PMW-PNN-PZT 세라믹스의 Bismuth 치환에 따른 미세구조 및 압전 특성 (Microstructure and Piezoelectric Properties of PMW-PNN-PZT Ceramics with Bismuth Substitution)

  • 김용진;류주현;신동찬
    • 한국전기전자재료학회논문지
    • /
    • 제29권6호
    • /
    • pp.332-336
    • /
    • 2016
  • In this study, in order to develop the composition ceramics for ultrasonic sensor with high $d_{33}*g_{33}$, $Pb_{1-3x/2}Bix(Mg_{1/2}W_{1/2})_{0.03}(Ni_{1/3}Nb_{2/3})_{0.09}(Zr_{0.5}Ti_{0.5})_{0.88}O_3$(PMW-PNN-PZT) system ceramics were prepared using CuO as sintering aids. And then, their microstructure, piezoelectric and dielectric characteristics were systemetically investigated with bismuth substitution. The PMW-PNN-PZT ceramic specimens could be sintered at sintering temperature of $940^{\circ}C$ by adding sintering aids. At x=0.015 specimen, the density, electromechanical coupling factor($k_p$), dielectric constant, piezoelectric constant($d_{33}$) and piezoelectric figure of merit($d_{33}*g_{33}$) indicated the optimal properties of $7.90g/cm^3$, 0.67, 2,511, 628 pC/N, and $17.7pm^2/N$, respectively, for duplex ultrasonic sensor application.

PLD법으로 제작된 xPb(Al0.5Nb0.5)O3-(1-x)Pb(Zr0.52Ti0.48)O3박막의 유전 및 압전 특성 (Dielectric and Piezoelectric Properties of xPb(Al0.5Nb0.5)O3-(1-x)Pb(Zr0.52Ti0.48)O3 Thin films Prepared by PLD)

  • 김민철;박용욱;최지원;강종윤;안병국;김현재;윤석진
    • 한국전기전자재료학회논문지
    • /
    • 제16권9호
    • /
    • pp.795-800
    • /
    • 2003
  • The dielectric and piezoelectric properties of the xPb(A $l_{0.5}$N $b_{0.5}$) $O_3$-(1-x)Pb(Z $r_{0.52}$ $Ti_{0.48}$) $O_3$ [xPAN-(1-x)PZT] thin films by pulsed laser deposition (PLD) were investigated as a function of PAN contents. The effect of texture on dielectric and piezoelectric properties of the 0.05PAN-0.95PZT thin films having the highest piezoelectric constant( $d_{33}$) was studied more precisely. For 0$\leq$x$\leq$0.15 compositions in xPAN-(1-x)PZT thin films, the well-developed perovskite phase with (111) preferred orientation was obtained at the deposition temperature of 50$0^{\circ}C$. With increasing PAN content, remanent polarization and coercive field decreased. The dielectric constant increased with an increase of PAN content until it reached 1450 at $\chi$= 0.05, and then decreased for higher PAN content. The maximum points of dielectric constant coincides with the maximum points of the piezoelectric constant $d_{33}$.33/.33/././.

PZT/PVDF O-3형 복합전체에 있어서 PZT 체적비 변화가 유전 및 압전특성에 미치는 영향 (Effects on PZT volume fraction on the dielectric and piezoelectric properties with PZT/PVDF O-3 composites)

  • 이덕출;김용혁
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제1권1호
    • /
    • pp.44-53
    • /
    • 1988
  • In this study, PZT/PVDF composites with O-3 phase connectivity were prepared by hot pressing method, and the dielectric and piezoelectric properties as a function of PZT volume fraction were investigated. A modified cubic model was introduced to explain the influence of the PZT volume fraction on the experimentally determined dielectric constant. As A n=0.125, the measured dielectric constant values agreed with the calculated values. It was found that dielectric constant .xi.$_{33}$ and piezoelectric coefficient d$_{33}$ increased with indreasing PZT volume fraction, and hydrostatic piezoelectric figure of merit d/aub h/.g$_{h}$ was improved relative to that of the PZT single phase material.l.l.l.

