• 제목/요약/키워드: finish coating

검색결과 40건 처리시간 0.039초

전극선 성분 변화에 따른 냉간금형용강의 와이어방전가공 특성 (Characteristics of Wire EDM for Cold Die Steel due to the Different Wire Electrode Component)

  • 왕덕현;정순성
    • 한국기계가공학회지
    • /
    • 제2권2호
    • /
    • pp.98-105
    • /
    • 2003
  • In the experimental study, wire EDM was conducted for cold die steel by changing the Wire electrode, peak discharge current and number of finish cut. From the micro structure analysis of SEM photographs, the size of irregular welded and added component on the EDMed surface is decreasing and size of EDMed plane surface is increasing as the decreasing peak current and increasing number of finish cut. From the analysis of coating effect, Zn component is highly contained in Br and Zn Wire EDMed surface and copper component is highly contained in Br and Al wire EDMed surface. Hardness values are Increasing as the increasing peak current and decreasing the number of finish cut The value of hardness is decreasing as Cu, Al, Zn and Br wire electrode because of the residual austenite effect of solid solution copper on solidification, and finally EDMed surface has the highest hardness values for every wire electrode. Yield strength values becomes larger and bending strength values become smaller due to the increasing the hardness. These results are increased as increasing brittleness with hardness.

  • PDF

Performance Characteristics of CVD Diamond Cutting Tools

  • Oles, E.J.;Cackowski, V.J.
    • The Korean Journal of Ceramics
    • /
    • 제2권4호
    • /
    • pp.203-211
    • /
    • 1996
  • CVD diamond tools are becoming more widely used in industry as an economic alternative to polycrystalline diamond (PCD) for machining non-ferrous and non-metallic materials. Although CVD diamond-sheet tools have been on the market for several years, diamond-coated carbide inserts have become available only recently, with the successful resolution of long-standing adhesion problems. Diamond coating morphology on the rake surface of the tool affects chip formation favorably, whereas a microscopically rough, faceted morphology on the flank surface of the tool produces a rough workpiece finish. Workpiece finish can be improved by using a coated tool with a larger nose radius. The tool life provided by diamond-coated tools(~30 $\mu\textrm{m}$ thick) can meet or exceed that of PCD tools, depending on the characteristics of the workpiece material. When using diamond-coated carbide tools in milling, a sharp-edged PCD tool should be used in the wiper position of the cutter to minimize workpiece roughness and burr formation.

  • PDF

원형단면의 정밀 원심 배럴가공에 관한 연구 (A Study on the Centrifugal Barrel Machining of Round Face)

  • 고준빈;김우강;원종호
    • 한국정밀공학회지
    • /
    • 제21권4호
    • /
    • pp.179-185
    • /
    • 2004
  • Surface finish technology is highly demanded in the wide field of industry applications from ultra-precision parts to rough casting parts. Therefore, many kinds of surface finish technologies have been developed for each purpose. Because surface of a car's wheel cast is very rough it becomes the reason of the corrosion. This surface is coated to complement such problem but because surface is rough, the result of coating is not good and the coated metal peels off well. Therefore before the wheel is coated, it is necessary to grind the surface. In this study, we devised the plant to apply a barrel machining to improve the surface roughness and enhance the productivity. Also we could obtain the optimum barrel machining conditions for the proper surface roughness.

Investigation of Streaky Mark Defect on Hot Dip Galvannealed IF Steel

  • Xinyan, Jin;Li, Wang;Xin, Liu
    • Corrosion Science and Technology
    • /
    • 제9권3호
    • /
    • pp.109-115
    • /
    • 2010
  • Interstitial-free (IF) steels are widely used for car body material. However, a few types of streaky mark defect are commonly found on hot dip galvannealed (GA) IF steel sheets. In the present study, both the phase structure of a streaky mark defect and the microstructure of the substrate just below it were characterized by optical microscopy (OM) and scanning electron microscopy (SEM). It was found that the bright streaky mark area was composed of ${\delta}$ phase while the dark normal area was full of craters. More than half of the grains at the uppermost surface of the substrate just below the streaky mark defect are unrecrystallized grains which could result from lower finish rolling temperature during hot rolling and be kept stable during the annealing process, while almost all the grains in the normal area are equiaxed grains. In order to confirm the effect of the unrecrystallized grains on the coating morphology, hot dip galvannealing simulation experiments were carried out in IWATANI HDPS. It is proved that the unrecrystallized grains accelerate the Fe-Zn reaction rate during galvannealing and result in a flatter coating surface and an even coating thickness. Finally, a formation mechanism of the streaky mark defect on the hot dip galvannealed IF steel sheet was discussed.

무기성 습식 처리 플라이애시를 활용한 단열 외피 마감재의 특성 평가 (Characterization of Insulation Finish Material Using Inorganic Wet Treatment Fly Ash)

  • 류화성;신상헌;송성용;김득모
    • 한국건설순환자원학회논문집
    • /
    • 제7권4호
    • /
    • pp.389-394
    • /
    • 2019
  • 본 연구에서는 기능성 무기 단열 소재인 TiO2와 무기성의 습식 처리 플라이애시를 사용하여 건축물의 열환경성을 향상할 수 있는 외장 마감재의 물리적 성능과 열환경성에 대한 평가를 수행하였다. 마감재의 성능 평가는 KS F 4715의 얇은 바름재의 기준과 열환경성은 별도의 단열 박스를 제작하여 외부 표면 온도와 내부 온도를 측정하였다. TiO2를 혼입한 경우 10%이상에서는 물리적 성능이 저하되는 것으로 나타났으며, 무기성의 습식 처리 플라이애시는 10%까지 물리적 성능이 증가되는 것으로 나타났다. 열환경성 평가에서는 무기성의 습식 처리 플라이애시의 표면 온도 저감 효과는 낮았으나 TiO2와 복합적으로 사용되는 경우, 표면 온도 저감 및 내부 온도 저감에 효과적인 것으로 나타났다. 결국, 열환경 제어를 위한 TiO2와 무기성의 습식처리 플라이애시의 최적 배합은 각각 5%를 혼합 사용할 때 최적인 것으로 나타났다.

