Objectives: The purpose of this study was to evaluate the effect of adhesive luting on the fracture resistance of zirconia compared to that of a composite resin and a lithium disilicate glass ceramic. Materials and Methods: The specimens (dimension: $2mm{\times}2mm{\times}25mm$) of the composite resin, lithium disilicate glass ceramic, and yttria-stabilized tetragonal zirconia polycrystal (Y-TZP) were prepared. These were then divided into nine groups: three non-luting groups, three non-adhesive luting groups, and three adhesive luting groups, for each restorative material. In the non-luting groups, specimens were placed on the bovine tooth without any luting agents. In the non-adhesive luting groups, only zinc phosphate cement was used for luting the specimen to the bovine tooth. In the adhesive luting groups, specimens were pretreated, and the adhesive luting procedure was performed using a self-adhesive resin cement. For all the groups, a flexural test was performed using universal testing machine, in which the fracture resistance was measured by recording the force at which the specimen was fractured. Results: The fracture resistance after adhesive luting increased by approximately 29% in the case of the composite resin, 26% in the case of the lithium disilicate glass ceramic, and only 2% in the case of Y-TZP as compared to non-adhesive luting. Conclusions: The fracture resistance of Y-TZP did not increased significantly after adhesive luting as compared to that of the composite resin and the lithium disilicate glass ceramic.
본 연구는 심미 치과보철물에 사용되는 지르코니아, lithium disilicate 코어와 전장도재 사이의 전단결합강도를 측정하고, 금속도재관을 대조군으로 설정하여 비교하였다. 직사각기둥 모양의 시편을 각각 10개씩 제작하여 코어와 전장도재 사이의 전단결합강도를 측정한 후 파절면의 양상을 실체현미경을 통해 관찰하였다. 제한된 조건하에 시행된 실험을 통하여 심미보철 분야에 널리 적용되고 있는 치과용세라믹 코어의 전단결합강도를 확인하였으며, 측정 후 비교분석된 결과는 다음과 같다. 2종의 치과용 세라믹 코어와 전장도재 간에 전단결합강도는 금속도재관의 전단결합강도와 유의한 차이가 있었다 (p<0.05). 본 실험 결과를 토대로 ZB군은 임상적으로 받아들여지는 전단결합강도 범위 내 분포를 보이지만, LB군은 임상허용 범위에 못 미치는 결과값을 보였다. 금속도재관과 달리 지르코니아, lithium disilicate 전부도재관은 모두 혼합형 파절양상을 보였다. 결론적으로 전단결합강도 실험에 사용된 시편이 임상적인 치과보철물의 형태와는 달리 실험을 위한 시편의 형태로 제작되어 임상적 결과를 반영하지 못했으며 구강 내의 상황과도 다르다는 한계점을 가지고 있다. 추후에는 이를 보완하여 치과보철물과 유사한 형태의 시편을 이용한 전단결합 강도의 측정과 구강 내 조건을 고려한 추가 실험이 필요하다고 생각된다.
PURPOSE. Translucency and colour stability are two most important aspects for an aesthetic dental restoration. Glass ceramic restorations are popular amongst clinicians because of their superior aesthetic properties. In the last decade, zirconia has generated tremendous interest due to its favorable mechanical and biological properties. However, zirconia lacks the translucency that lithium disilicate materials possess and therefore has limitations in its use, especially in esthetically demanding situations. There has been a great thrust in research towards developing translucent zirconia materials for dental restorations. The objective of the study was to evaluate and compare the transmittance of a translucent variant of zirconia to lithium disilicate. MATERIALS AND METHODS. Two commercially available zirconia materials (conventional and high translucency) and 2 lithium disilicate materials (conventional and high translucency) with standardized dimensions were fabricated. Transmittance values were measured for all samples followed by a microstructural analysis using a finite element scanning electron microscope. One way analysis of variance combined with a Tukey-post hoc test was used to analyze the data obtained (P=.05). RESULTS. High translucency lithium disilicate showed highest transmittance of all materials studied, followed by conventional lithium disilicate, high translucency zirconia and conventional zirconia. The difference between all groups of materials was statistically significant. The transmittance of the different materials correlated to their microstructure analysis. CONCLUSION. Despite manufacturers' efforts to make zirconia significantly more translucent, the transmittance values of these materials still do not match conventional lithium disilicate. More research is required on zirconia towards making the material more translucent for its potential use as esthetic monolithic restoration.
