• 제목/요약/키워드: porous aluminum oxide

검색결과 79건 처리시간 0.036초

The Effect of Catalysts merged with alumina on the Growing Characteristics of Carbon Nanotubes using AAO templates

  • Lee, In-Wha;Lee, Tae-Young;Yang, Ji-Hoon;Ha, Byoung-Ho;Yoo, Ji-Beom;Kim, Seong-Kyu;Park, Chong-Yun
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2002년도 International Meeting on Information Display
    • /
    • pp.697-700
    • /
    • 2002
  • Porous anodic aluminum oxide(AAO) templates prepared by anodizing method were used for growing multiwalled carbon nanotubes(CNTs). AAO templates with the homogeneous pore diameter and length were obtained by two step anodizing technique. Using AAO templates, vertically well-ordered two-dimensional carbon nanotube arrays were fabricated. We investigated the field emission property of CNTs grown using different catalyst metals in vacuum chamber (<$10^{-7}$ Torr) on AAO Template. To explain the different emission property, the surface reaction between catalysts and alumina pores which inserted carbon species of $C_2H_2$ using High resolution transmission electron microscopy (HRTEM) was studied.

  • PDF

Magnetic Interaction in FeCo Alloy Nanotube Array

  • Zhou, D.;Wang, T.;Zhu, M.G.;Guo, Z.H.;Li, W.;Li, F.S.
    • Journal of Magnetics
    • /
    • 제16권4호
    • /
    • pp.413-416
    • /
    • 2011
  • An array of FeCo nanotubes has been successfully fabricated in the pores of porous anodic aluminum oxide (AAO) templates by wetting templates method. The morphology and structure of the nanotube array were characterized by scanning electron microscopy, transmission electron microscopy and x-ray diffraction. The average diameter of the nanotubes was about 200 nm, and the length was more than 10 ${\mu}m$. Vibrating sample magnetometer and superconducting quantum interference device were used to investigate the magnetic properties of the nanotube array. Interaction between the nanotubes has been found to be demagnetizing as expected and the switching field distribution is broad.

Fabrication and Magnetic Properties of Co Nanostructures in AAO Membranes

  • Jung, J.S.;Malkinski, L.;Lim, J.H.;Yu, M.;O'Connor, C.J.;Lee, H.O.;Kim, E.M.
    • Bulletin of the Korean Chemical Society
    • /
    • 제29권4호
    • /
    • pp.758-760
    • /
    • 2008
  • Nanoporous AAO (Anodic Aluminum Oxide) membranes have many advantages as a template for variety of magnetic materials. Materials can be embedded into the pores by electrodeposition, sputtering or magnetic-field-assisted infiltration of magnetic nanoparticles. This work focuses on the fabrication of the magnetic structures in the AAO templates by electrodeposition. Our method allows the controlled growth of Co nanostructures within the porous alumina membrane in the form of dots, rods and long wires. The shape of Co nanostructures has been investigated by field emission scanning electron microscope (FESEM). The magnetic hysteresis loops of Co nanostructures were measured using SQUID at 5 K and 300 K. The magnetic properties of the Co nanostructures are proportional to their aspect ratios and can be controlled by changing the aspect ratios.

시편의 준비 방법 및 접촉저항이 알루미늄 합금의 아노다이징 피막 형성에 미치는 영향 (Effects of Specimen Preparation Method and Contact Resistance on the Formation of Anodizing Films on Aluminum Alloys)

  • 문성모
    • 한국표면공학회지
    • /
    • 제53권1호
    • /
    • pp.29-35
    • /
    • 2020
  • In this study, five different specimen preparation methods were introduced and their advantages and disadvantages were presented. One of them, an epoxy mounting method has advantages of constant exposure area, ease of surface preparation without touching the specimen surface during polishing or cleaning, use of small amount of material and ease of specimen reuse by polishing or etching. However, in order to eliminate unexpected errors resulting from preferable reaction at the specimen/epoxy interface and contact resistance between the specimen and copper conducting line for electrical connection, it is recommended to cover the wall side of the specimen with porous anodic oxide films and to remain the contact resistance lower than 1 ohm. The increased contact resistance between the specimen and Cu conducting line appeared to result in increases of anodizing voltage and solution temperature during anodizing by which thickness and hardness of anodizing film on Al2024 alloy were drastically decreased and color of the films became more brightened.

