• Title/Summary/Keyword: deformation-induced ${\varepsilon}$ martensite

Search Result 12, Processing Time 0.027 seconds

Dependence of Damping Capacity on Volume Fractions of Thermal and Deformation-induced ${\varepsilon}$ Martensites in an Fe-Mn Alloy (Fe-Mn 합금에서 열적 ${\varepsilon}$ 마르텐사이트와 변형유기 ${\varepsilon}$ 마르텐사이트 부피분율에 대한 진동감쇠능의 의존성)

  • Jun, Joong-Hwan;Hong, Kwon-Pyo;Choi, Chong-Sool
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.15 no.6
    • /
    • pp.272-278
    • /
    • 2002
  • The changes in damping capacity with volume fractions of thermal and deformation-induced ${\varepsilon}$ martensites were compared and analyzed in an Fe-23%-Mn alloy. The volume fraction of thermal ${\varepsilon}$ martensite increased with decreasing cooling temperature, whereas that of deformation-induced ${\varepsilon}$ martensite increased steeply up to 10%- of cold rolling and nearly saturated in further cold rolling. In the case of thermal ${\varepsilon}$ martensite, the damping capacity increased linearly with the increase in ${\varepsilon}$ martensite content. For the deformation-induced ${\varepsilon}$ martensite, however, the damping capacity increased continuously up to 70%- of ${\varepsilon}$ martensite, over which it decreased suddenly. TEM microstructures showed that the deterioration of damping capacity above 70%- of deformation-induced ${\varepsilon}$ martensite is ascribed to the introduction of perfect dislocations, which play a important role in inhibiting the movement of damping sources such as stacking fault boundaries inside ${\varepsilon}$ martensite, ${\varepsilon}$ martensite variant boundaries and ${\gamma}/{\varepsilon}$ interfaces.

Effect of Thermo-Mechanical Treatment on the Damping Capacity of Alloy with Deformation Induced Martensite Transformation (가공유기 마르텐사이트 변태를 갖는 합금의 감쇠능에 미치는 가공열처리의 영향)

  • Han, Hyun-Sung;Kang, Chang-Yong
    • Korean Journal of Materials Research
    • /
    • v.29 no.3
    • /
    • pp.160-166
    • /
    • 2019
  • This study investigates the effect of thermo-mechanical treatment on the damping capacity of the Fe-20Mn-12Cr-3Ni-3Si alloy with deformation induced martensite transformation. Dislocation, ${\alpha}^{\prime}$ and ${\varepsilon}-martensite$ are formed, and the grain size is refined by deformation and thermo-mechanical treatment. With an increasing number cycles in the thermo-mechanical treatment, the volume fraction of ${\varepsilon}-martensite$ increases and then decreases, whereas dislocation and ${\alpha}^{\prime}-martensite$ increases, and the grain size is refined. In thermo-mechanical treated specimens with five cycles, more than 10 % of the volume fraction of ${\varepsilon}-martensite$ and less than 3 % of the volume fraction of ${\alpha}^{\prime}-martensite$ are attained. Damping capacity decreases by thermo-mechanical treatment and with an increasing number of cycles of thermo-mechanical treatment, and this result shows an opposite tendency for general metal with deformation induced martensite transformation. The damping capacity of the thermo-mechanical treated damping alloy with deformation induced martensite transformation greatly affect the formation of dislocation, grain refining and ${\alpha}^{\prime}-martensite$ and then ${\varepsilon}-martensite$ formation by thermo-mechanical treatment.

The Effect of grain size on the damping capacity of Fe-26Mn-2Al alloy (Fe-26Mn-2Al 합금의 진동 감쇠능에 미치는 결정립 크기의 영향)

  • Kang, C.Y.;Eom, J.H.;Kim, H.J.;Sung, J.H.
    • Journal of Power System Engineering
    • /
    • v.11 no.1
    • /
    • pp.115-120
    • /
    • 2007
  • The effect of grain size on the damping capacity of Fe-26Mn-2Al alloy studied in this paper has been investigated after changing the microstructure by cold rolling and changing grain size. Micro structures in Fe-26Mn-2Al at room temperature consist of a large quantity of austenite and a small quantity of ${\varepsilon}\;and\;{\alpha}'$ martensite. And ${\varepsilon}\;and\;{\alpha}'$ martensite was increased by increasing the degree of cold rolling. The content of deformation induced martensite was increased with increasing the degree of cold rolling. Damping capacity was linearly increased with increasing ${\varepsilon}$ martensite content, which suggests that stacking faults and ${\varepsilon}$ martensite variant boundaries are the principle damping sources. With increasing the grain size in Fe-26Mn-2Al alloy, the damping capacity was increased due to increasing the volume fraction of ${\varepsilon}$ martensite by decrement in stability of austenite phase. With decreasing the grain size, the content of deformation induced martensite was decreased and the damping capacity was decreased.

