$\alpha$-Sialon/SiC Whisker 복합재료의 기계적 물성 및 마모 특성 연구 (Mechanical and Tribological Properties of $\alpha$-Sialon/SiC Whisker Composites)

  • 이병하;김인섭;이경희
    • 한국세라믹학회지
    • /
    • 제30권10호
    • /
    • pp.785-790
    • /
    • 1993
  • Sialon ceramics are presently seen as promising materials with high hardness, strength, fracture toughness and corrosion resistance for friction and wear applications. The objective of present work is to improve of mechanical properties and wear resistance of $\alpha$-Sialon(x=0.4) by addition of SiC whisker. $\alpha$-sialon(x=0.4)/SiC whisker composites were obtained by hot-isostatic pressing at 173$0^{\circ}C$ for 1 hour under 1757Kg/$\textrm{cm}^2$ N2 pressure after pressureless sintering the mixture of Si3N4, Y2O3, AlN at 1780~180$0^{\circ}C$ for 3~5 hours in N2 atmosphere. As the amount of SiC whisker content increased, relative density and hardness were decreased, however fracture toughness, bending strength and tribological properties were improved. Tribological properties of $\alpha$-Sialon/15 vol% SiC whisker composite were improved in spite of its low mechanical properties.

  • PDF

Microstructure, Mechanical and Wear Properties of Hot-pressed $Si_3N_4-TiB_2$ Composite

  • Kim, Hyun-Jin;Lee, Soo-Whon;Tadachika Nakayama;Koichi Niihara
    • The Korean Journal of Ceramics
    • /
    • 제5권4호
    • /
    • pp.324-330
    • /
    • 1999
  • $Si_3N_4$-$TiB_2$ with 2 wt% $Al_2O_3$ and 4 wt% $Y_2O_3$ additives was hot pressed in a flowing $N_2$ environment with varying $TiB_2$ content from 10 to 50 vol%. Variations of mechanical (hardness, fracture toughness, and flexual strength), and tribological properties as a function of $TiB_2$ content were investigated. As the content of $TiB_2$ increased, relative density decreased due to the chemical reaction of $TiB_2$in $N_2$ environment. The reduction of density causes mechanical properties to be degraded with an increase of $TiB_2$ in $Si_3N_4$. Tribological properties were dependent of microstructure as well as mechanical properties, however, they were degraded strongly by the chemical reaction of $Si_3N_4$-$TiB_2$ during hot pressing in $N_2$ environment. SEM and TEM observations, and X-ray diffraction analysis that the chemical reaction products at the interface are TiCN, Si, and $SiO_2$. Also, the comparison of XRD patterns of the $Si_3N_4$-40 vol% $TiB_2$ composites hot pressed at $1,750^{\circ}C$ for 1 hour between in $N_2$ and in Ar gas was made. The XRD peaks of Si and $SiO_2$ were not found in Ar, but still a weak peak of TiCN was presented.

  • PDF

액상소결 시의 β-SiC의 입자성장 방지 (Prevention of Grain Growth during the Liquid-Phase Assisted Sintering of β-SiC)

  • 길건영;노비얀토 알피안;한영환;윤당혁
    • 한국세라믹학회지
    • /
    • 제47권6호
    • /
    • pp.485-490
    • /
    • 2010
  • In our previous studies, continuous SiC fiber-reinforced SiC-matrix composites ($SiC_f$/SiC) had been fabricated by two different slurry infiltration methods: vacuum infiltration and electrophoretic deposition (EPD). 12 wt% of $Al_2O_3-Y_2O_3$-MgO with respect to SiC powder was used as additives for liquid-phase assisted sintering. After hot pressing at $1750^{\circ}C$ under 20 MPa for 2 h in Ar atmosphere, a high composite density could be achieved for both cases, whereas the problems such as large grain size and non-uniform distribution of liquid phase were observed, which was resulted in the relatively poor mechanical properties of composites. Therefore, efforts have been made to reduce the grain growth during the sintering, including the optimization for hot pressing condition and utilization of spark plasma sintering using a SiC monolith. Based on the results, spark plasma sintering was found to be effective method in decreasing the amount of sintering additive, time and grain growth, which will be explained in comparison to the results of hot pressing in this paper.

