The Effect of Boron Content and Deposition Temperature on the Microstructure and Mechanical Property of Ti-B-C Coating Prepared by Plasma-enhanced Chemical Vapor Deposition (PECVD법에 의해 증착된 Ti-B-C코팅막 내의 보론함량과 증착온도에 따른 미세구조 및 기계적 물성의 변화)

  • Ok, Jung-Tae;Song, Pung-Keun;Kim, Kwang-Ho
    • Journal of the Korean institute of surface engineering
    • /
    • v.38 no.3
    • /
    • pp.106-111
    • /
    • 2005
  • Ternary Ti-B-C coatings were synthesized on WC-Co and Si wafers substrates by a PECVD technique using a gaseous mixture of $TiCl_4,\;BCl_3,\;CH_4,\;Ar,\;and\; H_2$. The effects of deposition variables such as substrate temperature, gas ratio, $R_x=[BCl_3/(CH_4+BCl_3)]$ on the microstructure and mechanical properties of Ti-B-C coatings were investigated. From our instrumental analyses, the synthesized Ti-B-C coatings was confirmed to be composites consisting of nanocrystallites TiC, quasi-amorphous TiB2, and amorphous carbon at low boron content, on the contrary, nanocrystallites $TiB_2$, quasi-amorphous TiC, and amorphous carbon at relatively high boron content. The microhardness of the Ti-B-C coatings increased from $\~23 GPa$ of TiC to $\~38 GPa$ of $Ti_{0.33}B_{0.55}C_{0.11}$ coatings with increasing the boron content. The $Ti_{0.33}B_{0.55}C_{0.11}$ coatings showed lower average friction coefficient of 0.45, in addition, it showed relatively better wear behavior compared to other binary coatings of $TiB_2$ and TiC. The microstruture and microhardness value of Ti-B-C coatings were largely depend on the deposition temperature.

Wear Mechanism of Plasma-Sprayed Coating in Mo- and Co-Based Alloy

  • Lee, Soo W.
    • Tribology and Lubricants
    • /
    • v.11 no.5
    • /
    • pp.108-113
    • /
    • 1995
  • Wear and friction behavior of plasma-sprayed coatings in Mo- and Co-based alloy were studied for the application of piston-ring automobile engine. The plasma-sprayed coatings were varied with gun current density, gas flow, and distance. The surface roughness, microhardness, and wear volume were measured depending on the spray distances. The high temperature hardness value were also measured as a function of temperature. Ball-on-disc geometry configuration tribometer was utilized in air. The wear tests were performed in the temperature ranges from room temperature to 825$^{\circ}$C to investigate the tribological trend of the piston-ring materials in the lack of lubricant. The cross sections of wear track were investigated, using microscopy.

THERMAL CHANGE AND MICROHARDNESS IN CURING COMPOSITE RESIN ACCORDING TO VARIOUS CURING LIGHT SYSTEM (광중합기에 따른 복합레진 중합시 온도 변화와 미세경도에 관한 연구)

  • Lee, Dong-Jin;Kim, Dae-Eop;Yang, Yong-Sook;Lee, Kwang-Hee
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.31 no.3
    • /
    • pp.391-399
    • /
    • 2004
  • The purpose of this study was to compare curing efficiency of newly developed curing units to traditional halogen curing unit by measuring thermal change and surface microhardness according to curing light system. Materials and mathods : The types of curing units were traditional low intensity halogen light(Optilux 360), plasma arc light(Flipo), low heat plasma arc light(Aurys), low intensity LED(Starlight), and high intensity LED(Freelight2). Temperature at the tip of light guide was measured by a digital thermometer using K-type thermocouple. And after resin was filled to 2, 3, 4mm teflon mold, bottom temperature measured during curing. After 24 hours, microhardness of top surface and bottom surface of each resin specimen were measured. Results : The result of this study can be summarized as follows, 1. As measuring temperature of curing unit tips, Flipo is the highest as $52.4^{\circ}C,\;Freelight2(37.86^{\circ}C),\;Optilux360(32.68^{\circ}C),\;Aurys(32.34^{\circ}C),\;and\;Starlight(26.14^{\circ}C)$ were followed. 2. Flipo and Freelight2 were the highest similarly and Optilux360 and Aurys were similarly next and Starlight was lowest in temperature of bottom surface of resin mold. 3. Microhardness of top surface were generally similar, and Aurys was relatively low. 4. Optilux 360 and Freelight2 were the highest, and Flipo, Starlight, and Aurys were followed in microhardness of bottom surface. Conclusions : The results suggest that careful use of Flipo and Freelight2 might be able to cure greater depth of resin composite and do not cause thermal problems than other curing units.

