Preparation and rheological behavior of polystyrene/multi-walled carbon nanotube composites by latex technology

  • Woo, Dong-Kyun;Kim, Byung-Chul;Lee, Seong-Jae
    • Korea-Australia Rheology Journal
    • /
    • 제21권3호
    • /
    • pp.185-191
    • /
    • 2009
  • Polystyrene/multi-walled carbon nanotube (PS/MWCNT) composites were prepared by the use of latex technology. The monodisperse PS latex was synthesized by an emulsifier-free emulsion polymerization from styrene/potassium persulfate/water system in the presence of ethanol. The MWCNTs were first treated with acid mixture to eliminate impurities, dispersed in deionized water driven by ultrasonicator, and then mixed with the PS latex. From these mixtures, PS/MWCNT composites were prepared by freeze-drying and subsequent compression molding. In the small-amplitude oscillatory shear experiments, both complex viscosity and storage modulus increased with increasing MWCNT content. A pronounced effect of MWCNT content was observed, resulting in larger storage modulus and stronger yield behavior at low frequencies when compared to unmodified PS. It showed a transition from viscous to elastic behavior with increasing MWCNT content. Over the MWCNT content of 3 wt%, the storage modulus was higher than the loss modulus across all frequencies.

Aniline Terminated Waterborne Polyurethane/Multi-walled Carbon Nanotube 복합 코팅 용액의 제조 및 물성 (Preparation and Properties of Aniline Terminated Waterborne Polyurethane/Multi-walled Carbon Nanotube Composite Coating Solutions)

  • 홍민기;김병석;송기창
    • Korean Chemical Engineering Research
    • /
    • 제50권3호
    • /
    • pp.403-409
    • /
    • 2012
  • Poly (carbonate diol), isophrone diisocyanate와 dimethylol propionic acid로 부터 제조된 polyurethane prepolymer의 말단 NCO기를 aniline으로 capping시켜 aniline terminated waterborne polyurethane dispersion (ATWPUD)을 합성하였다. 이 ATWPUD와 물에 분산되어 있는 multi-walled carbon nanotube (MWCNT)를 혼합시켜 전도성 코팅 용액을 제조한 후, 이것을 polycarbonate 기재 위에 도포하여 코팅 막을 형성하였다. ATWPUD와 MWCNT를 혼합하여 얻어진 코팅 막의 표면저항 값은 $10^{7.6}{\sim}10^{7.7}{\Omega}/cm^2$로 순수한 waterborne polyurethane dispersion (WPUD)과 MWCNT의 혼합물로부터 제조된 코팅 막의 $10^{10.9}{\Omega}/cm^2$ 보다 우수한 전기전도도를 나타내었다. 또한 ATWPUD에 첨가되는 MWCNT의 양이 증가될수록 코팅 막의 전기전도도는 증가하였지만 연필경도 및 부착력은 감소되었다.

Characterization and influence of shear flow on the surface resistivity and mixing condition on the dispersion quality of multi-walled carbon nanotube/polycarbonate nanocomposites

  • Lee, Young Sil;Yoon, Kwan Han
    • Carbon letters
    • /
    • 제16권2호
    • /
    • pp.86-92
    • /
    • 2015
  • Multi-walled carbon nanotube (MWCNT)/polycarbonate (PC) nanocomposite was prepared by direct melt mixing to investigate the effect of the shear rate on the surface resistivity of the nanocomposites. In this study, an experiment was carried out to observe the shear induced orientation of the MWCNT in the polymer matrix using a very simple melt flow indexer with various loads. The compression-molded, should be eliminated. MWCNT/PC nanocomposite sample exhibited lower percolation thresholds (at 0.8 vol%) and higher electrical conductivity values than those of samples extruded by capillary and injection molding. Shear induced orientation of MWCNT was observed via scanning electron microscopy, in the direction of flow in a PC matrix during the extrusion process. The surface resistivity rose with increasing shear rate, because of the breakdown of the network junctions between MWCNTs. For real applications such as injection molding and the extrusion process, the amount of the MWCNT in the composite should be carefully selected to adjust the electrical conductivity.

