Workability and Mechanical Properties of Hybrid Fiber Reinforced Concrete Using Amorphous Steel Fiber and Polyamide Fiber

  • Kwon, Soon-Oh;Bae, Su-Ho;Lee, Hyun-Jin;Kim, Yo-Seb;Jun, Jin;Kim, Wha-Jung
    • 한국건설순환자원학회논문집
    • /
    • 제4권4호
    • /
    • pp.470-476
    • /
    • 2016
  • Many studies have been performed on hybrid fiber reinforced concrete for years, which is to improve some of the weak material properties of concrete. Studies on characteristics of hybrid fiber reinforced concrete using amorphous steel fiber and polyamide fiber, however, yet remain to be done. The purpose of this experimental research is to evaluate the workability and mechanical properties of hybrid fiber reinforced concrete using amorphous steel fiber and polyamide fiber. For this purpose, the hybrid fiber reinforced concrete containing amorphous steel fiber(ASF) and polyamide fiber(PAF) were made according to their total volume fraction of 0.5 % for water-binder ratio of 33 %, and then the mechanical properties such as the compressive strength, direct tensile strength, flexural strength, and flexural toughness of those were estimated. It was observed from the test results that the compressive strength was slightly decreased with increasing ASF and decreasing PAF and the effect of fiber combination on the flexural strength was not much but the flexural toughness was relatively largely increased with decreasing ASF and increasing PAF.

섬유혼입률에 따른 고성능 슬러리 충전 강섬유보강 시멘트 복합체의 휨성능 특성 (Flexural Performance Characteristics of High Performance Slurry Infiltrated Fiber Reinforced Cementitious Composite according to Fiber Volume Fraction)

  • 김승원;조현명;이학용;박철우
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제19권4호
    • /
    • pp.109-115
    • /
    • 2015
  • 본 연구는 SIFCON 형태의 고성능 강섬유보강 시멘트 복합체의 섬유혼입률에 따른 휨실험을 수행하였고, 실험결과를 바탕으로 휨성능을 평가하였다. 슬러리를 충전하는 형태로 일반 섬유보강시멘트와 달리 높은 섬유혼입률을 확보할 수 있는 장점을 가지고 있다. 주요 실험 변수는 섬유혼입률 8.0%, 7.5%, 7.0%, 6.5% 및 6.0% 이며, 각 변수에 대한 휨강도 및 휨인성 특성을 분석하였다. 그 결과, 높은 섬유혼입률로 인하여 초기균열 발생 이후에도 계속적으로 하중이 증가하였으며, 최대강도 이후 충분한 잔류강도를 확보하였다. 또한 최대 50MPa 수준의 높은 휨강도를 발현하였으며, 섬유혼입률에 따른 휨강도 및 휨인성은 비례하여 증가하는 경향으로 나타났다.

갈고리형 강섬유를 혼입한 보통 및 고강도 콘크리트의 휨강도 평가 (Evaluation of Flexural Strength for Normal and High Strength Concrete with Hooked Steel Fibers)

  • 오영훈
    • 콘크리트학회논문집
    • /
    • 제20권4호
    • /
    • pp.531-539
    • /
    • 2008
  • 본 연구에서는 강섬유보강 고강도콘크리트의 휨강도와 휨인성을 평가하기 위하여 실험을 수행하였으며, 이러한 실험 결과와 기존 연구자들의 실험 결과를 추가하여 강섬유보강 고강도콘크리트의 휨거동 특성을 분석하였다. 고강도 강섬유 콘크리트의 휨거동 특성은 강도와 인성으로 평가할 수 있으며, 이러한 특성은 콘크리트의 압축강도, 강섬유 혼입률 및 형상비, 강섬유계수와 같은 요소에 의해 영향을 받는 것으로 파악되었다. 아울러 기존 연구자에 의해 제안된 휨강도 산정식의 유효성을 평가하였으며, 강섬유 콘크리트의 휨강도는 콘크리트의 압축강도, 강섬유 혼입률 및 형상비, 강섬유계수와 같은 구조변수의 영향을 모두 고려하여 평가하는 것이 합리적이라고 판단되었다. 최종적으로 본 연구에서는 강섬유 혼입에 따른 휨강도의 상승분과 주요 구조변수간의 상관관계를 분석함으로써 보다 합리적인 휨강도 산정식을 제시하였다.

