Fire Test of Fiber Cocktail Reinforced High Strength Concrete Columns without Loading (섬유혼입공법을 적용한 고강도콘크리트 기둥의 비재하 내화시험)

  • Youm, Kwang-Soo;Jeon, Hun-Kyu;Kim, Heung-Youl
    • Journal of the Korea Concrete Institute
    • /
    • v.21 no.4
    • /
    • pp.465-471
    • /
    • 2009
  • To prevent the explosive spalling of the high strength concrete and control the rise of temperature in the steel rebar during fire, a fiber cocktail method has been proposed simultaneously with the use of polypropylene and steel fiber. After applying the fiber cocktail (polypropylene and steel fibers) into the mixture of high strength concrete with a compressive strength of between 40 and 100 MPa and evaluating the thermal properties at elevated temperatures, the fire test was carried out on structural members in order to evaluate the fire resistance performance. Two column specimens were exposed to the fire without loading for 180 minutes based on the standard curve of ISO-834. No explosive spalling has been observed and the original color of specimen surface was changed to light pinkish grey. The inner temperature of concrete dropped rapidly starting from 60mm deep. After 60 minutes of exposure to the fire, the temperature gradient of fiber cocktail reinforced high strength concrete was measured as 2.2oC/mm, which is approximately 5 times less than that of normal concrete. The final temperatures of steel rebar after 180 minutes of fire test resulted in 488.0oC for corner rebar, 350.9oC for center rebar, and 419.5oC for total mean of steel rebar. The difference of mean temperature between corner and center rebar was 137.1oC The tendency of temperature rise in concrete and steel rebar changed between 100oC and 150oC The cause of decrease in temperature rise was due to the water vaporization in concrete, the lower temperature gradient of the concrete with steel and polypropylene fiber cocktails, the moisture movement toward steel rebars and the moisture clogging.

Experimental Study of Bond Characteristics on Slab Reinforcement Corroded Before and After Casting (타설 전과 후에 부식시킨 슬래브 시험체의 철근 부착특성에 관한 실험적 연구)

  • Kim, Dae-Il;Cho, Seung-Ho;Chung, Lan
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2001.11a
    • /
    • pp.1035-1040
    • /
    • 2001
  • Recently, Sea-sand containing high levels of chloride is being applied to on reinforced concrete structures due to the exhaustion of river-sand and environmental problems, which affects directly corrosion of rebar in the RC structures. In this paper, characteristics of corroded rebar before and after casting were studied. Test results showed that bond strength of rebar corroded after casting was decreased with increase of corrosion level more rapidly than that of rebar corroded before casting.

  • PDF

Enhancements in Performance and Manufacturing Efficiencies of GFRP Rebar (GFRP 보강근의 성능 및 제작 효율화 방안)

  • You, Young Jun;Kim, Jang Ho;Park, Young Hwan;Park, Ji Sun
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.16 no.1
    • /
    • pp.110-119
    • /
    • 2012
  • Fiber reinforced polymer (FRP) reinforcing rebar with non-corrosive property is suggested as an alternative replacement to steel reinforcing rebar due to its enhanced durability and non-corrosive characteristics. Currently, a limited number of glass fiber reinforced polymer rebar (GFRP) are sold commercially due to their high cost, relatively low performances, and brittle failure characteristics. Therefore, the performance enhancements and cost reduction of GFRP rebar are needed to increase its applications in construction fields. The intent of this study is to develop high performance GFRP rebar by improving its tensile and shear properties. Also, in order to reduce manufacturing costs, factors such as material composition and manufacturing process were evaluated to improve manufacturing efficiency. Finally a GFRP rebar with enhanced material properties and less expensive than the GFRP rebar currently sold in the market was manufactured and evaluated for its application possibility in construction fields.

