중공 데크플레이트에 사용된 철선의 내부피복두께에 따른 부착응력-변형률 예측모델 (Bond Stress-Strain Predict Model with Inner Cover Thickness of Steel Wire Used in Void Deck Plate)

  • 김희현;최창식
    • 대한건축학회논문집:구조계
    • /
    • 제34권1호
    • /
    • pp.41-51
    • /
    • 2018
  • In case of evaluating the bond stress of a void deck plate using a wire steel, there is no standard formula considering both the influence on the void and the type of the reinforcing bar. Therefore we proposed a model equation considered the bond characteristics of the void deck plate. A total of 46 specimens was carried out a direct pull-out test and the test variables were the presence of a void body, type of reinforcing bar, the inner cover thickness according to the location of reinforcing bars and bond region. As a result of the comparison between the steel bar and steel wire, the bond stress of the steel wire with the relative rib area of 0.071 is 4.5 ~ 28.58% lower than that of the steel bar with 0.092 and the bond stress reduction rate increases when the inner cover thickness is insufficient. In the case of the inner cover thickness of $1.7d_b$ and $2.7d_b$, the bond stress was reduced to 48.7 ~ 68.4%. In the inner cover thickness was $4.9d_b$ and $5.2d_b$, the bond stresses were equivalent to those of the solid specimens. It was confirmed that the average bond stress and strain were affected by the inner cover thickness. Therefore the predicted model for one module of the void deck plate is proposed and verified by considering the bond characteristics of the void deck plate.

도넛형 이방향 중공슬래브의 부착특성에 관한 실험적 연구 (An Experimental Study for Bond Characteristics of Deformed Bar Embedded in Donut Type Biaxial Hollow Slab)

  • 정주홍;강성훈;이승창;최창식;최현기
    • 콘크리트학회논문집
    • /
    • 제25권2호
    • /
    • pp.155-163
    • /
    • 2013
  • 이 연구는 도넛형 이방향 중공슬래브에 매입된 이형철근의 부착특성 및 부착강도 산정을 위한 기초적인 연구이다. 도넛형 이방향 중공슬래브의 철근 부착특성 및 부착강도 산정을 위해 pull-out test를 수행하였다. 도넛형 중공형성체는 슬래브 내부에 배치되어 철근과 중공형성체 사이에 내부의 피복이 형성된다. 이러한 내부피복두께는 외부피복두께보다 상대적으로 작은 피복두께를 가지며 중공형상에 따라 $2.5d_b$보다 작은 내부피복두께가 형성되기 때문에 철근의 부착에 영향을 미치게 된다. 또한 중공형성체가 일정 간격으로 떨어져 배치되어 있으므로 인장철근을 감싸고 있는 피복두께의 조건이 철근의 길이방향으로 변하게 된다. 따라서 도넛형 이방향 중공슬래브의 부착특성을 알아보기 위해서 중공형성체 형상에 따라 부착구간을 구분하였다. 구간별로 내부피복두께에 따른 부착응력-슬립 관계를 확인하였으며, 중공형성체 전 구간에 걸친 부착응력분포를 확인하여 철근의 길이방향에 따른 부착응력의 발현정도를 확인하였다. 또한 구간별 부착응력-슬립 관계를 기반으로 하여 도넛형 중공슬래브의 부착강도를 산정할 수 있는 부착강도 산정 방법을 제안하였다.

옥상녹화에서 토심, 토양배합비 및 지피식물에 따른 식재지반 수분 및 온도변화 (Change of the Moisture and Temperature in Planting Ground as Effected by Different Soil Thickness, Soil Mixture Ratios and Ground Cover Plants in the Green Roof System)

