• 제목/요약/키워드: microtensile bond strength

검색결과 107건 처리시간 0.019초

상아질 접착제의 성상이 미세인장결합강도에 미치는 영향 (THE EFFECT OF ADHESIVE PROPERTY ON MICROTENSILE BOND STRENGTH TO HUMAN DENTIN)

  • 김현진;허복;김현철
    • Restorative Dentistry and Endodontics
    • /
    • 제29권3호
    • /
    • pp.281-287
    • /
    • 2004
  • The purposes of this study were to evaluate the effect of adhesive property on microtensile bond strength and to determine the failure mode. Flat occlusal dentin surfaces were prepared using low-speed diamond saw. The dentin was etched with 37% phosphoric acid. The following adhesives were applied to the etched dentin to manufacturer's directions: Scotchbond Multi-Purpose in group SM, Prime&Bond NT in group NT, Scotchbond Multi-Purpose followed by Tetric-flow in group TR. After adhesive application, a cylinder of resin-based composite was built up on the occlusal surface. Each tooth was sectioned vertically to obtain the $1{\;}{\times}{\;}1\textrm{mm}^2$ "sticks". Microtensile bond strength were determined. Each specimen was observed under stereomicroscope and scanning electron microscope (SEM) to examine the failure mode. Data were analyzed using one way ANOVA. The results of this study were as follows:1. The microtensile bond strength value were:group SM ($18.98{\pm}3.01MPa$). group NT ($16.01{\pm}4.82MPa$) and group TR ($17.56{\pm}3.22MPa$). No significant statistical differences were observed among the groups (P>0.05). 2. Most of specimens showed mixed failure. In group TR, there was a higher number of specimens showing areas of cohesive failure in resin.

All-in-one adhesive의 다층적용이 미세인장결합강도에 미치는 영향 (THE EFFECT OF MULTIPLE APPLICATION ON MICROTENSILE BOND STRENGTH OF ALL-IN-ONE DENTIN ADHESIVE SYSTEMS)

  • 손성애;허복
    • Restorative Dentistry and Endodontics
    • /
    • 제29권5호
    • /
    • pp.423-429
    • /
    • 2004
  • The purpose of this study was to evaluate the effect of multiple application of all-in-one dentin adhesive system on microtensile bond strength using confocal laser scanning microscope and microtensile bond strength test. Flat occlusal dentin surfaces were prepared using low-speed diamond saw. In group I, Scotchbond Multipurpose (SM) was applied by manufacturer's recommendation. In group II, after Adper Prompt L-Pop was applied for 15s and light cured for 10s. the second coat was re-applied and light-cured. In group III, after light-curing the second layer. the third coat was re-applied and light-cured. Specimens bonded with a resin-composite were sectioned into resin-dentin stick for measuring the adhesive layer thickness by confocal laser scanning microscope and evaluating micro-tensile bond strength. The adhesive layers of three-step dentin adhesive system. 3 coats of Adper Prompt L-Pop had significantly thicker than SM. 2 coats of Adper Prompt L-Pop (p < 0.05). However. there was no significant differences in bond strengths between SM and 3 coats of Adper Prompt L-Pop (p > 0.05). And SM. 3 coats of Adper Prompt L-Pop had significantly higher than 2 coats of Adper Prompt L-Pop in bond strengths (p < 0.05).

Bonding of a resin-modified glass ionomer cement to dentin using universal adhesives

  • Ugurlu, Muhittin
    • Restorative Dentistry and Endodontics
    • /
    • 제45권3호
    • /
    • pp.36.1-36.10
    • /
    • 2020
  • Objectives: This study aims to assess the effect of universal adhesives pretreatment on the bond strength of resin-modified glass ionomer cement to dentin. Materials and Methods: Fifty caries-free human third molars were employed. The teeth were randomly assigned into five groups (n = 10) based on dentin surface pretreatments: Single Bond Universal (3M Oral Care), Gluma Bond Universal (Heraeus Kulzer), Prime&Bond Elect (Dentsply), Cavity Conditioner (GC) and control (no surface treatment). After Fuji II LC (GC) was bonded to the dentin surfaces, the specimens were stored for 7 days at 37℃. The specimens were segmented into microspecimens, and the microspecimens were subjugated to microtensile bond strength testing (1.0 mm/min). The modes of failure analyzed using a stereomicroscope and scanning electron microscopy. Data were statistically analyzed with one-way analysis of variance and Duncan tests (p = 0.05). Results: The surface pretreatments with the universal adhesives and conditioner increased the bond strength of Fuji II LC to dentin (p < 0.05). Single Bond Universal and Gluma Bond Universal provided higher bond strength to Fuji II LC than Cavity Conditioner (p < 0.05). The bond strengths obtained from Prime&Bond Elect and Cavity Conditioner were not statistically different (p > 0.05). Conclusions: The universal adhesives and polyacrylic acid conditioner could increase the bond strength of resin-modified glass ionomer cement (RMGIC) to dentin. The use of universal adhesives before the application of RMGIC may be more beneficial in improving bond strength.

