Electrochemical Synthesis of Dumbbell-like Au-Ni-Au Nanorods and Their Surface Plasmon Resonance

  • Park, Yeon Ju;Liu, Lichun;Yoo, Sang-Hoon;Park, Sungho
    • Journal of Electrochemical Science and Technology
    • /
    • v.3 no.2
    • /
    • pp.57-62
    • /
    • 2012
  • In this report, we demonstrate that the longitudinal localized surface plasmon resonance mode can be suppressed when the nanorods were in dumbbell shape. The seed nanorods were synthesized by electrochemical deposition of metals into the pores of anodic aluminum oxide templates. The dumbbell-like nanorods were grown from seed Au-Ni-Au nanorods by a rate-controlled seed-mediated growth strategy. The selective deposition of Au atoms onto Au blocks of Au-Ni-Au nanorods produced larger diameter of Au nanorods with bumpy surface resulting in dumbbell-like nanorods. The morphology of nanorods depended on the reduction rate of $AuCl_4^-$, slow rate producing smooth surface of Au nanorods, but high reduction rate producing bumpy surface morphology. Through systematic investigation into the UV-Vis-NIR spectroscopy, we found that the multiple localized surface plasmon resonance (LSPR) modes were available from single-component Au nanorods. And, their LSPR modes of Au NRs with bumpy surface, compared to the smooth seed Au NRs, were red-shifted, which was obviously attributed to the increased electron oscillation pathways. While the longitudinal LSPR modes of smoothly grown Au NRs were blue-shifted except for a dipole transverse LSPR mode, which can be interpreted by decreased aspect ratio. In addition, dumbbell-like nanorods showed an almost disappeared longitudinal LSPR mode. It reflects that the plasmonic properties can be engineered using complex nanorods structure.

Annealing Effects of Seed Layers on the Properties of ZnO Nanorods (ZnO 나노로드 특성에 미치는 시드 막 열처리 영향)

  • Ma, Tae-Young;Park, Ki-Cheol
    • The Transactions of The Korean Institute of Electrical Engineers
    • /
    • v.67 no.6
    • /
    • pp.753-758
    • /
    • 2018
  • We investigated annealing effects of seed layers on the properties of ZnO nanorods grown on the seed layers. ZnO nanorods were grown by a hydrothermal method. ~100 nm-thick ZnO films were sputtered on oxidized Si wafers and quartz as seed layers. The ZnO films were annealed at $400^{\circ}C$, $600^{\circ}C$, and $800^{\circ}C$, respectively. ZnO nanorods were grown at $90^{\circ}C$ for 3 hours in the mixed solution of zinc nitrate hexahydrate and hexamethylenetetramine. X-ray diffraction was carried out to estimate the crystallinity and strain of ZnO films and nanorods. A field emission scanning electron microscope was employed to observe the morphology of the films and nanorods. PL(photoluminescence) measurements were conducted with 266 nm light. It was found that the annealing of seed layers increase the growth rate of nanorods, and change compressive strain of nanorods to tensile strain. The intensity of PL in the UV region reduced by using the annealed seed layers.

Growth of ZnO thin films by MOCVD using the buffer layers grown at high temperature (고온 버퍼층을 이용한 ZnO 박막의 MOCVD 성장)

  • Kim, Dong-Chan;Kong, Bo-Hyun;Cho, Hyung-Koun
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2006.06a
    • /
    • pp.108-109
    • /
    • 2006
  • ZnO semiconductor has a wide band gap of 3.37 eV and a large exciton binding energy of 60 meV, and displays excellent sensing and optical properties. In particular, ZnO based 1D nanowires and nanorods have received intensive attention because of their potential applications in various fields. We grew ZnO buffer layers prior to the growth of ZnO nanorods for the fabrication of the vertically well-aligned ZnO nanorods without any catalysts. The ZnO nanorods were grown on Si (111) substrates by vertical MOCVD. The ZnO buffer layers were grown with various thicknesses at $400^{\circ}C$ and their effect on the formation of ZnO nanorods at $300^{\circ}C$ was evaluated by FESEM, XRD, and PL. The synthesized ZnO nanorods on the ZnO film show a high quality, a large-scale uniformity, and a vertical alignment along the [0001]ZnO compared to those on the Si substrates showing the randomly inclined ZnO nanorods. For sample using ZnO buffer layer, 1D ZnO nanorods with diameters of 150-200 nm were successively fabricated at very low growth temperature, while for sample without ZnO buffer the ZnO films with rough surface were grown.

