고강도 콘크리트의 현장최적배합에 관한 연구 (The Study on the Optimum Mix Design of the High-Strength Concrete in Site)

  • 이상수;원철;김동석;안재현;박칠림
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1996년도 가을 학술발표회 논문집
    • /
    • pp.232-238
    • /
    • 1996
  • In this paper, the properties of high-strength concrete are described with respect to materials and mix conditions(water-cement ratio, chemical admixture, replacement of fly ash). As primary purposes of this study, the optimum mix design method of high-strength concrete to decrease unit cement contents is investigated, and the properties of fresh and hardened concretes are tested in terms of slump, air content and compressive strength. As results of this study, workability and strength development of the high-strength concrete depend on the water-cement ratio, replacement ratio of fly ash and dosage of the chemical admixture. The conditions which are proposed optimum mix design of the high-strength concrete show W/C 37%, S/A 42~45% and unit cement content 470~480kg/$\textrm{m}^3$. Based on the results, the applicability of high-strength concrete in site is clearly proved.

  • PDF

고성능콘크리트의 배합설계 (Mix Design of High Performance Concrete)

  • 정용욱;이승한;윤용호
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2005년도 봄학술 발표회 논문집(II)
    • /
    • pp.73-76
    • /
    • 2005
  • This study aims to suggest a simple and convenient design for a mix proportion method for high performance concrete by determining the optimum fine aggregate ratio and minimum binder content based on the maximum density theory. The mix design method introduced in this study adopted the optimum fine aggregate ratio with a minimum void and binder content higher than the minimum binder content level. The research results reveal that the method helps to reduce trial and error in the mixing process and is a convenient way of producing high performance concrete with self filler ability. In an experiment based on the mix proportion method, when aggregate with the fine aggregation ratio of 41$\%$ was used, the minimum binder content of high performance concrete was 470kg/$m^{3}$ and maximum aggregate capacity was $0.657m^{3}/m^{3}$. In addition, in mixing high performance concrete, the optimal slump flow to meet filler ability was 65$\pm$5cm, V load flow speed ranged from 0.5 to 1.5.

  • PDF

동애등에분변토와 코코피트가 혼합된 토양개량제가 모래의 이화학성에 미치는 영향 (Effects of Soil Amendment Blended with Soldier Fly Casts and Coco Peat on Physicochemical Properties of Sand Soil)

  • 김영선;이상범;함선규;임혜정;최영철;박관호
    • Weed & Turfgrass Science
    • /
    • 제3권2호
    • /
    • pp.143-149
    • /
    • 2014
  • 본 연구는 아메리카동애등에분변토(soldier fly casts; SFC)의 단점을 개량하기 위해 코코피트(cocopeat; Coco)와 혼합된 토양개량제의 골프장 토양개량제로서의 사용가능성을 평가하기 위해 모래와 혼합비율 별 물리화학성을 조사하였다. 토양개량제는 SFC, Coco, 25% SFC+75% Coco(Mix1), 50% SFC+50% Coco (Mix2) 및 75% SFC+25% Coco (Mix3)이었고, 각각 3%, 5%, 7% 및 10% 씩 혼합되어 모래상토를 조성하였다. SFC, Mix1, Mix2 및 Mix3는 토양 pH와 EC에서 고도의 상관성(P<0.01)을 나타내어 토양개량제의 혼합에 의해 모래상토의 토양화학성에 영향을 주었다. SFC, Coco, Mix1, Mix2 및 Mix3은 모세관공극, 비모세관공극 및 공극이 USGA기준에 적합하였고, 혼합비율이 증가할수록 모세관공극과 총공극이 증가하였으며(P<0.05), Mix1과 Mix3의 비모세관공극은 모세관공극과 수리전도도에서 부의 상관성을 보였다(P<0.01). Mix1, Mix2 및 Mix3에서 SFC는 상토의 모세관공극의 변화에 영향을 주었고, Coco는 모세관공극과 총공극의 변화에 영향을 주었다. 이들 결과를 종합할 때, SFC와 Coco가 혼합된 토양개량제(Mix1~3)는 SFC보다 모래상토의 모세관 공극과 수리전도도를 개선하여 SFC의 단점을 보완한 것으로 평가되었다.

혼수비에 따른 초경석고의 파절강도 (FRACTURE STRENGTH OF IMPROVED DENTAL STONE ACCORDING TO WATER/POWDER RATIO)

