화학증착법에 의하여 제조된 탄화규소 코팅층의 기계적 특성 (Mechanical Properties of Chemical Vapor Deposited SiC Coating Layer)

  • 이현근;김종호;김도경
    • 한국세라믹학회지
    • /
    • 제43권8호
    • /
    • pp.492-497
    • /
    • 2006
  • SiC coating has been introduced as protective layer in TRISO nuclear fuel particle of High Temperature Gas cooled Reactor (HTGR) due to excellent mechanical stability at high temperature. In order to inhibit the failure of the TRISO particles, it is important to evaluate the fracture strength of the SiC coating layer. ]n present work, thin silicon carbide coating was fabricated using chemical vapor deposition process with different microstructures and thicknesses. Processing condition and surface status of substrate.affect on the microstructure of SiC coating layer. Sphere indentation method on trilayer configuration was conducted to measure the fracture strength of the SiC film. The fracture strength of SiC film with different microstructure and thickness were characterized by trilayer strength measurement method nanoindentation technique was also used to characterize the elastic modulus and th ε hardness of the SiC film. Relationships between microstructure and mechanical properties of CVD SiC thin film were discussed.

Laser Diode의 무반사코팅 설계 및 특성에 관한 연구 (Study about Anti-Reflection Coating Design and Characteristic of Laser Diode)

  • 기현철;김효진;김희종;한정희;구할본
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 하계학술대회 논문집 Vol.8
    • /
    • pp.424-425
    • /
    • 2007
  • Anti-Reflection and High-reflection coating on the facet of semiconductor laser diode. To prevent internal feedback from both facets for realizing super luminescent diode and reducing the reflection-induced intensity noise of laser diode. Anti-Reflection coating Film was designed by Macleod Simulator. Coating Materials were decided $Ti_3O_5$ and $SiO_2$. Thickness of Coating layer $Ti_3O_5/SiO_2$ were 105[nm], 165[nm]. In the study Anti-Reflection coating Film was design for Laser diode and deposited by Ion-Assisted Deposition system. Then manufactured thin film measured electrical properties(L-I-V, Se, Resistor) and Optical properties(wavelength FFP). Slop-efficiency and FFP characteristic is 0.302[W/A], $22.3^{\circ}$(Horizontal), $24.4^{\circ}$(Vertical).

  • PDF

은 박막이 코팅된 베어링 표면의 구름 저항 거동 고찰 (An Experimental Study on the Rolling Resistance of Bearing Surfaces Covered by Pure Silver Film)

  • 양승호;공호성;윤의성;권오관
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1997년도 제25회 춘계학술대회
    • /
    • pp.101-110
    • /
    • 1997
  • An experimental study was performed to discover the tribological behaviors of pure silver coated 52100 bearing steel. Pure silver coatings ranging from 80 nm to several micrometers were produced by a thermal evaporation coating method. Experiments using a thrust ball bearing-typed rolling test-rig were performed for the investigations of the influence of coating thickness on the tribological rolling behavior. The existence of optimum film thickness which revealed minimum rolling resistance was discovered. A careful analysis on the contact surfaces for the optimum film thickness has been performed. The contact patches produced by the transferred silver films played an important role for the rolling resistance to keep low.

  • PDF

스프레이 코팅법으로 제조된 CNT/PVDF 압전 복합막의 자기분극 메커니즘 (Self-poling Mechanism of CNT/PVDF Piezoelectric Composite Films Prepared by Spray Coating Method)

  • 이선우
    • 한국전기전자재료학회논문지
    • /
    • 제26권7호
    • /
    • pp.550-554
    • /
    • 2013
  • Carbon nanotubes (CNT) / polyvinylidene fluoride (PVDF) piezoelectric composite films for nanogenerator devices were fabricated by spray coating method. When the CNT/PVDF mixture solution passes through the spray nozzle with small diameter by the compressed nitrogen gas, electric charges are generated in the liquid by a triboelectric effect. Then randomly distributed ${\beta}$ phase PVDF film could be re-oriented by the electric field resulting from the accumulated electrical charges, and might be resulted in extremely one-directionally aligned ${\beta}$ phase PVDF film without additional electric field for poling. X-ray diffraction patterns were used to investigate crystal structure of the CNT/PVDF composite films. It was confirmed that they revealed extremely large portion of the ${\beta}$ phase PVDF crystalline in the film. Therefore we could obtain the poled CNT/PVDF piezoelectric composite films by the spray coating method without additional poling process.