도말층 존재 유무에 따른 One-step 접착 시스템의 미세인장결합강도 (MICROTENSILE BONDING OF ONE-STEP ADHESIVES TO SHEARED AND NON-SHEARED DENTIN)

  • 송용범;진정희;이세준;이광원
    • Restorative Dentistry and Endodontics
    • /
    • 제27권3호
    • /
    • pp.299-309
    • /
    • 2002
  • The purposes of this study were to evaluate the microtensile bond strength of one-step adhesives accord ing to various dentin surface treatments and to observe the interface between resin(Z-100$^{TM}$) and dentin under SEM. In this study forty-five non-caries extracted human molars and three adhesive systems were used ; AlI-Bond 2(AB), One-Up Bond F(OU), AQ-Bond(AQ). ; In Group 1, 2, 3, AB was used and tooth surfaces were treated by smearing(S), ultrasonic cleansing(US), etching(E) respectively. In Group 4. 5, 6, One-Up Bond F was used and tooth surfaces were also treated as the same way above. In Groups 7, 8, 9, AQ Bond was used and tooth surfaces wet$.$e treated as the same way. Each specimen was prepared for microtensile bond testing, and were stored for 24hrs in 37$^{\circ}C$ distilled water. After that, microtensile bond strength for each specimen was measured. Specimens were fabricated to examine the failure patterns of interface between resin and dentin and observed under the SEM. The results were as follows ; 1. The results(mean$\pm$SD) of microtensile test were group 1, 25.69$\pm$4.31MPa; group 2, 40.93$\pm$10.94MPa; group 3, 47.65$\pm$8.85MPa; group 4, 35.98$\pm$9.14MPa; group 5, 39.66$\pm$8.45MPa; group 6, 43.26$\pm$13.01MPa; group 7, 25.07$\pm$4.2MPa;group 8, 30.4$\pm$4.74MPa;group 9, 33.61$\pm$7.88MPa. 2. One-Up Bond F was showed the highest value of 36.98$\pm$9.14MPa in dentin surface treatment with smearing, and there were significant differences to the other groups (p<0.05). 3. All-Bond 2 was showed the highest value of 40.93$\pm$10.94MPa in dentin surface treatment with ultra-sonic cleansing, but was no significant difference to One-Up Bond F(p>0.05) 4. All-Bond 2 was showed the highest value of 47.65$\pm$8.85MPa in dentin surface treatment with etch ing(10%phosphoric acid), and there were significant differences to the other groups(p<0.05). 5. All-Bond 2 was showed the highest value of 47.65$\pm$8.85MPa in dentin surface treatment according to manufacture's directions. but was no significant difference to One-Up Bond F(p>0.05). 6. AQ Bond was skewed the lowest microtensile bond strength with various dentin surface treatment, and the were significant differences to the other groups(p<0.05).

The effect of multiple application on microtensile bond strength of all-in-one dentin adhesive systems

  • Son, Sung-ae;Hur, Bock
    • 대한치과보존학회:학술대회논문집
    • /
    • 대한치과보존학회 2003년도 제120회 추계학술대회 제 5차 한ㆍ일 치과보존학회 공동학술대회
    • /
    • pp.567-567
    • /
    • 2003
  • The purpose of this study was to evaluate the effect of multiple application of all-in-one dentin adhesive system on microtensile bond strength using confocal laser scanning microscope and microtensile bond strength test. The dentin surface of human molars, sectioned to remove the enamel from the occlusal surface were prepared. In group I, Scotchbond Multipurpose(SM, 3M ESPE) was applied by manufature's recommended. In group II, after the all-in-one adhesive, Adper Prompt L-Pop was applied for 15s, and light cured for 10s, the second coat was re-applied and light-cured.(omitted)

  • PDF

Bovine teeth에 대한 수 종 상아질 접착제의 미세인장결합강도 (MICROTENSILE BOND STRENGTH OF DENTIN BONDING ADHESIVES ON BOVINE TEETH)

