• 제목/요약/키워드: high toughness

검색결과 824건 처리시간 0.026초

구치부 수복용 복합레진의 파괴특성에 관한 Acoustic Emission 연구 (ACOUSTIC EMISSION ANALYSIS FOR FRACTURE CHARACTERISTICS OF DENTAL POSTERIOR COMPOSITES)

  • 박진훈;김교한
    • Restorative Dentistry and Endodontics
    • /
    • 제17권1호
    • /
    • pp.153-165
    • /
    • 1992
  • Dental composite resin is a kind of the particle - reinforced composite material, and is widely used in recent dental restoration of anterior and posterior tooth region. The purpose of this study was to investigate the fracture behaviour according to volume fractions and external findings of the filler particles for better interpretation of the fracture characteristics of posterior dental composite resins by analytic method of fracture mechanics. The plane strain fracture toughness($K_{IC}$) and Acoustic Emission were determined with three - point bending test using the single edge notch specimen according to the ASTM - E399, and its analyzed data was compared with filler volume fractions derived from the standard ashing test and scanning electron fractographs of each specimen including the unfilled experimental resin as a control. The results were that the value of fracture toughness of the composite resin material was in the range from 0.85 MPa$\sqrt{m}$ to 1.60 MPa$\sqrt{m}$ and was higher than the value of the unfilled experimental resin, and the fracture behaviours dervied from Acoustic Emission analysis show prominent differences according to the volume fraction and the size of filler particles used in each composite resin. The degree of resistance against crack propagation seems to be increase and the fractographs demonstrate the high degree of surface roughness and irregularity according with the increase of fracture toughness value.

  • PDF

실리카 퓸을 이용한 자동차용 탄소섬유강화복합재의 인성 강화 (Toughness Enhancement of Carbon Fiber Reinforced Composites for Automobile using Silica Fume)

  • 임성묵;유재상;이원오
    • 융복합기술연구소 논문집
    • /
    • 제8권1호
    • /
    • pp.27-31
    • /
    • 2018
  • The age of electric vehicle is coming. One of the most important problems to be solved for popularization of electric vehicle is fuel economy. To increase fuel economy of electric vehicles, it is necessary to improve the performance of the battery or the car body should be lighter than now. To solve the problem of the car body, change the car body's material to carbon fiber reinforced composites can be an excellent answer. However, the part made from carbon fiber reinforced composites is vulnerable to accidents due to their high brittleness. In this study, ductile silica fume was added into the carbon fiber composites to enhance toughness. To examine this, various amounts and sizes of silica fume were considered and the toughness enhancement was examined by performing tensile tests.

선택적 레이저 용융 공정으로 제조된 AISI 316L 합금의 인장 및 충격 인성 특성에 미치는 응력 완화 열처리의 영향 (Effect of Stress Relieving Heat Treatment on Tensile and Impact Toughness Properties of AISI 316L Alloy Manufactured by Selective Laser Melting Process)

  • 양동훈;함기수;박순홍;이기안
    • 한국분말재료학회지
    • /
    • 제28권4호
    • /
    • pp.301-309
    • /
    • 2021
  • In this study, an AISI 316 L alloy was manufactured using a selective laser melting (SLM) process. The tensile and impact toughness properties of the SLM AISI 316 L alloy were examined. In addition, stress relieving heat treatment (650℃ / 2 h) was performed on the as-built SLM alloy to investigate the effects of heat treatment on the mechanical properties. In the as-built SLM AISI 316 L alloy, cellular dendrite and molten pool structures were observed. Although the molten pool did not disappear following heat treatment, EBSD KAM analytical results confirmed that the fractions of the low- and high-angle boundaries decreased and increased, respectively. As the heat treatment was performed, the yield strength decreased, but the tensile strength and elongation increased only slightly. Impact toughness results revealed that the impact energy increased by 33.5% when heat treatment was applied. The deformation behavior of the SLM AISI 316 L alloy was also examined in relation to the microstructure through analyses of the tensile and impact fracture surfaces.

수계공정에 의한 알루미나 테이프로 제조한 세라믹 인공치관용 알루미나 유리 복합체의 기계적 물성 (Mechanical Properties of Alumina-Glass Dental Composites Prepared from Aqueous-Based Tape Casting)

  • 이명현;김대준;이득용;이정훈;김창은
    • 한국세라믹학회지
    • /
    • 제36권10호
    • /
    • pp.1123-1131
    • /
    • 1999
  • Alumina-glass composites which are considered as the material of the choice for all dental crown was prepared by aqeous-based tape casting and sintering for 2h at 1120$^{\circ}C$ followed by glass infiltration for 2h at 1100$^{\circ}C$ Biaxial strength and fracture toughness of the composites were evaluated to determine the optimum composition of the tape as a function of the amount of constituent such as alumina binder and plasticizer. The strength and the fracture toughness of the alumina tape increased with increasing the contents of alumina and binder. These observations are consistent with in fluence of the constituents on mean alumuna particle distance in tapes suggesting that high strength of the glass infiltrated alumina composites is related to toughening by crack bowing. The biaxial strength and the fracture toughness of the composite containing the optimum constituent composition were 523 MPa and 3.3 MPa$.$1/2 respectively.

  • PDF

DC Potential Drop Method for Evaluating Material Degradation

  • Seok, Chang-Sung;Bae, Bong-Kook;Koo, Jae-Mean
    • Journal of Mechanical Science and Technology
    • /
    • 제18권8호
    • /
    • pp.1368-1374
    • /
    • 2004
  • The remaining life estimation for the aged components in power plants as well as chemical plants are very important because mechanical properties of the components are degraded with in-service exposure time in high temperatures. Since it is difficult to take specimens from the operating components to evaluate mechanical properties of components, nondestructive techniques are needed to evaluate the degradation. In this study, test materials with several different degradation levels were prepared by isothermal aging heat treatment at $630^{\circ}C$. The DC potential drop method and destructive methods such as tensile and fracture toughness were used in order to evaluate the degradation of 1Cr-1Mo-0.25V steels. In this result, we can see that tensile strength and fracture toughness can be calculated from resistivity and it is possible to evaluate material degradation using DC potential drop method, non-destructive method.