상온에서 작동되는 전고체전지 용 PEO/PPC 기반의 복합 고체 전해질 (PEO/PPC based Composite Solid Electrolyte for Room Temperature Operable All Solid-State Batteries)

  • 신소현;김성훈;조용현;안욱
    • 전기화학회지
    • /
    • 제25권3호
    • /
    • pp.105-112
    • /
    • 2022
  • 전고체전지의 상용화를 위해서는 상온에서 작동이 가능한 고체전해질 개발이 필수적이며 이온전도도가 높은 물질을 채택하여 전고체전지를 제조해야 한다. 따라서, 기존의 옥사이드 계열의 고체의 이온전도도를 높이기 위하여 이종원소가 도핑된 Li7La3Zr2O12 (LLZO)를 필러소재(Al, Nb-LLZO)로 사용하였으며, 상온에서 작동이 가능하도록 Poly(ethylene oxide)/Poly(propylene carbonate) (PEO/PPC) 기반의 가넷형 무기계 고체고분자 전해질을 제조하였다. 이원금속 원소를 도핑한 가넷형 무기계 필러와 PEO/PPC (1:1 비율로 섞인) 고분자를 1:2.4의 비율로 균일하게 교반하여 전해질을 합성해 상온과 60 ℃에서 전고체 전지의 전기학적 성능을 분석하였다. 제조한 복합 전해질은 이원금속의 도핑으로 인하여 이온전도도가 향상되었으며, PEO 단독으로 사용하는 전해질보다 PPC를 1:1로 첨가하였을 때 이온전도도 향상을 도와 60 ℃ 뿐만 아니라 상온에서 전고체 전지의 용량과 용량 유지율이 개선되었음을 확인하였다.

충남탄전, 대동누층군의 셰일과 탄질암에 관한 암석화학 및 환경지구화학적 특성 (Petrochemistry and Environmental Geochemistry of Shale and Coal from the Daedong Supergroup, Chungnam Coal Field, Korea)

  • 이찬희;이현구;김경웅
    • 자원환경지질
    • /
    • 제30권5호
    • /
    • pp.417-431
    • /
    • 1997
  • Characteristics of sedimentary rocks and enrichment of toxic elements in shale and coal from the Chungnam coal field were investigated based upon geochemistry of major, trace and rare earth elements. Shale and coal of the area are interbedded along the Traissic to the Jurassic Daedong Supergroup, which can be subdivided into grey shale, black shale and coal. The coal had been mined, however all the mines are abandonded due to the economic problems. The shale and coal are characterized by relatively low contents of $SiO_2$, and $Al_2O_3$ and high levels of loss-on-ignition (LOI), CaO and $Na_2O$ in comparison with the North American Shale Composite (NASC). Light rare earth elements (La, Ce, Yb and Lu) are highly enriched with the coal. Ratios of $Al_2O_3/Na_2O$ and $K_2O/Na_2O$ in shale and coal range from 30.0 to 351.8 and from 4.2 to 106.8, which have partly negative correlations against $SiO_2/Al_2O_3$ (1.24 to 6.06), respectively. Those are suggested that controls of mineral compositions in shale and coal can be due to substitution and migration of those elements by diagenesis and metamorphism. Shale and coal of the area may be deposited in terrestrial basin deduced from high C/S (39 to 895) and variable composition of organic carbon (0.39 to 18.40 wt.%) and low contents of reduced sulfur (0.01 to 0.05 wt.%). These shale and coal were originated from the high grade metamorphic and/or igneous rocks, and the rare earth elements of those rocks are slightly influenced with diagenesis and metamorphism on the basis of $Al_2O_3$ versus La, La against Ce, Zr versus Yb, the ratios of La/Ce (0.38 to 0.85) and Th/U (3.6 to 14.6). Characteristics of trace and rare earth elements as Co/Th (0.07 to 0.86), La/Sc (0.31 to 11.05), Se/Th (0.28 to 1.06), V/Ni (1.14 to 3.97), Cr/V (1.4 to 28.3), Ni/Co (2.12 to 8.00) and Zr/Hf (22.6~45.1) in the shale and coal argue for inefficient mixing of the simple source lithologies during sedimentation. These rocks also show much variation in $La_N/Yb_N$ (1.36 to 21.68), Th/Yb (3.5 to 20.0) and La/Th (0.31 to 7.89), and their origin is explained by derivation from a mixture of mainly acidic igneous and metamorphic rocks. Average concentrations in the shale and coal are As=7.2 and 7.5, Ba=913 and 974, Cr=500 and 145, Cu=20 and 26, Ni=38 and 35, Pb=30 and 36, and Zn=77 and 92 ppm, respectively, which are similar to those in the NASC. Average enrichment indices for major elements in the shale (0.79) and coal (0.77) are lower than those in the NASC. In addition, average enrichment index for rare earth elements in coal (2.39) is enriched rather than the shale (1.55). On the basis of the NASC, concentrations of minor and/or environmental toxic elements in the shale and coal were depleted of all the elements examined, excepting Cr, Pb, Rb and Th. Average enrichment indices of trace and/or potentially toxic elements (As, Cr, Cu, Ni, Pb, U and Zn) are 1.23 to 1.24 for shale and 1.06 to 1.22 for coal, respectively.