  • PDF

Effect of Deformation Induced Martensite on the Damping Capacity of Fe-26Mn-4Co-2Al Alloy (Fe-26Mn-4Co-2Al 합금의 감쇠능에 미치는 가공 유기 마르텐사이트의 영향)

  • Jeong, Kyu-Seong;Kang, Chang-Yong
    • Korean Journal of Materials Research
    • /
    • v.26 no.9
    • /
    • pp.493-497
    • /
    • 2016
  • This study was carried out to investigate the effect of deformation induced martensite on the damping capacity of Fe-26Mn-4Co-2Al damping alloy. ${\alpha}^{\prime}$ and ${\varepsilon}$-martensite were formed by cold working, and; deformation induced martensite was formed with according to the specific direction and the surface relief. With an increasing degree of cold rolling, the volume fraction of ${\alpha}^{\prime}$-martensite increased rapidly, while the volume fraction of ${\varepsilon}$-martensite decreased after rising to a maximum value at a specific level of cold rolling. Damping capacity was increased, and then decreased with an increasing of the degree of cold rolling. Damping capacity was influenced greatly by the volume fraction of ${\varepsilon}$-martensite formed by cold working, but the effect of the volume fraction of ${\alpha}^{\prime}$-martensite have a actually on effect on the damping capacity.

Effect of Heat Treatment Temperature on Amount of Stress-Induced ${\varepsilon}$ Martensite in an Fe-Mn Baesd Alloy (Fe-Mn계 합금에서 응력유기 ${\varepsilon}$ 마르텐사이트의 양에 미치는 열처리 온도의 영향)

  • Jee, K.K.;Han, J.H.;Jang, W.Y.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.17 no.6
    • /
    • pp.342-345
    • /
    • 2004
  • In this work, a new method of measuring volume fraction of deformation-induced ${\varepsilon}$ martensite is proposed using endothermic heat on reverse transformation. As grain size increases, the amount of ${\varepsilon}$ martensite forming on cooling increases. However, with a decrease in grain size, more ${\varepsilon}$ is induced by deformation, improving shape memory effect.

Effect of Thermo-mechanical Treatment on the Tensile Properties of Fe-20Mn-12Cr-3Ni-3Si Damping Alloy (Fe-20Mn-12Cr-3Ni-3Si 합금의 인장성질에 미치는 가공열처리의 영향)

  • Han, H.S.;Kang, C.Y.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.32 no.2
    • /
    • pp.61-67
    • /
    • 2019
  • This study was carried out to investigate the effect of thermo-mechanical treatment on the tensile properties of Fe-20Mn-12Cr-3Ni-3Si alloy with deformation induced martensite transformation. ${\alpha}^{\prime}$ and ${\varepsilon}$-martensite, dislocation, stacking fault were formed, and grain size was refined by thermo-mechanical treatment. With the increasing cycle number of thermo-mechanical treatment, volume fraction of ${\varepsilon}$ and ${\alpha}^{\prime}$-martensite, dislocation, stacking fault were increased, and grain size decreased. In 5-cycle number thermo-mechanical treated specimens, more than 10% of the volume fraction of ${\varepsilon}$-martensite and less than 3% of the volume fraction of ${\alpha}^{\prime}$-martensite were attained. Tensile strength was increased and elongation was decreased with the increasing cycle number of thermo-mechanical treatment. Tensile properties of thermo-mechanical treated alloy with deformation induced martensite transformation was affected to formation of martensite by thermo-mechanical treatment, but was large affected to increasing of dislocation and grain refining.

Correlationship between Tensile Properties and Damping Capacity of 316 L Stainless Steel (316 L 스테인리스강의 인장성질과 감쇠능의 관계)

  • Kwoon, Min-Gi;Kang, Chang-Yong
    • Korean Journal of Materials Research
    • /
    • v.24 no.1
    • /
    • pp.1-5
    • /
    • 2014
  • This study is experimentally investigated whether or not a relationship exists between the mechanical properties and damping capacity of cold-rolled 316 L stainless steel. Deformation-induced martensite was formed with surface relief and directionality. With the increasing degree of deformation, the volume fraction of ${\varepsilon}$-martensite increased, and then decreased, while ${\alpha}^{\prime}$-martensite increased rapidly. With an increasing degree of deformation, tensile strength was increased, and elongation was decreased; however, damping capacity was increased, and then decreased. Tensile strength and elongation were affected in the ${\alpha}^{\prime}$-martensite; hence, damping capacity was influenced greatly by ${\varepsilon}$-martensite. Thus, there was no proportional relationship between strength, elongation, and damping capacity.

