마그네슘 합금 스크랩의 진공증류에 관한 연구 (Study on the Distillation of Magnesium Alloy Scrap)

  • 위창현;유정민;장병록;유병돈
    • 대한금속재료학회지
    • /
    • 제46권1호
    • /
    • pp.13-19
    • /
    • 2008
  • To develop a recycling process of magnesium alloy scrap, a fundamental study on the distillation of magnesium alloy melt was carried out. Melt temperature, vacuum degree and reaction time were considered as experimental variables. The amount of vaporized magnesium melt per unit surface area of melt increases with the increase of melt temperature, reaction time and vacuum degree. The vapor condensed at the tip of water cooling Cu-condenser as a form of pine cone. Magnesium and zinc were vaporized easily from the melt. However, It's difficult to separate magnesium and zinc by vacuum distillation because vapor pressure of zinc is similar to one of magnesium. The contents of aluminum, manganese and iron, etc. in residual melt increase due to the decrease of magnesium and zinc content after the distillation of magnesium alloy.

용융-조직 성장에 의한 초전도성 $YBa_2Cu_3O_{7-x}$상의 생성 특성 (Phase Formation Characteristics of Superconducting $YBa_2Cu_3O_{7-x}$ Prepared by the Melt-Textured Growth)

  • 장현명;문길원
    • 한국세라믹학회지
    • /
    • 제27권5호
    • /
    • pp.677-683
    • /
    • 1990
  • Melt-textured growth of the YBa2Cu3O7-x phase from a supercooled melt created locally aligned, barshaped grains of the orthorhombic 1-2-3 phase. Based on all the observed phenomena, the gross mechanism of the melt-textrued growth of YBa2Cu3O7-x on the (100) plane of MgO was delineated by three basic patterns of reactions. These are : (ⅰ) formation of the aligned 1-2-3 phase and the Y-rich 2-1-1 phase at the bulk region away from the (100) plane of MgO ; (ⅱ) formation of the Cu-richprecipitates at the interfacial region by the selective interface-induced precipitation of the liquid phase ; (ⅲ) condensation reaction of the entrapped Cu-rich vapor with Mg atoms during the initial stage of rapid cooling from 130$0^{\circ}C$ to 98$0^{\circ}C$.

  • PDF

Synthesis and Hydrophilicities of Poly(ethylene 2,6-naphthalate)/ Poly(ethylene glycol) Copolymers

  • Son, Jun-Sik;Ji, Dong-Sun
    • Fibers and Polymers
    • /
    • 제4권4호
    • /
    • pp.156-160
    • /
    • 2003
  • Poly(ethylene 2,6-naphthalate) (PEN)/Poly(ethylene glycol) (PEG) copolymers were synthesized by two step reaction during the melt copolymerization process. The first step was the esterification reaction of dimethyl-2,6-naphthalenedicarbox-ylate (2,6-NDC) and ethylene glycol (EG). The second step was the condensation polymerization of bishydroxyethylnaphthalate (BHEN) and PEG. The copolymers contained 10 mol% of PEG units with different molecular weights. Structures and thermal properties of the copolymers were studied by using $^1{H-NMR}$, DSC, TGA, etc. Especially, while the intrinsic viscosities of PEN/PEG copolymers increased with increasing molecular weights of PEG, but the glass transition temperature, the cold crystallization temperature, and the weight loss temperature of the copolymers decreased with increasing molecular weights of PEG. Consequently, the hydrophilicities by means of contact angle measurement and moisture content of the copolymer films were found to be significantly improved with increasing molecular weights of PEG.

폴리아미드계 열가소성탄성체의 합성, 특성 및 응용 (Synthesis, Properties and Applications of Polyamide Thermoplastic Elastomers)

