Evaluation on the Possibility of Preparation of Nanosized Alumina Powder under W/O Emulsion Method Using Homogenizer (Homogenizer를 사용한 W/O 에멀젼법하에 나노크기 알루미나 분체 제조 가능성 평가)

  • Lee, Yoong;Hahm, Yeong-Min
    • Applied Chemistry for Engineering
    • /
    • v.21 no.5
    • /
    • pp.488-494
    • /
    • 2010
  • Under W/O emulsion method using a homogenizer, ${\alpha}$-alumina powder was prepared to evaluate the effects of experimental conditions on its properties, such as particle shape, extent of aggregation, average particle size and distribution. The experimental parameters were the change of type, quantity and composition of emulsifiers as well as the change of O : W volumetric ratio and agitation rate. As results, in the case of the use of single surfactant of SP80, sphere-like particles could be prepared and the average particle size was hardly affected by the agitation speed more than 16000 rpm regardless of SP80 quantity used. When the extent of aggregation among sphere-like particles prepared using $HLB_m$ = 5 of [SP80 & TW80] was compared with that prepared using SP80 at the same vol% surfactant and agitation speed, the former showed more or less low aggregation phenomena and average particle size was slightly reduced. In addition, the fraction of nano-sized particles with low aggregation was increased by the use of 0.1 vol% n-butanol, as a co-surfactant, with $HLB_m$ = 5 of [SP80 & TW80].

An Experimental Study on the Quality of Concrete with Municipal Solid Waste Incineration Ash (쓰레기 소각재 사용 콘크리트의 품질특성에 대한 실험적 연구)

  • Kim, Jae-Woo;Choi, Jae-Jin;Moon, Dae-Joong
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.2 no.4
    • /
    • pp.335-344
    • /
    • 2014
  • The Quality of municipal solid waste incineration ash (incineration ash) was analyzed for the purpose of the reusing for concrete material. The folwability and strength properties of concrete mixed with incinerator ash were investigated. CaO component was included more than 50% in chemical component of incinerator ash, mean size of 50% accumulated particle distribution of incinerator ash was about $25{\mu}m$. Particle shape of incinerator ash ($IA_1$) was massed the round shape with fine particle, particle shape of incinerator ash ($IA_2$) was piled up the sheet shape according to manufacture procedure. The Quality of concrete was effected by use of incinerator ash. When the incinerator Ash ($IA_2$) was used, slum of concrete was increased and dosage of high range water reducing agent was reduced. However, strength development of concrete was decreased. Dosage of high range water reducing agent was increased by combined use of incinerator ash ($IA_2$) and diatomite powder, but strength development of concrete was improved. Ratio of compressive strength and tensile strength was in the range 85%~105% of CEB-FIP model code.

Control of YAG($Y_{3}Al_{5]O_{12}$) Particle Shape prepared by Sol-Gel Process (솔-젤 공정(工程)을 이용(利用)하여 제조(製造)된 YAG($Y_{3}Al_{5}O_{12}$) 분말 입형제어)

  • Park, Jin-Tae;Kim, Chul-Joo;Yoon, Ho-Sung;Sohn, Jung-Soo
    • Resources Recycling
    • /
    • v.17 no.5
    • /
    • pp.52-59
    • /
    • 2008
  • Sol-gel process applied in this study was carried out by chelation of metal ions and citric acid. From the results of thermal gravimetric analysis and XRD analysis of gel powder obtained through sol-gel and heat treatment, gel powders are mostly amorphous, and crystallize completely at $900^{\circ}C$, and the crystalline structure of YAG increases with increasing calcinations temperature. Since YAG prepared by sol-gel & calcinations process was porous, and the sape and size was irregular and nonuniform, the shape and size of YAG powder had to be controlled. Therefore the effects of organic materials such as ethylene glycol and surfactant on the crystalline structure of YAG powder were investigated. Polyesterification of ethylene glycol and citric acid separated reaction area of metal ions in the solution and decreased the size of YAG primary particles. The addition of Igepal 630 as surfactant formed the droplet in the solution, and increased the size of primary particles which forms the aggregate of YAG In order to obtain monodispersed YAG particles of uniform size, gel powder prepared with organic materials had to be milled before calcination. And milling process was very important for obtaining YAG of uniform size.