  • PDF

Fabrication of the catalyst free GaN nanorods on Si grown by MOCVD

  • Ko, Suk-Min;Cho, Yong-Hoon
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2010.08a
    • /
    • pp.232-232
    • /
    • 2010
  • Recently light emitting diodes (LEDs) have been expected as the new generation light sources because of their advantages such as small size, long lifetime and energy-saving. GaN, as a wide band gap material, is widely used as a material of LEDs and GaN nanorods are the one of the most widely investigated nanostructure which has advantages for the light extraction of LEDs and increasing the active area by making the cylindrical core-shell structure. Lately GaN nanorods are fabricated by various techniques, such as selective area growth, vapor-liquid-solid (VLS) technique. But these techniques have some disadvantages. Selective area growth technique is too complicated and expensive to grow the rods. And in the case of VLS technique, GaN nanorods are not vertically aligned well and the metal catalyst may act as the impurity. So we just tried to grow the GaN nanorods on Si substrate without catalyst to get the vertically well aligned nanorods without impurity. First we deposited the AlN buffer layer on Si substrate which shows more vertical growth mode than sapphire substrate. After the buffer growth, we flew trimethylgallium (TMGa) as the III group source and ammonia as the V group source. And during the GaN growth, we kept the ammonia flow stable and periodically changed the flow rate of TMGa to change the growth mode of the nanorods. Finally, as the optimization, we changed the various growth conditions such as the growth temperature, the working pressure, V/III ratio and the doping level. And we are still in the process to reduce the diameter of the nanorods and to extend the length of the nanorods simultaneously. In this study, we focused on the shape changing of GaN nanorods with different growth conditions. So we confirmed the shape of the nanorods by scanning electron microscope (SEM) and carried out the Photoluminescence (PL) measurement and x-ray diffraction (XRD) to examine the crystal quality difference between samples. Detailed results will be discussed.

  • PDF

Growth of ZnO nanorods by vapor-solid method (기상증착법을 이용한 산화아연 나노로드의 성장)

  • 김나리;김재수;변동진;노대호;진정근;양재웅
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2003.11a
    • /
    • pp.122-122
    • /
    • 2003
  • In recent years, there has been increasing interest in quasi one-dimensional nanostructural systems, because of their numerous potential applications in various areas, such as materials sciences, electronics, optics, magnetism and energy storage. Specifically, zinc oxide (ZnO) is recognized as one of the most promising oxide semiconductor materials, because of its good optical, electrical, and piezoelectrical properties. The ZnO nanorods were synthesized using vapor-solid (VS) mechanism on soda lime glass substrate without the presence of metal catalyst. ZnO nanorods were prepared thermal evaporation of a Zn powder at 500. As-fabricated ZnO nanorods had an average diameter and length of 40nm and 3$\mu\textrm{m}$. Transmission electron microscopy revealed that the ZnO nanorods were single crystalline with the growth direction perpendicular to the (101) lattice plane. The influences of reaction time on the formation of the ZnO nanorods were investigated. The Photoluminescence measurements showed that the ZnO nanorods had a strong ultraviolet emission at around 380nm and a green emission at around 500nm.

  • PDF

Photoluminescence in MgO-ZnO Nanorods Enhanced by Hydrogen Plasma Treatment

  • Park, Sunghoon;Ko, Hyunsung;Mun, Youngho;Lee, Chongmu
    • Bulletin of the Korean Chemical Society
    • /
    • v.34 no.11
    • /
    • pp.3367-3371
    • /
    • 2013
  • MgO nanorods were fabricated by the thermal evaporation of $Mg_3N_2$. The influence of ZnO sheathing and hydrogen plasma exposure on the photoluminescence (PL) of the MgO nanorods was studied. PL measurements of the ZnO-sheathed MgO nanorods showed two main emission bands: the near band edge emission band centered at ~380 nm and the deep level emission band centered at ~590 nm both of which are characteristic of ZnO. The near band edge emission from the ZnO-sheathed MgO nanorods was enhanced with increasing the ZnO shell layer thickness. The near band edge emission from the ZnO-sheathed MgO nanorods appeared to be enhanced further by hydrogen plasma irradiation. The underlying mechanisms for the enhancement of the NBE emission from the MgO nanorods by ZnO sheathing and hydrogen plasma exposure are discussed.