  • PDF

BaCO3첨가량에 따른 PAN-PZI계 세라믹스의 압전 및 유전특성 (Piezoelectric and Dielectric Characteristics of PAN-PZT Ceramics with BaCO3Addition)

  • 박타리;이동균;최지원;강종윤;김현재;윤석진;고태국
    • 한국전기전자재료학회논문지
    • /
    • 제15권4호
    • /
    • pp.356-360
    • /
    • 2002
  • The piezoelectric properties of $0.05Pb(Al_{0.5}Nb_{0.5})O_3-0.95Pb(Zr_{0.52}Ti_{0.48})O_3+0.7wt%Nb_2O_5+o.5wt%MnO_2$ ceramics with the additive of BaCO$_3$were investigated. As the addition of BaCO$_3$increased from 0 to 0.4 wt%, the dielectric constant ($\epsilon^T _{33}$), piezoelectric constant ($d_33$), electromechanical coupling factor ($k_p$), and mechanical quality factor ($Q_m$) increased, while the dielectric loss ($tan\delta$) decreased. The highest piezoelectric and dielectric properties were observed at $1200^{\circ}C$ of the sintered temperature with 0.4 wt% of $BaCO_3$, and the properties of $d_33$, $k_p$, and $Q_m$ were 339 pC/N, 60% and 1754, respectively.

고에너지 밀링에 따른 PMN-PNN-PZT 세라믹의 유전 및 압전 특성 (Piezoelectric and Dielectric Properties of PMN-PNN-PZT Ceramic according to the High Energy Ball Milling)

  • 이유형;류주현;백동수
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.203-204
    • /
    • 2008
  • In this study, in order to develop the multilayer piezoelectric actuator and ultrasonic resonator, PMN-PNN-PZT ceramics were fabricated by the variations of ball size at sintering temperature of $900^{\circ}C$ and their piezoelectric and dielectric characteristics were investigated as a function of the variations of ball size. When the ball size was 3mm$\phi$, density, dielectric constant$({\varepsilon}r)$, electromechanical coupling factor(kp) and piezoelectric d constant$(d_{33})$ were increased. At the ball size of 3mm$\phi$, the specimen showed the optimum values of density=7.909g/$cm^3$, kp=0.592, Qm=1292, $d_{33}$=368pC/N, $\varepsioln_r$=1502, respectively.

  • PDF

PMN-PZ-PT 세라믹스를 이용한 적층형 액츄에이터의 변위특성 (Electric-Field-Induced Strain Properties of Multi Layer Ceramic Actuator Using PMN-PZ-PT Ceramics)

  • 하문수;정순종;고중혁;송재성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 하계학술대회 논문집 Vol.4 No.2
    • /
    • pp.620-623
    • /
    • 2003
  • Non-linear behaviors of multilayer piezoelectric ceramic actuator (MCA) were investigated under electrical and mechanical stress. DC 100 V bias was applied to the MCA to obtain displacement. Laser vibrometer, which using Doppler effect, was employed to characterize displacement caused by $d_{33}$ mode of MCA. To understand this non-linear behavior of MCA, displacement was measured and compared under different load states. By increasing load, electric field-induced strain and piezoelectric constant($d_{33}$) of MCA was decreased. We attribute this phenomenon to the domain wall motion and depoling of MCA under heavy load.

  • PDF

온도 및 압축응력 변화에 따른 PIN-PMN-PT 단결정의 유전 및 압전 특성 (Effect of Temperature and Compressive Stress on the Dielectric and Piezoelectric Properties of PIN-PMN-PT Single Crystal)

  • 임재광;박재환;이정호;이상구
    • 마이크로전자및패키징학회지
    • /
    • 제26권4호
    • /
    • pp.63-68
    • /
    • 2019
  • 온도 및 압축응력 변화에 따른 PIN-PMN-PT계 압전 단결정의 유전 특성과 압전 특성을 조사하였다. 단결정의 결정상은 110℃ 영역에서 강유전 rhombohedral 구조에서 tetragonal 구조로, 190℃ 영역에서 tetragonal 구조로부터 상유전 cubic 구조로 변화하였다. 전계 인가에 따른 분극 및 변위의 변화율로부터 압전상수와 비유전율을 계산하였으며, 이는 계측기로부터 측정된 값과 유사한 수준을 나타내었다. 샘플에 인가되는 압축응력이 증가할수록 압전상수 d33과 비유전율값은 증가하는 경향성을 나타내었다. 측정 온도 5℃에서 샘플에 인가되는 압축응력이 60 MPa인 경우 d33 값이 4500 pC/N로 계산되었으며, 측정 온도 60℃인 경우, 샘플에 인가되는 압축응력이 40 MPa 일 때 비유전율 62000이 계산되었다. 압축응력이 높아질 때 압전상수와 비유전율 값이 상승한 것은 rhombohedral 상에서 orthorhombic 상으로의 전이에 기인한 것으로 판단된다.