  • 엄정희;박찬운;박광선
    • 대한치과보철학회지
    • /
    • 제39권2호
    • /
    • pp.220-229
    • /
    • 2001
  • This study was performed to evaluate the fracture resistance of three improved die stone materials according to water/powder ratio. There are lots of handling conditions which affect the physical properties of improved dental stone, and it's well known that the water/powder ratio significantly affect the strength of die stone. If water/power ratio was incorrect, following disadvantages were showed : (1) susceptibility to dimensional change due to abrasion, (2) limited reproduction of fine detail, (3) lack of strength. The maxillary master casts were made of additional silicone impressions(Exaflex, GC America. Inc. USA). Three type IV die stones such as Fuji Rock (GC Europe Intreleuvenlaan, Leuven, Belgium), Velmix(Kerr, Manufacturing company, USA), and Crytal Rock( Maruishi Gypsum Co. Ltd, Japan) were tested. A total of 160 casts were prepared, separated, and tested on the Instron Testing Machine(Model 4201, Co. USA). The obtained results of this study were as follows : 1. Fuji Reck and Velmix less 3ml than the water/power ratio of manufacturer's instruction showed the highest resistance to fracture. According to increasing water/powder ratio, fracture resistance was significantly increased(P<0.05). Crystal Rock showed the highest fracture value when it was mixed with the water/power ratio of manufacturer's instruction. 2. Water/powder ratio of the manufacturer's instructions and less 3ml than that showed lower fracture value of hand mix than that of vacuum mix. Water/powder ratio of more 3ml, 6ml than manufacturer's instructions was not significantly different between hand mix and vacuum mix(p>0.05). 3. Velmix had the highest viscoelastic value among three die materials when it was mixed with the manufacturer's instruction. Viscoelasticity was decreased according to increasing water/powder ratio.

  • PDF

중탄산칼슘을 이용한 자기충전형 콘크리트의 특성에 관한 연구 (A Study on the Properties of Self-Compacting Concrete Using Ground Calcium Carbonate)

  • 최연왕;정문영;임흥빈;황윤태
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2002년도 봄 학술발표회 논문집
    • /
    • pp.73-78
    • /
    • 2002
  • This study examines self-compacting of concrete using Ground Calcium Carbonate(GCC) gathering in limestone mine of Banyans district in order to make self-compacting concrete in the range of design strength 300kgf/cm$^2$ and the optimal mix proportion of self-compacting concrete that can use in field structure. The result shows that the optimal GCC replacement ratio is 45$\pm$5% in the normal strength of design strength 300kgf/cm$^2$ and that the volume ratio of the optimal fine aggregate used as the way satisfying both viscosity and compacting ability without separating materials is 46%. The optimal volume ratio of the coarse aggregate considering the economical aspect of concrete is 50%. It is desirable that the optimal mix proportion satisfying self-compacting for replacement of GCC is decided through mix design according to each replacement ratio.

  • PDF

초유동 콘크리트의 배합설계에 관한 연구 (The Study on the Mix Design of the Super Flowing Concrete)

  • 권영호;이상수;안재현;박칠림
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1996년도 가을 학술발표회 논문집
    • /
    • pp.283-289
    • /
    • 1996
  • In this paper, the mix design of the super flowing concrete is described with respcet to basic concept, confined water ratio($\beta_p$), volume ratio of water-binder(w/b), volume ratio of fine aggregates($S_r$) and coarse aggregates($G_v$). The primary purposes of this study are to evaluate the effects of cementitious materials(fly ash, slag cement, portland cement), mixing factors ($\beta_p$, w/b, $S_r$, $G_v$)., and to propose the mix design method of the super flowing concrete. As results of this study, confined water ratio($\beta_p$) of cementitious materials is very high (0.99~1.1), and then the ranges of the optimum mixing factors to be satisfied with the super flowing concrete are $S_r$ 47$\ell$ 2%, $G_v$ 52$\ell$ 1%.

  • PDF

고로슬래그 미분말을 함유한 고유동 모르터의 유동성상에 미치는 영향 요인에 관한 연구 (A Study on the Factors Affecting the High Fluid Mortar Containing Ground Granulated Blast-furnace Slag)

  • 김재훈;윤상천;지남용
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2002년도 학술.기술논문발표회
    • /
    • pp.29-36
    • /
    • 2002
  • High fluid concrete unlike OPC concrete is made with various material, and the phase of fresh concrete is considerably different. In order to understand fluidity phase and mix properties of high fluid concrete, concrete is required to access as suspension structure which consists of aggregate and paste. The focus of this paper is to analyze the test results and quantify the effect of mix proportions of molar and fineness modulus of ,and on the properties of fresh mortar. The effect of water-binder ratio, sand-binder ration, content; of ggbs (by mass of total cementitious materials), and various contents of water reducing agent on the yield stress and plastic viscosity of the mix is studied. Based on the experimental results, the following conclusion; can be drawn: (1) The mixing time needed (or high fluid mortar was approximately two times more than that of ordinary portland mortar. (2) The fluidity phase of mortar could be explained by yield stress of mix and the fluidity of mortar. (3) As the content of ggbs increased, yield stress of mortar was decreased and plastic viscosity of it was increased. (4) For the high fluid mortar, it was appeared that sand-binder ratio should be below 1.5.

