Effect of RGD peptide coating of implant titanium surface on human mesenchymal stem cell response (양극산화 티타늄 표면에 서로 다른 RGD 펩타이드 코팅 방법이 인간간엽줄기세포 반응에 미치는 영향)

  • Kim, Min-Su;Jeong, Chang-Mo;Jeon, Young-Chan;Ryu, Jae-Jun;Huh, Jung-Bo;Yun, Mi-Jung
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.49 no.3
    • /
    • pp.245-253
    • /
    • 2011
  • Purpose: The aim of this in vitro study was to estimate surface characteristic after peptide coating and investigate biological response of human mesenchymal stem cell to anodized titanium discs coated with RGD peptide by physical adhesion and chemical fixation. Materials and methods: Fluorescence isothiocyanate (FITC) modified RGD-peptide was coated on the anodized titanium discs (diameter 12 mm, height 3 mm) using two methods. One was physical adhesion method and the other was chemical fixation method. Physical adhesion was performed by dip and dry procedure, chemical fixation was performed by covalent bond via silanization. In this study, human mesenchymal stem cell was used for experiments. The experiments consisted of surface characteristic evaluation after peptide coating, analysis about cell adhesion, proliferation, differentiation, and mineralization. Obtained data are statistically treated using Kruskal-Wallis test and Bonferroni test was performed as post hoc test (P=.05). Results: The evaluation of FE-SEM images revealed no diffenrence at micro-surfaces between each groups. Total coating dose was higher at physical adhesion experimental group than at chemical fixation experimental group. In cell adhesion and proliferation, RGD peptide coating did not show a statistical significance compared with control group (P>.05). In cell differentiation and mineralization, physical adhesion method displayed significantly increased levels compared with control group and chemical fixation method (P<.05). Conclusion: RGD peptide coating seems to enhance osseointegration by effects on the response of human mesenchymal stem cell. Especially physical adhesion method showed more effective than chemical fixation method on response of human mesenchymal stem cell.

Golf activity after total knee arthroplasty (슬관절 전치환술 후 골프활동)

  • Kim, Hyung-Jun;Cha, Seung-Han;Nam, Kyoung-Mo;Kim, Dong-Heon
    • Journal of Korean Orthopaedic Sports Medicine
    • /
    • v.11 no.1
    • /
    • pp.51-56
    • /
    • 2012
  • Purpose: Golf is a popular sports activity after total knee arthroplasty in old age patients. We evaluated golf and implant loosening through the radiologic method. We also evaluated correlation of patterns of golf activity and clinical outcome to suggest guidelines to the patients. Materials and Methods: We carried out a retrospective case-control study of 80 patients (80 knees) who underwent TKR between 2005 and 2008, and followed up more than 3 years. We divided patients who played golf after TKR as a study group and who did not participate sports activities as a control group. We calculated the sum of width of radiolucent line in 7 sections around femoral component, 7 sections around tibial components and 5 sections in patella component using American Knee Society Roentgenographic Evaluation and Scoring system respectively. The inclusion criteria, was BMI (body mass index) was between 25 and $30kg/m^2$, and UCLA activity-level rating System score was between 5 and 8. We also got the information of patients' patterns of golf activities such as 1. the interval from surgery to return to golf activity. 2. the frequency of golf activities 3. using spike or cart. We obtained the information from patient's questionnaire and telephone interview. We compared with the VAS (visual analogue scale) respectively. And handicaps and driving distance was evaluated as well. Results: The study group's mean sum of radiologic score was 0.84 mm and 0.69 mm in control group. This is not statistically significant (p=0.22). Too early returning to golf (p=0.01) and left knee replacement (p<0.01) were statistically significant factors affecting clinical outcomes of golf activities after total knee arthroplasty. Conclusion: We concluded that golf activities after total knee arthroplasty is not correlated with radiographic loosening, and we need to give an explanation to the patients about increased pain when returing to golf too early and left side arthroplasties.