PVA 용액법과 국산 산화알루미늄을 적용하여 대기 플라즈마 용사법으로 합성된 구형의 YAG:Ce3+ 형광체의 발광특성 (Optical Properties of Spherical YAG:Ce3+ Phosphor Powders Synthesized by Atmospheric Plasma Spraying Method Appling PVA Solution Route and Domestic Aluminium Oxide Seed)

  • 김용현;이상진
    • 한국분말재료학회지
    • /
    • 제30권5호
    • /
    • pp.424-430
    • /
    • 2023
  • YAG phosphor powders were fabricated by the atmospheric plasma spraying method with the spray-dried spherical YAG precursor. The YAG precursor slurry for the spray drying process was prepared by the PVA solution chemical processing utilizing a domestic easy-sintered aluminum oxide (Al2O3) powder as a seed. The homogenous and viscous slurry resulted in dense granules, not hollow or porous particles. The synthesized phosphor powders demonstrated a stable YAG phase, and excellent fluorescence properties of approximately 115% compared with commercial YAG:Ce3+ powder. The microstructure of the phosphor powder had a perfect spherical shape and an average particle size of approx imately 30 ㎛. As a result of the PKG test of the YAG phosphor powder, the synthesized phosphor powders exhibited an outstanding luminous intensity, and a peak wavelength was observed at 531 nm.

황산 용액에서 Al6061 합금의 아노다이징 피막 형성거동 (Formation Behavior of Anodic Oxide Films on Al 6061 Alloy in Sulfuric Acid Solution)

  • 문성모;정기훈;임수근
    • 한국표면공학회지
    • /
    • 제51권6호
    • /
    • pp.393-399
    • /
    • 2018
  • Formation behavior of aluminum anodic oxide (AAO) films on Al6061 alloy was studied in view of thickness, morphology and defects in the anodic films in 20 vol.% sulfuric acid solution at a constant current density of $40mA/cm^2$, using voltage-time curve, observation of anodized specimen colors and surface and cross-sectional morphologies of anodic films with anodization time. With increasing anodizing time, voltage for film formation increased exponentially after about 12 min and its increasing rate decreased after 25 min, followed by a rapid decrease of the voltage after about 28 min. Surface color of anodized specimen became darker with increasing anodizing time up to about 20 min, while it appeared to be brighter with increasing anodizing time after 20 min. The darkened and brightened surfaces with anodizing time are attributed to an increase in thickness of porous anodic oxide film and a chemical damage of the films due to heat generated by increased resistance of the film, respectively. Cross-sectional observation of AAO films revealed the formation of defects of crack shape at the metal/oxide interface after 15 min which prevents the growth of AAO films. Width and length of the crack-like defect increased with anodizing time up to 25 min of anodizing, and finally the outer part of AAO films was partly dissolved or detached after 30 min of anodizing, resulting in non-uniform surface structures of the AAO films.

Removal of Anodic Aluminum Oxide Barrier Layer on Silicon Substrate by Using Cl2 BCl3 Neutral Beam Etching

  • 김찬규;연제관;민경석;오종식;염근영
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2011년도 제40회 동계학술대회 초록집
    • /
    • pp.480-480
    • /
    • 2011
  • 양극산화(anodization)는 금속을 전기화학적으로 산화시켜 금속산화물로 만드는 기술로서 최근 다양한 크기의 나노 구조를 제조하는 기술로 각광받고 있으며, 이러한 기술에 의하여 얻어지는 anodic aluminum oxide(AAO)는 magnetic data storage, optoelectronic device, sensor에 적용될 수 있는 nano device 뿐만 아니라 nanostructure를 제조하기 위한 template 및 mask로써 최근 광범위 하게 연구되고 있다. 또한, AAO는 Al2O3의 단단한 구조를 가진 무기재료이므로 solid mask로써 다른 porous materials 보다 뛰어난 특성을 갖고 있다. 또한 electron-beam lithography 및 block co-polymer 에 의한 patterning 과 비교하여 매우 경제적이며, 재현성이 우수할 뿐만 아니라 대면적에서 나노 구조의 크기 및 형상제어가 비교적 쉽기 때문에 널리 사용되고 있다. 그러나, AAO 형성 시 생기게 되는 반구형 모양의 barrier layer는 물질(substance)과 기판과의 direct physical and electrical contact을 방해하기 때문에 해결해야 할 가장 큰 문제점 중 하나로 알려져 있다. 따라서 본 연구에서는 실리콘 기판위의 형성된 AAO의 barrier layer를 Cl/BCl3 gas mixture에서 Neutral Beam Etching (NBE)과 Ion Beam Etching (IBE) 로 각각 식각한 후 그 결과와 비교하였다. NBE와 IBE 모두 Cl2/BCl3 gas mixture에서 BCl3 gas의 첨가량이 60% 일 경우 etch rate이 가장 높게 나타났고, optical emission spectroscopy (OES)로 Cl2/BCl3 플라즈마 내의 Cl radical density와 X-ray photoelectron spectroscopy (XPS)로 AAO 표면 위를 관찰한 결과 휘발성 BOxCly의 형성이 AAO 식각에 크게 관여함을 확인 할 수 있었다. 또한, NBE와 IBE 실험한 다양한 Cl2/BCl3 gas mixture ratio 에서 AAO가 식각이 되지만, 이온빔의 경우 나노사이즈의 AAO pore의 charging에 의해 pore 아래쪽의 위치한 barrier layer를 어떤 식각조건에서도 제거하지 못하였다. 하지만, NBE에서는 BCl3-rich Cl2/BCl3 gas mixture인 식각조건에서 AAO pore에 휘발성 BOxCly를 형성하면서 barrier layer를 제거할 수 있었다.