Purpose: The purpose of this study was to compare the marginal and internal fit of lithium disilicate ceramic inlay produced by heat pressing that inlay pattern made by subtractive manufacturing and additive manufacturing method. Methods: A mandibular lower first molar that mesial occlusal cavity (MO cavity) die was prepared. After fabricating an epoxy resin model using a silicone impression material, epoxy resin die was scanned with a dental model scanner to design an MO cavity inlay. The designed STL pile was used to fabricate wax patterns and resin patterns, and then lithium disilicate ceramic inlays were fabricated using hot-press method. For the measurement of the marginal and internal gap of the lithium disilicate, silicone replica method was applied, and gap was measured through an optical microscope (x 80). Data were tested for significant differences using the Mann-Whitney Utest. Results: The marginal fit was 103.56±9.92㎛ in the MIL-IN group and 81.57±9.33㎛ in the SLA-IN group, with a significant difference found between the two groups (p<0.05). The internal fit was 120.99±17.52㎛ in the MIL-IN group and 99.18±6.65㎛ in the SLA-IN group, with a significant difference found between the two groups (p<0.05). Conclusion: It is clinically more appropriate to apply the additive manufacturing than subtractive manufacturing method in producing lithium disilicate inlay using CAD/CAM system.
Purpose: This study was to compare adaptations of lithium disilicate CAD/CAM crowns fabricated with different scanning systems. Methods: This study selected the mandibular right first molar as an abutment for experiments and produced 10 working models. Lithium disilicate crowns appropriate for each abutment were produced by using a CEREC$^{(R)}$ CAD/CAM system. The independent t-test was then used to compare and analyze the data obtained from the two groups(${\alpha}$=0.05). Results: Mean(SD) adaptation were $86.93(22.82){\mu}m$ for the InS group, $88.42(26.77){\mu}m$ for the ExS group. They were no statistically significant differences between groups for adaptation(p>0.05). Conclusion: Within the limitations of this study, the results suggest that the accuracy of all investigated optical scanner were satisfactory for clinical use. Further assessment and improvement of the lithium disilicate ceramic for the fabrication of FPDs is evidently still required.
PURPOSE. The purpose of this study was to evaluate and compare the translucency of shaded zirconia allceramic systems. MATERIALS AND METHODS. Translucency of 3 different zirconia all-ceramic systems colored by different techniques was compared with a lithium disilicate glass-ceramic (IPS e.max Press). Square-shaped specimens with 0.5 mm thickness were fabricated from In-Ceram YZ, ICE Zirkon and Katana systems in A1, A2 and A3.5 shades according to Vitapan Classical shade tab (n=11). Specimens were then veneered and glazed with corresponding veneer ceramic recommended by each zirconia system manufacturer and the total thickness was set to 1.5 mm. Translucency measurements were performed with VITA Easyshade Compact spectrophotometer after each stage and translucency parameter was calculated. Data were statistically analyzed with repeated measures ANOVA and Tukey multiple comparison test. RESULTS. The control group was significantly more translucent than the zirconia systems (P<.05). ICE Zirkon cores showed the least translucency; neither In-Ceram YZ nor Katana systems were superior to each other in terms of translucency. Translucency of all specimens was decreased after veneering, and the translucency rankings were changed. CONCLUSION. Coloring technique did not have a significant effect on translucency of zirconia cores. Although zirconia systems were less translucent than lithium disilicate glass ceramic, they had partial translucency and there were translucency differences among the zirconia systems. Chroma affected the translucency of precolored zirconia cores.
This investigation was designed to determine whether heat-pressing and/or simulated heat treatments affected the flexure strength and the microstructure of the lithium disilicate glass-ceramic in the IPS Empress 2 system. Four groups of the specimens were prepared as follows: group 1 - as-received material, group 2 - heat-pressed material; group 3 - heat-pressed and simulated initial heat-treated material; group 4 - heat-pressed and the simulated heat-treated material with full firings for a final restoration. The three-point bending test and the scanning elec-tron microscope (SEM) analysis was conducted for the purpose of this study. The flexure strength of group 2 was significantly higher than that of group 1. However, there were no significant differences in strength among group 2, 3, and 4, and between group 1 and 4. The SEM micrographs of the lithium disilicate glass-ceramic showed the closely packed, multi-directionally interlocking microstructure of numerous lithium disilicate crystals protruding from the glass matrix. The crystals of the heat-pressed materials (group 2, 3, and 4) were a little denser and about two times bigger than those of the as-received material (group 1). This change of microstructure is more obviously exhibited particularly between group 1 and 2. However, there was no a marked difference among group 2, 3, and 4 after the heat-pressing procedure. Although there were significant increase of the strength and some changes of the microstructure after the heat-pressing operation, the combination of the heat-pressing and the simulated subsequent heat treatments did not produce the increase of strength of IPS Empress 2 glass-ceramic.