  • PDF

The Effect of Platelet Derived Growth Factor - BB Loaded Chitosan/Calcium Metaphosphate on Bone Regeneration (혈소판유래성장인자를 함유한 Chitosan/Calcium Metaphosphate의 골조직재생효과에 관한 연구)

  • Lee, Seung-Yeol;Seol, Yang-Jo;Lee, Yong-Moo;Lee, Ju-Yeon;Lee, Seung-Jin;Kim, Suk-Young;Ku, Young;Rhyu, In-Chul;Han, Soo-Boo;Choi, Sang-Mook;Chung, Chong-Pyoung
    • Journal of Periodontal and Implant Science
    • /
    • v.31 no.1
    • /
    • pp.1-23
    • /
    • 2001
  • Chitosan is biodegradable natural polymer that has been demonstrated its ability to improve wound healing, and calcium metaphosphate(CMP) is a unique class of phosphate minerals having a polymeric structure. In this study, chitosan/CMP and platelet derived growth factor(PDGF-BB) loaded chitosan/CMP sponges were developed, and the effect of the sponges on bone regeneration and their possibility as scaffolds for bone formation by three-dimensional osteoblast culture were examined. PDGF-BB loaded chitosan/CMP sponges were prepared by freeze-drying of a mixture of chitosan solution and CMP powder, and soaking in a PDGF-BB solution. Fabricated sponge retained its 3-dimensional porous structure with $100-200\;{\mu}m$ pores. The release kinetics of PDGF-BB loaded onto the sponge were measured in vitro with $^{125}I-labeled$ PDGF-BB. In order to examine their possibility as scaffolds for bone formation, fetal rat calvarial osteoblastic cells were isolated, cultured, and seeded into the sponges. The cell-sponge constructs were cultured for 28 days. Cell proliferation, alkaline phosphatase activity were measured at 1, 7, 14 and 28 days, and histologic examination was performed. In order to examine the effect on the healing of bone defect, the sponges were implanted into rat calvarial defects. Rats were sacrificed 2 and 4 weeks after implantation and histologic and histomorphometrical examination were performed. An effective therapeutic concentration of PDGF-BB following a high initial burst release was maintained throughout the examination period. PDGF-BB loaded chitosan/CMP sponges supported the proliferation of seeded osteoblastic cells as well as their differentiation as indicated by high alkaline phosphatase activities. Histologic findings indicated that seeded osteoblastic cells well attached to sponge matrices and proliferated in a multi-layer fashion. In the experiments of implantation in rat calvarial defects, histologic and histomorphometric examination revealed that chitosan/CMP sponge promoted osseous healing as compared to controls. PDGF-BB loaded chitosan/CMP sponge further echanced bone regeneration. These results suggested that PDGF-BB loaded chitosan/CMP sponge was a feasable scaffolding material to grow osteoblast in a three-dimentional structure for transplantation into a site for bone regeneration.

  • PDF

Fracture resistance and marginal fidelity of zirconia crown according to the coping design and the cement type (코핑 디자인과 시멘트에 따른 지르코니아 도재관의 파절 저항성)

