• 제목/요약/키워드: ferroelectric thin films

검색결과 568건 처리시간 0.029초

화학적기계적연마 공정으로 제조한 BLT Capacitor의 Polishing Damage에 의한 강유전 특성 열화 (Degradation from Polishing Damage in Ferroelectric Characteristics of BLT Capacitor Fabricated by Chemical Mechanical Polishing Process)

  • 나한용;박주선;정판검;고필주;김남훈;이우선
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 하계학술대회 논문집 Vol.9
    • /
    • pp.236-236
    • /
    • 2008
  • (Bi,La)$Ti_3O_{12}$(BLT) thin film is one of the most attractive materials for ferroelectric random access memory (FRAM) applications due to its some excellent properties such as high fatigue endurance, low processing temperature, and large remanent polarization [1-2]. The authors firstly investigated and reported the damascene process of chemical mechanical polishing (CMP) for BLT thin film capacitor on behalf of plasma etching process for fabrication of FRAM [3]. CMP process could prepare the BLT capacitors with the superior process efficiency to the plasma etching process without the well-known problems such as plasma damages and sloped sidewall, which was enough to apply to the fabrication of FRAM [2]. BLT-CMP characteristics showed the typical oxide-CMP characteristics which were related in both pressure and velocity according to Preston's equation and Hernandez's power law [2-4]. Good surface roughness was also obtained for the densification of multilevel memory structure by CMP process [3]. The well prepared BLT capacitors fabricated by CMP process should have the sufficient ferroelectric properties for FRAM; therefore, in this study the electrical properties of the BLT capacitor fabricated by CMP process were analyzed with the process parameters. Especially, the effects of CMP pressure, which had mainly affected the removal rate of BLT thin films [2], on the electrical properties were investigated. In order to check the influences of the pressure in eMP process on the ferroelectric properties of BLT thin films, the electrical test of the BLT capacitors was performed. The polarization-voltage (P-V) characteristics show a decreased the remanent polarization (Pr) value when CMP process was performed with the high pressure. The shape of the hysteresis loop is close to typical loop of BLT thin films in case of the specimen after CMP process with the pressures of 4.9 kPa; however, the shape of the hysteresis loop is not saturated due to high leakage current caused by structural and/or chemical damages in case of the specimen after CMP process with the pressures of 29.4 kPa. The leakage current density obtained with positive bias is one order lower than that with negative bias in case of 29.4 kPa, which was one or two order higher than in case of 4.9 kPa. The high pressure condition was not suitable for the damascene process of BLT thin films due to the defects in electrical properties although the better efficiency of process. by higher removal rate of BLT thin films was obtained with the high pressure of 29.4 kPa in the previous study [2].

  • PDF

RF스퍼터링법을 이용한 강유전체 $LiNbO_3$ 박막의 제작과 특성연구 (The study on characteristics and fabrications of ferroelectric $LiNbO_3$ thin films using RF sputtering)

  • 최유신;정세민;최석원;이준신
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1998년도 하계학술대회 논문집 D
    • /
    • pp.1352-1354
    • /
    • 1998
  • $LiNbO_3$ transistor showed relatively stable characteristic, low interface trap density, and large remanent polarization. This paper reports ferroelectric $LiNbO_3$ thin films grown directly on p-type Si(100) substrates by 13.56 MHz rf magnetron sputtering system for FRAM applications. To take advantage of low temperature requirement for growing films, we deposited $LiNbO_3$ films lower than $300 ^{\circ}C$. RTA(Rapid Thermal Anneal) treatment was performed for as-deposited films in an oxygen atmosphere at $600^{\circ}C$ for 60 sec. We learned from X-ray diffraction that the RTA annealed films were changed from amorphous to poly-crystalline $LiNbO_3$ which exhibited (012), (015), and (022) orientations. The I-V characteristics of $LiNbO_3$ films before and after anneal treatment showed that RTA improved the leakage current of films. The leakage current density of films decreased from $10^{-5}$ to $10^{-7} A/cm^2$ at room temperature measurement. Breakdown electric field of the films exhibited higher than 500 kV/cm. The C-V curves showed the clockwise hysteresis represents ferroelectric switching characteristics. From C-V curves, we calculated dielectric constant of thin film $LiNbO_3$ as 27.5 which is close to that of bulk value.

  • PDF

BLT 타겟제조 및 강유전 박막 특성에 관한 연구 (A Study on BLT Target Preparation and Ferroelectric Property)

  • 김응권;박기엽;이규일;강현일;송준태
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 추계학술대회 논문집 Vol.15
    • /
    • pp.87-90
    • /
    • 2002
  • In recent year, BLT($Bi_{3.25}La_{0.75}Ti_{3}O_{12}$) has been one of promising substitute materials at the ferroelectric random access memory applications. We manufactured $Bi_{3.25}La_{0.75}Ti_3O_{12}$ Target with a ceramic process. The BLT target was sintered at ${1100^{\circ}C}$ for 4 hours. Using RF magnetron sputtering, a deposited BLT thin films were estimated about ferroelectric properly as a functions of post annealing temperatures. The BLT thin films showed a promoted ferroelectric characteristics at the post annealied sample of ${700^{\circ}C}$. This sample exhibited the (117) preferred crystal orientation, current density of $3{\times}10^{-8}A/cm^2$, a remanent polarization of $8{\mu}C/cm^2$ and a coercive field of 42.1 KV/cm respectively.