  • PDF

Densification Mechanism of NITE-SiC and $SiC_f/SiC$ Composites

  • 윤한기
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2006년 창립20주년기념 정기학술대회 및 국제워크샵
    • /
    • pp.181-184
    • /
    • 2006
  • Nano Infiltration Transient Eutectic Phase - Silicon Carbide (NITE-SiC) and $SiC_f/SiC$ composite have been fabricated by a Hot Pressing (HP) process, using SiC powder with an average size of about 30nm. Alumina ($Al_2O_3$) and Yttria ($Y_2O_3$) were used for additives materials. These mixed powders were sintered at the temperature a of $1300^{\circ}C$, $1650^{\circ}C$, $1800^{\circ}C$ and $1900^{\circ}C$ under an applied pressure of 20MPa. And unidirection and two dimension woven structures of $SiC_f/SiC$ composites were prepared starting from Tyranno SA fiber. Densification of microstructure gives an effect to density. Specially, Densification Mechanism basically is important from the sintering which use the HP. In this study, the densification of NITE-SiC and $SiC_f/SiC$ composite mechanism by a press displacement appears investigated. The mechanism on the densification of each sintering temperature was investigated. The each step is shows a with each other different mechanism quality.

  • PDF

A refined vibrational analysis of the FGM porous type beams resting on the silica aerogel substrate

  • Mohammad Khorasani;Luca Lampani;Abdelouahed Tounsi
    • Steel and Composite Structures
    • /
    • 제47권5호
    • /
    • pp.633-644
    • /
    • 2023
  • Taking a look at the previously published papers, it is revealed that there is a porosity index limitation (around 0.35) for the mechanical behavior analysis of the functionally graded porous (FGP) structures. Over mentioned magnitude of the porosity index, the elastic modulus falls below zero for some parts of the structure thickness. Therefore, the current paper is presented to analyze the vibrational behavior of the FGP Timoshenko beams (FGPTBs) using a novel refined formulation regardless of the porosity index magnitude. The silica aerogel foundation and various hydrothermal loadings are assumed as the source of external forces. To obtain the FGPTB's properties, the power law is hired, and employing Hamilton's principle in conjunction with Navier's solution method, the governing equations are extracted and solved. In the end, the impact of the various variables as different beam materials, elastic foundation parameters, and porosity index is captured and displayed. It is revealed that changing hygrothermal loading from non-linear toward uniform configuration results in non-dimensional frequency and stiffness pushing up. Also, Al - Al2O3 as the material composition of the beam and the porosity presence with the O pattern, provide more rigidity in comparison with using other materials and other types of porosity dispersion. The presented computational model in this paper hopes to help add more accuracy to the structures' analysis in high-tech industries.

