지오폴리머 기반 순환골재 혼입율에 따른 친환경성 인조석재의 특성 (Properties of Eco-friendly Artificial Stone according to the mixing ratio of Geopolymer-based recycled Aggregate)

  • 경석현;최병철;강연우;이상수
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2020년도 봄 학술논문 발표대회
    • /
    • pp.126-127
    • /
    • 2020
  • Recently, as interest in environmental issues increases, minimizing carbon dioxide generated during cement manufacturing is a problem to be solved. In order to solve such a problem, it is required to use an industrial by-product of recycled aggregate, blast furnace slag, and circulating fluidized bed boiler fly ash to replace it on the basis of geopolymer(=cementless). This study examines the characteristics of eco-friendly artificial stone according to the mixing ratio of geopolymer-based recycled aggregate. As a result of the experiment, when the addition rate of the alkali stimulant was 15% and the mixing ratio of the circulating aggregate was 70%, the flexural strength and compressive strength were the highest. Density and water absorption decreased as density of circulating aggregates increased and water absorption increased. However, when the mixing ratio of the circulating aggregate exceeded 70%, the flexural strength and compressive strength decreased. Therefore, in order to obtain strengths meeting the KS standards, the mixing ratio of recycled aggregate was set to 70%, and artificial stone was manufactured using industrial by-products.

  • PDF

C-S-H계 조강제 첨가에 따른 혼합시멘트의 조기 강도 발현 특성 (Characteristics of early strength development of blended cement according to the addition of C-S-H based Hardening acceleration)

  • 안태윤;라정민;박준형;김진만
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2022년도 가을 학술논문 발표대회
    • /
    • pp.127-128
    • /
    • 2022
  • In order to realize carbon neutrality in the international society, research on supplementary cementitious materials(SCMs) has been actively conducted as a way to reduce carbon dioxide emissions in the cement industry. However, the use of SCMs causes problems of initial hydration delay and strength reduction due to the reduction of tricalcium silicate(C3S) in the cement clinker. Therefore, in this study, the initial hydration and basic characteristics of cement mortar were confirmed by adding a C-S-H based hardening acceleration to blended cement mixed with Portland cement, blast furnace slag, fly ash, and limestone power. As a result of the heat of hydration and compressive strength test, it was confirmed that when hardening acceleration was added, the initial reactivity was high, so the heat of hydration was promoted, and the initial strength was increased. It is considered to be due to C-S-H seeding effect. Therefore, it is judged that the use of C-S-H based hardening acceleration can supplement the problem of initial hydration delay of blended cement in Korea.

  • PDF

혼화재 혼입에 따른 콘크리트 배합요소 산정을 위한 DNN 기반의 예측모델 제안 (Proposal of DNN-based predictive model for calculating concrete mixing proportions accroding to admixture)

  • 최주희;이광수;이한승
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2022년도 가을 학술논문 발표대회
    • /
    • pp.57-58
    • /
    • 2022
  • Concrete mix design is used as essential data for the quality of concrete, analysis of structures, and stable use of sustainable structures. However, since most of the formulation design is established based on the experience of experts, there is a lack of data to base it on. are suffering Accordingly, in this study, the purpose of this study is to build a predictive model to use the concrete mixing factor as basic data for calculation using the DNN technique. As for the data set for DNN model learning, OPC and ternary concrete data were collected according to the presence or absence of admixture, respectively, and the model was separated for OPC and ternary concrete, and training was carried out. In addition, by varying the number of hidden layers of the DNN model, the prediction performance was evaluated according to the model structure. The higher the number of hidden layers in the model, the higher the predictive performance for the prediction of the mixing elements except for the compressive strength factor set as the output value, and the ternary concrete model showed higher performance than the OPC. This is expected because the data set used when training the model also affected the training.

  • PDF

Predicting the compressive strength of SCC containing nano silica using surrogate machine learning algorithms

  • Neeraj Kumar Shukla;Aman Garg;Javed Bhutto;Mona Aggarwal;Mohamed Abbas;Hany S. Hussein;Rajesh Verma;T.M. Yunus Khan
    • Computers and Concrete
    • /
    • 제32권4호
    • /
    • pp.373-381
    • /
    • 2023
  • Fly ash, granulated blast furnace slag, marble waste powder, etc. are just some of the by-products of other sectors that the construction industry is looking to include into the many types of concrete they produce. This research seeks to use surrogate machine learning methods to forecast the compressive strength of self-compacting concrete. The surrogate models were developed using Gradient Boosting Machine (GBM), Support Vector Machine (SVM), Random Forest (RF), and Gaussian Process Regression (GPR) techniques. Compressive strength is used as the output variable, with nano silica content, cement content, coarse aggregate content, fine aggregate content, superplasticizer, curing duration, and water-binder ratio as input variables. Of the four models, GBM had the highest accuracy in determining the compressive strength of SCC. The concrete's compressive strength is worst predicted by GPR. Compressive strength of SCC with nano silica is found to be most affected by curing time and least by fine aggregate.