  • PDF

$Cl_{2}/CF_{4}$ 플라즈마에 Ar,$O_2$첨가에 따른 PZT 박막의 식각 손상 효과 (Reduce of Etching Damage of PZT Thiin Films in $Cl_{2}/CF_{4}$ Plasma with addition of Ar and $O_2$)

  • 강명구;김경태;김창일
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집
    • /
    • pp.21-25
    • /
    • 2001
  • In this study, recovery of plasma etching damage in PZT thin film with additive gas and re-annealing after etching have been investigated. The PZT thin films were etched as a function of Cl$_2$/CF$_4$ with addition of Ar and $O_2$ with inductively induced plasma. The etch rates of PZT thin films were 1450$\AA$/min at 30% additive Ar into (Cl$_2$(80%)+CF$_4$ (20%)) and 1100$\AA$/min at 10% additive $O_2$ into C(Cl$_2$(80%)+CF$_4$ (20%)). In order to recovery properties of PZT thin films after etching, the etched PZT thin films were re-annealed at various temperatures in at $O_2$ atmosphere. From the hysteresis curves, ferroelectrical properties are improved by $O_2$ re-annealing process. The improvement of ferroelectric behavior at annealed sample is consistent with the increase of the (100) and (200) PZT peaks revealed by x-ray diffraction (XRD). From x-ray photoelectron spectroscopy (XPS) analysis, intensity of Pb-O, Zr-O and Ti-O peak are increased and the chemical residue peak is reduced by $O_2$ re-annealing. The ferroelectric behavior consistent with the dielectric nature of Ti$_{x}$O$_{y}$ is recovered by $O_2$ recombination during rapid thermal annealing process.s.s.

  • PDF

솔-젤법 및 급속열처리에 의한 $Sr_{0.9}4$Bi_{2.1}$$Ta_2$$O_9$ 박막의 저온형성에 관한 연구 (Study on Low Temperature Formation of Ferroelectric $Sr_{0.9}4$Bi_{2.1}$$Ta_2$$O_9$ Thin Films by Sol-Gel Process and Rapid Thermal Annealing)

  • 장현호;송석표;김병호
    • 한국전기전자재료학회논문지
    • /
    • 제13권4호
    • /
    • pp.312-317
    • /
    • 2000
  • Ferroelectric S $r_{0.9}$/B $i_{2.1}$/T $a_{2}$/ $O_{9}$ solutions were synthesized using sol-gel process in which strontinum ethoxide bismuth ethoxide trantalum ethoxide were used a s startring materials. SBT thin films were coated on Pt/Ti/ $SiO_2$/Si substrates by spin-coating. rapid thermal annealing (RTA) was used to promote crystallization. Thin films were annealed at $700^{\circ}C$ for 1 hr in an oxygen atmosphere. This temperature is about 10$0^{\circ}C$ lower than the usual annealing temperature for SBT thin films. Pt top-electrode was deposited by sputtering and thin films were post-annealed at $700^{\circ}C$ for 30 min. to enhance electrical properties. As the RTA temperature increased the higher 2 $P_{r}$ values were obtained. At RTA temperature being 78$0^{\circ}C$ remanent polarization of S $r_{0.9}$/B $i_{2.1}$/T $a_{2}$/ $O_{9}$ thin film was 7.73 $\mu$C/cm $_2$ and the leakage current density was 1.14$\times$10$^{-7}$ A/c $m^2$ at 3 V. As RTA temperature increased the breakdown voltage was decreased. It is considered that the low-field breadown is caused by the rough surface of SBT films and forming bismuth metal in SBT thin films.films.lms.

  • PDF

Sol-gel법에 의해 제조된 강유전체 $Bi_{3.15}La_{0.85}Ti_3O_{12}$ 박막의 결정 배향성 조절 (Crystallographic orientation modulation of ferroelectric $Bi_{3.15}La_{0.85}Ti_3O_{12}$ thin films prepared by sol-gel method)