  • PDF

다공성 알루미나 템플레이트를 이용한 고분자 나노 구조 필름의 제조 및 응용 (Applications and Preparation of Nanostructured Polymer Films by Using a Porous Alumina Template)

  • 이준호;최진규;안명수;박은주;성상도;이한섭;최진섭
    • 공업화학
    • /
    • 제20권6호
    • /
    • pp.586-592
    • /
    • 2009
  • 나노 크기의 배향성을 갖는 구조물의 제작은 자연에 존재하는 여러 가지 형상의 모방을 가능하게 한다. 고분자는 가격이 매우 저렴하며 합성과 가공 그리고 그 구조가 잘 알려져 있는 장점을 갖고 있어 필름(film)의 표면에 이러한 나노 구조물을 제작하고 나노 구조의 특성을 발현하는데 손쉽게 활용할 수 있는 재료이다. 나노 구조물을 제작하는 방법 중 양극산화를 통하여 제작한 다공성 알루미나 템플레이트(porous alumina template)는 매우 규칙적으로 정렬되어 있고 제어하는 공정이 비교적 쉽고 경제적이기 때문에 이를 이용한 연구가 매우 활발하게 진행되고 있다. 본 총설에서는 양극산화 알루미나 템플레이트의 제작과 이를 이용한 나노 구조 고분자 필름의 제작을 설명하고 이러한 나노 구조 필름의 응용범위 및 응용에 필요한 특성에 대하여 기술하였다.

폐암 바이오마커 검출용 나노SPR 바이오센서 (Nano SPR Biosensor for Detecting Lung Cancer-Specific Biomarker)

  • 장은윤;염세혁;엄년식;한정현;김형경;신용범;강신원
    • 센서학회지
    • /
    • 제22권2호
    • /
    • pp.144-149
    • /
    • 2013
  • In this research, we developed a biosensor to detect lung cancer-specific biomarker using Anodic Aluminum Oxide (AAO) chip based on interference and nano surface plasmon resonance (nanoSPR). The nano-porous AAO chip was fabricated $2{\mu}m$ of pore-depth by two-step anodizing method for surface uniformity. NanoSPR has sensitivity to the refractive index (RI) of the surrounding medium and also provides simple and label-free detection when specific antibodies are immobilized to the Au-deposited surface of nano-porous AAO chip. To detect the lung cancer-specific biomarker, antibodies were immobilized on the surface of the chip by Self Assembled Monolayer (SAM) method. Since then lung cancer-specific biomarker was applied atop the antibodies immobilized layer. The specific reaction of the antigen-antibody contributed to the change in the refractive index that cause shift of resonance spectrum in the interference pattern. The Limit of Detection (LOD) was 1 fg/ml by using our nano-porous AAO biosensor chip.

Fabrication of Photo Sensitive Graphene Transistor Using Quantum Dot Coated Nano-Porous Graphene

  • 장야무진;이재현;최순형;임세윤;이종운;배윤경;황종승;황성우;황동목
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2013년도 제44회 동계 정기학술대회 초록집
    • /
    • pp.658-658
    • /
    • 2013
  • Graphene is an attractive material for various device applications due to great electrical properties and chemical properties. However, lack of band gap is significant hurdle of graphene for future electrical device applications. In the past few years, several methods have been attempted to open and tune a band gap of graphene. For example, researchers try to fabricate graphene nanoribbon (GNR) using various templates or unzip the carbon nanotubes itself. However, these methods generate small driving currents or transconductances because of the large amount of scattering source at edge of GNRs. At 2009, Bai et al. introduced graphene nanomesh (GNM) structures which can open the band gap of large area graphene at room temperature with high current. However, this method is complex and only small area is possible. For practical applications, it needs more simple and large scale process. Herein, we introduce a photosensitive graphene device fabrication using CdSe QD coated nano-porous graphene (NPG). In our experiment, NPG was fabricated by thin film anodic aluminum oxide (AAO) film as an etching mask. First of all, we transfer the AAO on the graphene. And then, we etch the graphene using O2 reactive ion etching (RIE). Finally, we fabricate graphene device thorough photolithography process. We can control the length of NPG neckwidth from AAO pore widening time and RIE etching time. And we can increase size of NPG as large as 2 $cm^2$. Thin CdSe QD layer was deposited by spin coatingprocess. We carried out NPG structure by using field emission scanning electron microscopy (FE-SEM). And device measurements were done by Keithley 4200 SCS with 532 nm laser beam (5 mW) irradiation.

  • PDF