• Title/Summary/Keyword: frost durability

Search Result 54, Processing Time 0.024 seconds

The Study of experiment on preventing frost damage at early age of mortar in low temperature using Reduction slag. (환원슬래그를 사용한 콘크리트의 내구성 평가에 관한 연구)

  • Min, Tae-Beom;Choi, Hyun-Kuk;Mun, Young-Bum;Kim, Hyeong-Cheol
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2016.10a
    • /
    • pp.150-151
    • /
    • 2016
  • In previous study, researchers studied development of early anti-freezing cement at low temperature (-5℃) using hydration characteristics of reduction slag. In this study, the durability of concrete using reduction slag was conducted. The experiment result, reduction slag makes high temperature and improves compressive strength due to quick setting. And then result of durability show that it is no problem. However, it is considered that further study is needed about high shrinkages which was indicated in dry shrinkage.

  • PDF

Evaluation of Chloride Penetration Resistance of Frost Concrete according to the water-cement ratio, during the Cold Wave (한파로 인한 초기 동해를 입은 콘크리트의 염해 저항성 평가)

  • Park, Dong-Cheon;Lee, Jun-Hae
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2020.11a
    • /
    • pp.165-166
    • /
    • 2020
  • The climate on the Korean Peninsula has been warmed recently, abnormal weather conditions such as heat waves, cold waves, and tropical nights have been detected frequently. Precisely, the number of days with cold waves in the winter has increased, and rapid changes of temperature in the morning and afternoon have occurred frequently in the 2000s. Due to the previous phenomenons, this research is focused on evaluating the concrete's Chloride Penetration Resistance and Durability, and the difference of the resistance according to the W/C.

  • PDF

A Study on the Resistance for Frost Damage of Polypropylene Fiber Reinforced Light Weight Polymer Cement Concrete (폴리프로필렌섬유보강 경량 폴리머 시멘트 콘크리트의 내동해성에 관한 연구)

  • 소형석;소승영;소양섭;박종호;탁재호
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1995.10a
    • /
    • pp.89-92
    • /
    • 1995
  • For the development of lilght weight cement concrete with high durability, this study used perlite and paper sludge ash by the light weight material, and polypropylene fiber by the reinforcment, and poly-acrylic ester emulsion by the matrix improvement. According to the increasing mixture ratio of fiber and use of polymer, the light weight polypropylene fiber reinforced polymer cement ratio of fiber and use of polymer, the light weight polypropylene fiber reinforced polymer cement concrete were showed high resistance for frost damage.

  • PDF

The Crack Inspection and Repair System on the Concrete Pier Caused by Frost Damage (동해를 입은 콘크리트 교각의 균열조사 및 보수시공)

  • 장태민;권영진;김철호;이병훈;최롱;오상근
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1996.10a
    • /
    • pp.551-556
    • /
    • 1996
  • It is the aim of this study to introduce the performence and application of new repair system for the concrete pier by durability failure caused frost damage. The elementary performance of this repair system is as follows (1) All the layer in the repair system are cement based, same with the mother con'c. (2) This repair use SBR admixture. (3) This cement and mortar powder for this repair system are premixed and ready to adding admixture at the job site.

  • PDF

The Evaluation of Surface Scaling and Resistance of Concrete to Frost Deterioration with Freezing-Thawing Action by Salt Water (염화물이 함유된 동결수의 동결융해 작용에 따른 콘크리트의 내동해성과 표면열화 평가)

  • Kim, Gyu-Yong;Kim, Moo-Han;Cho, Bong-Suk;Lee, Seung-Hoon
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.11 no.6
    • /
    • pp.143-151
    • /
    • 2007
  • This study presents the experimental results of frost durability including resistance to freezing-thawing and surface scaling of concrete. Mixing design was proportioned with the various water-binder ratio between 0.37 and 0.47 and three different binder compositions corresponding to Type I cement without any supplementary cementitious materials(OPC), Type II cement with 50% blast-furnace slag replacement(BFS50), and ternary cement with Type III cement, 15% fly ash, and 35% slag replacement (BFS35%+FA15%). Test results showed that the mixing design with BFS50% and BFS35%+FA15% exhibited higher durability factor than that made with OPC only. Finally, the use of blend cement containing slag can be used effectively in terms of frost durability of the concrete exposed to severe condition under coastal environment like as flying salt, sea water spray, etc.