$\beta-Sialon/SiC$ Whisker 복합재료의 기계적 물성 및 마찰 마모 특성 연구 (Mechanical and Tribological Properties of $\beta-Sialon/SiC$ Whisker Composite)

  • 김호균;소유영;김인섭;이병하
    • 한국세라믹학회지
    • /
    • 제31권11호
    • /
    • pp.1259-1264
    • /
    • 1994
  • $\beta$-Sialon has been regarded as one of promising materials showing high strength, fracture toughness, corrosion resistence and wear resistence. The improvement of the fracture toughness and tribological properties of $\beta$-Sialon (Z=1) has been attempeted by fabricating the $\beta$-Sialon/ SiC whisker composite. Each of green body composed of following ingredients, i.e., Si3N4, AlN, Y2O3 nd SiC, respectively, was first fired at 178$0^{\circ}C$ for 3hrs in N2 atmosphere and then post-HIPed at 173$0^{\circ}C$ for 1 hr under 170 MPa for N2 gas pressure. The fracture toughness, flexural strength and tribological properties increased with increasing SiC whisker content, despite the reduction of the relative density and hardness. $\beta$-Sialon/15 vol% SiC whisker showed a significant enhancement of wear resistance compared to the monolithic $\beta$-Sialon. The addition of SiC whisker caused the reduction of the density and hardness, but induced the increment of wear resistance.

  • PDF

원자력 압력용기강(SA508-3)의 탄소성 파괴인성 평가 (The Evaluation for Elastic-Plastic Fracture Toughness in a Reactor Pressure Vessel Steel(SA508-3))

  • 오세욱;윤한기;임만배
    • 한국해양공학회지
    • /
    • 제7권2호
    • /
    • pp.91-102
    • /
    • 1993
  • The elastic-plastic fracture thoughness J sub(IC) of Nuclear Reactor Vessel Steel(SA 508-3) which has high toughness was discussed at temperatures RT, $-20^{\circ}C$, $200^{\circ}C$ and 1/2/CT specimen was used for this study. Especially the two methods recommended in ASTM and JSME were compared. It was difficult to find J sub(IC) by ASTM R-curve method with the specimen used for this research, while JSME R-curve method yielded good result. The stretched zone width menthod gave slightly larger J sub(IC) values than those by the R-curve method for SA 508-3 steel.

  • PDF

발전플렌트용 10Cr페라이트 내열강의 라베스상 석출거동 및 기계적 성질 (Precipitation Behavior of Laves Phase and Mechanical Properties of 10%Cr Ferritic Heat-resistant Steel Applied to the Power Plants)

  • 강창룡;남기우;김헌주;김창규;배동수;이종문
    • 동력기계공학회지
    • /
    • 제5권1호
    • /
    • pp.97-103
    • /
    • 2001
  • The present study was investigated changes of precipitation behaviour of laves phase in ferrite single phase and ferrite-martensite dual phase and the mechanical properties of 10%Cr ferritic alloys. In the ferrite phase, laves phase was mainly precipitated, whereas in the martensite phase, carbide was preferentially formed during the initial stage of aging and with increasing aging time. Laves phase and carbide were simultaneously precipitated by precipitation of laves phase at around carbide. Strength and toughness were lowered by the disk-type precipitator in the initial stage of aging and toughness was recovered with increasing of aging time and then, decreasing by precipitation of laves phase.

  • PDF

세라미스 파괴인성평가에 있어서 IF법과 AE (Acoustic Emission and Indentation Fracture Method for the Engineering Ceramics)

  • 김부안;문창권
    • 한국해양공학회지
    • /
    • 제15권2호
    • /
    • pp.61-65
    • /
    • 2001
  • The fracture toughness of ceramics can be measure by such various methods as DT (double torsion), CN (chevron notch) etc. But, the application of these methods to the engineering ceramics is very difficult because of its very high hardness. So, IF (indentation fracture) method is generally used for the evaluation of fracture toughness of ceramics. The Median crack induced by the sharp Vickers indenter was compared with the detected AE (acoustic emission) signal. On the silicon nitride ceramics, the AE test results agree fairly well with the median crack occurance and growth process. But, on the alumina, very many complicated crack signals were detected besides median crack. It can be considered that the IF methods must be used in limited engineering ceramics materials.

  • PDF

$Si_3N_4$-Zr(Y)$O_2$ 복합체의 열처리에 따른 상분석 및 파괴인성 (Phase Analysis and Fracture Toughness of $Si_3N_4$-Zr(Y)$O_2$ Composites after Heat Treatment)

  • 김재룡;김종희
    • 한국세라믹학회지
    • /
    • 제28권1호
    • /
    • pp.53-59
    • /
    • 1991
  • The reaction product between Si3N4 and ZrO2 has been studied by heat treatment of Si3N4-Zr(Y)O2 composite in high vacuum(<10-5 torr) and in air at $700^{\circ}C$. ZrN was formed after heat treatment in vacuum and easily oxidized after heat treatment in air. The amount of ZrN is related to the Y2O3 content dissolved in ZrO2. After the heat treatment in air the toughness increased and the spalling due to the oxidation of ZrN in specimen surface was observed. As a result, it is suggested that the formation of ZrN phase in Si3N4-ZrO2 composite enhance the toughness of the composite in an oxidation conditon.

  • PDF