은 박막이 코팅된 베어링 표면의 구름 저항 거동 고찰 (An Experimental Study on the Rolling Resistance of Bearing Surfaces Covered by Pure Silver Film)

  • 양승호;공호성;윤의성;권오관
    • Tribology and Lubricants
    • /
    • 제13권3호
    • /
    • pp.85-92
    • /
    • 1997
  • An experimental study was performed to discover the tribological behaviors of pure silver coated 52100 bearing steel. Pure silver coatings ranging from 80 nm to several micrometers were produced by a thermal evaporation coating method. Experiments using a thrust ball bearing-typed rolling test-rig were performed for the investigations of the influence of coating thickness on the tribological rolling behavior. The existence of optimum film thickness which revealed minimum rolling resistance was discovered. A careful analysis on the contact surfaces for the optimum film thickness has been performed. The contact patches produced by the transferred silver films played an important role for the rolling resistance to keep low.

Adhesive Behaviors of the Aluminum Alloy-Based CrN and TiN Coating Films for Ocean Plant

  • Murakami, Ri-Ichi;Yahya, Syed Qamma Bin
    • International Journal of Ocean System Engineering
    • /
    • 제2권2호
    • /
    • pp.106-115
    • /
    • 2012
  • In the present study, TiN and CrN films were coated by arc ion plating equipment onto aluminum alloy substrate, A2024. The film thickness was about 4.65 ${\mu}m$. TiN and CrN films were analyzed by X-ray diffraction and energy dispersive X-ray equipments. The Young's modulus and the micro-Vickers hardness of aluminum substrate were modified by the ceramic film coatings. The difference in Young's modulus between substrate and coating film would affect on the wear resistance. The critical load, Lc, was 75.8 N for TiN and 85.5 N for CrN. It indicated from the observation of optical micrographs for TiN and CrN films that lots of cracks widely propagated toward the both sides of scratch track in the early stage of MODE I. TiN film began to delaminate completely at MODE II stage. The substrate was finally glittered at MODE III stage. For CrN film, a few crack can be observed at MODE I stage. The delamination of film was not still occurred at MODE II and then was happened at MODE III. This agrees with critical load measurement which the adhesive strength was greater for CrN film than for TiN film. Consequently, it was difficult for CrN to delaminate because the adhesive strength was excellent against Al substrate. The wear process, which the film adheres and the ball transfers, could be enhanced because of the increase in loading. The wear weight of ball was less for CrN than for TiN. This means that the wear damage of ball was greater for TiN than for CrN film. It is also obvious that it was difficult to delaminate because the CrN coating film has high toughness. The coefficient of friction was less for CrN coating film than for TiN film.

졸겔법에 의한 알루미나 박막의 제조 및 특성 (III) 저반사 코팅유리의 제조 (Preparation and Characterization of Alumina Thin Film by Sol-Gel Method (III) Preparation of Anti-Reflective Coating Glass)

  • 이재호;최세영
    • 한국세라믹학회지
    • /
    • 제32권1호
    • /
    • pp.57-62
    • /
    • 1995
  • The coating condition of reproducible anti-reflective coating film and the light transmittance characteristics of the prepared anti-reflective coating glass were investigated as a study for the preparation of single-layer anti-reflective coating glasss. In case of coating with the sol in which the solvent was substituted with the ethanol with the addition of 0.1 mol HNO3, the coated glass showed the minimum value of the refractive index of 1.464, light transmittance of 94.2% at 550nm standard wavelength which is 3.2% higher than that of the parent glass, and the reflectance in the entire wave range of visible light. The refractive index represented its minimum at the sol concentration of 1.0 mol per 100mols of water and the higher the sol concentration, the higher the refractive index, resulting in the decrease of the light transmitance. The production condition of the reproducible anti-reflective coating on glass with the maximum transmittance of 94.2% was 4cm/min of withdrawal speed, 40$0^{\circ}C$ and 1 hour of heat treatment temperature and time, resulting in the film thickness of 94nm.

