Search Result 164, Processing Time 0.027 seconds

Marginal and internal fit of nano-composite CAD/CAM restorations

  • Park, So-Hyun;Yoo, Yeon-Jee;Shin, Yoo-Jin;Cho, Byeong-Hoon;Baek, Seung-Ho
    • Restorative Dentistry and Endodontics
    • /
    • v.41 no.1
    • /
    • pp.37-43
    • /
    • 2016
  • Objectives: The purpose of this study was to compare the marginal and internal fit of nano-composite CAD-CAM restorations. Materials and Methods: A full veneer crown and an mesio-occluso-distal (MOD) inlay cavity, which were prepared on extracted human molars, were used as templates of epoxy resin replicas. The prepared teeth were scanned and CAD-CAM restorations were milled using Lava Ultimate (LU) and experimental nano-composite CAD/CAM blocks (EB) under the same milling parameters. To assess the marginal and internal fit, the restorations were cemented to replicas and were embedded in an acrylic mold for sectioning at 0.5 mm intervals. The measured gap data were pooled according to the block types and measuring points for statistical analysis. Results: Both the block type and measuring point significantly affected gap values, and their interaction was significant (p = 0.000). In crowns and inlays made from the two blocks, gap values were significantly larger in the occlusal area than in the axial area, while gap values in the marginal area were smallest (p < 0.001). Among the blocks, the restorations milled from EB had a significantly larger gap at all measuring points than those milled from LU (p = 0.000). Conclusions: The marginal and internal gaps of the two nano-composite CAD/CAM blocks differed according to the measuring points. Among the internal area of the two nano-composite CAD/CAM restorations, occlusal gap data were significantly larger than axial gap data. The EB crowns and inlays had significantly larger gaps than LU restorations.

Interface Phenomena between Prosthodontic Crown and Abutment Sprayed with Die Spacer (Die Spacer가 도포된 보철용 크라운과 어버트먼트의 계면현상)

  • Park, K.H.;Choe, H.C.
    • Journal of the Korean institute of surface engineering
    • /
    • v.40 no.4
    • /
    • pp.197-202
    • /
    • 2007
  • Fit of the restoration and its cementation procedure is crucial to both its short and long term prognosis. Marginal fit is affected by many variables during the fabrication process. These variables, being intrinsic properties of the materials or the clinical technique used, can cause changes in the size and shape of the definitive restoration. Even if all variables are controlled carefully, the seating of a restoration can still be affected due to insufficient space for the luting agent. The use of die spacer can reduce the elevation of a cast restoration of a prepared tooth, decreased seating time, improve the outflow of excess cement, and lower the seating forces. The purpose of this study was to evaluate the marginal fidelity according to die spacer application times and measurement site. Casting alloys were prepared and fabricated using non-precious metal at $950^{\circ}C$. Specimens are divided into four groups: I(die spacer painted casting for wax pattern), II(die spacer non painted casting for wax pattern). The specimens were cut and polished for marginal gap observation. The marginal gap was observed using scanning electron microscopy (SEM).

How adjustment could affect internal and marginal adaptation of CAD/CAM crowns made with different materials

  • Hasanzade, Mahya;Moharrami, Mohammad;Alikhasi, Marzieh
    • The Journal of Advanced Prosthodontics
    • /
    • v.12 no.6
    • /
    • pp.344-350
    • /
    • 2020
  • PURPOSE. Recently introduced hybrid and reinforced glass ceramic computer-aided design/computer-aided manufacturing (CAD/CAM) materials have been used for full-coverage restorations. However; the effect of adjustment and type of materials on internal and marginal adaptation are unknown. This study aimed to evaluate and compare the marginal and internal adaptations of crowns made of three different CAD/CAM materials before and after adjustment. MATERIALS AND METHODS. One acrylic resin maxillary first molar was prepared and served as the master die. Thirty-six restorations were fabricated using CAD/CAM system (CEREC Omnicam, MCXL) with three materials including lithium disilicate (IPS e.max CAD), zirconia-reinforced lithium silicate (Suprinity), and hybrid ceramic (Enamic). Internal and marginal adaptations were evaluated with the reference point matching technique before and after adjustment. The data were analyzed using mixed ANOVA considering α=.05 as the significance level. RESULTS. The effect of adjustment and its interaction with the restoration material were significant for marginal, absolute marginal, and occlusal discrepancies (P<.05). Before adjustment, Suprinity had lower marginal discrepancies than IPS e.max CAD (P=.18) and Enamic (P=.021); though no significant differences existed after adjustment. CONCLUSION. Within the limitations of this study, crowns fabricated from IPS e.max CAD and Suprinity resulted in slightly better adaptation compared with Enamic crowns before adjustment. However, marginal, axial, and occlusal discrepancies were similar among all materials after the adjustment.

