An Experimental Study on the Abrasion Tests as a Result of using Materials of Full Denture Occlusal Surface (총의치교합면의 사용재료에 따른 마모도 측정에 관한 실험적 연구)

  • Cha, Sung-Soo
    • Journal of Technologic Dentistry
    • /
    • v.5 no.1
    • /
    • pp.19-26
    • /
    • 1983
  • I got a conclusion as a result of that in case of constructing a full denture using acrylic resin teeth, porcelain teeth, and forming posterior occlusal surface of the artificial teeth by Type III Gold and Nickel crome alloy thus construdting a full denture and therefore comparing the above case with abrasion of Natural teeth. The result were as follows : 1. The abrasion of Natural teeth and the abrasion of full denture constructed by Type III gold has a close resemblance. 2. The one that has the hightest degree of abrasion is full denture that's using, with acrylic resin teeth, maxillary and mandibular And the lowest abrasion is natural teeth-natural teeth. 3. In case of single denture, that's opposing to natural teeth, the one that has the hightest degree of abrasion is a full denture that's using Acrylic resin teeth and the lowest abrasion is a full denture that's forming occlusal surface by Type III gold. 4. The single denture, which is opposing to type III gold teeth, was abraded above everything by full denture which is constructed by porcelain teeth. 5. In the same teeth, the abrasion of mandibular teeth was greater than that of mandibular teeth was greater than that of maxillary teeth. 6. The abrasion degree of Acrylic resin teeth has no direct mutual connection with material hardness which is opposing to.

  • PDF

Analysis of Bronze Artifacts and Gold Ornaments Excavated from Xiongnu Tombs No. 2~4 at Duurlig Nars in Mongolia (몽골 도르릭나르스 흉노 무덤 2~4호분 출토 청동 및 금제 유물 분석)

  • Yu, Hei-Sun
    • Journal of Conservation Science
    • /
    • v.28 no.2
    • /
    • pp.175-184
    • /
    • 2012
  • A purpose of this research is to find out characteristic of bronze artifacts and gold ornaments excavated from Xiongnu tombs No. 2~4 at Duurlig Nars in Mongolia through scientific analysis of them. The Tombs are comparatively small. There were still lots of relics remaining although the tombs had been already robbed. Also the tombs are evaluated important since the origin of them show coexisting of chinese and northern style. First of all, an analysis result about bronze vessels found in this site, they have high lead(Pb) content and relatively low tin(Sn) content, as compared with the Bronze Han Mirror and End-fittings of Bronze Parasol Rib. Especially in case of bronze tray and bronze lamp from the no. 2 tomb and also bronze cauldron from the no. 4 tomb contain only 1wt% of tin which means binary alloy composition(Cu-Pb). Also, in the case of gold ornaments found in the no. 2 tomb, they have comparatively high purity. And the research suppose that the high possibility of that they were used soldering using alloy of Au-Cu or diffused bonding(using malachite and copper oxide) for joining gold grains of gold granulation ornament. Further scientific research and analysis in Mongolia and other countries will provide more clues to solve mystery of Xiongnu culture.

A comparative study on the tensile bonding strength of gold alloy solder joints by dental soldering method (치과용 납착 방법에 따른 금합금 납착 연결부의 인장 결합강도 비교 연구)

  • Cho, Mi-Hyang;Lee, Myung-Kon
    • Journal of Technologic Dentistry
    • /
    • v.30 no.1
    • /
    • pp.49-55
    • /
    • 2008
  • In this study, to provide the fundamental data on stable connection method for successful implants prosthesis, We fabricated the solder joint of gold alloy bar specimens by gas flame soldering method and laser welding and soldering method. It compared and studied the tensile strength of two soldering method by universal testing machine. The results using universal testing machine were as follow : The mean of tensile strength of solder joint bar in gas flame soldering method specimens was 363.89 $\pm$17.62 MPa, and the mean strength of laser welding and soldering method was 125.91 $\pm$ 19.66 MPa, so gas flame soldering method was better than laser welding and soldering method and the finding better way to improve tensile strength is needed in laser welding method. On weak loading condition and the part which is needed an accuracy, laser welding method is more effective and on long-span prosthesis and frequent chewing loading part, laser welding technique is recommended first and applying additional gas flame soldering technique would be better for making much more successful prosthesis.