Effect of Microstructure on the Damping Capacity and Tensile Properties of Fe-Al-Mn Alloys (Fe-Al-Mn 합금의 진동감쇠능 및 인장성질에 미치는 미세조직의 영향)

  • Son, D.U.;Kim, J.H.;Lee, J.M.;Kim, I.S.;Kim, H.C.;Kang, C.Y.
    • Journal of Power System Engineering
    • /
    • v.8 no.4
    • /
    • pp.31-37
    • /
    • 2004
  • The damping capacity and strength of Fe-2Al-26Mn alloys have been studied for the development of new materials with high strength and damping capacity. Particularly, the effect of ${\alpha}'\;and\;{\varepsilon}$ martensite phase, which constitutes the microstructure of cold rolled Fe-Al-Mn alloys, has been investigated in terms of the strength and damping capacity of the alloys. The damping capacity rises with increasing the degree of cold rolling and reveals the maximum value at 25% reduction. The damping capacity is strongly affected by the volume fraction of ${\varepsilon}$ martensite, while the other phases, such as ${\alpha}'$ martensite and austenite phase, actually exhibit little effect on damping capacity. Considering that tensile strength increases and elongation decreases with increasing the volume fraction of ${\alpha}'$ martensite, it is proved that tensile strength is mainly affected by the amount of ${\alpha}'$ martensite.

  • PDF

The Effect of Alloy Elements on the Damping Capacity and Plasma Ion Nitriding Characteristic of Fe-Cr-Mn-X Alloys [I Damping Capacity] (Fe-Cr-Mn-X계 합금의 감쇠능 및 플라즈마이온질화 특성에 미치는 합금원소의 영향 [I 감쇠능])

  • Son, D.U.;Jeong, S.H.;Kim, J.H.;Lee, J.M.;Kim, I.S.;Kang, C.Y.
    • Journal of Power System Engineering
    • /
    • v.9 no.1
    • /
    • pp.70-75
    • /
    • 2005
  • The damping property of Fe-12Cr-22Mn-X alloys has been investigated to develop high damping and high strength alloy. Particularly, the effect of the phase of austenite, alpha and epsilon martensite, which constitute the structure of the alloys Fe-12Cr-22Mn-X alloys, on the damping capacity at room temperature has been investigated. Various fraction of these phases were formed depending on the alloy element and cold work degree. The damping capacity is strongly affected by ${\varepsilon}$ martensite while the other phase, such as ${\alpha}'$ martensite, actually exhibit little effect on damping capacity. In case of Fe-12Cr-22Mn-3Co alloy, the large volume fraction of ${\varepsilon}$ martensite formed at about 30% cold rolling, and in case of Fe-12Cr-22Mn-1Ti alloy, formed at about 20% cold rolling and showed the highest damping capacity. Damping capacity showed higher value in Fe-12Cr-22Mn-1Ti alloy than one in Fe-12Cr-22Mn-3Co alloy.

  • PDF

Dynamic plastic deformation behavior of Fe-X%Mn alloys (Fe-X%Mn 합금의 동적 소성변형거동)

  • Park, Hong Lae;Lee, Jeong Min;Sung, Wan;Kim, Won Baek;Choi, Chong Sool
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.8 no.4
    • /
    • pp.266-278
    • /
    • 1995
  • The high strain-rate dynamic plastic behavior of Fe-X%Mn alloys was investigated. The strain rate did not have an effect when tested under quasi-static strain rates($2{\times}10^{-3}/sec$ and $2{\times}10^{-1}/sec$). However, the true stress increased at all strain levels when the strain rate increased to $6{\times}10^3/sec$. Based on the experimental results, an constitution equation to calculate the dynamic strength for strain rates over $10^4/sec$ was determined. The Fe-5%Mn alloy containing athermal ${\alpha}^{\prime}$ martensite initially did not show work hardening. The work hardening increased with Mn content showing a maximum at 20% Mn. The high work hardening of Fe-20%Mn and Fe-30%Mn alloys appears to be closely related not only to the initial amounts of ${\varepsilon}$ martensite but to the strain induced transformation (${\gamma}{\rightarrow}{\varepsilon}$ and ${\varepsilon}{\rightarrow}{\alpha}^{\prime}$) occurring during each stages of deformation.

  • PDF