  • 송은주;김재문;김신;정태성
    • 대한소아치과학회지
    • /
    • 제34권3호
    • /
    • pp.420-429
    • /
    • 2007
  • 전통적인 3단계 total-etching 시스템인 제 4세대 상아질 접착제로부터 술식의 단순화를 이루며 진화한 제 5, 6세대 및 최근에 소개된 제 7세대 상아질 접착제를 상아질 표면처리방식과 적용단계별로 구분하여 bovine teeth 상아질에 대한 미세인장결합강도를 측정하여 그 효용성을 비교 평가하였다. Bovine incisor의 상아질 표면을 노출시키고, 적절한 표면처리 후 제조사의 지시에 따라 5종의 상아질 접착제; 제 4 세대로 Scotch $Bond^{TM}$ Multipurpose(3M ESPE, USA), $Adper^{TM}$ Single Bond 2(3M ESPE, USA), 제 5세대 $Clearfil^{(R)}$ SE Bond(KURARAY, JAPAN), 제 6세대 AQ $Bond^{TM}$(SUN MEDICAL, JAPAN), 제 7세대 $Clearfil^{(R)}$ tri-S Bond(KURARAY, JAPAN)를 각각 적용하여 미세인장결합강도를 측정하고 접착계면의 파절양상을 관찰하였다. 연구결과 미세인장결합강도는 $Clearfil^{(R)}$ SE Bond군에서 가장 높았으며 다음으로 Scotch $Bond^{TM}$ Multipurpose군, $Adper^{TM}$ Single Bond 2군, AQ $Bond^{TM}$군, $Clearfil^{(R)}$ tri-S Bond군의 순으로 나타났다. 계면의 파절양상은 상대적으로 미세인장강도가 높게 나타난 Scotch $Bond^{TM}$ Multipurpose, $Adper^{TM}$ Single Bond2, $Clearfil^{(R)}$ SE Bond군은 레진의 응집성 파절이 많이 발생하였고 상대적으로 미세인장강도가 낮은 AQ $Bond^{TM}$, $Clearfil^{(R)}$ tri-S Bond 군의 경우에는 대부분 접착성 파절이 관찰되었다. 이상의 결과를 종합하면 상아질 접착제의 미세인장결합강도는 각 접착시스템별로 다소의 차이를 보이며, 특히 제 6, 7세대 상아질 접착제가 이전 세대보다 낮은 것으로 나타났다.

  • PDF

한 단계 자가 산부식 접착제의 적용 방식이 미세인장 결합강도에 미치는 효과 (Influence of application methods of one-step self-etching adhesives on microtensile bond strength)

  • 최철규;손성애;하진희;허복;김현철;권용훈;박정길
    • Restorative Dentistry and Endodontics
    • /
    • 제36권3호
    • /
    • pp.203-210
    • /
    • 2011
  • 연구목적: 이 연구의 목적은 다양한 방식의 한 단계 자가 부식 접착제의 적용이 직접 복합 레진 수복의 미세 인장 강도에 미치는 영향을 평가하는 것이었다. 연구 재료 및 방법: 36개의 발거된 대구치를 사용하여, 3종류의 한 단계 자가 부식 접착제(Clearfil Tri-S Bond, Adper Prompt L-Pop, G-Bond)와 적용 방식에 따라 12개의 군으로 나누었다. 접착제를 다음의 방식으로 상아질에 적용하였다. 1) single coating, 2) double coating, 3) manual agitation, 4) ultrasonic agitation. 접착제 적용 후, 광중합 복합 레진으로 수복하였다. 24시간 동안 실온의 증류수에 보관한 후, 각 군당 15개의 시편을 준비하여 미세인장 결합 강도를 측정하였다. 결과: Manual agitation, ultrasonic agitation군은 single coating, double coating군에 비해 유의하게 높은 미세인장 결합 강도를 보였다. Double coating군은 single coating군에 비해 유의하게 높은 미세인장 결합 강도를 보였으며, manual agitation군과 ultrasonic agitation군 간에는 미세인장 결합 강도의 유의한 차이가 없었다. 접착제 종류에 따라 미세인장 결합 강도의 유의한 차이가 있었고, 그 중 Clearfil Tri-S Bond가 가장 높았다. 결론: 한 단계 자가 산부식 접착제의 적용 방법과 재료에 따라 미세인장 결합 강도에 유의한 차이가 있었다. 접착제 종류에 관계없이 manual agitation과 ultrasonic agitation은 유의하게 높은 미세인장 결합강도를 보였다.