  • Sim, Hun-Bo;Kim, Yu-Jin;Kim, Min-Jeong;Shin, Mee-Ran;Oh, Sang-Chun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.48 no.3
    • /
    • pp.194-201
    • /
    • 2010
  • Purpose: The purpose was to compare the marginal fidelity and the fracture resistance of the zirconia crowns according to the various coping designs with different thicknesses and cement types. Materials and methods: Zirconia copings were designed and fabricated with various thicknesses using the CAD/CAM system (Everest, KaVo Dental GmbH, Biberach., Germany). Eighty zirconia copings were divided into 4 groups (Group I: even 0.3 mm thickness, Group II: 0.3 mm thickness on the buccal surface and the buccal half of occlusal surface and the 0.6 mm thickness on the lingual surface and the lingual half of occlusal surface, Group III: even 0.6 mm thickness, Group IV: 0.6 mm thickness on the buccal surface and the buccal half of occlusal surface and the 1.0 mm thickness on the lingual surface and the lingual half of occlusal surface) of 20. By using a putty index, zirconia crowns with the same size and contour were fabricated. Each group was divided into two subgroups by type of cement: Cavitec$^{(R)}$ (Kerr Co, USA) and Panavia-$F^{(R)}$ (Kuraray Medical Inc, Japan). After the cementation of the crowns with a static load compressor, the marginal fidelity of the zirconia crowns were measured at margins on the buccal, lingual, mesial and distal surfaces, using a microscope of microhardness tester (Matsuzawa, MXT-70, Japan, ${\times}100$). The fracture resistance of each crown was measured using a universal testing machine (Z020, Zwick, Germany) at a crosshead speed of 1 mm/min. The results were analyzed statistically by the two-way ANOVA and oneway ANOVA and Duncan's multiple range test at $\alpha$=.05. Results: Group I and III showed the smallest marginal fidelity, while group II demonstrated the largest value in Cavitec$^{(R)}$ subgroup (P<.05). For fracture resistance, group III and IV were significantly higher than group I and II in Cavitec$^{(R)}$ subgroup (P<.05). The fracture resistances of Panavia-$F^{(R)}$ subgroup were not significantly different among the groups (P>.05). Panavia-$F^{(R)}$ subgroup showed significantly higher fracture resistance than Cavitec$^{(R)}$ subgroup in group I and II (P<.05). Conclusion: Within the limitation of this study, considering fracture resistance or marginal fidelity and esthetics, a functional ceramic substructure design of the coping with slim visible surface can be used for esthetic purposes, or a thick invisible surface to support the veneering ceramic can be used depending on the priority.

A study of the effects of PDGF-BB on the characteristics of bone stromal and periodontal ligament cells (혈소판유래성장인자-BB가 골간질세포와 치주인대세포의 성상에 미치는 영향)

  • Kwon, Young-Hyuk;Park, Joon-Bong
    • Journal of Periodontal and Implant Science
    • /
    • v.26 no.4
    • /
    • pp.949-965
    • /
    • 1996
  • The main goal of periodontal therapy is to restore the lost periodontal tissue and establish the attachment appratus. Current acceptable therapeutic techniques are included : removal of diseased soft tissue, demineralization of exposed root surface, using the barrier membrane for preventing the downgrowth of gingival epithelial cell, insertion of graft materials as a scaffolding action, and biological mediators for promoting the cell activity. The latest concept one among them has been studied which based on the knowledge of cellular biology of destructed tissue. Platelet-derived growth factor(PDGF) is one of the polypeptide growth factor which have been reported as a biological mediator to regulate activities of wound healing progress including cell proliferation, migration, and metabolism. The purposes of this study is to evaluate the influences of the PDGF as biological mediator to periodontal ligament and bone marrow cell. Both right and left maxillary first molar were extracted from rat which had treated with 0.4% ${\beta}-Aminopropionitril$ for 5 days, and feeded until designed date to sacrifice under anesthesisa. Periodontal ligament were removed from the extracted socket of the rat, and cultured with Dulbecco's Modified Essential Medium(DMEM) contained with 10% Fetal Bovine Serum, 100U/ml penicillin, $100{\mu}g/ml$ streptomycin, $0.5{\mu}g/ml$ amphotericin-B. Bone marrow cell were culture from bone marrow suspension with which washed out from femur with same medium. The study was performed to evaluate the effect of PDGF to periodontal ligament and bone cell, cell proliferation rate, total protein synthesis, and alkaline phosphatase activity of rat periodontal ligament(PDL) cell and bone stromal(RBS) cell in vitro. The effects of growth factors on both cells were measured at 3, 5th day after cell culture with (control group) or without growth factors(experimental group). The results were as follows: 1. The tendency of cell proliferation under the influence of PDGF showed more rapid proliferation pattern than control at 3 and 5 days after inoculation. 2. The activity of Alkaline phosphatase revealed 14, 80% increased respectively at 3, 5 days culture than control group. Measurements of ALPase levels indicated that PDL cells had significantly higher activity when compared with that of co-culture groups and GF only(P<0.05). And, ALPase activity in 10 days was higher than that of 7 days(P<0.05). 3. The tendency of formation of the mineralized nodule were observed dose-depend pattern of PDL cells. There was statistically significant difference among group l(PDL 100%), 2(PDL 70%:GF 30%), and 3(PDL 50%:GF 50%)(P<0.01). But, there was no difference among group 3, 4(PDL 30%:GF 70%), and 5(GF 100%). 4. Also, the number of nodule was greater in co-culture of PDL 70% and GF 30% than in culture of PDL 70%(P<0.05). From the above results, it is assumed that the PDGF on PDL cells and RMB cell culture. GF stimulates the cell growth, which is not that of PDL cells but GF. And, the activity of ALPase depends on the ratio of PDL cells, and ALPase may relate to the initial phase of nodule formation. Also, it is thought that the calcified nodule formation principally depends on PDL cells, is inhibited by GF, and affected by cell density. In conclusion, platelet-derived growth factor can promote rapid osteogenesis during early stage of periodontal tissue regeneration.

