• 제목/요약/키워드: ferrite

검색결과 2,075건 처리시간 0.038초

유전율제어에 의한 복합 Ferrite 전파흡수체의 성능향상 (Microwave Absorbing Characteristic Improvement by Permittivity Control of Ferrite Composite Microwave Absorber)

  • 신재영;권형주;오재희
    • 한국세라믹학회지
    • /
    • 제31권4호
    • /
    • pp.415-419
    • /
    • 1994
  • The material constants(the complex permeability and permittivity) of ferrite composite determine its microwave absorbing characteristics. Therefore, in order to improve the microwave absorbing characteristics, it is necessary to control the material constants of the ferrite composite. In this study, the method of improving microwave absorbing characteristics by control of permittivity of ferrite composite which has not satisfying matching condition in C-X band (4 GHz~12.4 GHz) was investigated. It was possible to control the permittivity by adjusting graphite loading ratio in the ferrite composite microwave absorber. It was also concluded that the control of permittivity of ferrite composite is effective method to improve the microwave absorbing characteristics.

  • PDF

Ba-Ferrite를 이용한 자기 연마재 개발 (Development of The Magnetic Abrasive Using Barium Ferrite)

  • 김희남;송승기;정윤중;윤여권;김희원;조상원;심재환
    • 한국안전학회지
    • /
    • 제18권2호
    • /
    • pp.46-49
    • /
    • 2003
  • The magnetic polishing is the useful method to finish some machinery fabrications by using magnetic power. This method is one of the precision techniques and has m aim for clean technology in the transportation of the pure gas in the clean pipes. The magnetic abrasive polishing method is not so common in the field of machine that it is not known to widely. There are rarely researcher in this field because of non-effectiveness of magnetic abrasive. Therefore, in this paper we deals with the development of the magnetic abrasive with the use of Ba-Ferrite. In this development, abrasive grain WA has been made by using the min bond fabricated at low temperature. And magnetic abrasive powder was fabricated from the Ba-Ferrite which was crushed into 200 mesh. The XRD analysis result shows that only WA abrasive and Ba-Ferrite crystal peaks were detected, explaining that resin bond was not any more to contribute chemical reaction. From SEM analysis, we found that WA abrasive and Ba-Ferrite were strongly bonding with each other.

페라이트 형상에 따른 둥근형 무전극 램프의 의존성 (Dependence of Round type electrodeless lamp according to Ferrite shape)

  • 김남군;양종경;이주호;박대희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 추계학술대회 논문집
    • /
    • pp.465-466
    • /
    • 2007
  • In electrode-less lamp, The key point in creating an efficient light source based on RF discharge is to minimize the RF power loss in the RF coupler which for Anderson's type of RF lamp is due to losses in the ferrite core. This loss depends on the particular ferrite material, its size, geometry, frequency in this kind of inductive lamp shows that the correct choice of discharge current has a crucial effect on the core loss. In this study, we measured Ferrite temperature in normal state, then analyzed electrical and optical characteristics according to ferrite shape. We were able to know that was ferrite of the antenna had relate closely with temperature and luminous of the lamp. Also we appraised temperature and electrical, optical properties during turn on the lamp.

  • PDF

저탄소 HSLA강의 천이 온도 미치는 미세 조직의 영향 (Effects of microstructure on impact transition temperature of low carbon HSLA steels)

  • 강주석;이창우;박찬경
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2008년도 춘계학술대회 논문집
    • /
    • pp.431-434
    • /
    • 2008
  • Effects of microstructure on the toughness of low carbon HSLA steels were investigated. Nickel decreased the ferrite-austenite transformation temperature, resulted in increase of the fraction of bainitic ferrite. However, it was decreased with increasing deformation amount at austenite region. Since fine austenite grains formed by dynamic recrystallization under large strain transformed to acicular ferrite or granular bainite rather than bainitic ferrite. The effective grain size, thus, was decreased by deformation and it resulted in lower ductile-brittle transition temperature (DBTT). The bainitic ferrite was thought to inhibit the fracture crack initiation and to delay the crack propagation by its high dislocation density and hard interlath $2^{nd}$ phase constituents, respectively. Thus, DBTT was also decreased by Ni addition in low carbon HSLA steels.

  • PDF

용융염법에 의한 Sr-ferrite의 생성기구 (Formation Mechanism of Sr-Ferrite by Molten Salt Method)

  • 박준홍;신효순;이병교
    • 한국세라믹학회지
    • /
    • 제31권10호
    • /
    • pp.1181-1187
    • /
    • 1994
  • Sr-ferrite powders were synthesized by molten salt method. The process of powder formation was investigated by controlling the size and shape (sphere and acicular) of starting materials. The morphology of resulting ferrite was plate-like regardless of the shape of starting materials, Fe2O3 powders. As a result, the formation of Sr-ferrite in the molten salt was proceeded by solution-precipitation.

