Study on Properties of Al2O3-TiO2 Composites by Wet Method I. Mechanical Properties of Al2O3-TiO2 Composites(2) (습식법에 의한 Al2O3-TiO2 복합체의 합성 및 특성연구 I. Al2O3-TiO2 복합체의 기계적 특성(2))

  • Ryu, Su-Chak
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.2
    • /
    • pp.153-158
    • /
    • 2002
  • $Al_2O_3$ composites powders with 1∼11 wt% $TiO_2$ were prepared by wet method and sintered at 1350$^{\circ}C$, 1450$^{\circ}C$ for 2h. Mechanical properties and microstructural evolution were investigated in this study. $Al_2O_3$-3 wt% $TiO_2$ composite were high bulk density of 2.37 g/$cm^3$ and low apparent porosity of 6.3%. The composites containing of 3 wt% $TiO_2$ showed moderately high bending strength of 68.9 MPa and the young's modulus of 35.5 MPa. The composites with increasing $TiO_2$ contents exhibit reduced thermal expansion coefficient due to the formation of $Al_2TiO_5$ phase.

A Study on CH4-SCR Reaction Characteristics of Mg-added Composite Alumina Pt Catalysts (Mg이 첨가된 복합 알루미나 Pt촉매의 CH4-SCR 반응특성에 관한 연구)

  • Won, Jong Min;Hong, Sung Chang
    • Applied Chemistry for Engineering
    • /
    • v.28 no.1
    • /
    • pp.87-94
    • /
    • 2017
  • In this study, a catalyst based on $Pt/Al_2O_3$ supported on Mg was prepared by a wet impregnation method to investigate the $CH_4-SCR$ reaction characteristics of various alumina supports. Alumina supported on $Pt/Al_2O_3$ catalyst was converted to an $Al_2O_3$ composite, and when Mg was added, oxygen species of the active metal Pt were controlled due to electrophobic characteristics. Oxygen-controlled Pt used as a reducing agent inhibited the oxidation of $CH_4$ to $CO_2$. The addition of Mg also promoted the adsorption of NO species and the conversion of NO to $NO_2$ due to the NOx storage property on the catalyst surface.

Microstructure and Mechanical Properties of $Ti_3Al-Nb$ Alloys and TiB(Ti-25Al-11Nb) Metal Matrix Composite Fabricated by Spark Plasma Sintering Process (방전플라즈마 소결법으로 제작된 $Ti_3Al-Nb$ 합금 및 TiB/(Ti-25Al-11Nb) 금속기 복합재료의 미세조직과 기계적 성질)

  • 이성열
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.27 no.1
    • /
    • pp.124-133
    • /
    • 2003
  • Ti-25Al-xNb (x=0, 3, 7, 11, 13 at. %) alloys and 18 vol. % TiB/(Ti-25Al-11Nb) metal matrix composite were fabricated by spark plasma sintering process at 900-120$0^{\circ}C$. Microstructural characteristics of the sintered bodies were identified by SEM, EDX analysis, X-ray diffraction, and differential scanning calorimeterric method. $Ti_3Al$ alloy was consisted of equiaxed $\alpha_2$ phase. $Ti_3Al-Nb$ alloys and the matix of TiB/(Ti-25Al-11Nb) metal matrix composite had the morphology that O phase was precipitated at the grain boundary of $\alpha_2$phase. Volume fraction of O phase and hardness were depended on the concentration of Nb in $Ti_3Al-Nb$ alloy, Rule of mixing could be applied to hardness and Young's modulus of 18 vol. % TiB/(Ti-25Al-11Nb) metal matrix composite.