SnO2가 첨가된 저온소결 (Na,K,Li)(Nb,Sb,Ta)O3계 세라믹스의 유전 및 압전 특성 (Dielectric and Piezoelectric Properties of Low Temperature Sintering (Na,K,Li)(Nb,Sb,Ta)O3 Ceramics Doped with SnO2)

  • 이광민;류주현;이지영
    • 한국전기전자재료학회논문지
    • /
    • 제28권11호
    • /
    • pp.690-693
    • /
    • 2015
  • In this paper, in order to develop excellent Pb-free composition ceramics for ultrasonic sensor. The $SnO_2$-doped ($Na_{0.525}K_{0.443}Li_{0.037})(Nb_{0.883}Sb_{0.08}Ta_{0.037})O_3$)(abbreviated as NKL-NST) ceramics have been synthesized using the ordinary solid state reaction method. The effect of $SnO_2$-doping on their dielectric and piezoelectric properties was investigated. The ceramics doped with 0 wt% $SnO_2$ have the optimum values of piezoelectric constant($d_{33}$), piezoelectric figure of merit($d_{33}.g_{33}$), planar piezoelectric coupling coefficient($k_p$) and density : $d_{33}=195[pC/N]$, $d_{33}.g_{33}=5.62pm^2/N.kp=0.40$, $density=4.436[g/cm^3]$. suitable for duplex ultrasonic sensor application.

Piezoelectric and Dielectric Properties of Low Temperature Sintered Pb(Mn1/3Nb2/3)0.02(Ni1/3Nb2/30.12(ZrxTi1-x)0.86O3 System Ceramics

  • Yoo, Ju-Hyun;Lee, Sang-Ho
    • Transactions on Electrical and Electronic Materials
    • /
    • 제10권4호
    • /
    • pp.121-124
    • /
    • 2009
  • In this study, in order to develop compositions of ceramics suitable for piezoelectric actuator and ultrasonic vibrator applications using low temperature sintering, multilayer, PMN-PNN-PZT ceramics were fabricated using $Li_2CO_3$ and $Na_2CO_3$ as sintering aids. Their structural, piezoelectric and dielectric characteristics were investigated according to the Zr/Ti ratio. As the Zr/Ti ratio increased, the electromechanical coupling factor $k_p$, and piezoelectric constant $d_{33}$ and the mechanical quality factor $Q_m$ all increased with Zr/Ti ratio and then decreased after the ratio exceeded 50/50. At the ratio of Zr/Ti =49/51 and sintering temperature of $900^{\circ}C$; the density, electromechanical coupling factor $k_p$, dielectric constant ${\varepsilon}_r$ piezoelectric $d_{33}$ constant and mechanical quality factor $Q_m$ all showed the optimum values of 7.900 $g/cm^3$, 0.576, 856, 312 pC/N, 1,326, respectively. These property values are very suitable for multilayer ceramics actuator applications.

BaTiO3 치환에 따른 NaNbO3-LiNbO3 세라믹스의 압전 및 유전특성 (Piezoelectric and Dielectric Properties of NaNbO3-LiNbO3 Ceramics according to the BaTiO3 Substitution)

  • 이상호;류주현;마석범;김성구
    • 한국전기전자재료학회논문지
    • /
    • 제22권3호
    • /
    • pp.205-209
    • /
    • 2009
  • In this study, in order to develop the composition ceramics for lead-free ultrasonic motor, (1-x-0.09)$NaNbO_{3-x}BaTiO_3-0,09LiNbO_3$ ceramics were fabricated using a conventional mixed oxide process and their piezoelectric and dielectric characteristics were investigated according to the $BaTiO_3$ substitution. All the specimens showed orthorhombic phase structure without secondary phase, $BaTiO_3$ substitution enhanced density, dielectric constant(${\epsilon}_r$) and electromechanical coupling factor($k_p$), However, mechanical quality factor was deteriorated. Curie temperature of specimens was observed as about $380^{\circ}C$. At the $BaTiO_3$ substitution of 4 mol%, density, electromechanical coupling factor($k_p$), dielectric constant(${\epsilon}_r$) and piezoelectric constant($d_{33}$) of specimen showed the optimum value of $4.493g/cm^3$, 0.236, 175, 70 pC/N, respectively.