  • PDF

The study on the shear bond strength of resin and porcelain to Titanium (티타늄에 대한 레진과 도재의 결합 강도에 관한 연구)

  • Park, Ji-Man;Kim, Yeong-Soon;Jun, Sul-Gi;Park, Eun-Jin
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.47 no.1
    • /
    • pp.46-52
    • /
    • 2009
  • Statement of problem: Recently, titanium has become popular as superstructure material in implant dentistry because titanium superstructure can be easily milled by means of computer-aided design and manufacture (CAD/CAM) technique. But retention form such as nail head or bead cannot be cut as a result of technical limitation of CAD/CAM milling and bond strength between titanium and porcelain is not as strong as that of conventional gold or metal alloy. Purpose: The objective of this study was to evaluate the shear bond strength of three different materials: heat curing resin, composite resin, porcelain which were bonded to grade II commercially pure Titanium (CP-Ti). Material and methods: Thirty seven CP-Ti discs with 9 mm diameter, 10 mm height were divided into three groups and were bonded with heat curing resin (Lucitone 199), indirect composite resin (Sinfony), and porcelain (Triceram) which were mounted in a former with 7 mm diameter and 1 mm height. Samples were thermocycled for 1000 cycles at between $5-55^{\circ}C$. Shear bond strength (MPa) was measured with Instron Universal Testing Machine with cross head speed of 1 mm/min. The failure pattern was observed at the fractured surface and divided into adhesive, cohesive, and combination failure. The data were analyzed by one-way ANOVA and Scheffe's multiple range test (${\alpha}=0.05$). Results: Lucitone 199 ($17.82{\pm}5.13\;MPa$) showed the highest shear bond strength, followed by Triceram ($12.97{\pm}2.11\;MPa$), and Sinfony ($6.00{\pm}1.31\;MPa$). Most of the failure patterns in Lucitone 199 and Sinfony group were adhesive failure, whereas those in Triceram group were combination failure. Conclusion: Heat curing resin formed the strongest bond to titanium which is used as a CAD/CAM milling block. But the bond strength is still low compared with the bond utilizing mechanical interlocking and there are many adhesive failures which suggest that more studies to enhance bond strength are needed.

Evaluation of titanium surface properties by $Nd:YVO_4$ laser irradiation: pilot study ($Nd:YVO_4$ 레이저 조사에 따른 티타늄의 표면특성 평가: 예비 연구)