스프레이 법으로 제작된 MWCNT 투명전도막의 특성

  • 장경욱
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2009년도 추계학술대회 논문집
    • /
    • pp.244-244
    • /
    • 2009
  • Carbon nanotubes (CNTs) have excellent electrical, chemical stability, mechanical and thermal properties. In this paper, networks of Multi-walled carbon nanotube (MWCNT) materials were investigated as transparent electrode. Sensor films were fabricated by air spray method using the multi-walled CNTs solution on glass substrates. The film that was sprayed with the MWCNT dispersion for 60 sec, was 300nm thick. And the electric resistivity and the light transmittance rate are $2{\times}10^2{\Omega}cm$ and 60%, respectively.

  • PDF

라텍스 기법으로 제조한 폴리스티렌/다중벽 탄소나노튜브 나노복합재료의 나노튜브 길이가 유변학적 특성에 미치는 영향 (Effect of Nanotube Length on Rheological Characteristics of Polystyrene/Multi-walled Carbon Nanotube Nanocomposites Prepared by Latex Technology)

  • 우동균;노원진;이성재
    • 폴리머
    • /
    • 제34권6호
    • /
    • pp.534-539
    • /
    • 2010
  • 라텍스 블렌딩 기법을 이용하여 폴리스티렌(PS)/다중벽 탄소나노튜브(MWCNT) 나노복합재료를 제조하여 나노튜브 길이에 따른 나노복합재료의 유변학적 특성을 고찰하였다. 나노복합재료 제조에 사용된 단분산 PS 입자는 무유화제 유화중합으로 제조하였고, MWCNT는 불순물 제거와 분산성 향상을 위해 표면개질 과정을 거친 후 사용하였다. 최종적인 나노복합재료는 단분산 PS 입자와 개질한 MWCNT를 초음파 교반조에서 분산시킨 후 동결건조 과정을 거쳐 제조하였다. 나노복합재료의 MWCNT 함량과 나노튜브 길이에 따른 유변학적 특성은 소진폭 진동 전단유동을 부과시켜 평가하였다. 본 연구에서 고찰한 PS/MWCNT 나노복합재료는 MWCNT의 함량이 증가할수록, 나노튜브 길이가 길수록 유변물성 향상 효과가 뚜렷하였다. 이는 MWCNT 함량이 증가할수록 나노복합재료의 유변학적 특성이 액체적 특성에서 점차 고체적 특성으로 변화하기 때문이며, 나노튜브 길이가 길수록 네트워크 구조를 달성하는 임계 농도가 작아지기 때문인 것으로 판단된다.

PP/CF/ MWCNT 나노복합체의 제조 및 특성평가 (Preparation and characteristics of PP/CF/MWCNT nanocomposites)

  • 김승범;남병욱;이규만
    • 반도체디스플레이기술학회지
    • /
    • 제10권1호
    • /
    • pp.107-111
    • /
    • 2011
  • Polypropylene(PP)/carbon fiber(CF)/multi-walled carbon nanotube(MWCNT) nanocomposites along with various CF and MWCNT contents were prepared in a Twin screw extruder. Electrical, mechanical property and morphology were investigated with a variation of CF and MWCNT contents. From the surface resistance of PP/CF/MWCNT composites, MWCNT can increase the conductivity of composites compared with PP/CF composites without MWCNT. It is suggested that MWCNT and CF can make the conductive network in the polymer matrix. Flexural modulus and Izod impact strength of the PP/CF/MWCNT composites were improved with the increase of CF contents. Morphology showed that length of CF in polymer matrix was shortened by torque during melt mixing with MWCNT. As a result of this phenomenon, the impact strength of composites was somewhat decreased.