  • PDF

Study on the Oxidation Resistance of Ti-Al-N Coating Layer (Ti-Al-N코팅층의 내산화 특성에 관한 연구)

  • 김충완;김광호
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.5
    • /
    • pp.512-518
    • /
    • 1997
  • The high temperature oxidation behaviors of titanium nitride films prepared by PACVD technique were studied in the temperature range of from 50$0^{\circ}C$ to 80$0^{\circ}C$ under air atmosphere. Ti0.88Al0.12N film, which showed the excellent microhardness from the previous work, was investigated on its oxidation resistance compared with pure TiN film. Ti-Al-N film showed superior oxidation resistance up to $700^{\circ}C$, whereas TiN film was fast oxidized into rutile TiO2 crystallites from at 50$0^{\circ}C$. It was found that an amorphous layer having AlxTiyOz formula was formed on the surface region due to outward diffusion of Al ions at the initial stage of oxidation. The amorphous oxide layer played a role as a barrier against oxygen diffusion, protected the remained nitride layer from further oxidation, and thus, resulted in the high oxidation resistive characteristics of Ti-Al-N film.

  • PDF

Improvement of Fatigue Strength and Characteristics of Nitrided ICr-lMo-0.25V turbine Rotor Steels at evaluated temperature (질화처리된 1Cr-1Mo-0.25V강의 고온화 피로특성평가)

  • 서창민;황병원;서창희
    • Proceedings of the Korea Committee for Ocean Resources and Engineering Conference
    • /
    • 2001.05a
    • /
    • pp.357-362
    • /
    • 2001
  • The purpose of this study is to investigate the effect of nitriding on the fatigue strength and fatigue life of turbine rotor steel (ICr-lMo-0.25V), and acquire data on the fatigue strength of nitrided turbine rotor steel at high temperature (538$^{\circ}C$). Specimens were nitrided with various layer thicknesses (160$\mu$m, 270$\mu$m and 290$\mu$m) using the nitemper method. A microstructure analysis, microhardness test, surface roughness test, and fracture surface analysis were also carried out at room temperature in order to investigate the mechanical properties of the nitrided specimens.

  • PDF

Study on Thermal Stability of Ni-P-Fe and Ni-P-B Layers Electroplated on Alloy 600 (Alloy 600에 전기 도금한 Ni-P-Fe 및 Ni-P-B 층의 열적 안정성 연구)

  • Kim, Myong-Jin;Kim, Joung-Soo;Kim, Dong-Jin;Kim, Hong-Pyo
    • Journal of the Korean institute of surface engineering
    • /
    • v.43 no.2
    • /
    • pp.57-63
    • /
    • 2010
  • In this study, thermal stability of the mechanical properties of Ni-P-B and Ni-P-Fe layers electroplated on Alloy 600 material was evaluated by measuring their microhardness, tensile strength, and elongation after heat treatment at $325^{\circ}C$ and $400^{\circ}C$. According to the results, there was no noticeable change in microhardness of the two electrodeposits before and after heat treatment at the temperatures for 30 days. In the case of a Ni-P-B electrodeposit, ultimate tensile strength (UTS) slightly increases with heat treatment time, while its elongation decreases, showing good thermal stability in the mechanical properties at high temperature. On the other hand, UTS and elongation of Ni-P-Fe decrease with heat treatment time, which is very unusual observation. This result was attributed to the bad microstructure of Ni-P-Fe having many defects in the deposit formed early stage of an electroplating process and their redistribution to link to become large ones during heat treatment.

