Zn-15%Al 합금의 가공연화 거동 (Work Softening Behavior of Zn-15%Al alloy)

  • 전중환;성기덕;김정민;김기태;정운재
    • 열처리공학회지
    • /
    • 제18권1호
    • /
    • pp.18-23
    • /
    • 2005
  • Effect of cold rolling on microstructural changes has been investigated for a Zn-15%Al alloy to elucidate the reason for its work softening behavior. Fully annealed microstructure of the Zn-15%Al alloy is characterized by ${\eta}$ grains and (${\eta}+{\alpha}$) lamellar colonies, where ${\eta}$ and ${\alpha}$ are Zn-rich HCP and Al-rich FCC phases, respectively. The hardness decreases continuously with increasing cold rolling degree, exhibiting work softening behavior. It is revealed that during the cold rolling, (${\eta}+{\alpha}$) lamellar colonies gradually change into equiaxed ${\eta}$ and ${\alpha}$ grains due to dynamic recrystallization at room temperature, while pre-existing ${\eta}$ grains are only deformed without recrystallization. Furthermore, cold rolling causes the precipitation of dissolved Al solutes in ${\eta}$ grains. In view of these results, change of (${\eta}+{\alpha}$) phases from lamellar to equiaxed morphology, which results in structural softness and increase in equiaxed ${\eta}/{\alpha}$ grain boundaries with higher mobility, and deterioration of solution hardening by precipitation of Al solutes from ${\eta}$ grains, are thought to contribute to the work softening of Zn-15%Al alloy.

Effect of Large $\alpha$-Silicon Carbide Seed Grains on Microstructure and Fracture Toughness of Pressureless-Sintered $\alpha$-Silicon Carbide

  • Young-Wook Kim;Kyeong Sik Cho;June-Gunn Lee
    • The Korean Journal of Ceramics
    • /
    • 제2권1호
    • /
    • pp.39-42
    • /
    • 1996
  • ${\alpha}-SiC$ powder with or without the addition of 0.1 wt% of large ${\alpha}-SiC$ partices(seeds) was pressureless-sintered at $1950^{\circ}C$ for 0.5, 2, and 4 h using $Y_3Al_5 O_{12}$ (yttrium aluminum garnet, YAG) as a sintering aid. The materials without seeds had an equiaxed grain struture. In contrast, the materials with seeds sintered for 2 and 4 h had a duplex microstructure with large elongated grains and amall equiaxed grains. Addition of large ${\alpha}-SiC$ seeds into ${\alpha}-SiC$ accelerated the grain growth of some ${\alpha}-SiC$ grains during sintering and resulted in the increased fracture toughness of the sintered materials. The fracture toughnesses of materials with or without seeds sintered for 4 h were 6.6 and $5.2 MPa \;m^{12}$, respectively.

  • PDF

YAG상 첨가 탄화규소-질화규소 복합재료의 기계적 특성 (Mechanical Properties of Silicon Carbide-Silicon Nitride Composites Sintered with Yttrium Aluminum Garnet)

  • 이영일;김영욱;최헌진;이준근
    • 한국세라믹학회지
    • /
    • 제36권8호
    • /
    • pp.799-804
    • /
    • 1999
  • Composites of SiC-Si3N4 consisted of uniformly distributed elongated $\beta$-Si3N4 grains and equiaxed $\beta$-SiC grains were fabricated with $\beta$-SiC,. $\alpha$-Si3N4 Al2O3 and Y2O3 powders. By hot-pressing and subsequent annelaing elongated $\beta$-Si3N4 grains were grown via$\alpha$longrightarrow$\beta$ phase transformation and equiaxed $\beta$-Si3N4 composites increased with increasing the Si3N4 content owing to the reduced defect size and enhanced crack deflection by elongated $\beta$-Si3N4 grains and the grain boundary strengthening by nitrogen incorporation. Typical flexural strength and fracture toughness of SiC-40 wt% Si3N4 composites were 783 MPa and 4.2 MPa.m1/2 respectively.

  • PDF

티타늄 합금(Ti-6Al-4V)의 조직변화에 따른 기계적 특성 평가 (The Evaluation of Mechanical properties on the Changes of Microstructure for Titanium Alloy (Ti-6Al-4V))

  • 권재도;배용탁;최성종
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2000년도 추계학술대회논문집A
    • /
    • pp.135-140
    • /
    • 2000
  • The characteristics of mechanical behavior were estimated for Ti-6Al-4V alloy with four kinds of microstructure prepared with heat treatments. For this study, impact test, tensile test and fatigue crack growth test were performed, and then compared mechanical properties on the four microstructures. Furthermore, for quantitative evaluation, fractal dimensions of crack pass were obtained using the box counting method. The main results obtained are summarized as follows. (1) The microstructures exhibited equiaxed microstructure, bimodal-microstructure and lamellar microstructure by heat treatment. (2) The impact absorbed energy and elongation is superior in the bimodal-microstructure, and the hardness and tensile strength are superior in the lamellar microstructure. (3) The fatigue crack growth rate is similar to all microstructures in the low ${\Delta}K$ region. The fatigue crack growth rate of equiaxed microstructure is fastest, and that of lamellar microstructure is lowest in the high ${\Delta}K$ region. (4) The fractal dimension D of lamellar microstructure is higher then that of the equiaxed microstructure and bimodal microstructure.

