THE EFFECT OF LIGATION METHOD ON THE FRICTIONAL FORGE BETWEEN ORTHODONTIC BRACKET AND ARCHWIRE (결찰양식이 교정용 브라켓과 교정선 사이의 마찰력에 미치는 영향)

  • Shin, Hyun-Jeong;Kwon, Oh-Won;Kim, Kyo-Han
    • The korean journal of orthodontics
    • /
    • v.28 no.5 s.70
    • /
    • pp.813-823
    • /
    • 1998
  • The frictional force has been considered as an harmful factor in an active unit where tooth movement occurs, but as an advantageous factor in anchor unit that resist tooth movement. That is, efficient tooth movement is planned by using ligation methods that have low levels of bracket-wire frictional force and the anchorage control can be achieved by using ligation methods that have high levels of bracket-wire frictional force that result in binding of the bracket accompanied by little or no tooth movement. The purpose of this study was to evaluate the frictional force generated between bracket and wire in accordance with the methods of ligation, the material of ligation and the passage of time under artificial saliva. Tested were 0.017x0.022 inch stainless steel wires in standard edgewise twin brackets for upper central incisors in a 0.018-inch slot. The wires were ligated into the brackets with elastomeric modules and stainless steel ligatures. Whole tie, half tie, twisting tie and double overlay tie were done with elastomeric modules. With 0.009-inch stainless steel ligature whole tie and half tie were done by needle holder and whole tie by ligature tying plier. With 0.012-inch stainless steel ligature whole ties were done by needle holder. Whole tie groups of elastomeric module were kept in artificial saliva bath at $37^{\circ}C$ for 28 days. The frictional force was recorded by means of an Instron universial testing instrument (4202 INSTRON, Instron Co., U.S.A.) at initial, 7, 14, 21, and 28 days. The results for ligated samples in a simulated oral environment revealed the fellowing : ${\cdot}$In elastomeric module whole tie, 28 days group was significantly greater mean static frictional force than any other group but there were no significant differences among any other group (p>0.05). ${\cdot}$Elastomeric module twisting ties were significantly greater mean static frictional forces than any other ligation method but there were no significant differences between twisting tie and double overlay tie (p>0.05). Twisting tie, double overlay tie, whole tie, half tie showed differences in decreasing order. ${\cdot}$Stainless steel half tie produced lower mean static frictional force than whole tie, ligation by ligature tying plier produced greater mean static frictional force than by needle holder and ligation with 0.012-inch stainless steel ligature produced greater mean static frictional force than with 0.009-inch stainless steel ligature (p<0.05). ${\cdot}$There were no significant differences between the mean static frictional forces of elastomeric whole tie and stainless steel whole tie (p>0.05).

  • PDF

Evaluation of friction of ceramic brackets in various bracket-wire combinations (브라켓 각도 변화에 따른 세라믹 브라켓의 마찰력 측정)

  • Cha, Jung-Yul;Kim, Kyung-Suk;Kim, Dong-Choon;Hwang, Chung-Ju
    • The korean journal of orthodontics
    • /
    • v.36 no.2 s.115
    • /
    • pp.125-135
    • /
    • 2006
  • The purpose of this study was to measure and compare the level of frictional resistance generated from three currently used ceramic brackets; 1, Crystaline $V^{(R)}$, Tomy International Inc., Tokyo, Japan; 2, $Clarity^{(R)}$, 3M Unitek, Monrovia, CA, USA; 3, $Inspire^{(R)}$, Ormco, Orange, CA, USA; with composite resin brackets, Spirit, Ormco, Orange, CA, USA; and conventional stainless steel brackets, Kosaka, Tomy International Inc., Tokyo, Japan used as controls. In this experiment, the resistance to sliding was studied as a function of four angulations $(0^{\circ},\;5^{\circ},\;10^{\circ}\;and\;15^{\circ})$ using 2 different orthodontic wire alloys: stainless steel (stainless steel, SDS Ormco, Orange, CA, USA), and beta-titanium (TMA, SDS Ormco, Orange, CA, USA). After mounting the 22 mil brackets to the fixture and $.019{\times}.025$ wires ligated with elastic ligatures, the arch wires were slid through the brackets at 5mm/min in the dry state at $34^{\circ}C$. Silica-insert ceramic brackets generated a significantly lower frictional force than did other ceramic brackets, similar to that of stainless steel brackets. Beta-titanium archwires had higher frictional resistance than did stainless steel, and all the brackets showed higher static and kinetic frictional force as the angulation increased. When the angulation exceeded $5^{\circ}$, the active configuration emerged and frictional force quickly increased by 2.5 to 4.5-fold. The order of frictional force of the different wire-bracket couples transposed as the angle increased. The silica-insert ceramic bracket is a valuable alternative to conventional stainless steel brackets for patients with esthetic demands.