GFRP 보강 다공성 콘크리트 블록의 내력 및 인성 평가 (Evaluation of Load Capacity and Toughness of Porous Concrete Blocks Reinforced with GFRP Bars)

  • 정승배;양근혁
    • 한국건축시공학회지
    • /
    • 제17권5호
    • /
    • pp.403-409
    • /
    • 2017
  • 본 연구에서는 다공성 블록의 내구성 향상을 위해 압축강도 3MPa 및 공극률 30%를 만족하는 배합설계를 확인하였으며, 선정된 배합에서 GFRP 보강 방법에 따른 보의 내력 및 인성 증가를 평가하였다. 다공성 콘크리트의 목표성능 만족을 위해서는 골재입도 15~20mm에서 물-시멘트 비 및 시멘트-골재 비가 각각 25% 및 15%로 추천될 수 있었다. GFRP로 보강된 다공성 콘크리트 보의 거동은 전단파괴에 의해 지배되었다. 이에 따라 GFRP의 휨 저항 발휘는 매우 적었으며, GFRP 보강근의 장부작용에 의한 전단내력상승은 결과적으로 다공성 콘크리트 보의 하중 저항성과 인성을 향상시켰다. GFRP 보강근을 압축과 인장측에 각각 1본(D9)씩 배근한 경우 내력은 무보강 보에 비해 약 2.1배 증가하였으며, 인성지수 $I_{30}$값은 43.4를 보임으로서 인성지수 값을 측정할 수 없었던 무보강 보에 비해 상당히 향상되었다.

유기계 섬유로 하이브리드 보강된 콘크리트의 휨 거동 및 염분침투저항성 (Chloride Penetration Resistance and Flexural Behavior of Hybrid Organic Fibers Reinforced Concrete)

  • 김승현;강민범;이동욱
    • 한국지반신소재학회논문집
    • /
    • 제14권4호
    • /
    • pp.105-115
    • /
    • 2015
  • 본 연구에서는 매크로섬유를 PP섬유로 대체하여 유기계 섬유들인 PVA섬유 6mm와 PP섬유 50mm로 하이브리드 보강된 콘크리트의 역학적 특성을 파악하기 위해 섬유의 체적비를 주요변수로 하이브리드 섬유 보강 콘크리트(HFRC) 4배합과 섬유가 없는 Plain콘크리트 1배합을 실험하여 비교하였다. 섬유의 체적비를 1%미만으로 제한하였다. 연구결과 유기계 섬유의 하이브리드 보강은 콘크리트의 강성 및 연성거동을 강섬유만큼 극대화시키지는 못하지만, Plain콘크리트와 비교시 매우 진전된 연성거동을 보이며 휨 인성지수와 등가휨강도 사이의 의미 있는 관계를 확인하였다. 그리고 유기계 섬유로 하이브리드 보강한 콘크리트에서도 섬유의 체적비가 증가할수록 연성이 증가하였고 섬유의 하이브리드를 위해 사용한 마이크로섬유인 PVA섬유보다 매크로섬유인 PP섬유가 콘크리트의 휨 거동에 미치는 영향이 크며, 염분침투시험에서도 섬유의 혼입이 염분침투를 억제하는 효과가 있는 것으로 확인되었다.

매크로 섬유의 저혼입에 따른 콘크리트 포장의 역학적 특성 (Mechanical Properties of Concrete Pavement by Low Fraction of Macro Fiber)

  • 최성용;박영환;정우태;박종섭
    • 한국도로학회논문집
    • /
    • 제14권6호
    • /
    • pp.1-11
    • /
    • 2012
  • PURPOSES : The purpose of the study was to examine dynamic features of concrete after mixing a little macro fiber with small aspect ratio and long length utilized for bridge, tunnel and shotcrete for tensile performance and crack control in domestic/overseas countries with cement concrete pavement mix. METHODS : Coarse aggregates with small aspect ratio and macro fibers with maximum length of approximately 32 mm are introduced in small quantities in the mix proportions of concrete pavement so as to prevent loss of the workability. Then, this study intends to evaluate the applicability of macro fibers in the mix proportions of concrete pavement by examining the basic construction performance, as well as the change of toughness, the equivalent bending strength and the flexural toughness index caused by compression, bending, tension and the flexural stress-displacement curve. RESULTS : As the results, in each kind of macro fiber, polyvinyl alcohol fiber and steel fiber displayed a good performance. CONCLUSIONS : In 0.2 and 0.3% of fiber contents, it is appeared that polyvinyl alcohol fiber has a large effect on improvement of tensile performance and steel fiber on improvement of deforming performance of bending stress.

Wire Mesh보강 포러스콘크리트의 성능평가에 관한 실험적 연구 (An Experimental Study on the Performance of Wire Mesh Reinforced Porous Concrete)

  • 권혁준;이택우;김선용;박승범
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2000년도 가을 학술발표회 논문집(II)
    • /
    • pp.1227-1232
    • /
    • 2000
  • In this study the mechanical properties of various wire mesh reinforcing porous concrete mixtures are investigated. A properly designed porous concrete pavements provides a durable riding surface. It also eliminates puddles and standing water, resulting in improved skid resistance. The most popular application is that of light-traffic volume roadways such as parking lots, resident roads, driveways, and sidewalks. Flexural strength and toughness index are examined for wire mesh reinforcing porous concrete. Type of Wire mesh is divided into three cases, A type, B type and C type. It shows A type is most excellent shape of destruction of slab specimen is similar to that of flexural specimen. The aim of this paper is to present the results of a pilot study undertaken to examine the extent to which wire mesh reinforced porous concrete can be used as a continuous paving materials.