  • PDF

수중불분리성 콘크리트의 해양공사 적용에 관한 기초적 연구 (A Fundamental Study on the Antiwashout Underwater Concrete for the Underwater Work of Ocean)

  • 김명식;윤재범;박세인
    • 콘크리트학회논문집
    • /
    • 제12권5호
    • /
    • pp.25-34
    • /
    • 2000
  • When concrete is placed underwater, it is diluted with separating cementitious material and as a result the quality of concrete becomes poor. To solve this problem, antiwashout underwater concrete is increasingly used for the construction and repair of the concrete structure underwater. The objective of this study is to investigate the characteristics of antiwashout underwater concrete as to the mix proportion, casting and curing water through experimental researches. The unit weight of water and cement, water-cement ratio, fine aggregate ratio, unit weight of antiwashout underwater agent and superplasticizer, and casting and curing water were chosen to measure the suspended solids, pH, air contents, slump flow, unit weight of hardened concrete, and compressive strength. From this study, the incremental modulus at mix proportion design and unit weight of antiwashout underwater agent were increased more than fresh water, and it is a optimum mix proportion that the unit weight of water(and cement) is 230kg/$\textrm{m}^3$(460kg/$\textrm{m}^3$), waterOcement ratio is 50%, fine aggregate ratio is 40%, unit weight of antiwashout underwater agent is 1.2% of water contents per unit weight of concrete, and unit weight of supeplasticizer is 2.5% of cement contents per unit weight of concrete when the antiwashout underwater concrete is used for the underwater work of ocean.

Analysis of Cutting Properties with Reference to Amount of Coolant used in an Environment-Conscious Turning Process

  • Yang, Seung-Han;Lee, Young-Moon;Kim, Young-Suk
    • Journal of Mechanical Science and Technology
    • /
    • 제18권12호
    • /
    • pp.2182-2189
    • /
    • 2004
  • In the recent years, environmentally conscious design and manufacturing technologies have attracted considerable attention. The coolants, lubricants, solvents, metallic chips and discarded tools from manufacturing operations will harm our environment and the earth's ecosystem. In the present work, the Tukey method of multiple comparisons is used to select the minimum level of coolant required in a turning process. The amount of coolant is varied in 270 designed experiments and the parameters cutting temperature, surface roughness, and specific cutting energy are carefully evaluated. The effects of coolant mix ratio as well as the amount of coolant on the turning process are studied in the present work. The cutting temperature and surface roughness for different quantity of coolant are investigated by analysis of variance (ANOVA) - test and a multiple comparison method. ANOVA-test results signify that the average tool temperature and surface roughness depend on the amount of coolant. Based on Tukey's Honestly Significant Difference (HSD) method, one of the multiple comparison methods, the minimum level of coolant is 1.0 L/min with 2% mix ratio in the aspect of controlling tool temperature. F-test concludes that the amount of coolant used does not have any significant effect on specific cutting energy. Finally, Tukey method ascertains that 0.5 L/min with 6% mix ratio is the minimum level of coolant required in turning process without any serious degradation of the surface finish. Considering all aspects of cutting, the minimum coolant required is 1.0 L/min with 6% mix ratio. It is merely half the coolant currently used i.e. 2.0 L/min with 10% mix ratio. Minimal use of coolant not only economically desirable for reducing manufacturing cost but also it imparts fewer hazards to human health. Also, sparing use of coolant will eventually transform the turning process into a more environment-conscious manufacturing process.

A Study on the Optimum Mix Proportion of the Mass Concrete Designed as Massive and Deep Structure

  • Kwon Yeong-Ho;Lee Hwa-Jin
    • 콘크리트학회논문집
    • /
    • 제17권2호
    • /
    • pp.293-302
    • /
    • 2005
  • This study describes data from determination of the optimum mix proportion and site application of the mass concrete placed in bottom slab and side wall having a large depth and section as main structures of LNG in-ground tank. This concrete requires low heat hydration, excellent balance between workability and consistency because concreting work of LNG in-ground tank is usually classified by under-pumping, adaptation of longer vertical and horizontal pumping line than ordinary pumping condition. For this purpose, low heat Portland cement and lime stone powder as cementitious materials are selected and design factors including unit cement and water content, water-binder ratio, fine aggregate ratio and adiabatic temperature rising are tested in the laboratory and batch plant. As experimental results, the optimum unit cement and water content are selected under $270kg/m^3$ and $l55{\~}l60 kg/m^3$ separately to control adiabatic temperature rising below $30^{\circ}C$ and to improve properties of the fresh and hardened concrete. Also, considering test results of the confined water ratio($\beta$p) and deformable coefficient(Ep), $30\%$ of lime stone powder by cement weight is selected as the optimum replacement ratio. After mix proportions of 5cases are tested and compared the adiabatic temperature rising($Q^{\infty}$, r), tensile and compressive strength, modulus of elasticity, teases satisfied with the required performances are chosen as the optimum mix design proportions of the side wall and bottom slab concrete. $Q^{\infty}$ and r are proved smaller than those of another project. Before application in the site, properties of the fresh concrete and actual mixing time by its ampere load are checked in the batch plant. Based on the results of this study, the optimum mix proportions of the massive concrete are applied successfully to the bottom slab and side wall in LNG in-ground tank.