In vitro evaluation methods on adaptation of fixed dental prosthesis (고정성 보철물의 적합도에 대한 실험적 평가방법)

  • Lee, Hyunho;Lee, Du-Hyeong;Lee, Kyu-Bok
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.33 no.2
    • /
    • pp.63-70
    • /
    • 2017
  • Clinically, the fit of fixed prosthesis is an essential element for successful restoration. The fit of prosthesis is largely classified into marginal fit and internal fit, and various methods to assess these have been introduced including microscopic margin measurement, cross-sectional measurement, silicone replica technique, 3-dimensional scanning data superposition, weight technique and micro CT scanning. Thus, this study is aimed at proposing a more convenient and accurate measurement method of fits in a digital environment by comparatively analyzing the advantages and disadvantages of each known method based on existing literature.

An Evaluation Validity of the Silicone Replica Technique at Measurement on Fit of Fixed Dental Prostheses (고정성 보철물의 적합도 측정 시 사용하는 실리콘 복제본 기술의 정확도 평가)

  • Kim, Jae-Hong;Kim, Ki-Baek
    • Journal of dental hygiene science
    • /
    • v.12 no.6
    • /
    • pp.566-571
    • /
    • 2012
  • Marginal and internal fit are very important factor for the clinical long-term success of fixed dental prostheses (FDPs). A variety of methods have been applied to the measuring marginal and internal fit of FDPs. The purpose of this study was to compare the marginal and internal fit of 2 different measuring methods silicone replica technique [SRT] and die cutting technique (DCT). SRT, the space between die and FDPs were filled with light-body silicone, then stabilized by medium-body silicone. DCT, the FDPs were cemented on definitive dies and embedded into epoxy. The silicone replicas and epoxies were sectioned mesio-distal and measured 4 locations (margin, rounded chamfer, axial, occlusal) and using a digital microscope at a magnification $\times$160. For the SRT the mean${\pm}$SDs fit (${\mu}m$) recorded were: margin $88.7{\pm}22.2$, rounded chamfer $90.6{\pm}25.0$, axial wall $61.5{\pm}21.8$, occlusal $134.9{\pm}30.8$. For the DCT the mean${\pm}$SDs fit (${\mu}m$) recorded were: margin $85.3{\pm}18.0$, rounded chamfer $85.4{\pm}24.7$, axial wall $62.0{\pm}21.3$, occlusal $131.7{\pm}30.5$. The mean${\pm}$SDs size (${\mu}m$) of SRT margin was $88.7{\pm}22.2$ and of DCT margin was $85.3{\pm}18.0$. There were no statistically significant difference (p<0.05) of the four parts between SRT and DCT. It is considered an appropriate case to use SRT at fit of FDPs.