Non-Vinyl Pre-coated Metal재의 성형성에 관한 연구 (Formability of Non-Vinyl Pre-coated Metal Sheet)

  • 김동환;김병민
    • 한국정밀공학회지
    • /
    • 제18권4호
    • /
    • pp.121-128
    • /
    • 2001
  • This study has been performed to investigate formability of non-vinyl PCM(pre-coated metal)sheet. First, physical test of PCM sheets were tested to evaluate finish coating characteristic of PCM. And then, test equipment was made for friction test and three non-vinyl PCM sheets were tested by straight pulling method. This paper provides the results of the friction tests showing the influence of sheet surface texture and process conditions. It was found that the influence of contact pressure and speed had an effect upon the level of friction. Also using tests, the scratch resistance of a series of polyester coating has been investigated. This investigation aims to clarify the process conditions that prevent the scratch of PCM to form the good electrical appliances such as microwave oven, air conditioner and refrigerator etc.

  • PDF

실험적 방법을 통한 Metal slitting saw의 형상 및 절삭 조건의 최적화 (Optimization of a geometric form and cutting conditions of a metal slitting saw by experimental method)

  • 정경득;고태조;김희술
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2000년도 춘계학술대회 논문집
    • /
    • pp.934-938
    • /
    • 2000
  • Built-up edge affects the surface integrity of the machined surface and tool wear. Tool geometry and cutting conditions are very important factors to remove BUE. In this paper, we optimized the geometry of the metal slitting saw .1nd cutting conditions to remove BUE by the experiment. In general, the metal slitting saw is plain milling cutter with thickness less of a 3/16 inch. This is used for cutting workpiece where high dimensional accuracy and surface finish are necessary. The experiment was planned with Taguchi method that is based on the orthogonal array of design factors(coating, rake angle, number of tooth, cutting speed, feed rate). Response table was made by the value of the surface roughness, the optimized tool geometry and cutting conditions through response table could be determined. In addition. the relative effect of factors were identified by the variance analysis. filially. coating and cutting speed turned out important factors.

  • PDF

DLC 코팅된 가이드레일을 이용한 볼베어링 직선 이송 스테이지의 진공환경 제어 특성 분석 (Experimental Control Characteristic Investigation of Ball Bearing Guided Linear Motion Stage with Diamond-like Carbon Coated Guide Rail)

  • 심종엽;김경호;황주호
    • 한국생산제조학회지
    • /
    • 제23권4호
    • /
    • pp.392-397
    • /
    • 2014
  • Recently, there is an increase in the need for precision linear stages with vacuum compatibility in such areas as lithography equipment for wafer or mask manufacturing, mask mastering equipment for optical data storage and electron beam equipment. A simple design, high stiffness and low cost can be achieved by using ball bearings. However, a ball bearing have friction and wear problems just as in ambient air. In order to decrease the friction, a special finish, a diamond-like carbon (DLC) film coating, is applied to the surface of a guide rail by sputtering deposition. This paper presents the result of an experimental investigation on the control performance of a ball bearing-guided linear motion stage under two environmental conditions: in air and vacuum. A comparison between the results with and without the DLC coating was also considered in the experimental investigation.

ENIG 표면처리 공정 및 특성에 관한 연구 (A Study on the ENIG Surface Finish Process and Its Properties)

  • 이홍기;손성호;이호영;전준미
    • 한국표면공학회지
    • /
    • 제40권1호
    • /
    • pp.32-38
    • /
    • 2007
  • Ni coating layers were formed using a newly developed electroless Ni plating solution. The properties of Ni coating layer such as internal stress, hardness, surface roughness, crystallinity, solderability and surface morphology were investigated using various tools. Results revealed that internal stress decreased with plating time and reached $40N/mm^2$ at 20 minutes of the plating time. Hardness increased with increasing P content and thickness. Surface roughness of the pad decreased with Ni and Ni/Au plating. Crystallinity decreased with increasing P content. Solderability based on wettability decreased with Ni and Ni/Au plating. Based on surface morphology, it is expected that Ni coating layer formed using a newly developed electroless Ni plating solution is lower than that formed using a commercial electroless Ni plating solution in possibility of black pad occurrence.

볼트 결합부 풀림에 관한 마찰 특성 (The Friction Characteristics on the Loosening of Bolted Joints)

  • 박태원;신귀수
    • 한국안전학회지
    • /
    • 제19권1호
    • /
    • pp.12-17
    • /
    • 2004
  • By using an experimental approach recently developed to determine the torque-tension relationship for bearing frictional characteristics of several typical bolted joints were studied. The experimental approach allows the direct determination of the bearing friction between the nut and its bearing surface. Detailed friction studies were made on the influences of the size and shape of the hole, the use of a slot in a bolted joint, contact area and position, and other factors such as turning speed, coating, and the use of wax on the bearing surface. The contact area and position of the washer have a marginal effect on the bearing friction. The organic coating on the nuts reduces the bearing friction significantly. Nuts with organic coating over a washer with zinc finish provide the smallest and the most consistent bearing friction. The results from the experimental investigation will be helpful for the better design of bolted joints bearing friction. The results from the experimental investigation Will be helpful for the better design of bolted joints.