• Title/Summary/Keyword: oxidation rate

Search Result 1,543, Processing Time 0.023 seconds

Influence of Oxidation Inhibitor on Carbon-Carbon Composites: 5. Studies on Anti-oxidation Properties of the Composites (산화억제제 첨가에 의한 탄소/탄소 복합재료의 물성에 관한 연구: 5. 탄소/탄소 복합재료의 내산화성 연구)

  • 박수진;서민강;조민석;이재락
    • Polymer(Korea)
    • /
    • v.24 no.2
    • /
    • pp.237-244
    • /
    • 2000
  • Phenolic resin used as a precursor of carbonized matrix for carbon-carbon composites was modified by addition of molybdenum disilicide (MoSi$_2$) in various concentrations of 0, 4, 12 and 20% by weight to improve the anti-oxidation properties of the composites. The green body was manufactured by a prepreg method and was submitted to carbonization up to 110$0^{\circ}C$. In this work, the oxidation behavior of carbon-carbon composites with MoSi$_2$ as an oxidation inhibitor was investigated at the temperature range of 600-100$0^{\circ}C$ in an air environment. The carbon-carbon composites with MoSi$_2$ showed a significantly improved oxidation resistance due to both the reduction of the porosity formation and the formation of mobile diffusion barrier for oxygen when compared to those without MoSi$_2$. Carbon active sites should be blocked, decreasing the oxidation rate of carbon. This is probably due to the effect of the inherent MoSi$_2$ properties, resulted from a formation of the protective layer against oxygen attack in the composites studied.

  • PDF

CO Oxidation Activities of Ni and Pd-TiO2@SiO2 Core-Shell Nanostructures

  • Do, Yeji;Cho, Insu;Park, Yohan;Pradhan, Debabrata;Sohn, Youngku
    • Bulletin of the Korean Chemical Society
    • /
    • v.34 no.12
    • /
    • pp.3635-3640
    • /
    • 2013
  • We prepared Ni and Pd-modified $TiO_2@SiO_2$ core-shell nanostructures and then analyzed them by scanning electron microscopy, optical microscopy, X-ray diffraction crystallography, FT-IR and UV-Visible absorption spectroscopy. In addition, their CO oxidation performance was tested by temperature-programmed mass spectrometry. The CO oxidation activity showed an order of Ni-$TiO_2@SiO_2$ ($900^{\circ}C$) < Ni-$TiO_2@SiO_2$ ($90^{\circ}C$) < Ni-$TiO_2@SiO_2$ ($450^{\circ}C$) in the first CO oxidation run, and greatly improved activity in the same order in the second run. The $T_{10%}$ (the temperature at 10% CO conversion) corresponds to the CO oxidation rate of $2.8{\times}10^{-5}$ molCO $g{_{cat}}^{-1}s^{-1}$. For Ni-$TiO_2@SiO_2$ ($450^{\circ}C$), the $T_{10%}$ was observed at $365^{\circ}C$ in the first run and at $335^{\circ}C$ in the second run. For the Pd-$TiO_2@SiO_2$ ($450^{\circ}C$), the $T_{10%}$ was observed at a much lower temperature of $263^{\circ}C$ in the first CO oxidation run, and at $247^{\circ}C$ in the second run. The CO oxidation activities of transition metal modified $TiO_2@SiO_2$ core-shell nanostructures presented herein provide new insights that will be useful in developing catalysts for various environments.

Fabrication of Ultrathin Silicon Oxide Layer by Low Pressure Rapid Thermal Oxidation and Remote Plasma Oxidation (저압급속열산화법과 플라즈마확산산화법에 의한 실리콘 산화박막의 제조)

  • Ko, Cheon Kwang;Lee, Won Gyu
    • Korean Chemical Engineering Research
    • /
    • v.46 no.2
    • /
    • pp.408-413
    • /
    • 2008
  • In this work, the use of LPRTO (low pressure rapid thermal oxidation) and remote plasma oxidation was evaluated for the preparation of ultra thin silicon oxide layer with less than 5 nm. The silicon oxide thickness grown by LPRTO was rapidly increased and saturated. The maximum thickness could be controlled at about 5 nm. As RF power and oxygen flow rate at a remote plasma oxidation increased, the behavior of oxide growth was almost the same as that of LPRTO. The oxide thickness of 4 nm was the maximum obtained by a remote plasma oxidation in this work. The quality of silicon oxide grown by LPRTO was comparable to the thermally grown conventional oxide.

