄는 소재는 손상예측이 가능하다. 본 연구에서는 차량용 소재로 이용하는 폴리프로필렌(PP)를 이용할 때 재료 내부에 발생될 손상 평가법을 고안하였다. PP 내부에 전도성을 부여하기 위해 탄소나노튜브(CNT)를 0.5 wt% 삽입하여 CNT/PP 복합재료를 제조하였다. 손상 평가를 하기 위해 시편 내부에 구리선을 삽입하여 가로와 세로, 대각선 구간을 설정하여 측정하였다. 시편의 모형은 $20^{\circ}$ 휘어진 시편을 사용하였다. 동적 압축 실험에 따른 전기저항 측정을 통해 구간별로 전기저항 변화도를 분석하였다. 동적 압축 실험에 따른 구간별 전기저항 변화도의 신호는 재료 내부에 전가된 응력을 나타내는 신호이다. 전기저항 측정 구간에서 전기저항 변화도가 높은 경우는 미세 손상이 발생되었음을 의미한다. 전기저항 측정법을 이용한 동적 압축 실험에 따른 예상 손상부위와 실제 파괴 실험을 통해 본 평가 방법을 이용하여 재료 내부 미세 손상을 예측할 수 있는 방법임을 확인하였다.

가토의 두정골 결손부 모델에서 수산화인회석에 4-hexylresorcinol을 혼합하여 만든 인공합성골이식재의 골형성효과에 대한 연구 (The Effect of a Hydroxyapatite and 4-hexylresorcinol Combination Graft on Bone Regeneration in the Rabbit Calvarial Defect Model)

  • 김민근;박용태;김성곤;박영욱;이석근;채원식
    • Maxillofacial Plastic and Reconstructive Surgery
    • /
    • 제34권6호
    • /
    • pp.377-383
    • /
    • 2012
  • Purpose: The aim of this study was to evaluate the effect of 4-hexylresorcinol and hydroxyapatite combination graft on bone regeneration in the rabbit calvarial defect model. Methods: Ten New Zealand white rabbits were used for this study. Bilateral round shaped defects (diameter: 8.0 mm) were created on the parietal bone. 4-hexylresorcinol and hydroxyapatite combination graft material was grafted into the right parietal bone defect area (experimental). The left bone defect area was not filled with anything (control). The animals were sacrificed at 4 weeks and 8 weeks after grafting. A micro-computerized tomography of each specimen was taken, and the specimens were stained for histological analysis. Results: The average value of bone mineral density (BMD) and Bone volume (BV) was higher in the experimental group than in the control group at 4 weeks and 8 weeks after surgery. However, the difference was not statistically significant (P>0.05) at 8 weeks after grafting. The BMD and BV in the experimental group at 4 weeks after surgery was significantly higher than those in the control group (P<0.05). Conclusion: 4-hexylresorcinol and hydroxyapatite combination graft material showed higher initial bone formation than the control, however, there was no difference at 8weeks after operation.

폴리머 코팅된 NiTi합금 교정선의 표면특성 (Surface Characteristics of Polymer Coated NiTi Alloy Wire for Orthodontics)

  • 조주영;김원기;최환석;이호종;최한철
    • 한국표면공학회지
    • /
    • 제43권3호
    • /
    • pp.132-141
    • /
    • 2010
  • NiTi alloy has been used for orthodontic wire due to good mechanical properties, such as elastic strength and frictional resistance, combined with a high resistance to corrosion. Recently, these wire were coated by polymer and ceramic materials for aesthetics. The purpose of this study was to investigate surface characteristics of polymer coated NiTi alloy wire for orthodontics using various instruments. Wires (round type and rectangular type) were used, respectively, for experiment. Polymer coating was carried out for wire. Specimen was investigated with field emission scanning electron microscopy(FE-SEM), energy dispersive x-ray spectroscopy(EDS) and atomic force microscopy(AFM). The phase transformation of non-coated NiTi wire from martensite to austenite occurred at the range of $14{\sim}15^{\circ}C$, in the case of coated wire, it occurred at the range of $16{\sim}18^{\circ}C$. Polymer coating on NiTi wire surface decreased the surface defects such as scratch which was formed at severe machined surface. From the AFM results, the average surface roughness of non-coated and coated NiTi wire was 13.1 nm, and 224.5 nm, respectively. From convetional surface roughness test, the average surface roughness of non-coated and coated NiTi wire was $0.046{\mu}m$, and $0.718{\mu}m$, respectively.

삼축압축시험에 의한 모래-점토 복합시료의 전단거동 특성 (Characteristics of Shear Behavior for Sand-Clay Composite by Triaxial Test)

  • 이진수;김재일;이강일
    • 한국지반신소재학회논문집
    • /
    • 제5권4호
    • /
    • pp.19-25
    • /
    • 2006
  • 모래-점토 복합시료의 제반 전단특성을 규명하기 위하여 연약지반에 설치한 배수재로서의 모래기둥의 직경(dw)과 배수영향원의 직경(de)비 즉, 배수간격비(n=de/dw), 모래기둥의 밀도 및 모래기둥과 주변 연약토의 강성을 달리한 공시체를 제작하여 실내 삼축압축시험을 실시하였다. 또한 모래기둥을 토목섬유등의 보강재로 감싼 경우에 있어서 지반의 보강정도 및 효과에 대해서도 시험이 이루어 졌다. 삼축압축시험 결과, 모래기둥의 직경과 밀도가 커질수록 전단강도가 증가하는 일반적인 경향을 보이나, 모래기둥을 보강재료로 감싼 경우의 전단강도 증가가 매우 크다. 그리고 배수간격비가 3이하를 경계로 하여 그 증가정도가 뚜렷하게 나타나고 모래의 전단거동과 유사하다. 간극수압계수는 배수간격비가 작아질수록 감소하는 경향으로 전단강도 결과에서와 같이 배수간격비가 3~4이하에서는 그 감소 정도가 크다.

  • PDF