• Title/Summary/Keyword: high and ultra-high strength concrete

Search Result 452, Processing Time 0.029 seconds

The site application with 700kg/$\textrm{cm}^2$ high strength concrete (700kg/$\textrm{cm}^2$ 고강도 콘크리트의 현장적용)

  • 권영호;박정국;이보근;박칠림
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1993.10a
    • /
    • pp.124-131
    • /
    • 1993
  • A successful site application with 700kg/$\textrm{cm}^2$ ultra-high strength concrete was made by research team of Daewoo Institute of Construction Technology in Jinhae. Trial mixings of concrete, the productivity of batcher plant, the elapsed time and the pumpability had been investigated for the site condition, before the site application. As results, the efficiency of production by automatic batcher plant systems was improved and the method of quality control was estabilished for the security of fluidity due to the elapsed time, the pumping and consolidation and so on. The concrete strength cores as well as cylinders was showed more than 700kg/$\textrm{cm}^2$ for the required age. And this study would be provided valuable data base for the practical utilization of high strength concrete. Further, this study would be given new possibilities of high rise RC constructions.

  • PDF

An Experimental Study on the Engineering Properties of Ultra-High Strength Concrete according to Types of Mineral Admixtures (광물질 혼화재 종류에 따른 초고강도 콘크리트의 공학적 특성에 관한 실험적 연구)

  • Joung Hyun-Woong;Kang Hoon;Lee Sang-Soo;Song Ha-Young;Kim Eul-Yong
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2005.05b
    • /
    • pp.29-32
    • /
    • 2005
  • In this study, the experiment was carried out to investigate and analyze the strenth properties and flowability of ultra-high strength concrete accroding to types of mineral admixtures. The main experimental variables were water/binder ratio 25.0, 27.5 and 30.0$\%$, water content 155, 160, 165, and 170kg/$m^{3}$ and mineral admixtures such as fly ash, silica fume and meta kaolin. According to the test results, the principle conclusions are summarized as follows. 1) In case of using admixtures, superplasticizer amount need more than plain concrete. 2) According to kinds of admixtures, the viscosity of concrete show much difference. 3) The compressive strength of concrete that use admixtures becomes low in early-age strength, but appeared by higher than plain concrete in long-term strength. 4) Meta kaolin is excellent in side but has viscosity enlargement efficiency a little. But, problem estimates that is not to make design strength 600 and 700kgf/$cm^{2}$ if use mixing condition with water-binder ratio properly.

  • PDF

A potential review on the influence of nanomaterials on the mechanical properties of high strength concrete

  • P. Jagadesh;Karthik Prabhu ;Moutassim Charai;Ibrahim Y. Hakeem;Emrah Madenci;Yasin Onuralp Ozkilic
    • Steel and Composite Structures
    • /
    • v.48 no.6
    • /
    • pp.649-666
    • /
    • 2023
  • In the current scenario, conventional concrete faces a substantial challenge in the modern era of the construction industry. Today's structures are massive, featuring innovative designs and strict time constraints. Conventional concrete does not provide the required compressive strength, tensile strength, flexural strength, toughness, and cracking resistance. As a result, most of engineers and professionals prefer to use ultra-high-performance concrete (UHPC), based on its wide advantages. Several advantages like mechanical and durability properties of UHPC provides dominant properties than the traditional concrete. Mix proportions of UHPC consists of higher powder content which provides maximum hydration and pozzolanic reaction, thereby contributing to the enhancement of the UHPC properties. Apart from that the nanomaterials provides the filler behavior, which will further improve the density. Enhanced density and mechanical properties lead to improved durability properties against water absorption and other typical chemicals. Nanomaterials are the most adopted materials for various applications, ranging in size from 0.1 nanometers to 100 nanometers. This article explores the effects of nanomaterial application in UHPC as a replacement for cementitious material or as an additive in the UHPC mix. The physical and durability properties modifications and improvements of UHPC, as well as negative effects, limitations, and shortcomings, are also analyzed.

Shrinkage Properties of Ultra High Strength Steel Fiber Reinforced Concrete (초고강도 강섬유보강 콘크리트의 수축특성)

  • Koh Kyoung Taek;Pei Chang Chun;Lee Gun Cheol;Kang Soo Tae;Kim Sung Wook;Han Cheon Goo
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2005.11a
    • /
    • pp.647-650
    • /
    • 2005
  • This paper is to investigate the shrinkage properties of ultra high strength concrete(UHSC) incorporating $5\%$ of expansive additives(EA) along with $1\%$ of shrinkage reducing agent(SRA). UHSC subjected to steam curing and incorporated with steel fiber exhibited higher compressive strength than control UHSC by as much as50MPa at 7days, while at 28days, noticeable change in compressive strength was not observed between UHSC mixtures. Control UHSC subjected to steam curing had a $922{\times}10^6$ of autogenous shrinkage strain value, which was 6.7 times of drying shrinkage strain value at 42 days. The combination of EA and SRA resulted in a decrease in autogenous shrinkage by as much as half of control mixture. Steam curing contributed to the reduction of autogenous shrinkage by as much as $11\%$ compared with that of standard curing.