Synthesis and Characterization of Al2O3/ZrO2, Al2O3/TiO2 and Al2O3/ZrO2/TiO2 Ceramic Composite Particles Prepared by Ultrasonic Spray Pyrolysis

  • Shim, In-Soo;Lee, Chang-Seop
    • Bulletin of the Korean Chemical Society
    • /
    • v.23 no.8
    • /
    • pp.1127-1134
    • /
    • 2002
  • Fine ceramic particles of zirconia toughened alumina (ZTA), titania toughened alumina (TTA), and zirconia-titania toughened alumina (ZTTA) have been synthesized by ultrasonic spray pyrolysis (USP) at various temperatures from starting salt solutio ns of various compositions aiming for the development of catalytic material. These particles were characterized for properties such as shape, size and size distribution, diffraction pattern, and chemical and phase composition of elements by scanning electron microscopy (SEM), particle size analyzer (PSA), x-ray diffraction (XRD), and inductively coupled plasma-atomic emission spectroscopy (ICP-AES). Chemical compositions and sizes of ceramic composites have been controled by the stoichiometry of salt solutions and the flow rate of spraying solutions. The optimum experimental conditions for the various composite particle syntheses have been proposed.

A Study on the Alumina Ceramic Composite Dispersed With the Zirconia (지르코니아-알루미나 세라믹 복합재료에 관한 연구)

  • Park, Jae-Sung;Lee, Yeong-Sin
    • 전자공학회논문지 IE
    • /
    • v.49 no.2
    • /
    • pp.1-8
    • /
    • 2012
  • The effects of the addition of either monoclinic $ZrO_2(pure)$ or tetragonal $ZrO_2$ containing 5.35wt% $Y_2O_3(Y-TZP)$ on the mechanical properties and thermal shock resistance of $Al_2O_3$ ceramics were investigated. The addition of $ZrO_2$(m) and Y-TZP increased sintered density of $Al_2O_3$. The Vickers hardness also increased as the volume fraction of Y-TZP increased going through a maximum at 20wt%. The hardness of the specimens was found to be dependent on the sintered density. The higher volume fraction of either $ZrO_2(m)$ or Y-TZP resulted in the higher fracture toughness of the composite was. This result may be taken as evidence that toughening of $Al_2O_3$ can be achieved by not only the transformation toughening but microcrack toughening of $ZrO_2$. The thermal shock property for $Al_2O_3-ZrO_2$ composites was improved by increasing the volume fraction of monoclinic $ZrO_2(pure)$. The grain size increased as the volume fraction of $ZrO_2$ did.

Thermal Characteristics of SiC Whisker Reinforced $Al_2$O$_3$-SiC Composite (SiC 휘스커 보강 $Al_2$O$_3$-SiC 복합체의 열간특성)

  • 김윤주;나용한
    • Journal of the Korean Ceramic Society
    • /
    • v.35 no.1
    • /
    • pp.1-4
    • /
    • 1998
  • SiC whisker reinforced Al2O3-SiC composite was fabricated by reaction synthesis method whish is cost ef-fective and allows good dispersion of whiskers. Fracture strength at room temperature showed the highest value with 150$0^{\circ}C$ reaction temperature because a lot of SiC whiskers was formed. Fracture strength at 135$0^{\circ}C$ did not show big differences with reaction temperature due to agglomeration of whiskers and formation of sil-icon oxynitride during hot MO(modulus of rupture) test probably promoting grain boundary sliding.

  • PDF

Mechanical Properties and Fabrication of Nanostructured Ti3Al-Al2O3 Composite from Mechanically Synthesized Powders by Pulsed Current Activated Sintering (기계적 합성된 분말로부터 펄스전류활성 소결에 의한 나노구조 Ti3Al-Al2O3 복합재료 제조 및 기계적 특성)

  • Shon, In-Jin;Wang, Hee-Ji;Suh, Chang-Yul;Cho, Sung-Wook;Kim, Wonbaek
    • Korean Journal of Metals and Materials
    • /
    • v.49 no.5
    • /
    • pp.374-379
    • /
    • 2011
  • Nano-powders of $Ti_3Al$ and $2Al_2O_3$ were synthesized from $3TiO_2$ and 5Al powders by high energy ball milling. A nanocrystalline $Al_2O_3$ reinforced composite was consolidated by pulsed current activated sintering within 2 minutes from mechanochemically synthesized powders of $Al_2O_3$ and $Ti_3Al$. Nanocrystalline materials, have received much attention as advanced engineering materials due to their improved physical and mechanical properties. The relative density of the composite was 99.5%. The average obtained hardness and fracture toughness values were 1510 kg/$mm^2$ and $9\;MPa{\cdot}m^{1/2}$, respectively.