A Study for the development of the Korean orthodontic bracket (한국형 교정치료용 Bracket의 개발에 관한 연구)

  • Chang, Young-Il;Yang, Won-Sik;Nahm, Dong-Seok;Moon, Seong-cheol
    • The korean journal of orthodontics
    • /
    • v.30 no.5 s.82
    • /
    • pp.565-578
    • /
    • 2000
  • The aim of this study was development of the Straight-Wire Appliance(SWA) suitable lot the treatment or Korean. To accomplish the object of this study, Korean adult with normal occlusion were selected with following criteria : 1) no functional abnormality in the craniofacial area, 2) good dental arch form and posterior occlusal relationship, 3) Angle Class I occlusal relationship, 4) no experience of orthodontic, nor prosthodontic treatment, especially, no dental treatment on labial and buccal surfaces of teeth, 5) good racial profile. Impression were taken for upper and lower dental arches or the selected normal occlusion samples and the orthodontic dental stone models were fabricated. 5 well-trained orthodontists had examined the acquired dental stone models to select study samples which satisfy the Six keys to optimal occlusion of Andrews. 155 pairs of dental stone models (92 pairs of Male, 63 of Female) were finally selected. 3 dimensional digitization were performed with the Coordinate Measuring Machine(CMM, MPC802, WEGU-Messtechnik, Germany) and measuring of Angulation, Inclination, In-and-Out, Molar offset angle and Arch form were accomplished with a measuring software to achieve data for the development of SWA. Before the measurement, error study was performed on the 3 dimensional digitization with CMM, and the analysis of reliability of computerized measuring method adapted in this study and conventional manual method Presented by Andrews was performed. Results of this study were as to)lows : 1. Equi-distance digitization with mesh size 0.25 mm, 0.5 mm and 1.0 mm were acceptable in 3 dimensional digitization of dental stone model with the CMM, and the digitization with 1.0 mm mesh size was recommendable in terms of efficiency. 2. Computerized measuring method with 3 dimensional digitization was more reliable than manual measuring method of Andrews. 3. Data were collected for the development of SWA suitable for the morphological characteristics of Korean with the computerized measuring method with 3 dimensional digitization.

  • PDF

A study on the shear bond strengths of orthodontic brackets according to surface treatments and polymerizing techniques. (도재표면의 처리방법과 접착제의 중합방식에 따른 교정용 브라켓의 전단강도의 연구)

  • Kim, Young-Joo;Cha, Kyung-Suk;Lee, Jin-Woo
    • The korean journal of orthodontics
    • /
    • v.29 no.4 s.75
    • /
    • pp.445-456
    • /
    • 1999
  • As a result of increased education and communication, the field of orthodontics has recently been expanded to include a greater number of adult treatment procedures. With this increased demand for adult orthodontic treatment, a problem that frequently arises is the placement of appliances on teeth restored with porcelain. But conventional acid-etching is ineffective in the preparation of porcelain surface for mechanical retention of orthodontic attachments. Also, it is possible to damage on porcelain. The purpose of this study was to evaluate the effect of composite bonding materials and the porcelain surface treatment methods on shear bond strength, and to observe the porcelain fracture rates. To accomplish this purpose, this study was carried out with feldsphatic porcelain, Ceram II. Porcelain surface treatment methods were divided into intact glazed porcelain which had not treatment and surface roughening. Surface roughening by etching with Hydroluoric acid(HF), sandblasting with Microetcher II and compound treatment with etching and sandblasting. Bonding materials were Ortho-two and Transbond. All porcelain specimens were applicated with porcelain primer. 1. In comparision according to porcelain surface treatment, surface roughening groups by HF etching and sandblasting had higher shear bond than intact group. No significant difference was found in Transbond group. 2. Ortho-two group had the higher shear bond strength than that of Transbond group in B:.u etching and sandblasting. 3. E(Transbond. Intact)group had the lowest shear bond strength in all experimental group. The bond strength was higher than clinically successful bond strength. 4. Non-treated group had very higher porcelain rates than treated group. 5. This study indicates that porcelain surface-roughening may not be necessary to attachment of orthodontic brackets to porcelain surfaces.

