This study was carried out to control the stalk curing period in Burley Tobacco, for its period was longer than 40 days. The 5 methods were treated to shorten the stalk curing period. The curing period was shortened for 1~3 days by the harvesting methods and the amount of predehydration, but it was shortened for 8 days by the hanging methods(sloping and horizontal curing)and the hanging density(90 plants/3.3m2) without the decrease of quality. In the ventilating condition of the curing house, the curing period could be controlled for 5 dyes with the quality like the conventional cured leaves by closing the curing house from the late curing stage. But when the curing house was not ventilated earlier, however the curing period was shortened but its quality was decreased.
Choi, Jun Seong;Jung, Chul Ho;Lee, Chan Hee;Lim, in su
International Journal of Highway Engineering
/
v.19
no.2
/
pp.67-74
/
2017
PURPOSES : The objective of this study is to ascertain the curing period of cementless cold central plant recycled asphalt base-layer, using mechanical analyses and specimen quality tests on the field. METHODS : Cold central plant recycled asphalt base-layer mixture was produced in the plant from reclaimed asphalt, natural aggregate, filler for the cold mix, and the modified emulsion AP using asphalt mix design and plant mix design. In order to examine the applicability of the curing period during the field test, the international standards for the possibility of core extraction and the degree of compaction and LFWD deflection were analyzed. Moreover, Marshall stability test, porosity test, and indirect tensile strength test were performed on the specimens of asphalt mix and plant mix design. RESULTS : The plant production process and compaction method of cementless cold central plant recycled asphalt base-layer were established, and the applicability of the optical moisture content for producing the mixture was verified through the field test. In addition, it was determined that the core extraction method of the conventional international curing standard was insufficient to ensure performance, and the LFWD test demonstrated that the deflection converges after a two-day curing. However, the back-calculation analysis reveals that a three-day curing is satisfactory, resulting in a general level of performance of dense asphalt base-layer. Moreover, from the result of the specimen quality test of the asphalt mix design and plant mix design according to the curing period, it was determined that the qualities satisfied both domestic and international standards, after a two-day curing. However, it was determined that the strength and stiffness after three-day curing are higher than those after a two-day curing by approximately 3.5 % and 20 %, respectively. CONCLUSIONS:A three-day curing period is proposed for the cementless cold central plant recycled asphalt base-layer; this curing period can be demonstrated to retain the modulus of asphalt-base layer in the field and ensure stable quality characteristics.
The cement industry is a major source of carbon dioxide emissions. Reduction in emissions in this sector is an important issue. Calcium silicate cement is a type of alternative to ordinary Portland cements which contributes to the reduction in carbon dioxide emissions. However, because the type of cement is a non-hydraulic material, there are limitations to its application in the field. The effects of pre-curing periods on the physical characteristics of ordinary Portland cement pastes with calcium silicate cement in the present study were investigated. The Independent variable is the pre-curing period. The pre-curing period varied from 0 to 5 hrs, considering the hydration characteristics of ordinary Portland cement. The carbonation curing of the ordinary Portland cement pastes with the calcium silicate cement after pre-curing was conducted. The concentration of gaseous CO2 was fixed at 20 %. The test results showed that the pre-curing period led to the pore structural change of the pastes, which in turn could affect the further reaction under the long-term curing condition.
Proceedings of the Korea Concrete Institute Conference
/
1998.04b
/
pp.695-702
/
1998
The purpose of this study is to investigate the mechanical properties of precast concrete cured by accelerated curing methods such as, steam curing method and warm water curing method varing maximum temperature of curing along to the period of curing. Some specimens are cured by accelerated curing method(warm water curing method) and then deposited in the storehouse. The others are deposited in the storehouse directly. All of these are cured until being tested to compare these two group's mechanical characteristics for each period 3days, 7days, 28days. The goal of this comparison is to estimate the efficiency of accelerated curing method in the case of precast concrete stocked in the field or warehouse for a long term and to make guide line for factory manager to make a economical products of concrete of a good quality. We can conclude some guide lines 1) It is not efficient to cure concrete with accelerated method at higher than 80℃. 2) The continuing of curing period more than 36hr makes damage to concrete in using accelerated curing method. 3) The strength revelation of concrete cured by accelerated curing methods, added rice husk ash more delayed than OPC concrete done but the strength of maximum value is higher than OPC concrete. 4) It is not efficient to use accelerated curing method in the case of storing the products for more than 7days in the aspect of mechanical properties.