  • PDF

티타늄 합금(Ti-6Al-4V)의 조직변화에 따른 기계적 특성 평가 (The Evaluation of Mechanical Properties on the Changes of Microstructure for Titanium Alloy (Ti-6Al-4V))

  • 권재도;배용탁;최성종
    • 대한기계학회논문집A
    • /
    • 제26권4호
    • /
    • pp.609-616
    • /
    • 2002
  • The characteristics of mechanical behavior are investigated for Ti-6Al-4V alloy. Four kinds of the specimens are prepared under different heat treatments in order to produce different microstructures. In the present investigations, impact, tensile and fatigue crack growth tests are performed for each test specimen. The results obtained through the investigations are compared. Additionally fr actal dimensions of crack pass are obtained using the box counting method. The results are, 1) the microstructures shows as equiaxed, bimodal and Widmanstatten microstructures respectively, 2) the impact energy and elongation are superior fur the bimodal microstructure, and the hardness and tensile strength are superior fur the Widmanstatten microstructure, 3) the fatigue crack growth rate is similar to all microstructures in low ΔK region while that of equiaxed microstructure is the largest, and that of Widmanstatten microstructure is the lowest in high ΔK region respectively, 4) the fractal dimension D of Widmanstatten microstructure shows higher value than that of the equiaxed and bimodal microstructures under 200 magnification view of the SEM micrographs.

자유형 단조 공정에 의한 Ti-6Al-4V 빌렛 제조기술 (Manufacturing Process of the Ti-6Al-4V Billet by the Open-die Forging)

  • 김국주;최승식;황창률;김종식;염종택;이종수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2006년도 춘계학술대회 논문집
    • /
    • pp.377-380
    • /
    • 2006
  • Manufacturing process of Ti-6Al-4V alloy billet was investigated with FEM simulation and experimental analysis. Before the breakdown process of Ti-6Al-4V alloy ingot, FEM simulation for the breakdown processes of Ti-6Al-4V alloy ingot was used to calculate the forging load and state variables such as strain, strain rate and temperature. In order to breakdown the ingot structure and make an equiaxed structure billet, two different processes were employed for a VAR/VAR processed Ti-6Al-4V alloy ingot. Firstly, the ingot was cogged in single-phase $\beta$ field at the temperature of $1,100^{\circ}C$. In the process, the coarse and inhomogeneous structure developed by the double melting process was broken down. The second breakdown was performed by upsetting and cogging processes in $\alpha+\beta$ phase field to obtain the microstructure of fine equixed $\alpha$ structure in the matrix of transformed $\beta$. Finally, the mechanical properties of Ti-6Al-4V alloy billet made in this work were compared with those of other billet and ring product.

  • PDF

액장 소결에 의한 $\beta-SiC-ZrB_2$ 복합체의 제조와 특성 (Properties and Manufacture of the $\beta-SiC-ZrB_2$ Composited Densified by Liquid-Phase Sintering.)

  • 신용덕;주진영
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제48권2호
    • /
    • pp.92-97
    • /
    • 1999
  • The mechanical and electrical properties of the hot-pressed and annealed $\beta-Sic$+39vol.%$ZrB_2$ electroconductive ceramic composites were investigated as a function of the liquid forming additives of $Al_2O_3+Y_2O_3(6:4wt%)$. In this microstructures, no reactions and elongated $\alpha$-SiC grains with equiaxed $ZrB_2$, gains were observed between $\beta-SiC$ and $ZrB_2$, and the relative density was over 97.6% of the theoretical density. Phase analysis of the composites by XRD revealedmostly of $\alpha$-SiC(6H, 4H), $ZrB_2$, and weakly $\beta-SiC$(15R) phase. The fracture toughness decreased with increasing $Al_2O_3+Y_2O_3$ contents and showed the highest of $6.37MPa.m^{\fraction ane-half}$ for composite added with 4wt% $Al_2O_3+Y_2O_3$ additives at room temperature. The electrical resistivity increased with increasing $Al_2O_3+Y_2O_3$contents and showed the lowest of $1.51\times10^{-4}\Omega.cm$ for composite added with $Al_2O_3+Y_2O_3$ additives at $25^{\circ}C$. This reason is the increasing tendency of pore formation according to amount of liquid forming additives $Al_2O_3+Y_2O_3$. The electrical resistivity of the composites was all positive temperature coefficient resistance(PTCR) against temperature up to $700^{\circ}C$.