충격보강제가 보강된 PPS (polyphenylene sulfide)/MWCNT (multi-walled carbon nanotube) 나노복합체의 물성연구 (Properties of impact modifier reinforced PPS/MWCNT Nanocomposite)

  • 박지수;김승범;남병욱
    • 반도체디스플레이기술학회지
    • /
    • 제11권2호
    • /
    • pp.75-80
    • /
    • 2012
  • Polymer composites which have electrical properties have been studied in various industries. The Multi-walled carbon nanotube (MWCNT) are thought to be reinforcements for polymers because of their high aspect ratio and specially mechanical, thermal and electrical properties. We introduced MWCNT and impact modifier in order to improve thermal and mechanical properties of Polyphenylene sulfide (PPS) and give electric characteristic to PPS. The thermal properties were investigated by Differential scanning calorimeter (DSC) and Thermogravimetric analysis (TGA). The morphology, mechanical properties and electrical characteristic were performed by Field emission scanning electron microscopy (FE-SEM), Izod impact tester and surface resistance meter. As a result, we could find that the PPS/MWCNT composites have high conductivity and good mechanical properties than neat PPS resin.

Cycling Performance of Supercapacitors Assembled with Polypyrrole/Multi-Walled Carbon Nanotube/Conductive Carbon Composite Electrodes

  • Paul, Santhosh;Kim, Jae-Hong;Kim, Dong-Won
    • Journal of Electrochemical Science and Technology
    • /
    • 제2권2호
    • /
    • pp.91-96
    • /
    • 2011
  • Polypyrrole (PPy)/multi-walled carbon nanotube (MWCNT)/conductive carbon (CC) composites are synthesized by the chemical oxidative polymerization method. The morphology analysis of the composite materials indicates uniform coating of PPy over MWCNTs and conductive carbon. The electrochemical performances of PPy/MWCNT/CC composites with different compositions are evaluated in order to optimize the composition of the composite electrode. Galvanostatic chargedischarge measurements and electrochemical impedance spectroscopy studies prove the excellent cycling stability of the PPy/MWCNT/CC composite electrodes.

Synthesis and Electrochemical Characterization of Polypyrrole/Multi-walled Carbon Nanotube Composite Electrodes for Supercapacitor Applications

  • Paul, Santhosh;Lee, Yoon-Sung;Choi, Ji-Ae;Kang, Yun-Chan;Kim, Dong-Won
    • Bulletin of the Korean Chemical Society
    • /
    • 제31권5호
    • /
    • pp.1228-1232
    • /
    • 2010
  • The nanocomposites of polypyrrole (PPy) and multi-walled carbon nanotube (MWCNT) with different composition are synthesized by the chemical oxidative polymerization method. In these composites, the MWCNTs are uniformly coated by PPy with different thickness. The electrochemical properties of the composite electrodes are investigated by cyclic voltammetry, galvanostatic charge-discharge cycling and electrochemical impedance spectroscopy. The full cells assembled with the PPy/MWCNT composite electrodes deliver initial specific capacitances ranging from 146.3 to 167.2 F/g at 0.5 mA/$cm^2$ and exhibit stable cycling characteristics. The effect of content of MWCNT in the composite on cycling performance of the cells is also investigated.

다중벽 탄소나노튜브 혼입 알칼리 활성 슬래그 복합재료의 열전 에너지 수확 성능평가 (Evaluation on the thermoelectric energy harvesting performance of multi-walled carbon nanotube-embedded alkali activated slag composites)

  • 박형민;양범주
    • 도시과학
    • /
    • 제9권1호
    • /
    • pp.1-6
    • /
    • 2020
  • The thermoelectric characteristics of alkali activated slag composites containing multi-walled carbon nanotubes (MWCNT) was investigated in the present study. Three different MWCNT contents and exposed temperatures were considered, and their thermoelectric-related properties and internal structures were analyzed. It was found that the alkali activated slag composite with MWCNT 2.0 wt.% and the exposed temperature of 150℃ were the optimal condition to obtain the highest Seebeck coefficient and power factor. Based on the feasibility study, the extended size thermoelectric module with 130 elements was fabricated, and tested the electricity production capacity. Consequently, the present thermoelectric module produced 30.83 ㎼ of electricity at ∆T=178.4℃.