S-Thiolation and Oxidation of Glycogen Phosphorylase b and Peroxidation of Liposome Initiated by Free Radical Species

  • Lee, Kyu-Sun;Lee, Hyung-Min;Park, Young-Mee;Chang, Byeong-Doo;Chung, Tae-Young;Choi, Eun-Mi
    • BMB Reports
    • /
    • v.29 no.1
    • /
    • pp.81-87
    • /
    • 1996
  • The relationship of S-thiolation and oxidation of glycogen phosphorylase b and peroxidation of phosphatidyl choline liposome by xanthine oxidase (XOD), 2,2'-azobis(2-amidinopropane) hydrochloride (AAPH), and 2,2'-azobis(dimethylvaleronitrile) (AMVN)-generated free radicals was investigated, Glycogen phosphorylase b was S-thiolated in the presence of glutathione and oxidized in the absence of it by XOD, AAPH and AMVN. In XOD-initiated reaction, the rates of S-thiolation and oxidation of phosphorylase were very similar and addition of liposome to the reaction mixture showed little inhibition of the modifications. In AAPH-initiated reaction, the rate of oxidation was higher than that of S-thiolation and addition of liposome increased oxidation of the protein but had no effect on S-thiolation. In AMVN-initiated reaction, S-thiolation was higher than oxidation and addition of liposome increased S-thiolation remarkably but showed no effect on oxidation. The effect of liposome on modifications of protein in AAPH and AMVN reaction seemed to be caused by certain reactive degradation products or intermediates of liposome by free radical attack. Peroxidation of liposome was not observed in XOD-initiated reaction. Liposome was gradually peroxidized by AAPH reaction. The peroxidation was inhibited by addition of GSH and phosphorylase. Peroxidation of liposome by AMVN was extreamly fast, and was not affected by GSH and phosphorylase.

  • PDF

Decomposition of Humic Acid and Reduction of THM Formation Potential by Ozone and Combined Ozone/Ultraviolet Oxidation (오존 및 오존/UV 산화법을 이용한 휴믹산의 분해와 THM 발생능의 감소)

  • Park, Ju-Seok;Park, Tae-Jin;Kwon, Bong-Kee
    • Journal of Korean Society of Water and Wastewater
    • /
    • v.10 no.4
    • /
    • pp.55-63
    • /
    • 1996
  • This research was based on comparing ozonation with combined ozone/ultraviolet oxidation through the methods of reducing THM produced during water treatment. The results were as follows ; 1. The decline of THM concentration was appeared according as ozone dosage increases with ozonation and combined ozone/ultraviolet oxidation. The more effective method was the treatment of irradiating UV then ozonation. In the beginning of reaction the decline rate of THM formation potential was low, I thought it was because that the reaction of ozone and humic acid needed times to be steady state, or that THM formation potential existed according to humic acid. 2. The effect of combined ozone/ultraviolet oxidation when ozone dosage was 4.2mg/L min was almost the same that of ozonation when ozone dosage was 8.6mg/L min. 3. In experiment of TOC decline through ozonation and combined ozone/ultraviolet oxidation, TOC concentration was also dropped according to increasing ozone dosage and the more effective results were showed in treatment of irradiating UV than ozonation. But the similar TOC remove rates were showed in experiment of changing with ozone dosage during combined ozone/ultraviolet oxidation TOC remove rates were low in proportion to the remove rates of THM formation potential, it was considered that humic acid was made low molecule itself though ozonation and ozone/ultraviolet oxidation. Moreover, the high degree of remove efficiency will be get though the treatment of activated carbon of GAC treatment after combined ozone/ultravilet oxidation.