  • PDF

A Comparative Analysis of Stress Distribution in the Implant Supporting Bone by Occlusal Loading location Utilizing the Finite Element Method (유한요소법을 이용한 교합 하중 위치에 따른 임플란트 지지골의 응력분포 비교분석)

  • Lee, Myung-Kon;Kim, Young-Jick;Kim, Chi-Young
    • Journal of Technologic Dentistry
    • /
    • v.27 no.1
    • /
    • pp.105-113
    • /
    • 2005
  • The purpose of this study is to evaluate the effect of loading at three different occlusal surface position of the gold alloy crown on the stress distributions in surrounding bone, utilizing 3-dimensional finite element method. A three dimensional finite element model of an implant with simplified gold alloy crown and supporting bone was developed for this study. A oblique or vertical load of 100 N was applied at the following position at each FE model : 1) center of occlusal surface, 2) a point on the buccal side away from center of occlusal surface (COS) by 2.8mm, 3) a point on the lingual side away from COS by 2.8mm. In the results, Minimum von Mises stresses under vertical load or oblique load of 100N were about 6MPa at the center of occlusal surface and about 40MPa at the point on the buccal side, respectively. From the results we could come to the conclusion that occlusive loading position could be an important factor for establishment of structural safety of supporting bone.

  • PDF

Effect of the Sprue Design on the Fitness of Implant Prosthesis (주입선의 설계가 임플란트 보철물의 적합도에 미치는 영향)

  • Hwang, Sung-Taek;Ahn, Jae-Seok;Shin, Sang-Wan
    • Journal of Technologic Dentistry
    • /
    • v.30 no.2
    • /
    • pp.57-63
    • /
    • 2008
  • Statement of problem: Conventional techniques for implant framework fabrication produce significant error that is inconsistent with passive-fit requirement for osseointegrated implants. One of the etiologic factors which cause the errors is a sprue which may deform the framework during solidification and contraction. Purpose: This study was aimed to evaluate objectively effect of the sprue design on the accuracy of fit of implant prosthesis. Materials and method: Three different designs were considered relative to effect of casting accuracy. The first design had straight sprues and a button of excess alloy at the non-casting end of the sprues. The second was runner bar design(with the button). The last was straight sprues design(without the button). Gold cylinder and laboratory analogue had been used to diminish variables affecting to casting accuracy. Gold alloy and pressure-vacuum casting machine had been used. Marginal gap had been measured by SEM. One-way ANOVA and Duncan test had been used for statistical analysis. Results: The first design showed $79.87{\pm}13.95{\mu}m$ marginal gap. The second and third were $40.17{\pm}15.8{\mu}m$ and $35.17{\pm}9.95{\mu}m$ respectively. Conclusion: Straight sprues without button and runner bar designs were more accurate than straight sprues with button design(P<.05).

  • PDF

각종 의치상재료가 상악총의치의 유지에 미치는 영향에 관한 실험적 연구

  • Lee, Eun-Ho
    • The Journal of the Korean dental association
    • /
    • v.12 no.9
    • /
    • pp.667-677
    • /
    • 1974
  • A testing machine was devised and constructed for the purpose of measuring the retentive forces of maxillary complete denture bases in subjects. Forth complete denture bases were made for ten subjects with three different denture base materials, following the usual denture construction technique. Retentive forces of the forty dentures were determined at seven locations. The tests on each base were repeated three times at intervals of 5 minutes. Differences in retention values were evaluated statistically. 1) Differences in retention values were found by the differences of the denture base materials, but acrylic resin was similar to chromium cobalt alloy. 2) The chromium cobalt alloy and acrylic resin bases from master models revealed the best retention values, the gold alloy base from master model was the poor second and the acrylic resin base from snap model was the third. 3) The retention values for hook-1 revealed higher than that for hook-2 and the retention values for hook-3 revealed the lowest value.