Prediction of Bending Strength of Concrete Beams with Compressive Strength of 80 MPa (80 MPa의 압축강도를 갖는 콘크리트 보의 휨강도 예측)

  • Kim, Kyoung-Chul;Yang, In-Hwan;Joh, Chang-Bin
    • Journal of the Korea Concrete Institute
    • /
    • v.29 no.4
    • /
    • pp.335-343
    • /
    • 2017
  • This paper aims at investigating the bending strength of high-strength concrete beams with compressive strength of 80 MPa. The experimental parameters included nominal yielding strength of rebar with 400 and 600 MPa, rebar ratio ranging from 0.98 to 1.97%, and shear span-effective depth ratios (a/d) of 6.0 and 4.8. Experimental results were discussed regarding load-deflection relationship, ductility, bending strength, and prediction of bending strength of beams. Test results indicate that the use of high-strength rebar increased bending strength but decreased ductility. As span-effective depth ratio increased, the ductility of test beams decreased. In addition, test results of bending strength were compared with predictions from the current KCI code, Eurocode 2 and Korean Highway Design Specification (KHDC). The design code predictions for bending strength underestimated the experimental results. Therefore, the current design code predictions for bending strength of high-strength concrete beams would provide conservative design. Predictions of bending strength from KCI code using strength reduction factors and those from Eurocode 2 as well as KHDC using material factors were similar each other.

Development of Steel Pipe Splice Sleeve for High Strength Reinforcing Bar(SD500) and Estimation of its Structural Performance under Monotonic Loading (SD500 고강도 철근용 강관 스플라이스 슬리브 철근이음 개발 및 구조성능 평가)

  • Lee, Sang-Ho;Kim, Hyong-Kee
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.11 no.6
    • /
    • pp.169-180
    • /
    • 2007
  • Among several splicing system of reinforcing bar, the grout-filled splice sleeve system has been applied widely. However, as the splice sleeve for high strength rebar as SD500 is not yet made in korea, the development of splice sleeve for high strength reinforcing bar are required as soon as possible. It is the purpose of this study to develop the steel pipe sleeve for high strength rebar as SD500 and estimate its structural performance by monotonic loading test. The experimental variables adopted in this study are the development length of rebars, types of sleeve etc. The results of this study showed that the developed steel pipe splice sleeve system for high strength reinforcing bar as SD500 retained the structural performance required in domestic, ACI and AIJ criteria. And it is considered that the study result presented in this paper can be helpful in developing reasonable design method of steel pipe splice sleeve system for high strength reinforcing bar as SD500.

The Rebar Modulation Method in the Area of the Nuclear Power Plant Structures (원전구조물 부위별 철근모듈화 방안 연구)

  • Lee, Byung-Soo;Bang, Chang-Joon;Kim, Hun Jin;Lim, Sang-Joon;Park, Jong-Hyuk
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2013.11a
    • /
    • pp.15-16
    • /
    • 2013
  • Because of the complicated shape and the overcrowded arrangement of rebar, there are some problems in applying the rebar modulation for the Nuclear Power Plant Structures. In order to resolve these problems, we have been studying the rebar modulation method applying techniques of the high strength rebar for NPP Structure. After reviewing the rebar drawing of the NPP structures and performing the mock-up test, the rebar modulation method in the various area of the NPP Structure has been established. I will introduce this method and the future plan of the research.

  • PDF

Flexural Experiments on Reinforced Concrete Beams Strengthened with ECC and High Strength Rebar (ECC와 고장력 철근으로 보강된 철근콘크리트 보의 휨 실험)

  • Cho, Hyun-Woo;Bang, Jin-Wook;Han, Byung-Chan;Kim, Yun-Yong
    • Journal of the Korea Concrete Institute
    • /
    • v.23 no.4
    • /
    • pp.503-509
    • /
    • 2011
  • ECC is a micro-mechanically designed cementitious composite which exhibits tightly controlled crack width and strain hardening behavior in uniaxial tension while using a moderate amount of reinforcing fiber, typically less than 2% fiber volume fraction. Recently, a variety of applications of this material ranging from repair and retrofit of structures, cast-in-place structures, to precast structural elements requiring high ductility are developed. In the present study, a retrofitting method using ECC reinforced with high strength rebar was proposed to enhance load-carrying capacity and crack control performance of deteriorated reinforced concrete (RC) beams. Six beam specimens were designed and tested under a four-point loading setup. The flexural test revealed that load-carrying capacity and crack control performance were significantly enhanced by the use of ECC and high strength rebar. This result will be useful for practical field applications of the proposed retrofitting method.