플라이애쉬와 고로슬래그를 사용한 3성분계 고성능 콘크리트의 강도 및 촉진 중성화에 대한 실험적 고찰 (An Experimental Study on Compression Strength and Carbonation Resistance for Ternary High-Performance Concrete with fly-sah, granulated blast furnace)

  • 권영락;김홍삼;이찬영;정해문;안태송
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2008년도 춘계 학술발표회 제20권1호
    • /
    • pp.445-448
    • /
    • 2008
  • 콘크리트는 골재, 시멘트와 물이 주 구성성분이지만 현대 구조물의 다양화 및 해양환경 구조물의 증가로 해수에 대한 저항성이 우수한 콘크리트의 개발과 환경적 측면에서의 자원재활용이라는 사회적 관심 또한 증폭되고 있다. 따라서 내구성 향상, 고강도화, 현장에서의 워커빌리티 향상, 운반, 경제성 향상 등의 고성능 콘크리트의 필요성이 요구되어 오고 있다. 또한 고강도 영역의 고성능 콘크리트는 단위결합재량이 많으므로 수화열의 상승으로 콘크리트 균열에 의한 내구성능 저하의 원인이 되어 왔다. 따라서 본 연구에서는 수화열의 억제 목적으로 Plain 실험체와 기본적으로 플라이애쉬 20%, 고로 슬래그 미분말 30%, 45% 치환한 조건에서 물-결합재비 26%, 30%, 34%인 실험체를 제작하여 이에 따른 압축강도 및 중성화 특성과 중성화 영역과 미중성화 영역을 대상으로 XRD(X-ray diffraction) 분석을 통하여 혼화재 치환량에 의한 특성을 평가하였다.

  • PDF

무기계고화재의 슬러지 개량토 제조에 관한 융합연구 (Convergent Study on the Preparation of Sludge Modified Soils of Inorganic Consolidation Soil)

  • 한두희
    • 한국융합학회논문지
    • /
    • 제8권2호
    • /
    • pp.157-162
    • /
    • 2017
  • 제지슬러지 소각재, 용광로 슬래그 미세분말 생석회, 무수석고 및 프라이애쉬 등을 혼합하여 무기계고화재를 제조하였다. 슬러지 처리용으로 개발된 고화재의 주성분은 SiO, $Al_2O_3$, $TiO_2$, $Fe_2O_3$, $Mn_2O_3$, CaO, MgO, $Na_2O$, $K_2O$, $P_2O$, $SO_3$이었다. 시멘트와 달리, 개발된 고화재에는 발암물질로 알려진 $Cr^{6+}$가 함유되지 않았다. 중금속 및 기름 오염토를 고화재와 혼합한 후 7일간 양생하여 빗물용출실험을 시행한 결과 중금속이 미미하였다. 하수슬러지 케이크 및 음식물쓰레기와 고화재를 각각 혼합하여 7일 양생 후 토양성분실험을 한 결과 중금속 함량이 환경기준치 이하로 나타났다. 슬러지, 고화재 및 첨가제 혼합시료를 비이커에 혼합한 후 암모니아 농도를 측정한 결과 3일 후 0이 되었다.

친환경 무기계 토양개량 고화제에 의한 해양오염토 처리 (Soil Treatment by Eco-Friendly Consoildation Soil)

  • 한두희
    • 융합정보논문지
    • /
    • 제7권1호
    • /
    • pp.67-73
    • /
    • 2017
  • 제지슬러지 소각재, 용광로 슬래그, 미세분말 생석회, 무수석고 및 프라이애쉬를 주성분으로 하는 고화제를 염분을 함유한 해양토양에 알맞도록 제조하였다. 고화제이 주성분은재활용된 세라믹 종류이며 이중 CaO가 고화작용에 있어서 중요한 역할을 한다. 고화처리 후 중성화 시간은 약 2주일이었으며, 표준사를 사용하여 1주일 양성 후 모르타르 실험에서 압축강도는 약 12N/mm2 정도로 나타났다. 이것은 수도권 매립지에 사용되고 있는 고화제에 비하여 14배 정도의 강도이다. 염분 함유된 해양토양에 적용하여 평판재하실험을 한 결과 5일정도 지나면 대형도저가 지나갈 수 있을 정도의 항복하중을 얻었다. 일축압축강도 실험에서는 5일 경과 후 약 300kPa의 전단강도를 얻었다. 인천지역과 같이 해양 매립이 많이 이루어지고 있는 지역의 연약지반 보완작업에 유용하게 적용될 것으로 파악된다.