Removal of superficial dentin surface to restore decreased bond strength caused by sodium hypochlorite

  • Song, Mi-Yeon;Hwang, Ho-Keel;Jo, Hyoung-Hoon
    • 대한치과의사협회지
    • /
    • 제53권12호
    • /
    • pp.958-966
    • /
    • 2015
  • Objective: Sodium hypochlorite (NaOCl) decreases the bond strength of resin composite. The purpose of this study was to compare the effect of antioxidant and superficial dentin surface removal on the microtensile bond strength of NaOCl-treated dentin. Materials and Methods: Twenty non-carious human third molars were used in this study. The dentin surfaces were treated with 5.25% NaOCl for 10 min, followed either by treatment with 10% ascorbic acid or superficial dentin surface removal. Two-step self-etch adhesive and resin composite were used for restoration. The bonded specimens were subjected to the microtensile bond strength test. Statistical analysis was performed using one-way analysis of variance (ANOVA) and Tukey's test (p < 0.05). Results: The bond strength after removal of the superficial dentin surface following NaOCl irrigation was similar to that in the control group. The group treated with 10% ascorbic acid demonstrated significantly higher bond strength than the other groups. Conclusion: NaOCl irrigation-induced reduction in dentin bond strength could be recovered by either treatment with 10% ascorbic acid or simple removal of the superficial dentin surface.

Unground enamel에 대한 all-in-one adhesive의 1회 또는 2회 적용이 미세인장 결합강도에 미치는 영향 (Effects of one or two applications of all-in-one adhesive on microtensile bond strength to unground enamel)

  • 손창용;김현철;허복;박정길
    • Restorative Dentistry and Endodontics
    • /
    • 제31권6호
    • /
    • pp.445-451
    • /
    • 2006
  • 이 연구에서는 미세인장결합강도 실험과 주사전자현미경을 이용하여 unground enamel에 대한 all-in-one adhesive의 1회 또는 2회 적용에 따른 효과를 평가하였다. 발거된 하악 대구치의 설측 치관부를 사용하여 3개씩 5개의 군으로 분류하였다. SE군은 Clearfil$^{tm}$ SE Bond를 적용하였다. LP1 군, LP2 군은 Adper Prompt L-Pop$^{tm}$을 각각 1회 , 2회 적용하였다. XN1 군, XN2 군은 Xeno$^{R}$III를 각각 1회, 2회 적용하였다. 그런 다음 복합 레진 Z100을 적층 충전하였다. 법랑질 표면의 접착제를 아세톤으로 제거하고 주사 전자 현미경을 이용하여 산 부식 양상을 관찰하였다 미세인장결합강도 측정을 위해 표본을 절단하여 레진과 치아의 접착 계면이 1 mm$^2$이 되도록 하여 실험하였다. 실험의 결과는 One-way ANOVA를 사용해 분석한 다음 Duncan's post-hoc test로 사후 검정 하였다. 본 연구의 결과 all-in-one adhesive의 1회와 2회 적용간에는 유의한 차이가 나타나지 않았으며 two-step self-etching adhesive와 all-in-one adhesive의 산 부식 양상 모두 얕고 불규칙 하였다.

와동벽에서 접착제의 두께가 미세인장 결합강도에 미치는 영향 (The effect of adhesive thickness on microtensile bond strength to the cavity wall)

  • 이화언;김현철;허복;박정길
    • Restorative Dentistry and Endodontics
    • /
    • 제32권1호
    • /
    • pp.9-18
    • /
    • 2007
  • 이 연구의 목적은 와동벽에서 다른 위치에서의 상아질 접착제의 두께를 평가하고, 이런 다양한 접착제의 두께와 미세 인장 강도 사이의 관계를 평가하기 위한 것이다. 여섯 개의 인간 대구치에 모든 상아질 면이 노출되도록 I급 와동을 형성하였다 3개의 치아는 filled adhesive ($Clearfil^{TM}$ SE bond)를 와동 내에 도포하였고, 다른 3개의 치아는 unfilled adhesives ($Scotchbond^{TM}$ Multi Purpose)를 도포하였다. 형광 현미경을 이용하여 접착층의 형태와 두께를 관찰하였다. 접착제의 두께는 수직 와동벽을 따라 와동 변연, 와동벽 1/2, 와동 내각의 세 지점에서 측정되었다. $Scotchbond^{TM}$ Multi Purpose와 $Clearfil^{TM}$ SE bond가 와동 변연과 와동벽 1/2, 와동 내각에서의 접착제의 두께를 재현하여 미세 인장 결합 강도를 측정하였다. 이 실험의 결과에서 두 가지 상아질 접착제 모두에서 와동 내각에서의 접착제의 두께가 와동 변연과 와동벽 1/2위치에서의 두께보다 두꺼웠으며, 와동 내각의 두꺼운 접착제의 미세 인장 결합 강도는 와동 변연과 와동벽 1/2에서의 얇은 접착제 두께의 미세 인장 결합 강도보다 유의성 있게 높게 나타났다.