Finite element analysis for longitudinal vibration of nanorods based on doublet mechanics

  • Ufuk Gul;Metin Aydogdu
    • Advances in nano research
    • /
    • v.15 no.5
    • /
    • pp.411-422
    • /
    • 2023
  • In the present study, the axial vibration of the nanorods is investigated in the framework of the doublet mechanics theory. The equations of motion and boundary conditions of nanorods are derived by applying the Hamilton principle. A finite element method is developed to obtain the vibration frequencies of nanorods for different boundary conditions. A two-noded higher order rod finite element is used to solve the vibration problem. The natural frequencies of nanorods obtained with the present finite element analysis are validated by comparing the results of classical doublet mechanics and nonlocal strain gradient theories. The effects of rod length, mode number and boundary conditions on the axial vibration frequencies of nanorods are examined in detail. Mode shapes of the nanorods are presented for the different boundary conditions. It is shown that the doublet mechanics model can be used for the dynamic analysis of nanotubes, and the presented finite element formulation can be used for mechanical problems of rods with unavailable analytical solutions. These new results can also be used as references for the future studies.

Cadmium Sulphide Nanorods: Synthesis, Characterization and their Photocatalytic Activity

  • Giribabu, Krishnamoorthy;Suresh, Ranganathan;Manigandan, Ramadoss;Vijayaraj, Arunachalam;Prabu, Raju;Narayanan, Vengidusamy
    • Bulletin of the Korean Chemical Society
    • /
    • v.33 no.9
    • /
    • pp.2910-2916
    • /
    • 2012
  • Cadmium sulphide (CdS) nanorods were prepared by a single precursor thermal decomposition (SPTD) method. The formation of CdS nanorods and their structure, morphology and elemental composition were studied by means of FT-IR, XRD, FE-SEM, HR-TEM and EDAX analysis. Photoluminescence (PL) and lifetime measurements were recorded to study the luminescence properties of the material. The PL spectrum of the CdS nanorods showed one broad peak and four shoulders and the cause for this emission was discussed. The PL emissions from the band edge and deep trap state of the CdS nanorods were studied by lifetime measurements. Further, the synthesized CdS nanorods showed an increase in efficiency of photocatalytic degradation of methylene blue (MB) and rhodamine B (RhB). The increase in the photocatalytic activity was attributed to the mixed phase of the CdS nanorods.

Effects of Boron Concentration in ZnO:Al Seed Films on the Growth and Properties of ZnO Nanorods (ZnO:Al 시드 막의 보론 농도가 ZnO 나노로드의 성장 및 특성에 미치는 영향)

  • Ma, Tae-Young;Park, Ki-Cheol
    • The Transactions of The Korean Institute of Electrical Engineers
    • /
    • v.66 no.10
    • /
    • pp.1488-1493
    • /
    • 2017
  • Boron-doped ZnO:Al films were deposited by rf magnetron sputtering. The structural and optical property variations of the films with the boron amounts were studied. ZnO nanorods were grown on $SiO_2/Si$ wafers and glass by a hydrothermal method. ~50 nm-thick boron-doped ZnO:Al films were deposited on the substrates as seed layers. The mixed solution of zinc nitrate hexahydrate and hexamethylenetetramine in DI water was used as a precursor for ZnO nanorods. The concentration of zinc nitrate hexahydrate and that of hexamethylenetetramine were 0.05 mol, respectively. ZnO nanorods were grown at $90^{\circ}C$ for 2 hours. X-ray diffraction was conducted to observe the crystallinity of ZnO nanorods. A field emission scanning electron microscope was employed to study the morphology of nanorods. Optical transmittance was measured by a UV-Vis spectrophotometer, and photoluminescence was carried out with 266 nm light. The ZnO nanorods grown on the 0.5 wt% boron-doped ZnO seed layer showed the best crystallinity.