  • 주진희;윤용한
    • KIEAE Journal
    • /
    • 제10권3호
    • /
    • pp.11-16
    • /
    • 2010
  • This paper has attempted to investigate the change in soil moisture volume and temperature of architecture by planting ground(soil thickness and soil mixture ratio) and ground cover plants(Sedum sarmentosum, Zoysia japonica, Chrysanthemum zawadskii) for middle region green roof system. For this, a test was conducted on the roof of Konkuk University building from April 2009 to October 2009. In terms of treatment, five types(SL, $P_7P_1L_2$, $P_6P_2L_2$, $P_5P_3L_2$, $P_4P_4L_2$) depending on soil mixture ratio and two types(15cm, 25cm) by soil depth were created. Results of soil moisture volume by soil mixture ratio in the 15cm soil thickness showed that the difference was significance between simple soil and mixture soil treatment, however, the statistical significance was not recognized according to soil mixture ratio. In case of 25cm soil thickness, soil moisture volume by soil mixture ratio was more higher 7Vol.%~10Vol.% in the mixture soil than simple soil treatment. In terms of districts planted ground cover plants, soil volume moisture differed among plants in the order Zoysia japonica 17.74 Vol.%$34.86^{\circ}C$, district non-planted $27.49^{\circ}C$, Sedum sarmentosum $25.11^{\circ}C$, Chrysanthemum zawadskii $23.08^{\circ}C$, Zoysia japonica $24.45^{\circ}C$ respectively So, concrete surface showed more higher $5^{\circ}C{\sim}15^{\circ}C$ than other things among the all the time. Result of inner temperature of the architecture and soil, it was measured inner of architecture $25.69^{\circ}C$, inner district non-planted $24.29^{\circ}C$, Chrysanthemum zawadskii $23.90^{\circ}C$, Zoysia japonica $24.02^{\circ}C$, Sedum sarmentosum $25.13^{\circ}C$, respectively.

굴삭기 Tank Cover 부품 뒤틀림 불량 저감에 대한 연구 (A study on reduction of springback defects in excavator tank cover part)

  • 전용준;이하성;김동언;허영무
    • Design & Manufacturing
    • /
    • 제12권1호
    • /
    • pp.52-57
    • /
    • 2018
  • With the recent strengthening of environmental regulations and the need for cost reduction, excavators, a type of construction equipment, are being miniaturized while components are being developed in consideration of stability. In the case of excavator press parts, mainly high-strength steel sheets are being used to enhance stability and reduce weight. However, in the case of high-strength materials, there is a need to research product forming methods to reduce Springback in defects arising in parts assembly due to Springback that result from the internal residual stress that occurs in press forming being released after product forming. Accordingly, regarding the tank cover, an excavator press-forming part, this study selected a method to reduce distortion through analysis of the Springback occurrence rate and Springback causes through a forming analysis. A forming analysis was conducted for the Springback of the tank cover. Deformations of 13.714 mm in the upper part and 6.244 mm in the inner part of the product occurred, while wrinkles occurred on the sides of the product due to uneven thickness. A forming analysis was conducted for the major shapes of the product to investigate the causes of Springback. Distortion deformation due to the bead in the center of the product was confirmed to be a large factor. A Springback reduction method of correcting uneven thickness in the product sides, a Springback reduction method of removing the bead, and a correction method of restriking after the final forming were used in a forming analysis to determine the degree of Springback reduction. For the forming method to correct uneven thickness in the sides, deformation was reduced by 12% in the upper side compared to the existing model, but deformation in the inner side increased by 1%. For the restriking forming method, deformation decreased by 25% in the upper side and 13% in the inner side. For the bead removal method, deformation decreased by 28% in the upper side and 13% in the inner side, the largest Springback correction results. This indicates that the bead has a large affect on Springback.

몰타르 시험편(W/C:0.4) 내부철근의 분극특성에 미치는 재령년수의 영향 (The Effect of Passing Aged Years to the Polarization Characteristics of Embedded Steel Bar of Mortar Specimen(W/C:0.4))