  • PDF

An Experimental Study on Effect of Water-to-Binder Ratio and Admixture on Autogenous Shrinkage of Ultra High Strength Concrete (W/B와 혼화재 치환율이 초고강도 콘크리트의 자기수축에 미치는 영향에 관한 실험적 연구)

  • Kim, Tae-Hoon;Kim, Ji-Won;Sohn, Yu-Shin;Yoon, Young-Soo
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2006.05b
    • /
    • pp.13-16
    • /
    • 2006
  • This paper investigates the shrinkage behavior of Ultra High Strength(UHSC) having three water-to-cementitious material ratio, 0.20, 0.16, 0.12. All of mixtures have same design compressive strength. Free shrinkage test for autogenous and drying shrinkage using $100{\times}100{\times}400$ prismatic specimen was conducted. On all mixture, Effects of fly ash and blast-furnace slag on each shrinkage test results were also investigated. The largest portion of autogenous shrinkage was observed in UHSC12 (w/b=0.12) and the measured strain was as high as 80% of the total drying shrinkage strain. The autogenous shrinkage of UHSC decreased as the amount of fly ash increased as demonstrated in the literature. However, the results of the effect of blast-furnace slag on autogenous shrinkage were somewhat different from previous researches.

  • PDF

Evaluation of Shear Strength of Perfobond Rib in Ultra High Performance Concrete (초고성능 콘크리트에 대한 Perfobond Rib 전단연결재 거동 평가)

  • Kang, Jae-Yoon;Jung, Woo-Tai
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.16 no.7
    • /
    • pp.5015-5020
    • /
    • 2015
  • Push-out test is performed on perfobond shear connectors applying ultra high performance concretes with compressive strength higher than 80 MPa to evaluate their shear resistance. The test variables are chosen to be the diameter and number of dowel holes and, the change in the shear strength of the perfobond rib connector is examined with respect to the strength of two types of UHPC: steel fiber-reinforced concrete with compressive strength of 180 MPa and concrete without steel fiber with compressive strength of 80 MPa. The test results reveal that higher concrete strength and larger number of holes increased the shear strength, and that higher increase rate in the shear strength was achieved by the dowel action.

Proposed New Model for the Stress-Strain Relationship of Ultra High-Strength Concrete (초고강도 콘크리트의 응력-병형률 모델 제안)

  • 박훈규;이정화;윤영수;장일영
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1997.04a
    • /
    • pp.406-412
    • /
    • 1997
  • This paper presents the newly developed model for the stress-strain relationship of ultra high- strength concrete on the basis of the more refined statistical to analysis the various test results available in the literature to be more rigorous in accuracy and generalized scheme. Through the comprehensive analysis of the previously existing equations for each model, multiple curves equation has turned out to be most appropriate to simulate the linearly varying ascending branch and brittle type of descending one. The principal variables to model the stress-strain relationship such as the modulus of elasticity, ultimate strain and deformation characteristics due to stress softening phenomenon were extensively studied to be simplified in the function of the concrete compressive strength.

  • PDF

Fireproofing Method for High Strength Concrete using Densified Spray Resistive Materials and Gypsum Board (고밀도 내화뿜칠재와 석고보드를 이용한 고강도 콘크리트 내화공법)

  • Song, Young-Chan;Kim, Yong-Ro;Oh, Jae-Keun;Kim, Ook-Jong
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2009.05a
    • /
    • pp.471-472
    • /
    • 2009
  • Recently, UH-PH SC (Ultra High PH Strength Concrete) used in High rise building is the material increases in tendency. Thus, the results indicate that it is possible to fireproof panels, fire protection of materials.

  • PDF

Experimental Study on Hysteretic Behavior of 100 MPa Ultra High-Strength Concrete Tied Columns (100 MPa 초고강도 콘크리트 띠철근 기둥의 이력거동에 관한 실험적 연구)

  • Kim, Jong-Keun;Shin, Sung-Woo
    • Journal of the Korea Concrete Institute
    • /
    • v.18 no.2 s.92
    • /
    • pp.161-168
    • /
    • 2006
  • An experimental investigation was conducted to examine the hysteretic behaviors of ultra-high strength concrete tied columns. The purpose of this study is to investigate the safety of ultra-high strength concrete columns with 100 MPa compressive strength for the requirement of ACI provisions. Eight 1/3 scaled columns were fabricated to simulate an 1/2 story of actual structural members with the cross section $300{\times}300mm$ and the aspect ratio 4. The main variables are axial load ratio, configurations and volumetric ratios of transverse reinforcement. The results show that the deformability of columns are affected by the configurations and volumetric ratios of transverse reinforcement. Especially, it has been found that the behavior of columns are affected by axial load ratio rather than the amounts and the configurations of transverse reinforcement. Consequently, to secure the ductile behavior of 100 MPa ultra-high strength concrete columns, ACI provisions for the requirement of transverse steel may considered axial load level and the details of transverse reinforcement.

A Fundamcntal Study on the Propertice of High Performance Concrete using High Flowable Portland Cement (고유동포틀랜드시멘트를 이용한 고성능콘크리트의 기초적 특성에 관한연구)

  • 홍성윤;김병권;박춘근;조동원
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1995.10a
    • /
    • pp.45-49
    • /
    • 1995
  • The fundamental properties of High Performance Concrete(HPC) were studied using high flowable portland cement which was developed at the Sangyong Cement Ind. Co.,Ltd. The results obtained are as follows. (1)The slump of HPC using high flowable portland cement maintains for 120min. (2)Ultra high strength greater than 800kg/$\textrm{cm}^2$ can be designed without using silica fume and other additives. (3)The value of drying shrinkage and adiabatic temperature rise of HPC are less than those of concrete made with OPC.

  • PDF