  • PDF

THE POSITIONING ERRORS IN BONDING LINGUAL BRACKETS (설측브라켓 부착시 위치오차에 관한 연구)

  • Choi, Joon-Kyu;Hwang, Hyeon-Shik;Kim, Jong-Chul
    • The korean journal of orthodontics
    • /
    • v.28 no.1 s.66
    • /
    • pp.99-111
    • /
    • 1998
  • The purpose of this study was to evaluate the positioning errors according to the method of bonding lingual brackets. Dental models of twenty orthodontic patients with malocclusion were selected for this study. The positioning errors were measured on each model that brackets were bonded to. Three different bonding methods were used. For the first method the bracket was bonded intimately to the lingual surface of the model. For the second method, the bracket was bonded intimately to the lingual surface after setting up using articulator. The passive bracketing, bonding the bracket ligated first to ideal archwire, was used after setting up as the last method. The results were as follows: 1. The brackets bonded without setting up showed greater angulation errors in the upper 1st premolar and the lower canine than those in other bonding methods. The brackets bonded without passive bracketing showed greater positioning errors in upper central incisor, lower 1st and End premolars. 2. The brackets bonded without setting up showed greater torque error in lower 2nd premolar than those in other bonding methods. The brackets bonded without passive bracketing showed greater torque errors in all upper teeth, lower 1st and 2nd premolars. 3. The brackets bonded without passive bracketing showed greater rotation errors between upper central incisors, lower central incisors, lower lateral and central incisor, lower canine and lateral incisor. 4. The brackets bonded without setting up showed greater in-out errors between upper canine and lateral incisor than those in other bonding methods. The brackets bonded without passive bracketing showed greater in-out errors between upper central incisors, upper central and lateral incisors, upper 1st and 2nd premolars, lower lateral and central incisors, lower canine and lateral incisor. These results suggest that there is a large amount of positioning error in lingual brackets even by an indirect bonding technique, and it may be reduced by passive bracketing.

  • PDF

THE EFFECT OF LIGHT CURED GLASS IONOMER CEMENT ON THE SHEAR BOND STRENGTH OF ORTHODONTIC BRACKETS (광중합형 글래스 아이오노머 시멘트 교정용 브라켓의 전단결합강도에 미치는 영향)

  • Kim, Cheol;Yoon, Young-Jooh;Kim, Kwng-Won
    • The korean journal of orthodontics
    • /
    • v.27 no.2
    • /
    • pp.327-334
    • /
    • 1997
  • The purpose of this study was to evaluate clinical applicability of light cured glass ionomer cement as a othodontic adhesive. The metal brackets and plastic brackets were bonded with light cured glass ionomer cement(Fuji Ortho $LS^{(R)}$) after polishing with a slurry of pumice, surface conditioning with 10% polyacrylic acid and chemically cured resin(Mono-$Lok2^{(R)}$) after acid etching with 38% phosphoric acid on the extracted human bicuspids. The shear bond strength was tested with a universal testing machine(HGS-100A, Shimadzu Co., Japan) after storage in normal saline at $37^{\circ}C$ or 24 hours and 48 hours. The results were as follows: 1. The shear bond strength of light cured glass ionomer cement group polished with a slurry of pumice was significantly lower than that of chemically cured resin group(P<0.01). 2. The shear bond strength of light cured glass ionomer cement group conditioned with 10% polyacrylic acid was significantly lower than that of chemically cured resin group(P<0.01). 3. The shear bond strength of light cued glass ionorner cement group conditioned with 10% polyacrylic acid was slightly higher than that of light cured glass ionomer cement group polished with a slurry of pumice, but there was no significant difference(P>0.05). 4. There was no significant difference between metal bracket group and plastic bracket group irrelevant off enamel conditioning(P>005). In summary, although the shear bond strength of light cured glass lionomer cement was lower than that of chemically cured resin, it night be clinically applicable.

  • PDF

The shear bond strength and adhesive failure pattern in bracket bonding with different light-curing methods (브라켓 접착시 광중합방식에 따른 전단결합강도와 파절양상 비교)

  • Shin, Jai-Ho;Lim, Yong-Kyu;Lee, Dong-Yul
    • The korean journal of orthodontics
    • /
    • v.34 no.4 s.105
    • /
    • pp.333-342
    • /
    • 2004
  • The purpose of this study was to evaluate the clinical effectiveness of a plasma arc light and light emitting diode (LED), compared with shear bond strength and the failure pattern of brackets bonded with visible light in direct bonding. Brackets were bonded with Transbond XT to 60 human premolars embedded in the resin blocks according to different light-curing methods. Then, the shear bond strength of each group was measured using a universal testing machine (Instron) and the adhesive failure pattern after debonding was visually examined by light microscope. The results were as follows: 1. The shear bond strength showed no significant difference between the visible light and light emitting diode, but the plasma arc light exhibited a significantly lower shear bond strength compared with the visible light and light emitting diode. 2. In the visible light and light emitting diode, adhesive failure patterns were similar. Bond failure occurred more frequently at the enamel-adhesive interface. 3. The bonding failure of brackets bonded with plasma arc light occurred more frequently at the bracket-adhesive interface. The results of this study suggest that plasma arc light, light emitting diode and visible light are all clinically useful in the direct bonding of orthodontic brackets.