  • 이남열;윤성민;이원재;신웅철;류상욱;유인규;조성목;김귀동;유병곤
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 하계학술대회 논문집 Vol.4 No.2
    • /
    • pp.851-856
    • /
    • 2003
  • We have investigated the material and electrical properties of $Bi_{4-x}La_xTi_3O_{12}$ (BLT) ferroelectric thin film for ferroelectric nonvolatile memory applications of capacitor type and single transistor type. The 120nm thick BLT films were deposited on $Pt/Ti/SiO_2/Si$ and $SiO_2/Nitride/SiO_2$ (ONO) substrates by the sol-gel spin coating method and were annealed at $700^{\circ}C$. It was observed that the crystallographic orientation of BLT thin films were strongly affected by the excess Bi content and the intermediate rapid thermal annealing (RTA) treatment conditions regardeless of two type substrates. However, the surface microstructure and roughness of BLT films showed dependence of two different type substrates with orientation of (111) plane and amorphous phase. As increase excess Bi content, the crystallographic orientation of the BLT films varied drastically in BLT films and exhibited well-crystallized phase. Also, the conversion of crystallographic orientation at intermediate RTA temperature of above $450^{\circ}C$ started to be observed in BLT thin films with above excess 6.5% Bi content and the rms roughness of films is decreased. We found that the electrical properties of BLT films such as the P-V hysteresis loop and leakage current were effectively modulated by the crystallographic orientations change of thin films.

  • PDF

스퍼터링법에 의한 강유전성 $Pb_{1+x}$($Fe_{0.5}$$Nb_{0.5}$)$O_3$ 박막의 제조 및 전기적 특성에 관한 연구 (Preparation and Electrical Properties of the Ferroelectric $Pb_{1+x}$($Fe_{0.5}$$Nb_{0.5}$)$O_3$ Thin Films by Sputtering Method)

  • 장영일;김장엽;임대순;김병호
    • 한국세라믹학회지
    • /
    • 제35권3호
    • /
    • pp.294-302
    • /
    • 1998
  • $Pb_{1+x}$($Fe_{0.5}$$Nb_{0.5}$)$O_3$ films have been synthesized on Pt/Ti/$SiO_2$/Si substrates using rfmagnetron sputtering Concentration of Fe and Nb in the deposited films was adjusted to near stoichiometry through the control of target composition, Films deposited with adjusted to near stoichiometry showed better electrical properties such as dielectic and leakage characteristics. Crystallinity and dielectric constant increased with increasing excess PbO upto 9 mol% This study also showed that dielectric constant and leakage current characteristics improved by optimum content of $O_2$ flow during deposition.

  • PDF

PZT 강유전 박막의 전기적 특성 (Electrical Characteristics of PZT Ferroelectric Thin Films)

  • 김현권;백동수;최형욱;김준한;박창엽
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1993년도 정기총회 및 추계학술대회 논문집 학회본부
    • /
    • pp.225-227
    • /
    • 1993
  • Pb(Zr, Ti)$O_3$ ferroelectric thin layers were deposited onto Pt/$SiO_2$/Si substrates by Sol-Gel processing and annealed by RTA at $600^{\circ}C$ for $20{\sim}30\;sec$. microstructure of the films was examined by XRD and SEM analysis. Electrical properties of PZT thin films with different Zr/Ti ratio yield $P_r$ ranging $10{\sim}21{\mu}C/cm^2$, $E_c$, ranging $37.5{\sim}137.5\;kV/cm$, switching times faster than 180nsec, and leakage current about $20{\mu}A/cm^2$. The film was endured about $10^{10}$ fatigue cycles.

  • PDF

CeO2Buffer Layer를 이용한 Pt/BLT/CeO2/Si 구조의 특성 (Characterization of Pt/BLT/CeO2/Si Structures using CeO2 Buffer Layer)

  • 이정미;김경태;김창일
    • 한국전기전자재료학회논문지
    • /
    • 제16권10호
    • /
    • pp.865-870
    • /
    • 2003
  • The MFIS (Metal-Ferroelectric-Insulator-Semiconductor) capacitors were fabricated using a metalorganic decomposition method. Thin layers of CeO$_2$ were deposited as a buffer layer on Si substrate and BLT thin films were used as a ferroelectric layer. The electrical and structural properties of the MFIS structure were investigated. X -ray diffraction was used to determine the phase of the BLT thin films and the quality of the CeO$_2$ layer. The morphology of films and the interface structures of the BLT and the CeO$_2$ layers were investigated by scanning electron microscopy. The width of the memory window in the C-V curves for the MFIS structure is 2.82 V. The experimental results show that the BLT-based MFIS structure is suitable for non-volatile memory FETs with large memory window.

Sol-Gel법에 의한 강유전체 PZT 박막의 제작 (Preparation of Ferroelectric PZT thin films by Sol-Gel processing)

  • 이병수;유도현;신태현;조기선;육재호;김용혁;김형권;지승한;이덕출
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2000년도 하계학술대회 논문집 C
    • /
    • pp.1685-1686
    • /
    • 2000
  • Crack-free and homogeneous com ceramic and epitaxial lead zirconate titanat ferroelectric thin films with perovskite structure been prepared by sol-gel processing. Ti-isoprop and lead acetate trihydrate and zirconium-pro are used raw materials. EAcAc is used as a cat 2-Methoky ethanol is used as a solvent annealing temperatures of the thin films are 0$^{\circ}C$.