강섬유의 형태에 따른 SFRC보의 휨거동에 관한 연구 (Fiber Type Effects on the Flexural Behavior of Steel Fiber Reinforced Concrete Beams)

  • 전찬기
    • 대한토목학회논문집
    • /
    • 제12권4호
    • /
    • pp.95-106
    • /
    • 1992
  • 강섬유의 형태가 콘크리트의 휨거동에 미치는 영향을 알아 보기 위하여 5종의 강섬유를 사용한 실험을 실시하였다. 강섬유 혼입율은 1~2%로 변화를 주었고 전단 스팬비와 철근비는 고정하였다. 형태가 다른 강섬유의 보강 효과를 비교 분석하기 위한 방법으로 섬유 보강 효과 지수를 채택하였고, 인성 효과를 분석하기 위하여 유효 인성 지수를 제안하였으며, 이들 지수들은 강섬유 보강 효과를 비교 분석하는데 유용한 방법으로 평가되었다. 실험 결과에 의하면 강섬유 혼입율은 양단이 hook 형태인 강섬유의 경우에는 1% 이내가 효과적이며, dog bone 형태인 강섬유는 1~2%, 기타 강섬유는 2% 정도가 적절하였다. 강섬유의 혼입으로 인한 휨강도 및 파괴인성의 증진 효과는 무근 콘크리트보의 경우가 철근 콘크리트보의 경우보다 크게 나타났다. 또한 강섬유의 형태에 의한 휨강도와 인성의 증진 효과는 양단이 hook나 dog bone(paddled)형태의 강섬유가 섬유 혼입율이 상대적으로 낮음에도 straight나 crimped 및 wavy 형태보다 우수한 것으로 판명되었다.

  • PDF

이층 포설 콘크리트 포장의 국내 적용을 위한 강섬유 보강 콘크리트 기초 물성평가 (Estimation of The Basic Properties of Two-Lift Concrete Pavement to Apply Korea Condition)

  • 원홍상;류성우;홍종용;조윤호
    • 한국도로학회논문집
    • /
    • 제12권1호
    • /
    • pp.47-54
    • /
    • 2010
  • 본 연구에서는 콘크리트 포장의 균열, 스폴링 등의 파손문제를 해결하기 위해 국내 시공사례가 없는 이층 포설 공법의 도입 및 기술 경제적 타당성을 검토하고자 하였다. 본 포장공법중 하나인 강섬유 보강 콘크리트(SFRC, Steel Fiber Reinforced Concrete)의 포장 배합 적용성이 검토되었다. 강섬유 함량과 포장 높이가 산정되었으며, 강섬유 보강 콘크리트의 물성 평가를 위해 압축강도, 휨강도, 휨인성 지수, 인장강도, 피로강도를 측정하였다. 슬럼프와 공기량은 대부분이 시방 기준을 만족하였으며, 28일 강도도 교통개방을 할 수준 정도로 발현되었다. 휨강도 실험 결과, 강섬유 보강 콘크리트가 무보강 콘크리트에 비해 휨인성은 증가하였지만 휨강도는 증가하지 않았다. 에너지 흡수능력, 피로 저항성 및 동결 융해저항성은 강섬유 보강 콘크리트가 무보강 콘크리트에 비해 향상되었다. 향후, 시험시공을 통해 강섬유 보강 콘크리트의 현장 적용성 및 공용성을 평가할 것이다.

Influence of loading rate on flexural performance and acoustic emission characteristics of Ultra High Performance Concrete

  • Prabhat Ranjan Prem;Vignesh Kumar Ramamurthy;Vaibhav Vinod Ingle;Darssni Ravichandran;Greeshma Giridhar
    • Structural Engineering and Mechanics
    • /
    • 제89권6호
    • /
    • pp.617-626
    • /
    • 2024
  • The study investigated the behavior of plain and fibered Ultra-High Performance Concrete (UHPC) beams under varying loading conditions using integrated analysis of the flexure and acoustic emission tests. The loading rate of testing is -0.25 -2 mm/min. It is observed that on increasing loading rate, flexural strength increases, and toughness decreases. The acoustic emission testing revealed that higher loading rates accelerate crack propagation. Fiber effect and matrix cracking are identified as significant contributors to the release of acoustic emission energy, with fiber rupture/failure and matrix cracking showing rate-dependent behavior. Crack classification analysis indicated that the rise angle (RA) value decreased under quasi-static loading. The average frequency (AF) value increased with the loading rate, but this trend reversed under rate-dependent conditions. K-means analysis identified distinct clusters of crack types with unique frequency and duration characteristics at different loading rates. Furthermore, the historic index and signal strength decreased with increasing loading rate after peak capacity, while the severity index increased in the post-peak zone, indicating more severe damage. The sudden rise in the historic index and cumulative signal strength indicates the possibility of several occurrences, such as the emergence of a significant crack, shifts in cracking modes, abrupt failure, or notable fiber debonding/pull-out. Moreover, there is a distinct rise in the number of AE knees corresponding to the increase in loading rate. The crack mapping from acoustic emission testing aligned with observed failure patterns, validating its use in structural health monitoring.