Effect of Process Parameters on Microhardness of Ni-Al2O3 Composite Coatings (Ni-Al2O3 복합코팅의 마이크로 경도에 대한 공정변수의 영향)

  • Jin, Yeung-Jun;Park, Simon
    • Journal of the Korean Society of Industry Convergence
    • /
    • v.25 no.6_2
    • /
    • pp.1037-1045
    • /
    • 2022
  • In this study, nanoscale Al2O3 ceramic particles were used due its exceptionally high hardness characteristics, chemical stability, and wear resistance properties. These nanoparticles will be used to investigate the optimal process conditions for the electro co-deposition of the Ni-Al2O3 composite coatings. A Watts bath electrolytic solution of a controlled composition along with a fixed agitation speed was used for this study. Whereas the current density, the pH value, temperature and concentration of the nano Al2O3 particles of the electrolyte were designated as the manipulative variables. The experimental design method was based on the orthogonal array to find the optimum processing parameters for the electro co-deposition of Ni-Al2O3 composite coatings. The result of confirmation experimental based on the optimal processing condition through the analysis of variance ; EDX analysis found that the ratio of alumina increased to 8.65 wt.% and subsequently the overall hardness increased to 983 Hv. Specially, alumina were evenly distributed on Nickel matrix and particles were embedded more firmly and finely in Nickel matrix.

Nanocrystallization of Metallic Powders during High Pressure Torsion Processing (금속분말의 고압비틀림 성형시 나노결정화)

  • Yoon, Seung-Chae;Kwak, Eun-Jeong;Kim, Taek-Soo;Hong, Sun-Ig;Kim, Hyoung-Seop
    • Transactions of Materials Processing
    • /
    • v.16 no.5 s.95
    • /
    • pp.360-363
    • /
    • 2007
  • Microstructure and microhardness of metallic powders of pure copper were studied after high pressure torsion(HPT) processing with 10 turns of die rotation and high pressure of 6 GPa. The grain size of copper decreases drastically after HPT and reaches nanometer size ranges. During HPT, the hardness of consolidates of copper powders increases with increasing the temperature of HPT processing. Examinations of the fracture surfaces indicated evidence of ductile fracture. The results proved that HPT of copper powders has a beneficial effect for homogeneous deformation with reducing grain size.

Analyses of Sever Plastic Deformation Behavior of Hot Isostatic Pressed Ni-base Superalloy during High Pressure Torsion Process (열간정수압성형공정으로 제조된 니켈기 초내열합금의 고압비틀림 공정을 통한 강소성 변형거동 분석)

  • Lee, D.J.;Lee, Y.;Kim, H.-K.;Kwon, Y.-N.;Kim, H.S.;Yoon, E.Y.
    • Transactions of Materials Processing
    • /
    • v.25 no.4
    • /
    • pp.254-260
    • /
    • 2016
  • In this study, hot isostatic pressed Ni-base superalloy was subjected by high-pressure torsion process to improve the dispersion of gamma prime phase, mechanical properties and remove prior particle boundaries. The resulting microstructural size decreases and prior particle boundaries removed with increasing strain by high-pressure torsion process. Moreover, the microhardness values and room temperature tensile strength were enhanced. However, the tensile elongation was decreased as increasing strain due to fast crack propagation along the refined and well dispersed gamma prime particles.

Effects of Deposition Variables on Plasma-Assisted CVD of TiN Films (TiN박막의 증착특성에 미치는 플라즈마 화학증착변수들의 영향)

  • 이정래;김광호;신동원;박찬경
    • Journal of the Korean Ceramic Society
    • /
    • v.31 no.10
    • /
    • pp.1188-1196
    • /
    • 1994
  • TiN films were deposited onto high speed steel(SKH9) and silicon wafer by plasma-assisted chemical vapor deposition(PACVD) using a TiCl4/N2/H2/Ar gas mixture. The effects of deposition temperature, R.F. power, and H2 concentration on the deposition of TiN were studied. The residual chlorine content and the microhardness of TiN films were also investigated. It was found that TiN films grew with a columnar structure of a strong (200) preferred orientation regardless of the substrate type and the deposition variables. The TiN films consisted of columnar-grains of about 50 to 100 nm in diameter. The columnar grains themselves contained much finer fibrous grains. As deposition temperature increased, the residual chlorine content decreased sharply. R. F. powder enhanced the deposition rate largely. Increasing of H2 concentration had little effect on the residual chlorine.

  • PDF