Synthesis and Characterization of Ultrafine $\beta$-SiC Powder by Vapor Phase Reaction (기상합성법에 의한 $\beta$-SiC 초미분말 합성 및 특성)

  • 어경훈;이승호;유용호;소명기
    • Journal of the Korean Ceramic Society
    • /
    • v.35 no.11
    • /
    • pp.1190-1196
    • /
    • 1998
  • Ultrafine ${\beta}$-SiC powders were synthesized by the vapor phase reaction of TMS[Si(CH3)4] in hydrogen The reaction temperature and TMS concentration were varied from 1000 to 1400$^{\circ}C$ and from 1 to 10% respectively. The average particle size and phase of the powders were analyzed by TEM and XRD. Ultrafine ${\beta}$-SiC powders were synthesized above 1000$^{\circ}C$ and the crystallinity of the powders increased with increasing reaction temperature. Shape of the particles were spherical and had average size of about 20 nm which showed no difference as the reaction temperature and TMS concentration increased. From the FT-IR analysis the absorption bands of Si-C of the powders shifted to higher wavenumber as the reaction temperature increased,. Under the condition of total gas flow above 1500cc/min ${\beta}$-SiC and poly-Si powders were obtained simultaneously. The Si-O bond intensity was increased under the condition of total gas flow rate above 1000cc/min which might be due to oxidation formed on poly-Si.

  • PDF

Synthesis of iron oxide powders by hydrothermal process

  • Bae, Dong-Sik;Park, Chul-Won;Gam, Jig-Sang;Han, Kyong-Sop
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.11 no.4
    • /
    • pp.176-179
    • /
    • 2001
  • Iron oxide powders were prepared under high temperature (up to $175^{\circ}C$) and pressure conditions( up to 129 pasi) by precipitation from metal nitrates with aqueous potassium hydroxide. Various types of iron oxide powders were obtained at different conditions. The size and the shape of the particles can be controlled as afunction of starting solution pH. The average particles size of the synthesized iron oxide powders increased, the particle shapes of the powders became fibrous, and the crystalline phase of the powder changes from iron oxide to iron hydroxide with increasing solution pH. The effects of synthesis parameters are discussed.

  • PDF

Preparation of Monodispersed $SiO_2/ZnO$ Composite Fine Powders by Sol-Gel Method (졸-겔법엔 의한 단분산 $SiO_2/ZnO$ 복합미립자의 졔조)

  • Lee, Chang-Woo;Shim, Won;Hahm, Yeong-Min;Hur, Yun-Haeng
    • Journal of environmental and Sanitary engineering
    • /
    • v.13 no.3
    • /
    • pp.58-65
    • /
    • 1998
  • Monodispersed $SiO_2/ZnO$ composite fine powders were prepared by Sol-Gel processing and their surface electrical and UV absorbance properties were investigated. Pseudomorph ZnO fine powders were microcapsuled by $SiO_2/ZnO$ sol fabricated using TEOS[tetraethylorthosilicate, purity 98% and ethanol as a solvent with $NH_3$ catalyst. The effects of experimental parameters such as molar ratio of starting materials on the final particle size and shape of $SiO_2/ZnO$ composite fine powder were discussed. As a result, we could controlled the size of monodispersed $SiO_2/ZnO$ composite fine powders without agglomeration, as well as the good dispersibility in aquous solution. The prepared powders were observed to have the mean particle sizes of $0.26-0.78{\mu}m$ with standard deviations of $0.020-0.063{\mu}m$.

  • PDF

The Investigation of Reaction Parameters on the Reactivity in the Preparation of SiC by SHS (자전연소합성법에 의한 SiC 분말 제조시 반응변수의 영향)

  • Shin, Chang-Yun;Won, Hyung-Il;Nersisyan, Hayk;Won, Chang-Whan
    • Journal of the Korean Ceramic Society
    • /
    • v.43 no.7 s.290
    • /
    • pp.427-432
    • /
    • 2006
  • The preparation of SiC powder by SHS in the system of $SiO_2-Mg-C$ was investigated in this study. The effects of various processing parameters such as the initial pressure of inert gas in reactor, the content of Mg and C in mixture and the size of $SiO_2$ particles on the synthesis of SiC by SHS methode were investigated. The minimum initial pressure of inert gas in reactor for SHS reaction in this system was 5 atm, and as the pressure increased, and the concentration of unreacted Mg decreased. At 50 atm of the initial inert gas pressure in reactor, the optimum composition for the preparation of pure SiC was $SiO_2+2.5Mg+1.2C$. SiC powder synthesized in this condition had a mixture of ${\alpha}-SiC\;and\;{\beta}-SiC$ with an irregular shape and the particle size of $0.5{\sim}0.8{\mu}m$.