  • 이강석;최명찬;김성만;장영욱
    • Elastomers and Composites
    • /
    • 제45권3호
    • /
    • pp.156-164
    • /
    • 2010
  • 열가소성 탄성체(TPE)는 사용 온도 범위에서 일반 열경화성 고무와 같은 고무 탄성을 지니면서 용융 가공이 가능한 친환경 소재로써 산업 전반에 걸쳐 활용도가 꾸준히 증가하고 있다. 폴리아미드계 TPE (TPAE)는 하드세그멘트가 엔지니어링 플라스틱인 폴리아미드로 이루어져 있고, 소프트 세그먼트가 유리전이온도가 낮은 폴리에테르로 이루어진 다중 블록 공중합체로써 우수한 기계적 물성, 내화학성, 내열성 및 가공성을 나타낸다. 이러한 폴리아미드계 TPE는 하드 세그먼트와 소프트 세그먼트의 구조 및 상대적 조성에 따라 탄성체에서부터 연질 폴리아미드까지의 광범위한 특성이 발현되며, 또한, 다양한 무기 입자와의 하이브리드화를 통한 기능성 소재로의 활용이 기대되는 소재이다. 본 보문에서는 이러한 TPAE를 합성 할 수 있는 중합 방법과 특성 및 응용 분야에 대해 정리하였다.

초미세발포 사출성형을 이용한 천정형 에어컨 4-way 판넬의 공정 최적화에 관한 연구 (A Study on the Process Optimization of Microcellular Foaming Injection Molded Ceiling Air-Conditioner 4-Way Panel)

  • 김주권;이정희;김종선;이준한;곽재섭
    • 한국기계가공학회지
    • /
    • 제17권6호
    • /
    • pp.98-104
    • /
    • 2018
  • Deflected 4-way panels of ceiling air conditioners produced by injection molding process have caused dew condensation at the edge of products. In order to prevent this drawback with reducing weight and deformation, this study proposed renovated process adopting microcellular foaming. According to results from 2-sample t-test and analysis of variance(ANOVA), the critical factors affecting weight were melt temperature and injection speed. In addition, the vital effects on deformation were structure at the edge, mold temperature and cooling time. Optimal conditions of these parameters were derived by regressive analysis with CAE and response surface method(RSM), and then applied to an actual design and process stage to analyze performance. As a results, it clearly showed that new process improved process capability as well as reduced both weight and deformation by 18.8% and 71.9% respectively compared to the conventional method.

고분자의 자체발포를 이용한 세라믹 다공질체 (Ceramic Foams by the Self-Blowing of Polymer)

  • 백종원;김득중
    • 한국세라믹학회지
    • /
    • 제41권7호
    • /
    • pp.555-559
    • /
    • 2004
  • 폴리실록산 고분자의 자가 발포과정을 이용하여 세라믹 다공질체를 제조하였다. 고분자가 가교반응을 하는 과정에서 발생하는 물과 알콜 증기를 이용하면 고분자 용융액 내에 기공을 형성할 수 있다. 세라믹 다공질체 내의 기공의 크기와 모양은 고분자 용융액의 점도에 따라 크게 달라진다. 충진제인 A1$_2$O$_3$ 함량이 증가하면 기공 크기는 감소하며 이는 A1$_2$O$_3$의 입자크기가 감소하여도 비슷한 양상을 보였다. 고분자 용융액의 점도는 고분자의 가교반응정도에 따라서도 영향을 받는다. 발포 전에 13$0^{\circ}C$에서 열처리를 하면 점도는 증가하며 다공질체의 기공 안정성은 증가한다. 제조된 세라믹 다공질체의 밀도와 압축강도는 발포과정에서의 승온속도에 따라 다른 값을 보였다.

유기티타늄을 촉매로 한 폴리트리메틸렌테레프탈레이트 합성에 관한 연구 (Synthesis of Poly(trimethylene terephthalate) Using an Organic Titanium Compound as a Catalyst)

  • Pio Sifuentes;Kim, Kap-Jin
    • 한국섬유공학회:학술대회논문집
    • /
    • 한국섬유공학회 2003년도 봄 학술발표회 논문집
    • /
    • pp.335-336
    • /
    • 2003
  • The synthesis of poly(trimethylene terephthalate) (PTT), whose application is being expanded very rapidly to new apparel and carpet materials, was investigated by melt condensation polymerization using 1,3-propanediol (PDO) and terephthalic acid (TPA). No catalyst was used in the 1st step reaction (esterification), but tetrabutyl titanate(TBT) was used as a polyesterification catalyst ranging from 25 to 75 ppm based on the weight of TPA used in the 2nd step reaction (polyesterification). The molar ratio of PDO to TPA was set as 2.2:1. The effect of reaction conditions on the color and intrinsic viscosity of the final product was investigated. (omitted)