  • 문경만;원종필;박동현;이성열;정진아;이명훈;백태실
    • Corrosion Science and Technology
    • /
    • 제13권1호
    • /
    • pp.20-27
    • /
    • 2014
  • The structures of reinforced concrete has been extensively increased with rapid development of industrial society. Futhermore, these reinforced concretes are easy to expose to severe corrosive environments such as sea water, contaminated water, acid rain and seashore etc.. Thus, corrosion problem of inner steel bar embedded in concrete is very important in terms of safety and economical point of view. In this study, multiple mortar test specimen(W/C:0.4) with six types having different cover thickness each other was prepared and was immerged in seawater solution for five years to evaluate the effect of cover thickness and immersion years to corrosion property of embedded steel bar. And the polarization characteristics of these embedded steel bars was investigated using electrochemical methods such as measuring corrosion potential, cathodic polarization curve, and cyclic voltammogram. At the beginning of immersion, the corrosion potentials exhibited increasingly nobler values with increasing cover thickness. However, after immersed for 5 years, the thicker cover of thickness, the corrosion potentials shifted in the negative direction, and the relationship between corrosion potential and cover thickness was not in good agreement with each other. Therefore, it is considered that the thinner cover of thickness, corrosive products deposited on the surface of the embedded steel bar plays the role as a resistance polarization which is resulted in decreasing the corrosion rate as well as shifting the corrosion potential in the positive direction. As a result, it seemed that the evaluation which corrosion possibility of the reinforced steel would be estimated by only measuring the corrosion potential may not be a completely desirable method. Therefore, it is suggested that we should take into account various parameters, including cover thickness, passed aged years as well as corrosion potential for more accurate assessment of corrosion possibility of reinforced steel which is exposed to partially or fully in marine environment for long years.

조선왕조실록 태백산사고본 표지 및 내지의 비파괴적 특성 연구 (Non-Constructive analysis for the cover and inner paper in the Taebaeksan volume of Joseon Dynasty annals)

  • 조정혜;김강재;엄태진
    • 펄프종이기술
    • /
    • 제42권3호
    • /
    • pp.28-36
    • /
    • 2010
  • Today We have three full series of the annals of Joseon Dynasty. Taebaeksan volume which is one of them shows comparatively good maintenance but Taebaeksan volume also decomposed in patches. The size of cover and inner paper were increased in late Joseon Dynasty, but the weight, thickness and basis weight bears no relation to each other. The oxidation index of paper in annals of pre-periods of King Sunjo shows very high value. After the annals of King Sunjo, the oxidation index of paper is very similar to today's Hanji. L.a.b values of inner paper in the Taebaeksan volume are similar generally. The average length of fiber using image analysis soft ware is 8.08~9.92 mm, that like immediate value of measurement. The air fraction of fiber's range is 1.20~2.12%. It lower than today's Hanji. After considering the factors of the length of fiber, air fraction and FE-SEM, we reached that no difference between raw material of inner paper in the Taebaeksan volume.

Effect of Air Gap Thickness on Top Heat Loss of a Closed-loop Oscillating Heat Pipe Solar Collector

  • Nguyen, Kim-Bao;Choi, Soon-Ho;Yoon, Doo-Ho;Choi, Jae-Hyuk;Oh, Cheol;Yoon, Seok-Hun
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제33권7호
    • /
    • pp.994-1002
    • /
    • 2009
  • In this paper, effect of air gap thickness between absorber plate and glass cover on top heat loss of a closed loop oscillating heat pipe (CLOHP) solar collector was investigated. The CLOHP, which is made of copper with outer diameter of 3.2mm and inner diameter of 2.0mm, comprises 8 turns with heating, adiabatic and cooling section. The heating section of the heat pipe was attached to absorber plate which heated by solar simulator simulated by halogen lamps. The cooling section of the heat pipe was inserted into collector's cooling section that made of transparent acrylic. Temperatures of absorber plate, glass cover, and ambient air measured by K-type thermocouple and were recorded by MV2000-Yokogawa recorder. Top heat loss coefficients and top heat loss of the collector corresponding to some cases of air gap thickness were determined. The result of experiment shows the optimal air gap thickness for minimum top heat loss of this solar collector.

