Bae, Sang Jun;Eum, Hyang Lan;Kim, Byung-Sup;Yoon, Jungro;Hong, Sae Jin
Horticultural Science & Technology
/
v.33
no.2
/
pp.233-241
/
2015
Kimchi cabbage 'Choon Gwang' cultivar that was grown in highlands in Gangneung was subjected to predrying, room cooling, and forced air cooling, and then packed with/without 0.02 mm HDPE film to investigate the effect of postharvest treatment on quality characteristics during 8 weeks storage at $2^{\circ}C$ (RH $90{\pm}5%$). Weight loss in forced air cooling and room cooling was lower than 3-4% with 0.02 mm HDPE film liner treatment during storage. However, it was only below 10% in room cooling without liner treatment and forced air cooling without liner treatment led to the highest weight loss, above 15%. Conversely, the control had lower weight loss than the others. SSC was $2-4^{\circ}brix$ for all treatments and there was no difference between postharvest treatments and liner treatments. Color index and firmness both showed no differences with/without 0.02 mm HDPE film and postharvest treatments. In sensory evaluation, forced air cooling with liner treatment was effective, with the highest score, especially in appearance and crispness. After 6 weeks, control kimchi cabbage without liner treatment was damaged seriously in appearance and the internal color had changed to brown. Room cooling and predrying with liner treatment changed the start of internal browning to after 8 weeks storage.
Purpose: This study aimed to identify the impact of physical surface roughing with a polishing tool onto the pre-sintering yttria-stabilized tetragonal zirconia polycrystals (TZP) core and liner treatment for chemical bonding on the bond strength of TZP core and veneering ceramic. Methods: Overall, 80 specimens were classified into two groups (non-liner, NL; and usingliner, UL ) depending on the use of liner, and these two groups were then subclassified into four groups depending on the polishing tool used. (1) Non-liner groups: NS, non-liner+stone point; NC, non-liner+carbide bur; NP, non-liner+paper cone point; NT, non-liner+silicon point. (2) Using-liner groups: US, using-liner+stone point; UC, using-liner+carbide bur; UP, usingliner+paper cone point; UT, using-liner+silicon point. The pre-sintering surface roughing values and shapes were observed, and after burning up the veneering ceramic, the shear bond strength was measured using a universal testing machine. For significance testing, a one-way analysis of variance and Tukey's multiple comparison test were conducted. An optical microscope was used to observe the fracture plane, and the following results were obtained. Results: Surface roughness NP (4.09±0.51 ㎛) represented a higher value than other groups (p<0.001). In shear bond strength, NS (35.21±1.44 MPa) of the NL group showed the highest bond strength (p<0.001). The UL group did not show a statistically significant difference between groups (p=0.612). Conclusion: Our study findings reveal that the bond strength of TZP core and veneering ceramic was improved by pre-sintering physical surface treatment than by chemical bonding with liner surface treatment.
Hong, Sae Jin;Kim, Byung-Sup;Kim, Byeong-Sam;Eum, Hyang Lan
Journal of Bio-Environment Control
/
v.27
no.2
/
pp.125-131
/
2018
The effect of 1-methylcyclopropene (1-MCP) in the storability of kimchi cabbage at cold storage condition was investigated. Kimchi cabbage (Brassica campestris L. cv Ryouckgwang) was divided four groups, forced air cooling (FAC), FAC + 0.03 mm linear low density polyethylene liner (Liner), $FAC+2{\mu}L{\cdot}L^{-1}$ 1-MCP (1-MCP), and FAC + 1-MCP + Liner. After each treatment kimchi cabbage was stored at $2^{\circ}C$, 95% RH. Quality parameters were weight loss, soluble solids content (SSC), firmness, and color ($CIE\;L^*$, $a^*$, $b^*$, chroma, hue angle). Weight loss during storage was showed significant difference by Liner treatment. In particular FAC + 1-MCP + Liner treatment showed 12.5% reduction after 6 weeks of storage period and minimized the weight loss rate compared to other treatments. SSC of kimchi cabbage was $2.5^{\circ}Brix$ at harvest and FAC + 1-MCP + Liner treatment maintained the SSC until 3 weeks, while in other treatments gradually were increased. The firmness of kimchi cabbage was 24.0 N immediately after harvest and the firmness at harvest time tended to be maintained at 22.6 N after 6 weeks of storage in FAC + 1-MCP + Liner treatment. During the storage period, the color change of the kimchi cabbage leaf can be confirmed by $CIE\;a^*$ and hue angle value. 1-MCP treatment alone did not affect the color change, however 1-MCP + Liner treatment was able to maintain the chromaticity at harvest time while minimizing the change of $CIE\;a^*$ and hue angle. These results suggest that 1-MCP treatment is not effective for the storage of kimchi cabbage but can be maintained for up to 6 weeks when treated with Liner.