PURPOSE. Pre-surface treatments of coping materials have been recommended to enhance the bonding to the veneering ceramic. Little is known on the effect on shear bond strength, particularly with new coping material. The aim of this study was to investigate the shear bond strength of veneering ceramic to three coping materials: i) metal alloy (MA), ii) zirconia oxide (ZO), and iii) lithium disilicate (LD) after various pre-surface treatments. MATERIALS AND METHODS. Thirty-two (n = 32) discs were prepared for each coping material. Four pre-surface treatments were prepared for each sub-group (n = 8); a) no treatment or control (C), b) sandblast (SB), c) acid etch (AE), and d) sandblast and acid etch (SBAE). Veneering ceramics were applied to all discs. Shear bond strength was measured with a universal testing machine. Data were analyzed with two-way ANOVA and Tukey's multiple comparisons tests. RESULTS. Mean shear bond strengths were obtained for MA ($19.00{\pm}6.39MPa$), ZO ($24.45{\pm}5.14MPa$) and LD ($13.62{\pm}5.12MPa$). There were statistically significant differences in types of coping material and various pre-surface treatments (P<.05). There was a significant correlation between coping materials and pre-surface treatment to the shear bond strength (P<.05). CONCLUSION. Shear bond strength of veneering ceramic to zirconia oxide was higher than metal alloy and lithium disilicate. The highest shear bond strengths were obtained in sandblast and acid etch treatment for zirconia oxide and lithium disilicate groups, and in acid etch treatment for metal alloy group.
Purpose: To quantify the effect of the crystallization process on lithium disilicate ceramic crowns that are fabricated using a computer-aided design/computer-aided manufacturing(CAD/CAM) system, and to determine whether they are clinically acceptable by comparing values before and after the crystallization process. Methods: The maxillary first molar was selected as the abutment for the experiments. Ten working models were prepared. Marginal and internal gap of 4 groups of lithium disilicate crowns(n=10) fabricated with conventional method. Comparison was performed using the silicone replica technique and 3D superimposition analysis. The marginal and internal gaps of the restoration were measured before and after the crystallization process of this prosthesis. The average value of each part(the average of values measured before and after the crystallization) was statistically analyzed using paired t-test(α=0.05). Results: The results from the second phase of this research, which compared the average value of the gap between the marginal and internal fits of the lithium disilicate single crown before and after the crystallization process, indicated that the marginal gap was larger and the internal gap was smaller after the crystallization process, and this difference was statistically significant (P<0.05) in all the parts evaluated. Conclusion: While the shrinkage that occurs during crystallization does affect the marginal and internal fit of the prosthesis, it cannot be concluded to be a major effect because the resultant distortion was within the clinically acceptable range.
Purpose: This study investigates the effect of repeated use of lithium disilicate glass-ceramics on color stability. Methods: In this study, 2 types of lithium disilicate glass-ceramics were used and they were divided into 4 groups after 1st, 2nd, 3rd, and 4th heat pressing. The L*, a*, and b* values of all specimens were measured using the VITA Easyshade Advance 4.0. These values was used to determine the ∆E value and transparency. IBM SPSS Statistics ver. 24.0, a statistical significance level of 0.05 and one-way ANOVA were used for all data. Results: In all groups, the L* and b* values were the lowest in the specimens subjected to the 4th heat pressing and the corresponding a* value was the highest. All specimens showed ∆E values of ≤3.3, indicating color changes that were not visible with the naked eye, and the color difference increased with the number of repeated heat pressing. The transparency of all specimens decreased as the number of repeated uses increased. Conclusion: According to the number of repeated heat pressing, the color difference of Rosetta SP (HASSBIO) was larger than that of IPS e.max Press (Ivoclar Vivadent), but it was clinically acceptable in all groups. Moreover, transparency decreased as the number of heat presses increased in all groups. According to the above findings, the lithium disilicate glass-ceramic has high color stability due to repeated heat pressing, implying that it can be used in clinical settings regularly.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.