  • PDF

Removal of nitrogen and sulfur odorous compounds and their precursors using an electrolytic oxidation process (산화전리수를 이용한 질소와 황 계열 악취 및 악취전구물질의 제거)

  • Shin, Seung-Kyu;An, Hea-Yung;Kim, Han-Seung;Song, Ji-Hyeon
    • Journal of Korean Society of Water and Wastewater
    • /
    • v.25 no.2
    • /
    • pp.223-230
    • /
    • 2011
  • An electrolytic oxidation process was applied to remove odorous compounds from non-point odor sources including wastewater pipelines and manholes. In this study, a distance between the anode and the cathode of the electrolytic process was varied as a system operating parameters, and its effects on odor removal efficiencies and reaction characteristics were investigated. Odor precursors such as sediment organic matters and reduced sulfur/nitrogen compounds were effectively oxidized in the electrolytic process, and a change in oxidation-reduction potential (ORP) indicated that an stringent anaerobic condition shifted to a mild anoxic condition rapidly. At an electrode distance of 1 cm and an applied voltage of 30 V, a system current was maintained at 1 A, and the current density was 23.1 $mA/cm^{2}$. Under the condition, the removal efficiency of hydrogen sulfide in gas phase was found to be 100%, and 93% of ammonium ion was removed from the liquid phase during the 120 minute operating period. Moreover, the sulfate ion (${SO_4}^{2-}$) concentration increased about three times from its initial value due to the active oxidation. As the specific power consumption (i.e., the energy input normalized by the effective volume) increased, the oxidation progressed rapidly, however, the oxidation rate was varied depending on target compounds. Consequently, a threshold power consumption for each odorous compound needs to be experimentally determined for an effective application of the electrolytic oxidation.

High-Temperature Oxidation of Ti Containing Stainless Steel in O2-N2 Atmosphere

  • Onishi, Hidenori;Saeki, Isao;Furuichi, Ryusaburo;Okayama, Toru;Hanamatsu, Kenko;Shibayama, Tamaki;Takahashi, Heishichiro;Kikkawa, Shinichi
    • Corrosion Science and Technology
    • /
    • v.3 no.4
    • /
    • pp.140-147
    • /
    • 2004
  • High temperature oxidation of Fe-19Cr and Fe-19Cr-0.2Ti alloys is studied at 1173-1373 K in 16.5 kPa $O_2$ - balances $N_2$ atmosphere aimed at clarifying the effect of titanium addition. Oxidation rate of Fe-19Cr alloy was accelerated with titanium. For both alloys chromium rich $(Fe,\;Cr)_2O_3$ was formed as a major oxidation product. On Fe-19Cr-0.2Ti alloy, a thin layer composed of spinel type oxide and titanium oxide was also formed and an internal oxidation of titanium was observed. Titanium was concentrated at the oxide surface and internal oxidation zone but a small amount of titanium was also found in the intermediate corundum type $(Fe,\;Cr)_2O_3$ layer. Crystals of corundum type $(Fe,\;Cr)_2O_3$ formed on Fe-19Cr alloy are coarse but that formed on Fe-19Cr -0.2Ti alloys were fine and columnar. Reason for the difference in oxidation kinetics and crystal structure will be discussed relating to the distribution of aliovalent titanium in corundum type $(Fe,\;Cr)_2O_3$ oxide layer.

Oxidation-Deficient Silkworm Hemolymph as a Medium Supplement for Insect Cell Culture

  • Kim, Eun-Jeong;Park, Ji-Young;Kim, Sam-Eun;Park, Tai-Hyun
    • Biotechnology and Bioprocess Engineering:BBE
    • /
    • v.3 no.2
    • /
    • pp.87-90
    • /
    • 1998
  • Hemolymph is oxidized and darkens visibly during the collection from silkworm due to the activity of tyrosinase in it. Toxic quinones are produced by the oxidation and consequently inhibit the cell growth. Heat treatment can be used to prevent the oxidation ; however, the oxidation may occur during the collection of hemolymph before it is heat-treated. It makes the hemolymph collection difficult especially on a large-scale preparation. Hemolymphs collected from 257 different strains of silkworms were examined to select the slowly oxidized hemolymphs. Hemolymphs collected from mutant strains such as Lemone, TBO, Cre, Y4, and wEb showed relatively slow color changes. Oxidation rates of the hemolymphs were measured by the absorbance change using a spectrophotometer. The hemolymph of wEb showed the slowest oxidation. The absorbance of this mutant hemolymph reached the saturation value at 20$^{\circ}C$ in 450 min, whereas the total oxidation time of the wild-type (Baekokjam) hemolymph at the same temperature was 120 min. We tested if this mutant hemolymph is useful as a medium supplement for insect cell culture. Cell growth rate and final cell concentration in the medium supplemented with the wEb hemolymph were almost same as those in the medium supplemented with the wild-type hemolymph. Hemolymph is collected on a small scale by clipping the abdominal leg; however, this method is not appropriate fro large scale preparation. Centrifugation after chopping the silkworm hemolymph by a blending mixer is a more appropriate procedure for large scale collection. Slowly oxidized wEb hemolymph resulted in higher cell concentration than the wild-type hemolymph when hemolymph was collected by the large scale preparation method.