  • PDF

Age-Hardening Behavior and Structural Changes in a Commercial Dental Au-Ag-Cu-Pd Alloy

  • Kim, Hyung-Il;Park, Seok-Kyu
    • Journal of Biomedical Engineering Research
    • /
    • v.15 no.4
    • /
    • pp.389-394
    • /
    • 1994
  • The age-hardening behavior and the structural changes in a commercial dental Au-Ag-Cu-Pd alloy were investigated by means of hardness test, optical and scanning electron microscopic observation, energy dispersive spectroscopy and X-ray diffraction study. The drastic reduction in hardness by prolonged aging occurred after a rapid increase in hardness at the initial stage by the isothermal aging at $350^{\circ}C$. This softening was due to the broad precipitates formation of the lamellar structure which was composed of the f.c.t. AuCu I ordered f.c.t. phase containing Pd and the f.c.c. Ag-rich $\alpha$1 solid solution f.c.c.phase containing Au.

  • PDF

Charactristice of a colored Galvanized Coating using Ti-Zn Alloy System (Zn-Ti계용융아연 도금강판의 착색화 특성)

  • 전선호
    • Journal of the Korean institute of surface engineering
    • /
    • v.30 no.5
    • /
    • pp.320-332
    • /
    • 1997
  • The development of colored surface on zinc coating by the oxidation of a melten alloy of zinc with a minor amount of oxygen-avid additive such as tianium has been studied. Using a galvanizing Zinc alloy containing 0.1 to 0.3wt%Ti, gold, purple or blue color was developed clearly and stably, depending upon the extent of oxidation, by air cooling after hot dipping in a bath at temperature of $550^{\circ}C$ to $600^{\circ}C$. The source of the color is light interference with surface oxide layer. THe final color depends on the thickness of the color depends on the thickness of $TiO_2$, played So compositing, temperature and time at elevated temperature after are all controlling variables. Since oxidation film such as $TiO_2$ played role of passivation film, the corrosion resistance in a colored galvanized steel sheet. It is also thought that surface oxide layer of $TiO_2$ inhibited dissolution of the coating layer.

  • PDF

THE STRESS ANALYSIS OF SUPPORTING TISSUE AND IMPLANT ACCORDING TO CROWN RESTORATIVE MATERIALS AND TYPE OF IMPLANT (수복재료와 임플랜트 종류에 따른 임플랜트 및 지지조직의 응력분포)

  • Choi Chang-Hwan;Oh Jong-Suk;Vang Mong-Sook
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.40 no.1
    • /
    • pp.53-67
    • /
    • 2002
  • This study was aimed to analyze the stress distribution of implant and supporting tissue in single tooth implant restoration using Branemark $system^{(R)}$(Nobel Biocare, Gothenberg, Sweden) and Bicon system(Bicon Dental Implants, Boston, MA). Two dimensional finite element analysis model was made at mandibular first premolar area As a crown materials porcelain, ceromer, ADA type III gold alloy were used. Tests have been performed at 25Kgf vertical load on central fossa of crown portion and at 10Kgf load with $45^{\circ}$ lateral direction on cusp inclination. The displacement and stresses of implant and supporting structures were analyzed to investigate the influence of the crown material and the type of implant systems by finite element analysis. The results were obtained as follows : 1. The type of crown material influenced the stress distribution of superstructure, but did not influence that of the supporting alveolar bone. 2. The stress distribution of ceromer and type III gold alloy and porcelain is similar. 3. Stress under lateral load was about twice higher than that of vertical load in all occlusal restorative materials. 4. In Bicon system, stress concentration is similar in supporting bone area but CerOne system generated about 1.5times eater stress more in superstructure material. 5. In Branemark models, if severe occlusal overload is loaded in superstvucture. gold screw or abutment will be fractured or loosened to buffer the occlusal overload but in Bicon models such buffering effect is not expected, so in Bicon model, load can be concentrated in alveolar bone area.