An Experimental Study on Compression Strength and Carbonation Resistance for Ternary High-Performance Concrete with fly-sah, granulated blast furnace

플라이애쉬와 고로슬래그를 사용한 3성분계 고성능 콘크리트의 강도 및 촉진 중성화에 대한 실험적 고찰

  • 권영락 (한국도로공사 도로교통연구원) ;
  • 김홍삼 (한국도로공사 도로교통연구원) ;
  • 이찬영 (한국도로공사 도로교통연구원) ;
  • 정해문 (한국도로공사 도로교통연구원) ;
  • 안태송 (한국도로공사 도로교통연구원)
  • Published : 2008.04.24

Abstract

It is essential that concrete component is made up with aggregate, cement and water. But today, Public concern is increasing of a variety structure and ocean environmental, resource recycle. Also, According to heat of hydration rising, Concrete is make a causative of concrete-crack. Concrete-crack cause a falling-off in quality of concrete. consequently, High-performance concrete is evaluated by concrete material properties and carbonation resistance with different admixture(fixing fly-ash 20%), granulated blast furnace slag replacement ratio (30%, 45%) different W/B (26%, 30%, 34%) and XRD(X-ray Diffraction) analysis.

콘크리트는 골재, 시멘트와 물이 주 구성성분이지만 현대 구조물의 다양화 및 해양환경 구조물의 증가로 해수에 대한 저항성이 우수한 콘크리트의 개발과 환경적 측면에서의 자원재활용이라는 사회적 관심 또한 증폭되고 있다. 따라서 내구성 향상, 고강도화, 현장에서의 워커빌리티 향상, 운반, 경제성 향상 등의 고성능 콘크리트의 필요성이 요구되어 오고 있다. 또한 고강도 영역의 고성능 콘크리트는 단위결합재량이 많으므로 수화열의 상승으로 콘크리트 균열에 의한 내구성능 저하의 원인이 되어 왔다. 따라서 본 연구에서는 수화열의 억제 목적으로 Plain 실험체와 기본적으로 플라이애쉬 20%, 고로 슬래그 미분말 30%, 45% 치환한 조건에서 물-결합재비 26%, 30%, 34%인 실험체를 제작하여 이에 따른 압축강도 및 중성화 특성과 중성화 영역과 미중성화 영역을 대상으로 XRD(X-ray diffraction) 분석을 통하여 혼화재 치환량에 의한 특성을 평가하였다.

Keywords