  • PDF

유도가열 및 근적외선 가열방법에 의한 표면처리 강판 도포층의 가열 및 건조 특성 (Heating & Drying Characteristics of Coating Layer by Induction Heating and Short-wave Infrared Heating)

  • 김태수;양재원
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 제5회 압연심포지엄 신 시장 개척을 위한 압연기술
    • /
    • pp.249-257
    • /
    • 2004
  • Drying and curing characteristics of PCM resins using the induction heater and short-wave infrared emitter module was studied to develop a compact oven system for the high speed CCL and post-treatment equipment. Drying of the polyester resins using the induction heater and infrared heater showed that the blistering tendency of polyester resin coating increased regardless of additives and colors of resins as the heating rate and/or dry film thickness increased. The blistering of polyester resin coating layer occurred when the heating speed was over than $25^{\circ}C/sec$ for the dry film thickness of $19\~20um$, which is the typical thickness of finish coating in CCL. So did it when the heating speed was over than $40^{\circ}C/sec$ for the dry film thickness over than 10 um. The heating efficiency of paint coated steels by the infrared heating was strongly dependent on the colors of paint coating and generally increased for the dark surface and/or coating. But the faster drying of the PCM resin coatings increased the blistering tendency of coating layer. The blistering limit for the typical finish coating by the infrared heating was estimated as the heating rate slower than $20^{\circ}C/sec$ regardless of colors of PCM resins.

  • PDF

소수성 CNT/PVDF 복합막에서 CNT의 분산과 전도성의 관계 (Relations Between Dispersion of CNTs and Electrical Conductivity in the Hydrophobic CNT/PVDF Composite Film)

  • 이선우
    • 한국전기전자재료학회논문지
    • /
    • 제28권7호
    • /
    • pp.462-466
    • /
    • 2015
  • In this paper, we investigated the relations between dispersion of CNTs (carbon nanotubes) and electrical conductivity in the CNT/PVDF (polyvinylidene fluoride) composite film. By adding hydrophobic CNTs as filler into the PVDF matrix, we fabricated hydrophobic and electrically conducting polymer coating film. Dispersion of CNTs in the CNT/PVDF composite film plays a significant role in terms of electrical conductivity and wetting property. Spray coating method was used to form the CNT/PVDF composite films by injecting the dispersed CNTs in the PVDF solution with different weight ratios from 0.7 wt% to 7 wt%. We investigated the electrical properties and contact angles of the CNT/PVDF composite films with the CNT concentration. Finally we discussed the conducting mechanism and feasibility of the CNT/PVDF composite film for the conducting polymer films.

APPLICATION OF DISPROPORTIONATION REACTION TO SURFACE TREATMENT

  • Oki, Takeo
    • 한국표면공학회지
    • /
    • 제29권5호
    • /
    • pp.478-481
    • /
    • 1996
  • Disproportionation reaction is very important and interesting reaction to be applied to such surface treatment as metal, alloy, compound coating, a surface etching and so on. In gaseous system, the reaction of Al chloride is applied to Al and Al alloy coating, and the similar reaction of Ti chloride is also used for Ti, Ti alloy and Ti compound coating. As for aqueous system, this reaction is utilized to such metal coat as Sn etc. and metal etching such as Cu, Fe and so on. Also in molten salts system, this reaction has many application for surface treatment like metal, alloy and compound coatings for corrosion, wear, heat resistance and so forth. For instance, carbide film, nitride film, boride film, alloy film, quite new different film from the components of substrate material are coated in single and multiple component film system by the disproportionation reaction.

  • PDF