광물성 혼화재료의 종류 및 혼입율에 따른 숏크리트의 역학적 특성 및 염해 저항성 (Mechanical Properties And Chlorde Penetration Resistance of Shotcrete according to Mineral Admixture Types and Supplemental Ratio)

  • 한승연;윤경구;남궁경;이겨레;엄영도
    • 한국산학기술학회논문지
    • /
    • 제16권7호
    • /
    • pp.4960-4968
    • /
    • 2015
  • 본 논문에서는 숏크리트 구조물의 염해 내구성을 개선하고자 광물성 혼화재의 종류 및 혼입량에 따라 유럽의 시험규준인 NT BUILD 492에 준하여 염해 저항성을 평가하였다. 또한 정적강도 및 염소이온 침투저항성 등의 역학적 특성을 함께 평가하였다. 부순 골재를 사용하여 굵은 골재 최대치수 10mm의 숏크리트용 혼합쇄석 골재를 제작하였다. 재령 28일 압축강도를 기준으로 실리카퓸 15% 혼입 변수가 67.55MPa로 가장 높은 강도를 나타냈으며, 플라이애시와 고로슬래그는 혼입률이 증가할수록 강도가 감소하는 것으로 나타났다. 염소이온 침투저항성 시험에서는 기본 배합에서 "높음" 등급으로 나타났으며, 혼화재료의 경우 플라이애시를 제외하고 모든 변수에서 침투저항성이 매우 증가하는 경향을 보였다. 촉진 염화물 확산 침투시험으로 KCL, ACI, FIB 기준에 대한 내구수명을 평가하였다. 시험결과 실리카퓸 15%를 혼입한 변수에서 가장 낮은 확산계수를 얻었다, KCI 기준으로 약 65년의 내구수명을 갖는 것으로 나타났으며, FIB 기준으로 131년의 내구수명을 갖는 것으로 나타났다. KCI, ACI, FIB 기준 중 모든 변수에서 KCI 기준의 내구수명이 가장 낮은 것으로 평가되었다.

보수재료로서 고로슬래그 미분말 및 플라이애쉬를 혼입한 SAE 에멀젼 기반 폴리머 시멘트 모르타르의 휨접착 및 인장접착 특성 (Properties of Adhesion in Flexure and Tension of Polymer Cement Mortar Using SAE Emulsion with Blast-Furnace and Fly Ash as a Repair Material)

  • 조영국
    • 한국건축시공학회지
    • /
    • 제19권6호
    • /
    • pp.485-494
    • /
    • 2019
  • 본 연구는 고로슬래그 미분말 및 플라이애쉬를 혼입한 SAE 에멀젼 기반 폴리머 시멘트 모르타르의 휨과 인장특성에 대하여 실험하여 혼화재의 혼입효과를 평가하고자 하였다. PCM은 폴리머 시멘트비와 혼화재의 혼입율을 변화시켜 시험편을 제작하였으며, 휨강도, 휨접착강도, 인장강도 및 인장접착강도 시험을 실시하였다. 연구결과, 혼화재의 혼입에 따른 휨강도 및 휨접착강도 개선은 거의 발현되지 않았으나, 인장강도 및 인장접착강도에서는 혼화재의 혼입에 따른 강도개선 효과를 얻을 수 있었다. 특히 PCM의 인장 접착강도는 P/C 20%, 고로슬래그 미분말 혼입율 10%에서 최대 3.35MPa로 보통시멘트 모르타르의 약 2.36배, 혼화재를 혼입하지 않은 PCM의 약 1.32배의 높은 강도를 나타냈으며 인장접착강도/인장강도비는 평균 48.7%를 나타냈다. 본 연구를 통하여 PCM의 인장 및 인장접착강도 개선을 위해서는 혼화재 혼입율 5% 또는 10%를 제안할 수 있었다.

폐콘크리트로부터 회수된 시멘트 페이스트 미분말의 시멘트 원료화 연구 (Manufacture of Ordinary Portland Cement Clinker Using Cement Paste of the Waste Concrete)

  • 안지환;김형석;조진상;한기천;한기석;김환
    • 한국세라믹학회지
    • /
    • 제40권8호
    • /
    • pp.804-810
    • /
    • 2003
  • 건설폐기물 중 폐콘크리트를 40$0^{\circ}C$로 가열한 후 ball mill로 분쇄하여 재생골재를 생산할 때 발생된 미분말을 보통 포틀랜드 시멘트의 SiO$_2$, CaO, A1$_2$O$_3$원에 대한 대체원료물질로서 활용하고자 하였다. 클링커를 제조하기 위한 주원료는 석회석, shale, 전로슬래그, fly ash를 이용하였고, modulus는 LSF:91.0, SM:2.60, IM:1.60로 고정한 후 shale에 대해 미분말을 25, 50, 15, 100%까지 치환하여 클링커를 제조하였다. 클링커의 주요생성광물은 1,45$0^{\circ}C$에서 OPC와 같은 광물상인 $C_3$S, $\beta$-C$_2$S, $C_3$A, $C_4$AF 상으로 나타났다. 조합원료의 반응성을 비교하기 위해 시차열분석을 실시하고, 소성성지수를 구한 결과, 클링커의 광물상 생성온도는 plain과 유사했으며, 소성성지수는 48.6-51.4 정도로 나타났다.