Effect of machining precision of single ceramic restorations on the marginal and internal fit (단일 도재 수복물의 가공 정밀도가 변연 및 내면 적합도에 미치는 영향)

  • Son, Keunbada;Yu, Beom-Young;Lee, Kyu-Bok
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.58 no.4
    • /
    • pp.313-320
    • /
    • 2020
  • Purpose: The purpose of this study was to evaluate the machining precision and the marginal and internal fit of single restorations fabricated with three types of lithium disilicate ceramic blocks and to evaluate the correlation. Materials and methods: Single restorations were designed using a CAD software program. The crown designed model file was extracted from the CAD software program. Three types of lithium disilicate blocks (Rosetta; HASS, IPS e.max CAD; Ivoclar vivadent, VITA Suprinity; VITA) were milled using a milling machine. For the fabrication of the crown scanned model file, the intaglio surface of the restoration was digitized using a contact scanner. Then, using the three-dimensional inspection software (Geomagic control X; 3D Systems), the process of the overlap of the crown designed model and the scanned model and 3-dimensional analysis was conducted. In addition, the marginal and internal fit of the crowns was evaluated by a silicone replication method. The difference among three types of single ceramic crown was analyzed using a Kruskal-Wallis H test, and Spearman correlation analysis was performed to analyze the correlation between machining precision and fitness (α=.05). Results: There was a significant difference in the machining precision and the marginal and internal fit according to the type of ceramic block (P<.001). In addition, the machining precision and the marginal and internal fit were positively correlated (P<.001). Conclusion: The marginal fit of crowns fabricated according to the types of ceramic blocks was within the clinically acceptable range (< 120 ㎛), so it can be regarded as appropriate machining precision applicable to all clinical as aspects in terms of the marginal fit.

Evaluation of marginal fidelity of copy-milled and CAD/CAM all ceramic crowns

  • Jeong Seung-Mi;Kang Dong-Wan;Wolf Christoph
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.39 no.3
    • /
    • pp.243-249
    • /
    • 2001
  • Statement of the problem. The interest in all-ceramic restorations has increased as more techniques have become available. With the introduction of machinable dental ceramics and CAD/CAM systems or Copy-milling systems there is a need for evaluating the quality levels of these new fabrication techniques. Purpose. This study was to evaluate the fitting accuracy of machined all-ceramic crowns made out of an industrially prefabricated feldspathic porcelain. Material and Methods. Three master models with different cutting depth (0.8mm/1.0mm/1.2mm)were produced using a palladium-silver alloy. A total of 36 working dies, 12 of each form, was used for the modellation of prototype resin copings and 36 additional crowns, 12 of each cutting depth, were produced by using the $CEREC^{(R)}2$ system for all crowns. The maginal fit of all 72 crowns was then evaluated on their respective master die at 54 circularly staggered points of measurement per crown under a fixation pressure of 30 N by using a computerized video image system. Results. The medians of the copy-milled $CELAY^{(R)}$ crowns ranged from 29 to $36{\mu}m$. The highest value for the marginal gap was found in group B (cutting depth 1.0mm) at $107{\mu}m$. The median for the $CEREC^{(R)}2$ crowns was found between 43.5 and $70{\mu}m$. The maximum values for all three groups ranged from $181{\mu}m$ to $286{\mu}m$. With $286{\mu}m$ the highest value for marginal gap was found in group C. the Kruskal-Wallis test and multiple comparisons analysis procedure revealed a significant influence of the production technique on the marginal fit in all three groups (p<0,02). Conclusion. 1. The $CELAY^{(R)}$ system is capable to produce all-ceramic crowns with a significantly better marginal fit than the $CEREC^{(R)}2$ system. 2. As far as premolar crowns produced with the $CEREC^{(R)}2$ system are concerned, the cutting depth has a significant influence on fitting accuracy. 3. The production of crowns with an acceptable marginal fit is possible with both systems. However, adhesive luting is recommended for milled feldspathic porcelain crowns.