Effect of Reaction Factors on the Properties of Complex Oxide Powder Produced by Spray Roasting Process (분무배소법에 의해 생성되는 복합산화물 분말들의 특성에 미치는 반응인자들의 영향)

  • 유재근;이성수;박희범;안주삼;남용현;손진군
    • Resources Recycling
    • /
    • v.9 no.4
    • /
    • pp.16-27
    • /
    • 2000
  • In order to produce raw material powder of advanced magnetic material by spray roasting process, newly modified spray roasting system was developed in this work. In this spray roasting system, raw material solution was effectively atomized and sprayed into the reaction furnace. Also, uniform temperature distribution inside reaction furnace made thermal decomposition process fully completed, and produced powder was effectively collected in cyclone and bag filter. This system equipped with apparatus which can purify hazard produced gas. In this study complex acid solution was prepared by dissolution of mill scale and ferro-Mn into the acid solution, and the pH of this complex acid solution was controlled about to 4. It was conformed that mill scale and ferro-Mn containing a lot of impurities such as $SiO_2$, P and Al could be used as raw material by reducing the impurities content of complex acid solution below 20 ppm. Complex oxide powder of Fe-Mn system was produced by spraying purified complex acid solution into the spray roaster through nozzle, and the variations of produced powder characters were studied by changing he reaction conditions such as reaction temperature, the injection velocity of solution and air, nozzle tip size and concentration of solution. The morphology of produced powder had spherical shape under the most experimental conditions, and concentration of solution. The morphology of produced powder has spherical shape under the most experimental conditions, and the composition and the particle size distribution were almost uniform, which tells the excellence of this spray roasting system. The grain size of most produced powder was below 100 nm. From the above results, it will be possible to produce ultra fine oxide powder from the chloride of Fe, Mn, Ni, Cu and rare earth by using this spray roasting system, and also to produce ultra fine pure metal powder by changing reaction atmosphere.

  • PDF

Comparing Thermal and Chemical Decomposition of Up-Cycled Ammonium Paratungstate(APT) (업싸이클링된 암모늄 파라텡스텐의 열적 및 화학적 분해법 비교)

  • Chung, Jun-Ki;On, Jin-Ho;Kim, Sung-Jin;Park, Sang-Yeup
    • Korean Journal of Materials Research
    • /
    • v.25 no.6
    • /
    • pp.274-278
    • /
    • 2015
  • The possibility of using the chemical precipitation method of up-cycled ammonium paratungstate (APT) was studied and compared with the thermal decomposition method. $WO_3$ particles were synthesized by chemical precipitation method using a 1:2 weight ratio of APT: Di-water. For thermal decomposition, APT powder was heated for 4h at $600^{\circ}C$ in air atmosphere. The reaction products were characterized by X-ray diffraction (XRD), X-ray fluorescence spectrometer (XRF), particle size analyzer (PSA), and field emission-scanning electron microscopy (FE-SEM). Thermogravimetric analysis (TGA) of the up-cycled APT allowed for the identification of the sequence of decomposition and reduction reactions that occurred during the heat treatment. TGA data indicated a total weight loss of 10.78% with the reactions completed in $658^{\circ}C$. The XRD results showed that APT completely decomposed to $WO_3$ by thermal decomposition and chemical precipitation. The particle size of the synthesized $WO_3$ powders by thermal decomposition with 2 h of planetary milling was around $2{\mu}m$ During the chemical precipitation process, the particle size of the synthesized $WO_3$ powders showed a round-shape with ${\sim}0.6{\mu}m$ size.

Direct Preparation of Fine Nickel Powder by Slurry Reduction Method for MLCC (슬러리환원법에 의한 MLCC용 미세 니켈 분말 직접 제조)

  • Shin, Gi-Wung;Ahn, Jong-Gwan;Kim, Dong-Jin;Kim, Sang-Bae;Ahn, Jea-Woo
    • Journal of the Mineralogical Society of Korea
    • /
    • v.23 no.3
    • /
    • pp.191-197
    • /
    • 2010
  • Fine nickel metal powder of uniform morphology, narrow size distribution, and high purity was prepared from high purity metal solution. Slurry reduction method for the synthesis of metal powder was applied with a special interest in their fine and spherical shape. The products were characterized by scanning electron microscopy (SEM) and X-ray diffraction (XRD). Well dispersed ultrafine nickel powder with the particle size range of 100~200 nm was produced from Ni-hydrazine precursor using hydrazine as a reductant for 90 min reaction in 4.5 M NaOH solution.