  • PDF

미세조직적 인자가 밀소둔된 Ti-6Al-4V 합금의 피로 및 피로균열전파 거동에 미치는 영향 (Effect of Microstructural Factors on Fatigue and Fatigue Crack Propagation Behaviors of Mill-Annealed Ti-6Al-4V Alloy)

  • 박상후;김수민;이다은;안수진;김상식
    • 대한금속재료학회지
    • /
    • 제56권12호
    • /
    • pp.845-853
    • /
    • 2018
  • To understand the effect of microstructural factors (i.e., the size of ${\alpha}$ phase, equiaxed vs bimodal structure) on high cycle fatigue (HCF) and fatigue crack propagation (FCP) behaviors of mill-annealed Ti-6Al-4V (Ti64) alloy, three specimens of EQ (equiaxed)-8 (8 indicates the size of ${\alpha}$ grain), BM (bimodal)-8, and BM-16 were studied. The uniaxial HCF and FCP tests were conducted at an R ratio of 0.1 under sinusoidal fatigue loading. The microstructural influence (i.e., EQ vs BM) was not significant on the tensile properties of mill-annealed Ti64 alloy, and showed an increase in tensile strength and elongation with decreasing gauge thickness from 50 mm to 1.3 mm. The microstructure, on the other hand, affected the resistance to HCF substantially. It was found that the EQ structure in mill-annealed Ti64 has better resistance to HCF than the BM structure, as a result of different crack initiation mechanism. Unlike HCF behavior, the effect of microstructural features on the FCP behavior of mill-annealed Ti64 was not significant. Among the three specimens, BM-16 specimen showed the highest near-threshold ΔK value, probably because it had the greatest slip reversibility with large ${\alpha}$ grains. The effect of microstructural factors on the HCF and FCP behaviors of mill-annealed Ti64 alloy are discussed based on fractographic and micrographic observations.

질화규소의 기계적 성질 및 접촉 손상: I. ${\alpha}/{\beta}$ 상분율의 영향 (A Study on the Mechanical Properties and Contact Damage of Silicon Nitrides : 1. Effect of ${\alpha}/{\beta}$ Phase Fraction)

  • 이승건
    • 한국분말재료학회지
    • /
    • 제5권1호
    • /
    • pp.15-21
    • /
    • 1998
  • The effect of $\alpha$/$\beta$ phase on the mechanical properties and contact damage of silicon nitrides $Si_3N_4$) was investigated. Silicon nitride materials were prepared from two starting powders, at selective increasing hot-pressing temperatures to coarsen the microstructures: (i) from relatively coarse $\alpha$-phase powder, essentially equiaxed $\alpha$-$Si_3N_4$ grains, with limited, slow transformation to $\beta$-$Si_3N_4$ grain; (ii) from relatively fine $\alpha$-phase powder, a more rapid transformation to $\beta$-$Si_3N_4$, with attendant grain elongation. The resulting micro-structure thereby provided a spectrum of $\alpha$/$\beta$ phase ratios, grain sizes, and grain shapes. Fracture strength, hardness, and toughness were measured, and contact damage and strength degradation after indentation were investigated by Hertzian indentation using spherical indenter. A brittle to ductile transition in $Si_3N_4$ depended on $\alpha$/$\beta$ phase ratio as well as grain size. Silicon nitride with elongated $\beta$ grains showed a superior, contact damage resistance.

  • PDF

등축정 Ti-6Al-4V 합금의 $\alpha,\;\beta$ 구성상의 고온변형거동 규명 (High temperature deformation behavior of $\alpha\;and\;\beta$ phase of Ti-6Al-4V alloy with an equiaxed microstructure)

  • 이유환;염종택;박노광;이종수;김정한
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2005년도 춘계학술대회 논문집
    • /
    • pp.295-298
    • /
    • 2005
  • High temperature deformation behavior of $\alpha\;and\;\beta$ phase of Ti-6Al-4V was investigated within the framework of a self-consistent approach at various temperature ranges. To examine the flow behavior of u-phase, Ti-7.0Al-1.5V alloy was used, whose chemical composition is close to that of the $\alpha$ phase in Ti-6Al-4V at hot working temperatures. The flow stress of $\beta$ phase was predicted by using self-consistent approach. The flow stress of $\alpha$ phase was higher than that of $\beta$ phase above $750^{\circ}C$, while the $\beta$ phase revealed higher flow stress than a phase at $650^{\circ}C$. It was found that the relative strength and strain rate ratio between $\alpha\;and\;\beta$ phase significantly varied with temperature. From this approach, the mode for grain matrix deformation was proposed as a mixed type of both iso-stress and iso-strain rate modes.