Effects of Saliva Contamination on Shear Bond Strength with Conventional, Moisture Insensitive, and Self-Etching Primers (Moisture Insensitive Primer와 Self-Etching Primer를 사용한 교정용 브라켓 접착 시 타액오염이 전단결합강도에 미치는 영향 비교)

  • Oh, Yoonjeong;Oh, Sohee
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.46 no.1
    • /
    • pp.21-28
    • /
    • 2019
  • The aim of this study was to compare the shear bond strengths of orthodontic bracket with Conventional primer (CP), Moisture insensitive primer (MIP), and Self-etching primer (SEP). In addition, the effect and the timing of saliva contamination on shear bond strength was evaluated. A total of 135 bovine mandibular incisors were used in the study and divided into 3 groups. Group I, II and III were used CP, MIP, SEP, respectively. Each group was then divided into three subgroups: the group without saliva contamination, the group with primer application after saliva contamination, and the group with saliva contamination after primer application. After the primer application, the metal bracket for the lower incisor was attached and the shear bond strength was measured. The mean shear bond strengths was highest with CP and lowest with SEP in dry condition. However, CP showed a significant decrease in shear bond strength in the presence of saliva contamination. MIP and SEP showed no significant decrease in shear bond strength with saliva contamination.

Direct detection of cariogenic streptococci in metal brackets in vivo using polymerase chain reaction (교정용 메탈 브라켓에서 자가중합효소연쇄반응을 통한 치아우식증 원인균의 탈출)

  • Ahn, Sug-Joon;Lee, Shin-Jae;Baek, Seung-Hak;Kim, Tae-Woo;Chang, Young-Il;Nam, Dong-Seok;Lim, Bum-Soon
    • The korean journal of orthodontics
    • /
    • v.35 no.4 s.111
    • /
    • pp.312-319
    • /
    • 2005
  • Streptococcus mutans and Streptococcus sobrinus are major etiological agents in enamel demineralization around orthodontic appliances. This study was designed to examine the prevalence of these streptococci on orthodontic brackets in vivo using polymerase chain reaction. Four incisor brackets in the upper and lower arches were removed and collected from 80 patients at the time of debonding. The genomic DMA of adhered bacteria was extracted and each dextranase gene of S. mutans and S. sobrinus was amplified using the specific oligonucleotide primers. The results showed that the maxillary incisor brackets were colonized by both cariogenic streptococci to a somewhat higher degree than that taken from the mandible. The prevalence of S. mutans was $50.0\%$ on the maxillary incisor brackets and $33.8\%$ on the mandibular incisor brackets, and that of S. sobrinus was $17.5\%$ and $15.0\%$, respectively. Both species were detected on the maxillary incisor brackets of 7 patients $(8.8\%)$ and the mandibular incisor brackets of 5 patients $(6.3\%)$. These results suggest that cariogenic streptococci can adhere to the incisor brackets and may be resident species on the incisor brackets.

A Change of Shear Bond Strength of Orthodontic Resin Adhesives under Water Immersion (침수후 시간에 따른 교정용 레진접착제의 전단결합강도 변화)

  • Lee, Je-Jun;Kim, Jong-Chul
    • The korean journal of orthodontics
    • /
    • v.28 no.5 s.70
    • /
    • pp.783-789
    • /
    • 1998
  • The purpose of this study was to evaluate the changes of shear bond strengths and failure patterns in orthodontic resin adhesives according to the water immersion time. Metal brackets were bonded to the specimens involving the premolars with chemical-cured($Concise^{\circledR}$) and light-cured($Transbond^{\circledR}$) adhesives. The shear bond strength was measured on universal testing machine and the failure patterns were assessed with the adhesive remnant index(ARI) after storage in distilled water at $37^{\circ}C$ for 1 day, 1 week and 1, 3, and 6 months, respectively. The results were as follows. 1. The shear bond strengths at the 6 month in both Concise and Transbond were significantly higher than those at the 1 day, 1 week and 1 month(p<0.05). There were positive correlations between shear bond strength and water immersion time in both Concise and Transbond(P<0.01). 2. There were no significant differences in shear bond strength between Concise and Transbond. 3. The brackets were failed primarily at the bracket base-adhesive interface and there was no significant difference in the incidence of ARI scores according to the water immersion time.