Purpose: This study aimed to compare the shear bond strength between zirconia cores and veneer ceramics as per the sand blasting and liner treatments. Methods: The following 4 groups of zirconia-veneering ceramic specimens were prepared: (1) Group I, untreated; (2) Group II, with 110 ㎛ aluminium oxide (Al2O3) sandblasting; (3) Group III, with liner (IPS e.max ZirLiner; Ivoclar Vivadent); and (4) Group IV, with 110 ㎛ Al2O3 sand blasting and liner. Surface roughness was measured for all the prepared specimens, and the surface morphology was observed using a scanning electron microscope. All the samples (n=40) were fixed with measuring jigs, and shear bond strengths were obtained using a universal testing machine with a crosshead speed of 0.5 mm/min. The shear bond strength data were analyzed using one-way analysis of variance and t-test. The post hoc comparison was performed using the Tukey's test (α=0.05). Results: A significant difference in the surface roughness was observed between the specimens of groups I and II (p<0.05). Surface treatment with liner and sandblasting showed higher shear bond strength between zirconia core and veneering ceramic (p<0.05). Conclusion: The sand blasting and liner treatment increased the shear bond strength between zirconia core and veneering ceramic.
This study aimed to illuminate the correlatives between the surface processing of Zirconia core and the shear bond strength. The specimens were made by precipitating for two minutes in color liquid and drying to produce a colored Zirconia core following the manufacturer's instructions. The specimens were divided into 4 subgroups according to the surface treatment-sandblasted+liner treatment, SLT group; sandblasted treatment, ST group; liner treatment, LT group; non treatment (control), NT group. The specimens were put on the device with regard to ISO/TS 11405, then tested the shear bond strength with 1 mm shearing speed per minute using the Instron multi-purpose tester. The collected data was analysed by one way ANOVA and t-test. After applying the liner and sandblast to the Zirconia core, shear bond strength value were SLT (23.19 MPa), ST (21.17 MPa), LT (20.53 MPa) and NT (16.46 MPa) in the order. There was a significant difference in the surface roughness between NT and ST group (p<0.001), and in the compressive shear bond strength between NT and SLT group (p<0.05). Therefore, sandblasted plus liner treatment on pre-sintered substructure increased the bond strength of veneering ceramic, compared with other surface treatments.
Proceedings of the Korean Society of Marine Engineers Conference
/
2002.05a
/
pp.141-146
/
2002
The cast iron cylinder liner of the marine engine must be scrapped after its inner surface was definitely worn out due to the friction between the surface and piston ring during the operating. In this research, the restoring method of the worn out cast iron cylinder liner are discussed based on the results of experimental work of the thermal plastic deformation technique.