  • PDF

Surface Modified Glass-Fiber Effect on the Mechanical Properties of Glass-Fiber Reinforced Polypropylene Composites

  • Park, Sanghoo;Kim, Su-Jong;Shin, Eun Seob;Lee, Seung Jun;Kang, Beom Mo;Park, Kyu-Hwan;Hong, Seheum;Hwang, Seok-Ho
    • Elastomers and Composites
    • /
    • 제54권3호
    • /
    • pp.182-187
    • /
    • 2019
  • To improve the mechanical properties of glass-fiber-reinforced polypropylene (PP) composites through interfacial adhesion control between the PP matrix and glass fiber, the surface of the glass fiber was modified with PP-graft-maleic anhydride (MAPP). Surface modification of the glass fiber was carried out through the well-known hydrolysis-condensation reaction using 3-aminopropyltriethoxy silane, and then subsequently treated with MAPP to produce the desired MAPP-anchored glass fiber (MAPP-a-GF). The glass-fiber-reinforced PP composites were prepared by typical melt-mixing technique. The effect of chemical modification of the glass fiber surface on the mechanical properties of composites was investigated. The resulting mechanical and morphological properties showed improved interfacial adhesion between the MAPP-a-GF and PP matrix in the composites.

전바나듐계 레독스-흐름 전지용 IPA-co-HDO-co-(TPA/MA) 음이온교환막의 합성 및 특성 (Synthesis and Characterization of IPA-co-HDO-co-(TPA/MA) Anion-Exchange Membrane for All-Vanadium Redox Flow Battery)

  • 정재철;곽노석;황택성
    • 폴리머
    • /
    • 제35권6호
    • /
    • pp.593-598
    • /
    • 2011
  • 본 연구에서는 전바나듐 레독스-흐름 전지용 음이온교환막의 제조를 위하여 isophthalic acid (IPA), 1,6-hexanediol(HDO), terephthalic acid(TPA), maleic anhydride(MA)의 용융 축합중합 방법에 의해 IPA-co-HDO-co-(TPA/MA)(IHTM) 공중합체를 합성하였다. 합성된 IHTM 공중합체 아민화 반응을 trimethylamine으로 하였으며, UV 가교 반응을 통하여 음이온교환막을 제조하였다. IHTM 공중합체의 구조 및 열안정성을 FTIR, $^1H$ NMR, TGA 분석을 통하여 확인하였다. 또한 IHTM 음이온교환막의 함수율, 이온교환용량, 전기저항, 전기전도도를 중량법, 적정법 및 LCR 미터로 측정하였으며, 전바나듐 레독스-흐름 전지의 효율 실험을 하였다. 막의 이온교환용량, 전기저항, 전기전도도는 각각 1.10 meq/g, $1.98{\Omega}{\cdot}cm^2$, 0.009 S/cm로 우수하게 나타났으며, 전바나듐 레독스-흐름 전지의 충 방전효율, 전압효율 및 에너지효율은 각각 96.5, 74.6, 70.0%이었다.

다이머산계 폴리아미드의 합성 및 특성에 관한 연구 (Synthesis and Characterization of Dimer Acid-Based Polyamides)

  • 박현주;전호균;오상택
    • 접착 및 계면
    • /
    • 제17권4호
    • /
    • pp.136-140
    • /
    • 2016
  • 본 연구에서는 aliphatic diamine 또는 aromatic diamine을 함유하는 다이머산계 폴리아미드 수지를 축합중합법으로 합성하였으며, FT-IR로 폴리아미드가 합성되었음을 확인하였다. Diamine의 구조에 따라 합성된 폴리아미드의 기계적, 열적 특성을 확인하였다. 방향족 diamine 함유 폴리아미드(DAP)의 경우 지방족 diamine 함유 폴리아미드(DAH) 보다 인장강도와 전단접착강도가 우수하였다. DSC thermogram에서 DAP는 DAH 보다 높은 $T_g$$T_m$을 나타내었다. DAP의 연화점은 $112-115^{\circ}C$이고, DAH는 $98-121^{\circ}C$이었다.