모르타르(W/C:0.6)의 철근의 부식전위와 양극분극 및 임피던스 특성에 미치는 재령 년수 (Effect of Period of Immersion on Corrosion Potential, Anodic Polarization, and Impedance Characteristics of Reinforced Steel in Mortar (W/C: 0.6))

  • 정재현;문경만;이성열;이명훈;백태실
    • 한국해양공학회지
    • /
    • 제30권4호
    • /
    • pp.327-333
    • /
    • 2016
  • Reinforced concrete structures have found wide usage in land and maritime applications. However, the corrosion of reinforced concrete has been recognized as a serious problem from economic and safety standpoints. In previous studies, the corrosion behavior of the inner steel bar embedded in mortar (W/C: 0.4, 0.5) was investigated using electrochemical methods. In this study, multiple mortar test specimens (W/C: 0.6) with six different cover thicknesses were prepared and immersed in flowing seawater for five years. Subsequently, equations related to the cover thickness, period of immersion, and corrosion characteristics of the embedded steel bar were evaluated using electrochemical methods. Prior to immersion, the corrosion potentials indicated an increase with increasing cover thickness, and after five years, all corrosion potentials demonstrated a trend in the positive direction irrespective of the cover thickness. However, the relationships between the corrosion potential and cover thickness were not in complete agreement. Furthermore, after five years, all of the corrosion potentials indicated values that were nobler compared to those obtained prior to immersion, and their corrosion current densities also decreased compared to their values obtained prior to immersion. It was considered that the embedded steel bar was easily corroded because of the aggression of water, dissolved oxygen, and chloride ions; a higher W/C ratio also assisted the corrosion process. The corrosive products deposited on the surface of the steel bar for five years cast a resistance polarizing effect shifting the corrosion potential in the nobler direction. Consequently, it was considered that the W/C ratio of 0.6 showed nearly same results as those of W/C of 0.4 and 0.5. Therefore, the corrosion potential as well as various parameters such as the cover thickness, period of immersion, and W/C ratio must be considered at once for a more accurate evaluation of the corrosion property of reinforced steel exposed to marine environment for a long period.

콘크리트 표면의 유체이동특성과 최소피복두께 결정을 위한 제안 (Fluid Transport Properties of Skin Concrete and New Suggestion to Determine Minimum Cover Concrete)

  • 이창수;윤인석
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2002년도 가을 학술발표회 논문집
    • /
    • pp.543-546
    • /
    • 2002
  • This paper discussed micro - structure of skin concrete to understand transport properties from surface and seek thickness from surface which is seriously influenced on durability. Concrete at nearer surface has high porosity relative to inner concrete. The porosity of concrete and ISAT value at region from surface to 20 mm depth is decreased with depth. On the other hand, according to the result of ASTM C 1202 with specimen thickness, critical depth which affects fast ionic penetration through interfacial transition zone (ITZ) equals 35mm and the critical depth would be directly influenced by the effects of ITZ on chloride diffusion unrelated with W/C ratio.

  • PDF

피로 및 내구성을 고려한 LNG 저장탱크의 수명평가 프로그램 개발 (The Development of Life Evaluation Program for LNG Storage Tank considering Fatigue and Durability)

  • 김정훈;김영구;조영도
    • 한국가스학회지
    • /
    • 제21권3호
    • /
    • pp.39-45
    • /
    • 2017
  • LNG 산업의 핵심시설인 LNG 저장탱크는 주로 9% 니켈강형 내조와 프리스트레스 콘크리트의 외조로 구성되어 있다. 1896년 상업운전 이후 내조의 피로와 외조의 내구성 저하로 인한 구조물 성능 열화의 위험성 증대에 선제적으로 대응할 수 있도록 수명평가 프로그램이 필요하다. 이 연구는 LNG 저장탱크의 내조에 대해 피로평가와 외조의 내구성(탄산화, 염해)을 평가할 수 있는 수명평가 프로그램을 개발하였다. 내조 탱크는 3가지의 주요 시나리오를 정의하여 구조해석과 마이너 손상법칙이 적용된 피로수명 해석이 수행된다. 외조 탱크의 탄산화 평가는 이산화탄소 함량과 침투 깊이 데이터를 이용하여 콘크리트 피복두께에 따른 탄산화 진전을 예측한다. 외조 탱크의 염해 평가는 다양한 입력조건 고려와 신뢰도 있는 결과를 도출하기 위해 공개 프로그램인 Life-365프로그램에 연계하는 방안으로 구축하였다.