This paper presents a study of the properties and behavior of self-compacting concretes (SCC) in the hot climate. The effect of curing environment and the initial water curing period on the properties and behavior of SCC such as compressive strength, ultrasonic pulse velocity (UPV) and sorptivity of the SCC specimens were investigated. Three Water/Binder (W/B) ratios (0.32, 0.38 and 0.44) have been used to obtain three ranges of compressive strength. Five curing methods have been applied on the SCC by varying the duration and the conservation condition of SCC. The results obtained on the compressive strength show that the period of initial water curing of seven days followed by maturation in the hot climate is better in comparison with the four other curing methods. The coefficient of sorptivity is influenced by W/B ratio and the curing methods. It is also shown that the sorptivity coefficient of SCC specimens is very sensitive to the curing condition. The SCC specimens cured in water present a low coefficient of sorptivity regardless of the ratio W/B. Furthermore, the results show that there is a good correlation between ultrasonic pulse velocity and the compressive strength.
This study was conducted to find out the stalk curing methods that can reduce photobleaching, and shorten the curing period in burley to bacco stalk curing. The results obtained summarized as follows. In the ventilation window-plot, the temperature within the curing house was high and the curing period was shortened, too. The rate of photobleached leaves of whole plant stalk curing-plot was higher than those of any other plots. In the ventilation window-plot, the labor of operating the curing house was saved and the yield and visual quality of cured leaves were high, too. For reducing the photobleaching of leaves, following procedures are desirable; to prevent the lower leaves from drying up and overripening at maturing stage, cut the stalk after first or second priming, shorten the curing period as possible when the 80% of leaf bodies changed brown.
Moist curing of concrete is a time consuming procedure. It takes minimum 28 days of curing to obtain the characteristic strength of concrete. However, under certain situations such as shortage of time, weather conditions, on the spot changes in project and speedy construction, waiting for entire curing period becomes unaffordable. This situation demands early strength of concrete which can be met using accelerated curing methods. It becomes necessary to obtain early strength of concrete rather than waiting for entire period of curing which proves to be uneconomical. In India, accelerated curing methods are used to arrive upon the actual strength by resorting to the equations suggested by Bureau of Indian Standards' (BIS). However, it has been observed that the results obtained using above equations are exaggerated. In the present experimental investigations, the results of the accelerated compressive strength of the concrete are used to develop the regression models for predicting the short term and long term compressive strength of concrete. The proposed regression models show better agreement with the actual compressive strength than the existing model suggested by BIS specification.
Proceedings of the Korea Concrete Institute Conference
/
2000.10b
/
pp.939-944
/
2000
This study examines both strength development and pore volume of high temperature curing mortar, using a blast-furnace slag powder (BFS). This study experiments with various pre-steaming period, differing curing temperature and the replacement of BFS. According to the results, the strength development of BFS mortar is stronger when higher curing temperature are used(as opposed to standard curing). Also, regardless of the curing method, pore volume decreases as the curing time increases. From these results we can identify the optimum conditions required pre-steaming period, differing curing temperature and the replacement to produce BFS mortar properties.
Proceedings of the Korean Institute of Building Construction Conference
/
2022.04a
/
pp.91-92
/
2022
This study is a basic study on carbonation curing technology of concrete using supercritical CO2, and carbonation curing was carried out by exposing concrete to supercritical CO2 for a certain period of time. In the case of conventional carbonation curing, long-term curing was performed for several weeks by controlling the concentration of CO2, but by using supercritical CO2, more rapid carbonation curing was carried out using constant temperature and pressure conditions to improve durability through surface modification of concrete. This experiment was conducted with the goal of deriving the optimal carbonation curing conditions by measuring the carbonation depth by exposing concrete for a certain period of time to conditions above the supercritical level. As a result, it was confirmed that the carbonation depth increased as the curing time increased, and the curing time could be shortened compared to the carbonation curing according to the existing CO2 concentration.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.