Flexural behavior of ultra high performance concrete beams reinforced with high strength steel

  • Wang, Jun-Yan;Gu, Jin-Ben;Liu, Chao;Huang, Yu-Hao;Xiao, Ru-Cheng;Ma, Biao
    • Structural Engineering and Mechanics
    • /
    • v.81 no.5
    • /
    • pp.539-550
    • /
    • 2022
  • A detailed experimental program was conducted to investigate the flexural behavior of ultra high performance concrete (UHPC) beams reinforced with high strength steel (HSS) rebars with a specified yield strength of 600 MPa via direct tensile test and monotonic four-point bending test. First, two sets of direct tensile test specimens, with the same reinforcement ratio but different yield strength of reinforcement, were fabricated and tested. Subsequently, six simply supported beams, including two plain UHPC beams and four reinforced UHPC beams, were prepared and tested under four-point bending load. The results showed that the balanced-reinforced UHPC beams reinforced with HSS rebars could improve the ultimate load-bearing capacity, deformation capacity, ductility properties, etc. more effectively owing to interaction between high strength of HSS rebar and strain-hardening characteristic of UHPC. In addition, the UHPC with steel rebars kept strain compatibility prior to the yielding of the steel rebar, further satisfied the plane-section assumption. Most importantly, the crack pattern of the UHPC beam reinforced with HSS rebars was prone to transform from single main crack failure corresponding to the normal-strength steel, to multiple main cracks failure under the condition of balanced-reinforced failure, which validated by the conclusion of direct tensile tests cooperated with acoustic emission (AE) source locating technique as well.

Bond Characteristics of Ultra High Performance Concrete (초고성능 콘크리트(UHPC)의 부착특성에 관한 연구)

  • Kook, Kyung-Hun;Shin, Hyun-Oh;Kwahk, Im-Jong;Yoon, Young-Soo
    • Journal of the Korea Concrete Institute
    • /
    • v.22 no.6
    • /
    • pp.753-760
    • /
    • 2010
  • Ultra high performance concrete (UHPC), is characterized by its high compressive strength and advanced tensile behavior that is much superior to those of conventional concrete. In order to apply this new material in practice, the bond characteristics of UHPC were evaluated in this study. Pull-out tests between UHPC and deformed steel rebar were carried out according to the modified RILEM test method, and were verified by finite element analysis. From the test results showed that UHPC presents 5 to 10 times higher bond strength compared to normal strength concrete, this study suggested remarkably reduced development length and concrete cover comparing to existing specifications. The test results of 700 MPa high strength steel rebar demonstrated the applicability of high strength steel to UHPC. In addition, the transfer length measurements of seven-wire strand in UHPC specimens indicated that the transfer length limit set by the current design code is very conservative for UHPC.

Post-cracking behavior of UHPC on the concrete members reinforced by steel rebar

  • Rahdar, H.A.;Ghalehnovi, M.
    • Computers and Concrete
    • /
    • v.18 no.1
    • /
    • pp.139-154
    • /
    • 2016
  • Since the concrete strength around the reinforcement rebar affects the tension stiffening, the tension stiffening effect of ultra high performance concrete on the concrete members reinforced by steel rebar is examined by testing the specimens with circular cross section with the length 850 mm reinforced by a steel rebar at the center of a specimen's cross section in this research. Conducting a tensile test on the specimens, the cracking behavior is evaluated and a curve with an exponential descending branch is obtained to explain the post-cracking zone. In addition, this paper proposes an equation for this branch and parameters of equation is obtained based on the ratio of cover thickness to rebar diameter (c/d) and reinforcement percentage (${\rho}$).