  • PDF

Pb-ferrite와 첨가물의 효과 (A Study about Pb-ferrite & effect of Annex)

  • 배진호;사공건
    • 전기의세계
    • /
    • 제23권5호
    • /
    • pp.61-65
    • /
    • 1974
  • Ba-ferrite and Sr-ferrite are mostly used for permanent magnetic materials. In this work, we investigated Pb-ferrite which is studying now at abroad. We studied the most appropriate mole percent of PbO to Fe$_{2}$O$_{3}$, calcinating temperature and time, sintering temperature and time, and further investigated effects of the annex(NaBiO$_{3}$) The method of appraisment is the microscope for meta and B-H curve by flaxmeter.

  • PDF

Mechanical alloying법으로 제조한 Sr-ferrite 분말의 자기적 이방성 (Magnetic anisotropy of Sr-ferrite powder produced via mechanical alloying)

  • 배재원;손성우;정국철;황동하;권해웅
    • 한국자기학회:학술대회 개요집
    • /
    • 한국자기학회 2002년도 동계연구발표회 논문개요집
    • /
    • pp.90-91
    • /
    • 2002
  • 영구자석 재료용 Sr-ferrite의 제조에 mechanical alloying (기계적 합금화)기술을 적용해서 초미세 결정립으로 구성된 고보자력의 Sr-ferrite를 제조해서 높은 보자력을 실현할 수 있는 것으로 보고하고 있다[1]. 그러나 이 새로운 방법으로 제조한 Sr-ferrite는 높은 보자력을 갖기는 하지만, 대단히 미세한 결정립들이 결합하여 입자를 구성하고 있어 자장을 가해서 입자를 배향시키기가 어렵다. 따라서 이 재료는 등방성 분말로 밖에 이용할 수 없는 결정적인 문제점이 있다. (중략)

  • PDF

전파흡수체용 Rubber-Ferrite Composite에 관한 연구 (A Study on Rubber-Ferrite Composite for Electromagentic Absorber)

  • 김동일;박연준;박재석
    • 한국항해항만학회:학술대회논문집
    • /
    • 한국항해항만학회 1996년도 The Korean Institute of Navigation 1996년도 한·중 국제학술 심포지움 및 추계학술발표회 논문집
    • /
    • pp.111-116
    • /
    • 1996
  • To realize the RF layer of Rubber Ferrite-Air-Solid Ferrite(RF-A-F) that proposed by Y.Naito it is tried to grasp the formulation of composition by varying the ratio of mole and element of Complex Isotropic Ferrite Nix-A0.1-Zn(1-x-0.1)*Fe2O4 As a result it was found that the characteristics of the electromagnetic wave absorber constructed by the selected formulation of compositionin in RF-A-F type were improved.

  • PDF

국산 플럭스 코어드 와이어 용접에서 입열량이 용접부의 미세조직과 인성에 미치는 영향 (A Study on the Effect of Heat Input on the Microstructure and Toughness of Weldments Made by Domestic Flux Cored Wires.)

  • 고진현;국정한
    • Journal of Welding and Joining
    • /
    • 제11권4호
    • /
    • pp.57-69
    • /
    • 1993
  • In the present study, the microstructure and Charpy V notch toughness of multipass $CO_2$ FCA weldment in three different heat inputs(1-3KJ/mm)were investigated. The weldments using two different domestic FCAW wires(AWS E71T-1 and E71T-5 equivalent) in C-Mn steel were chemically analysed. The following conclusions can be inferred. 1. T-1 wire Showed a stable arc transfer, less spatter and harsh, a better bead spreading and easy slag removal, whereas T-5 wire suffered from the arc stability, which tended to increase spatter and produce a more convex bead. 2.The microsturctures of the top beads of the weldments in three different heat inputs consisted of coarse-grained boundary ferrite and Widmanstatten ferrite side plate with increasing heat inputs. The modest fraction of acicular ferrite in the two wire weldments was observed in the 2KJ/mm heat input. 3.The fine-grained reheated zones of both welds consisted of a duplex microstructure of polygonal ferrite and second phases. 4. The basic flux weldment of T-5wires showed a higher Charpy impact property than that of T-1 wires because of a higher fraction of acicular ferrite in the weld microstructure.

  • PDF