  • Kim, Ae-Ra;Park, Ji-Yoon;Kim, Yeon;Jun, Sei-Won;Seo, Yoon-Jeong;Park, Sang-Won
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.51 no.3
    • /
    • pp.167-174
    • /
    • 2013
  • Purpose: This study was conducted to evaluate the roughness and surface alternations of three differently blasted titanium discs treated by $Nd:YVO_4$ Laser irradiation in different conditions. Materials and methods: Thirty commercially pure titanium discs were prepared and divided into three groups. Each group was consisted of 10 samples and blasted by $ZrO_2$ (zirconium dioxide), $Al_2O_3$ (aluminum oxide), and RBM (resorbable blasted media). All the samples were degreased by ultrasonic cleaner afterward. Nine different conditions were established by changing scanning speed (100, 300, 500 mm/s) and repetition rate (5, 15, 35 kHz) of $Nd:YVO_4$ Laser (Laser Pro D-20, Laserval $Korea^{(R)}$, Seoul, South Korea). After laser irradiation, a scanning electron microscope, X-ray diffraction analysis, energy dispersive X-ray spectroscopic analysis, and surface roughness analysis were used to assess the roughness and surface alternations of the samples. Results: According to a scanning electron microscope (SEM), titanium discs treated with laser irradiation showed characteristic patterns in contrast to the control which showed irregular patterns. According to the X-ray diffraction analysis, only $Al_2O_3$ group showed its own peak. The oxidation tendency and surface roughness of titanium were similar to the control in the energy dispersive X-ray spectroscopic analysis. The surface roughness was inversely proportional to the scanning speed, whereas proportional to the repetition rate of $Nd:YVO_4$. Conclusion: The surface microstructures and roughness of the test discs were modified by the radiation of $Nd:YVO_4$ laser. Therefore, laser irradiation could be considered one of the methods to modify implant surfaces for the enhancement of osseointegration.

The Study of Usefulness of Metal Artifact Reduction Algorithm and Artifacts Caused by Metallic Hip Prosthesis on PET/CT (PET/CT에서의 고관절 삽입물에 의한 인공물과 Metal Artifact Reduction Algorithm의 유용성에 대한 고찰)

  • Park, Min Soo;Ham, Jun Cheol;Cho, Yong In;Kang, Chun Goo;Park, Hoon-Hee;Lim, Han Sang;Lee, Chang Ho
    • The Korean Journal of Nuclear Medicine Technology
    • /
    • v.16 no.2
    • /
    • pp.35-43
    • /
    • 2012
  • Purpose : PET/CT performed CT-based attenuation correction generates the beam hardening artifact by metallic implant. The attenuation correction causes over or underestimate of the area adjacent to metallic hip prosthetic material and change of $^{18}F$-FDG uptake. Also, the image quality and the diagnosability on genitourinary disease are reduced. Therefore, this study will evaluate the usefulness of MAR (Metal Artifact Reduction) algorithm method to improve the image quality on PET/CT. Materials and Methods : PET/CT was performed by fixing hip prosthesis in SPECT/PET phantom. In PET images with and Without MAR algorithm, the Bright streak, Dark streak, Metal region and Background area that appeared on CT were confirmed, and the change of each SUV (standardized uptake value) was analyzed. Also, in 15 patients who underwent total hip arthroplasty, each MAR algorithm and Without MAR algorithm and non attenuation correction was evaluated. Results : In PET image Without MAR algorithm, SUV of Bright streak region was $0.98{\pm}0.48$ g/ml; Dark streak region was $0.88{\pm}0.02$ g/ml; Metal region was $0.24{\pm}0.16$ g/ml, Background area was $0.91{\pm}0.18$ g/ml. In SUV of PET image with MAR algorithm, Bright streak region was $0.88{\pm}0.49$ g/ml, Dark streak region was $0.63{\pm}0.21$ g/ml, Metal region was $0.06{\pm}0.07$ g/ml, Background was $0.90{\pm}0.02$ g/ml. SUV generally decreased when applying MAR algorithm. In PET image Without MAR algorithm, SUVs of Bright region were higher than those measured in the Background, and it was false positive uptake. But, in PET image with MAR algorithm, SUVs of Bright region were similar to the Background, and false positive uptake disappeared. Conclusion : MAR algorithm could reduce an increase of $^{18}F$-FDG uptake due to attenuation correction in the hip surrounding tissue. However, decrease of SUV in Dark streak region should be considered in the future. Therefore, this study propose that the diagnostic accuracy can be improved in genitourinary diseases adjacent to metallic hip prosthesis, if provided PET images with and Without MAR algorithm, and non attenuation correction images at the same time.