Consideration of the Effect of Miscellaneous Factors on Frost Resistance of High Strength Concrete by Using the Factorial Design Method

  • Kwon Young-Jin
    • Journal of the Korea Concrete Institute
    • /
    • v.16 no.2 s.80
    • /
    • pp.269-275
    • /
    • 2004
  • Factorial design method is applied to investigate the effects of various factors simultaneously rather than to conduct a series of single-factor experiment. As the results, frost resistance of the concrete specimens, in both W/C ratio of 0.28 and 0.35, was highly affected by the type of coarse aggregate that is, andesite produced more durable concrete than the limestone. Durability factor of the specimens, with W/C ratio of 0.28, which were demolded after I day and transferred to the curing room was higher than those demolded after 2 days. This stated the efficiency of the high early curing in high strength concrete.

A Study on the Effect of Experimental Factors for the Durability Inspection of High Strength Concrete (고강도콘크리트의 내구성진단을 위한 영향인자 파악을 위한 연구)

  • Kwon, Young-Jin;Kim, Moo-Han
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.1 no.2
    • /
    • pp.123-130
    • /
    • 1997
  • The effect of experimental factors on the Freeze-Thaw durability in the High Strength Concrete has been analyzed and investigated with [DESIGN of EXPERIMENT: L16). The Experimental parameters included the type of aggregate and mixer, the conditions of aggregates, and the difference of mixing temperature, procedure and placing, etc. It is aim of this study to provide the fundamental data on the effect of various factors on the frost resistance of high strength concrete for the practical use and research data accumulation of durability inspection. The results of this experiment indicate that the freeze-thaw durability of high strength concrete is markedly affected by the coarse aggregate source, mixing temperature and curing conditions.

  • PDF

Effect of rubber particles on properties and frost resistance of self-compacting concrete

  • Miao Liu;Jianhua Xiao;En Yang;Lijuan Su
    • Advances in concrete construction
    • /
    • v.16 no.5
    • /
    • pp.269-276
    • /
    • 2023
  • In order to study the effect of rubber particle size and admixture on the frost resistance of self-compacting concrete, three self-compacting concrete specimens with equal volume replacement of fine aggregate by rubber particles of different particle sizes were prepared, while conventional self-compacting concrete was made as a comparison specimen. The degradation law of rubber aggregate self-compacted concrete under freeze-thaw cycles was investigated by fast-freezing method test. The results show that the rubber aggregate has some influence on the mechanical properties and freeze-thaw durability of the self-compacting concrete. With the increase of rubber aggregate, the compressive strength of self-compacting concrete gradually decreases, and the smaller the rubber aggregate particle size is, the smaller the effect on the compressive strength of the matrix; rubber aggregate can improve the frost resistance of self-compacting concrete, and the smaller the rubber particle size is, the more obvious the effect on the improvement of the frost resistance of the matrix under the same dosage. Through the research of this paper, it is recommended to use 60~80 purpose rubber aggregate and the substitution rate of 10% is chosen as the best effect.

A Study on the Analysis of Scaling Failure Cause in L-Shoulder Concrete Structure (L형측구 콘크리트 구조물의 표면박리파손 원인분석에 관한 연구)

  • Jeon, Sung Il;Nam, Jeong Hee;Ahn, Sang Hyeok;An, Ji Hwan
    • International Journal of Highway Engineering
    • /
    • v.16 no.6
    • /
    • pp.27-37
    • /
    • 2014
  • PURPOSES : The purpose of this study is to verify the causes of surface scaling at L-shoulder concrete structure. METHODS : From the literature reviews, mechanisms of frost damage were studied and material properties including strength, air void, spacing factor and scaling resistance of L-shoulder concrete structure were analyzed using core specimens taken by real fields. RESULTS : The spacing factor of air void has relatively high correlation of surface conditions : lower spacing factor at good surfacing condition and vice versa. If the compressive strength is high, even thought spacing factor does not reach the threshold value of reasonable durability, the surface scaling resistance shows higher value. Based on these test results, the compressive strength also provide positive effect on the surface scaling resistance. CONCLUSIONS : The main causes of surface scaling of L-shoulder could be summarized as unsuitable aid void amount and poor quality of air void structure. Secondly, although the compressive strength is not the governing factor of durability, but it shows the positive effect on the surface scaling resistance.