  • PDF

Influence of final crystallization process on precision of fit of monolithic CAD/CAM-generated restorations by lithium disilicate: A comparative study (리튬 디실리케이트 최종 결정화 과정이 CAD/CAM으로 제조된 수복물의 적합도에 미치는 영향)

  • Kim, Jae-Hong;Kim, Ki-Baek
    • Journal of Technologic Dentistry
    • /
    • v.41 no.4
    • /
    • pp.271-278
    • /
    • 2019
  • Purpose: To quantify the effect of the crystallization process on lithium disilicate ceramic crowns that are fabricated using a computer-aided design/computer-aided manufacturing(CAD/CAM) system, and to determine whether they are clinically acceptable by comparing values before and after the crystallization process. Methods: The maxillary first molar was selected as the abutment for the experiments. Ten working models were prepared. Marginal and internal gap of 4 groups of lithium disilicate crowns(n=10) fabricated with conventional method. Comparison was performed using the silicone replica technique and 3D superimposition analysis. The marginal and internal gaps of the restoration were measured before and after the crystallization process of this prosthesis. The average value of each part(the average of values measured before and after the crystallization) was statistically analyzed using paired t-test(α=0.05). Results: The results from the second phase of this research, which compared the average value of the gap between the marginal and internal fits of the lithium disilicate single crown before and after the crystallization process, indicated that the marginal gap was larger and the internal gap was smaller after the crystallization process, and this difference was statistically significant (P<0.05) in all the parts evaluated. Conclusion: While the shrinkage that occurs during crystallization does affect the marginal and internal fit of the prosthesis, it cannot be concluded to be a major effect because the resultant distortion was within the clinically acceptable range.

Study on methodology for the assessment of internal and marginal adaptation on fixed dental prosthesis (고정성 보철물의 내면 및 변연적합도를 평가하는 방법에 대한 고찰)

  • Pyo, Se-Wook;Lee, Jun-Jae;Han, Jung-Suk;Lim, Young-Jun
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.32 no.3
    • /
    • pp.158-168
    • /
    • 2016
  • This article is to review various methods used to investigate internal and marginal adaptation of fixed dental prostheses, and to summarize a merit, worth, and limitation of each method, using some results of previous studies. The methods of measuring internal and marginal gap are divided into two categories in this study; in vivo and in vitro. In vivo methods are clinical evaluations, including exploration, radiography, and impression technique. In vitro methods are laboratory evaluations such as direct view, cross-sectioning, and silicone replica technique using microscope. Measuring by micro computed tomography (CT) or profilometer is also in vitro methods. In recent years, the development of scanning systems is able to analyze 3-dimensional internal and marginal space in detail. As measuring and analyzing technology become more advanced, the ability to thoroughly examine crown adaptation is becoming both simpler and more efficient.

Marginal fit evaluation of 3 unit fixed dental prostheses fabricated by rapid prototyping method (쾌속 조형 기술을 이용하여 제작된 3본 고정성 보철물의 적합도 평가)

  • Kim, Ki-Baek;Kim, Jae-Hong;Kim, Woong-Chul;Kim, Hae-Young;Kim, Ji-Hwan
    • Journal of Technologic Dentistry
    • /
    • v.34 no.2
    • /
    • pp.105-111
    • /
    • 2012
  • Purpose: The purpose this study was to evaluate the marginal fitness of metal copings fabricated using rapid prototyping method and to compare the fitness with copings by conventional method. Then clinical availability of fixed dental prostheses (FDPs) fabricated using rapid prototyping method shall be confirmed based on marginal fitness. Methods: Ten same cases of3 unit FDPs epoxy models (abutment teeth 14 and 16) were manufactured. Each of ten epoxy models were scanned by 3shape D-700 scanner to be designed by experienced technician, and photopolymer 3 unit FDPs were fabricated using rapid prototyping methodand fabricated using Lost wax technique (LW) with same models. Marginal fitness of 3 unit FDPs were measured by silicone replica technique. T-test of independent sample for statistical analysis was executed with SPSS 12.0K for Windows. (${\alpha}$=.05) Results: Significantly higher mean (SD) marginal fitness (P<.000) were observed in the RP group $(95.9(18.0){\mu}m$ compared to the conventionally LW group $(80.1(13.8){\mu}m$. Conclusion: Marginal fitness of LW group showed excellent rather than RP group. However marginal fitness of 3 unit FDPs fabricated by RP method did not get out of clinical allowance value range significantly to allow clinical application.