상압소결 $SiC/Si_3N_4$ 복합체의 마찰마모특성 (Tribological properties of pressureless-sintered $SiC/Si_3N_4$ composites)

  • 백용혁;최웅;서영현;김인섭;김주영
    • 한국결정성장학회지
    • /
    • 제9권2호
    • /
    • pp.260-265
    • /
    • 1999
  • $\alpha$-SiC에 ${\alpha}-Si_3N_4$ 를 10~30 vol%까지 10 vol% 간격으로 혼합하고 소결 조제로$Al_2O_3$$Y_2O_3$를 각각 6wt% 로 첨가하여 $1,780^{\circ}C$에서 2시간동안 질소 분위기에서 상압소결하여 $Si_3N_4$ 복합체를 제조하였다. 상대 이론 밀도 및 꺽임 강도는 ${\alpha}-Si_3N_4$를 20 vol% 첨가하였을 때 92% 및 3,560 MPa로 가장 우수하였으며, 비마모량도 $2.68{\times}10^{-3}\;mm^2$ 으로 가장 작았다. 그리고, 파괴 인성$(K_{1c})$)은 ${\alpha}-Si_3N_4$를 30vol% 첨가하였을 때 $4.9\;MN/m^{3/2}$로 가장 좋았으나 이 경우 기공의 영향으로 내마모성은 저하된 것을 확인할 수 있었다.

  • PDF

용융침투법으로 제조한 유리-알루미나 복합체: Ⅰ. 알루미나 입도 효과 (Glass-alumina Composites Prepared by Melt-infiltration: Ⅰ. Effect of Alumina Particle Size)

  • 이득용;장주웅;김대준;박일석;이준강;이명현;김배연
    • 한국세라믹학회지
    • /
    • 제38권9호
    • /
    • pp.799-805
    • /
    • 2001
  • 상용 알루미나 분말(0.5${\mu}$m, 3${\mu}$m)을 die-press법을 이용하여 1120$^{\circ}$C에서 2시간 1차 소결하여 다공성 전성형체를 제조하고 1100$^{\circ}$C에서 4시간 $La_2O_3-Al_2O_3-SiO_2$계 유리를 용융 침투시켜 치밀한 유리-알루미나 복합체를 제조하였다. 알루미나 입도가 유리-알루미나 복합체의 충진율, 미세조직, 젖음성, 기공률 및 크기, 기계적 특성에 미치는 영향을 조사하였다. 입도 범위가 0.1∼48${\mu}$m로 넓고 bimodal size 입도 분포를 가지면서 random orientation을 가진 3${\mu}$m 알루미나가 분산된 복합체가 최적의 기계적 특성 및 충진률이 관찰되었으며 강도와 인성값은 각각 519MPa, $4.5MPa{\cdot}m^{1/2}$이었다.

  • PDF

자가치유성을 갖는 고분자개질 방수아스팔트-몬모릴로나이트 composite 제조: 2. 3-aminopropyltriethoxysilane에 의한 몬모릴로나이트(K-10)의 실란화 최적화 검증 (Preparation of Self-repairing Polymer-modified Waterproofing Asphalt-montmorillonite Composite: 2. Validation of Optimized Silylation of Montmorillonite (K-10) Using 3-aminopropyltriethoxysilane)

  • 이은주;이종훈;임광희
    • Korean Chemical Engineering Research
    • /
    • 제55권3호
    • /
    • pp.409-418
    • /
    • 2017
  • 자가치유성을 갖는 고분자개질 빙수아스팔트-몬모릴로나이트(MMT) composite 제조를 위하여 양이온($Na^+$)교환 처리된 K-10 (Na-MMT-K)에 대한 3-aminopropyltriethoxysilane (APS) 개질의 특성을 규명하고 적정개질조건을 FTIR, XRD, NMR 및 TGA 등의 분석을 통하여 제시되었다. APS 개질된 Na-MMT-K (S-Na-MMT-K)에 대한 FTIR 분석에서 실란화 반응과 관련된 실록산 결합(Si-O), 아민기, -$CH_2$- 및 -OH 기의 피크의 세기를 비교하였다. 그 결과로서 적정 반응시간, 적정교반시간, 적정농도 및 적정반응온도는 각각 2~3 h, 20 min, 7.5 w/v% 및 $50^{\circ}C$가 도출되었다. 또한 TGA 결과로부터 도출된 적정개질조건도 FTIR 분석에서 도출한 적정개질조건과 거의 일치하였다. 이 도출된 적정개질조건들은 Lee 등의 XRD 분석에서 제시된 기준(criterion)에 의해 도출된 적정반응시간, 적정교반시간, 적정 APS농도 및 적정반응온도와 거의 일치하였다. 따라서 XRD 분석에서 제시된 기준(criterion)이 검증되었다.