  • PDF

SURFACE CHARACTERISTICS AND BIOACTIVITY OF ANODICALLY OXIDIZED TITANIUM SURFACES (양극산화에 의한 티타늄 산화막의 표면 특성 및 생체 활성에 관한 연구)

  • Lee, Sang-Han;Cho, In-Ho
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.45 no.1
    • /
    • pp.85-97
    • /
    • 2007
  • Statement of problem: Recently, anodic oxidation of cp-titanium is a popular method for treatment of titanium implant surfaces. It is a relatively easy process, and the thickness, structure, composition, and the microstructure of the oxide layer can be variably modified. Moreover the biological properties of the oxide layer can be controlled. Purpose: In this study, the roughness, microstructure, crystal structure of the variously treated groups (current, voltage, frequency, electrolyte, thermal treatment) were evaluated. And the specimens were soaked in simulated body fluid (SBF) to evaluate the effects of the surface characteristics and the oxide layers on the bioactivity of the specimens which were directly related to bone formation and integration. Materials and methods: Surface treatments consisted of either anodization or anodization followed thermal treatment. Specimens were divided into seven groups, depending on their anodizing treatment conditions: constant current mode (350V for group 2), constant voltage mode (155V for group 3), 60 Hz pulse series (230V for group 4, 300V for group 5), and 1000 Hz pulse series (400V for group 6, 460V for group 7). Non-treated native surfaces were used as controls (group 1). In addition, for the purpose of evaluating the effects of thermal treatment, each group was heat treated by elevating the temperature by $5^{\circ}C$ per minute until $600^{\circ}C$ for 1 hour, and then bench cured. Using scanning electron microscope (SEM), porous oxide layers were observed on treated surfaces. The crystal structures and phases of titania were identified by thin-film x-ray diffractmeter (TF-XRD). Atomic force microscope (AFM) was used for roughness measurement (Sa, Sq). To evaluate bioactivity of modified titanium surfaces, each group was soaked in SBF for 168 hours (1 week), and then changed surface characteristics were analyzed by SEM and TF-XRD. Results: On basis of our findings, we concluded the following results. 1. Most groups showed morphologically porous structures. Except group 2, all groups showed fine to coarse convex structures, and the groups with superior quantity of oxide products showed superior morphology. 2. As a result of combined anodization and thermal treatment, there were no effects on composition of crystalline structure. But, heat treatment influenced the quantity of formation of the oxide products (rutile / anatase). 3. Roughness decreased in the order of groups 7,5,2,3,6,4,1 and there was statistical difference between group 7 and the others (p<0.05), but group 7 did not show any bioactivity within a week. 4. In groups that implanted ions (Ca/P) on the oxide layer through current and voltage control, showed superior morphology, and oxide products, but did not express any bioactivity within a week. 5. In group 3, the oxide layer was uniformly organized with rutile, with almost no titanium peak. And there were abnormally more [101] orientations of rutile crystalline structure, and bonelike apatite formation could be seen around these crystalline structures. Conclusion: As a result of control of various factors in anodization (current, voltage, frequency, electrolytes, thermal treatment), the surface morphology, micro-porosity, the 2nd phase formation, crystalline structure, thickness of the oxide layer could be modified. And even more, the bioactivity of the specimens in vitro could be induced. Thus anodic oxidation can be considered as an excellent surface treatment method that will able to not only control the physical properties but enhance the biological characteristics of the oxide layer. Furthermore, it is recommended in near future animal research to prove these results.