Statement of problem: The failure of adhesion between the resilient denture liner and the denture base is a serious problem in clinic. Purpose: The purpose of this study was to evaluate the effect of denture base resin surface pretreatments (mechanical and/or chemical) on the tensile bond strength between a resilient liner and processed denture resin. Material and method. Acrylic-based resilient liners (Soft liner; GC co., Japan & Coe-Soft; GC America Inc. USA) and silicone-based resilient liners (Mucosoft, Parkell Inc., USA & Dentusil; Bosworth co., USA) were used. Specimens in each soft lining material were divided two groups with or without mechanical pretreatment. Each denture base specimen received 1 of 4 chemical pretreatments including: (1) no treatment, (2) 30-s acetone treatment, (3) 15-s methylene chloride treatment, (4) 180-s methyl methacrylate treatment. All specimens were thermocycled and placed under tension until failure in a universal testing machine. Results: 1. Silicone-based resilient liners exhibited significantly higher tensile bond strengths than acrylic-based resilient liners (P<.05). 2. Grinding the denture base resin improved tensile bond strengths of silicone-based resilient liners, but reduced tensile bond strengths of acrylic-based resilient liners (P<.05). 3. In acrylic-based resilient liners, treating with acetone significantly increased the bond strength of Soft liner and treating with methyl methacrylate significantly increased the bond strength of Coe-Soft (P<.05). However they were not effective compared to silicone-based resilient liner. 4. In silicone-based resilient liners, treating with all chemical etchants significantly increased the bond strength of Mucosoft to denture base, and treating with methylene chloride and methyl methacrylate increased the bond strength of Dentusil to denture base (P<.05). Conclusion: Although chemical and mechanical pretreatments were not effective on tensile bond strength of acrylic-based resilent liner to denture base, treating the denture base resin surface with appropriate chemical etchants after mechanical pretreatment significantly increased the tensile bond strength of silicone-based resilient liner to denture base.
Journal of the Korea Academia-Industrial cooperation Society
/
v.8
no.5
/
pp.1166-1172
/
2007
Drainage pipeline system repaired by trenchless technology using liners can be defined between partial and entire collapse. The liners in the partial collapse pipeline are subjected to only uniform groundwater pressure on the surface. This research evaluates practical and useful cured-in-placed pipe (CIPP) design equations based on experimental results and finite element analysis results. Also, stability evaluation of pipe liner system with edge treatment is performed using finite element analysis. The CIPP equation should be used to design liner pipe system.
Kim, Byung-Joo;Son, Jung-Ho;Park, Jin-Soo;Choi, Ho-Jung
Proceedings of the KSME Conference
/
2001.06a
/
pp.663-668
/
2001
Strength evaluation was carried out for the cylinder liner of a low-speed marine engine. Calculation of temperature distribution, nonlinear structural analysis, material test, and fatigue strength evaluation are briefly introduced in this paper. Strengths of five liner models are compared, and the effect of materials experiencing different heat treatment is evaluated. Structural analysis including boundary and material non-linearities was performed for axisymmetric liner models. High cycle (fatigue limit) and low cycle (fatigue life) fatigue analyses are carried out. As results, localized high stress was occurred next to the mount line. Maximum stresses are varied significantly with respect to different liner models and different materials.
Song Jin-Hwa;Hong Ki-Jung;Chang Chang-Hwan;Kim Young-Sub
Journal of Applied Reliability
/
v.6
no.1
/
pp.51-61
/
2006
Failure analyses were conducted on a crank shaft and a chock liner by using X-ray diffraction, optical microscopy and SEM/EDS techniques. In the crank shaft, a crack developed where a maximum tensile stress coincided with band structure formed by hot forging. The maximum tensile stress was observed to originate from volume expansion during high frequency induction heat treatment and the band structure to develop between upper and lower dies during hot forging. In the chock liner, the wear mechanism varied with the chemical affinity and hardness of liner material relative to friction pair of housing liner. Brass of low chemical affinity and hardness compared to housing liner showed uniform adhesive wear. STS 304 and STS 420J2 of high chemical affinity showed galling and scoring respectively.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.