  • PDF

Characteristics of Microbial Arsenic Oxidation under Denitrification Environment (미생물에 의한 탈질 과정 동안의 비소 동시 산화 특성 평가)

  • Oh, Seolran;Kim, Dong-Hun;Moon, Hee Sun
    • Journal of Soil and Groundwater Environment
    • /
    • v.24 no.4
    • /
    • pp.1-10
    • /
    • 2019
  • Recently, groundwater contamination by mixed occurrence of arsenic (As) and nitrate ($NO_3{^-}$) has been a serious environmental issue all around world. In this study, we investigated the microbial As(III) oxidation characteristic under denitrification process to examine the feasibility of the microbial consortia in wetland sediment to simultaneously treat these two contaminants. The detail objectives of this study were to investigate the effects of $NO_3{^-}$ on the oxidation of As(III) in anaerobic environments and observe the microbial community change during the As oxidation under denitrification process. Results showed that the As(III) was completely and simultaneously oxidized to As(V) under denitrification process, however, it occurred to a much less extent in the absence of sediment or $NO_3{^-}$. In addition, the significant increase of As(III) oxidation rate in the presence of $NO_3{^-}$ suggested the potential of As oxidation under denitrification by indigenous microorganisms in wetland sediment. Genera Pseudogulbenkiania, and Flavisolibacter were identified as predominant microbial species driving the redox process. Conclusively, this study can provide useful information on As(III) oxidation under denitrifying environment and contribute to develop an effective technology for simultaneous removal of As(III) and $NO_3{^-}$ in groundwater.

Oxidation Behavior of the HVOF-sprayed $\textrm{Cr}_{3}\textrm{C}_{2}$-NiCr Coating Layer (HVOF 용사된 $\textrm{Cr}_{3}\textrm{C}_{2}$-NiCr 용사층의 산화 거동)

  • Kim, Byeong-Hui;Seo, Dong-Su
    • Korean Journal of Materials Research
    • /
    • v.8 no.8
    • /
    • pp.757-765
    • /
    • 1998
  • This study was performed to investigate the influence of fuel/oxygen ratio (F/O= 3.2, 3.0, 2.8) on the oxidation behavior of two kinds of (20wt%NiCr claded $\textrm{Cr}_{3}\textrm{C}_{2}$, and 7wt%NiCr mixed $\textrm{Cr}_{3}\textrm{C}_{2}$) composite powder with different manufacturing method. The results show that the oxidation behavior between the 20wt% NiCr claded $\textrm{Cr}_{3}\textrm{C}_{2}$ and 7wt% NiCr mixed $\textrm{Cr}_{3}\textrm{C}_{2}$ coating was widely different. The surface morphology of the coating composed of 7wt% NiCr mixed $\textrm{Cr}_{3}\textrm{C}_{2}$ was changed to porous with F/O ratio by the aggressive evolution of gas phases($\textrm{CO}_2$, CO and $\textrm{CrO}_3$) and the oxide cluster composed of Ni and Cr were grown after oxidation at $1000^{\circ}C$ for 50 hours. But the surface morphology of the coating composed of 20wt% NiCr claded $\textrm{Cr}_{3}\textrm{C}_{2}$ was not changed to porous after oxidation at $1000^{\circ}C$ for 50 hours. Therefore, the reason for high oxidation rate is due to activation of $\textrm{Cr}_{3}\textrm{C}_{2}$ to oxidation by entrapped oxygen gases within coating layer, and to closely relate with the decomposition of $\textrm{Cr}_{3}\textrm{C}_{2}$ to $\textrm{Cr}_{7}\textrm{C}_{3}$ phase. Accordingly, On the evidence of these results, the study about the oxidation behavoir of the HVOF sprayed $\textrm{Cr}_{3}\textrm{C}_{2}$ coating depending on hydrogen flow rate must be done.

  • PDF