CT Based 3-Dimensional Treatment Planning of Intracavitary Brachytherapy for Cancer of the Cervix : Comparison between Dose-Volume Histograms and ICRU Point Doses to the Rectum and Bladder

  • Hashim, Natasha;Jamalludin, Zulaikha;Ung, Ngie Min;Ho, Gwo Fuang;Malik, Rozita Abdul;Ee Phua, Vincent Chee
    • Asian Pacific Journal of Cancer Prevention
    • /
    • v.15 no.13
    • /
    • pp.5259-5264
    • /
    • 2014
  • Background: CT based brachytherapy allows 3-dimensional (3D) assessment of organs at risk (OAR) doses with dose volume histograms (DVHs). The purpose of this study was to compare computed tomography (CT) based volumetric calculations and International Commission on Radiation Units and Measurements (ICRU) reference-point estimates of radiation doses to the bladder and rectum in patients with carcinoma of the cervix treated with high-dose-rate (HDR) intracavitary brachytherapy (ICBT). Materials and Methods: Between March 2011 and May 2012, 20 patients were treated with 55 fractions of brachytherapy using tandem and ovoids and underwent post-implant CT scans. The external beam radiotherapy (EBRT) dose was 48.6Gy in 27 fractions. HDR brachytherapy was delivered to a dose of 21 Gy in three fractions. The ICRU bladder and rectum point doses along with 4 additional rectal points were recorded. The maximum dose ($D_{Max}$) to rectum was the highest recorded dose at one of these five points. Using the HDRplus 2.6 brachyhtherapy treatment planning system, the bladder and rectum were retrospectively contoured on the 55 CT datasets. The DVHs for rectum and bladder were calculated and the minimum doses to the highest irradiated 2cc area of rectum and bladder were recorded ($D_{2cc}$) for all individual fractions. The mean $D_{2cc}$ of rectum was compared to the means of ICRU rectal point and rectal $D_{Max}$ using the Student's t-test. The mean $D_{2cc}$ of bladder was compared with the mean ICRU bladder point using the same statistical test. The total dose, combining EBRT and HDR brachytherapy, were biologically normalized to the conventional 2 Gy/fraction using the linear-quadratic model. (${\alpha}/{\beta}$ value of 10 Gy for target, 3 Gy for organs at risk). Results: The total prescribed dose was $77.5Gy{\alpha}/{\beta}10$. The mean dose to the rectum was $4.58{\pm}1.22Gy$ for $D_{2cc}$, $3.76{\pm}0.65Gy$ at $D_{ICRU}$ and $4.75{\pm}1.01Gy$ at $D_{Max}$. The mean rectal $D_{2cc}$ dose differed significantly from the mean dose calculated at the ICRU reference point (p<0.005); the mean difference was 0.82 Gy (0.48-1.19Gy). The mean EQD2 was $68.52{\pm}7.24Gy_{{\alpha}/{\beta}3}$ for $D_{2cc}$, $61.71{\pm}2.77Gy_{{\alpha}/{\beta}3}$ at $D_{ICRU}$ and $69.24{\pm}6.02Gy_{{\alpha}/{\beta}3}$ at $D_{Max}$. The mean ratio of $D_{2cc}$ rectum to $D_{ICRU}$ rectum was 1.25 and the mean ratio of $D_{2cc}$ rectum to $D_{Max}$ rectum was 0.98 for all individual fractions. The mean dose to the bladder was $6.00{\pm}1.90Gy$ for $D_{2cc}$ and $5.10{\pm}2.03Gy$ at $D_{ICRU}$. However, the mean $D_{2cc}$ dose did not differ significantly from the mean dose calculated at the ICRU reference point (p=0.307); the mean difference was 0.90 Gy (0.49-1.25Gy). The mean EQD2 was $81.85{\pm}13.03Gy_{{\alpha}/{\beta}3}$ for $D_{2cc}$ and $74.11{\pm}19.39Gy_{{\alpha}/{\beta}3}$ at $D_{ICRU}$. The mean ratio of $D_{2cc}$ bladder to $D_{ICRU}$ bladder was 1.24. In the majority of applications, the maximum dose point was not the ICRU point. On average, the rectum received 77% and bladder received 92% of the prescribed dose. Conclusions: OARs doses assessed by DVH criteria were higher than ICRU point doses. Our data suggest that the estimated dose to the ICRU bladder point may be a reasonable surrogate for the $D_{2cc}$ and rectal $D_{Max}$ for $D_{2cc}$. However, the dose to the ICRU rectal point does not appear to be a reasonable surrogate for the $D_{2cc}$.