Effects of Specimen Thickness and Notch Shape on Fracture Mode Appearing in Drop Weight Tear Test (DWTT) Specimens of API X70 and X80 Linepipe Steels (API X70 및 X80 라인파이프강의 DWTT 시편 파괴 형태에 미치는 시편 두께와 노치 형태의 영향)

  • Hong, Seokmin;Shin, Sang Yong;Lee, Sunghak;Kim, Nack J.
    • Korean Journal of Metals and Materials
    • /
    • v.48 no.8
    • /
    • pp.705-716
    • /
    • 2010
  • Effects of specimen thickness and notch shape on fracture mode appearing in drop weight tear test (DWTT) specimens of API X70 and X80 linepipe steels were investigated. Detailed microstructural analysis of fractured DWTT specimens showed that the fractures were initiated in normal cleavage mode near the specimen notch, and that some separations were observed at the center of the fracture surfaces. The Chevron-notch (CN) DWTT specimens had broader normal cleavage surfaces than the pressed-notch (PN) DWTT specimens. Larger inverse fracture surfaces appeared in the PN DWTT specimens because of the higher fracture initiation energy at the notch and the higher strain hardening in the hammer-impacted region. The number and length of separations were larger in the CN DWTT specimens than in the PN DWTT specimens, and increased with increasing specimen thickness due to the plane strain condition effect. As the test temperature decreased, the tendency to separations increased, but separations were not found when the cleavage fracture prevailed at very low temperatures. The DWTT test results, such as upper shelf energy and energy transition temperature, were discussed in relation with microstructures and fracture modes including cleavage fracture, shear fracture, inverse fracture, and separations.

General Fragmentations of Alkaloids in Electrospray Ionization Tandem Mass Spectrometry

  • Shim, Hee Jung;Lee, Ji Ye;Kim, Byungjoo;Hong, Jongki
    • Mass Spectrometry Letters
    • /
    • v.4 no.4
    • /
    • pp.79-82
    • /
    • 2013
  • Various types of alkaloids observed in several herbal medicines were analyzed by electrospray ionization tandem mass spectrometry in positive ion mode. In the present study, MS/MS spectralpatterns were investigated for eight-types of alkaloids (aporpine, protoberberine, tetrahydroprotoberberine, benzylisoquinoline, protopine, phthalide, morpine, and bisbenzylisoquinoline). For aporpine- and protoberberine-type alkaloids, main fragmentations occurred at substituted groups on rigid ring structures, not showing ring fusion. Interesting fragmentations due to iminolization and retro-Diels-Alder (RDA) reaction were observed in MS/MS spectra of protopine- and tetrahydroprotobereberine-type alkaloids. Also, several types of fragmentations such as inductive cleavage and ${\alpha}$-cleavage, or bond cleavage between two ring structures were observed depending on their structural characteristics. These fragmentation patterns are expected to allow instant classification of the specific alkaloid type in various MS/MS spectra of alkaloids.

The Effects of the Microstructures on the Fatigue Crack Propagation Behaviors of Cast Irons (주철의 피로전파거동에 미치는 미세조직의 영향)

  • Kim, Sug-Won;Park, Jin-Sung;Lee, Hyung-Chul;Kim, Dong-Keun;Woo, Kee-Do
    • Journal of Korea Foundry Society
    • /
    • v.25 no.1
    • /
    • pp.16-22
    • /
    • 2005
  • This study aims to investigate the effects of the microstructures and nodule type on the fatigue characteristics of cast iron. Fatigue tests were carried out in tension-tension mode using a servo-hydraulic testing machine with load control mode operating at a frequency of 15 Hz. The tests were conducted at stress ratio R=Kmin/Kmax, of 0.1. Initial crack ${\Dalta}K$ values were highly performed with increase in tensile strength of DCI fatigue specimens. ${\Dalta}K_{th}$ region, fatigue crack propagation was primarily advanced through cell boundary and in periphery of near nodule. Fatigue crack propagation rate of D2 consisted with 2Phase(Ferrite+Pearlite) was slow due to crack closure enhanced by crack deflection and occurred crack branching. The generation of crack branch was occurred due to interaction of crack-nodule. At Threshold and Paris zone, the fractographs of the fatigue fracture surface for DCI show typical striations of a ductile fracture and isolated cleavage planes near graphite. The effect of microstructure on fatigue crack propagation of GC strongly depends on the type of flake. The generation of crack branch occurred due to interaction of crack-nodule. The fractographs of the fatigue fracture surface for GC show cleavage plane along the flake graphite.

Effects of Cr, B, Ti and Si on Rolling Characteristics in Fe-30at.%A1 Alloy (Fe-30at.%A1 합금의 압연성에 미치는 Cr, B, Ti 및 Si 첨가효과)

  • Choi, Dap-Chun;Lee, Ji-Sung
    • Journal of Korea Foundry Society
    • /
    • v.23 no.2
    • /
    • pp.77-85
    • /
    • 2003
  • Some alloying elements such as Cr, B, Ti and Si were added individually or as a mixture to Fe-30 at.%Al alloys. The alloys were melted using an arc furnace and then heat-treated for homogenization at 1000$^{\circ}C$ for 7 days and followed by rolling at 1000$^{\circ}C$. The alloying elements on rolling characteristics were investigated by the microstructures and fracture mode before and after rolling. The microstructures before rolling showed that all of the alloys had equiaxed grains. On the other hand, the microstructures of rolling plane as well as its perpendicular plane became elongated after rolling. The alloys such as Fe-30Al, Fe-30Al-3Ti, Fe-30Al-0.5B, Fe-30Al-5Cr and Fe-30Al-3Ti-0.5B revealed better rolling behaviour from the point that intergranular and cleavage fractures were not fundamentally occurred. But the addition of 5Ti or 3Si to Fe-Al alloys had detrimental effects. The Ti-added alloy system such as Fe-30Al-5Ti, Fe-30Al-5Ti-5Cr, Fe-30Al-3Ti-5Cr and Fe-30Al-5Ti-0.5B were cracked through grain and showed cleavage fracture. The Si-added alloy system such as Fe-30Al-5Si, Fe-27Al-3Si and Fe-27Al-5Cr-3Si were cracked along the grain boundary and showed intergranular fracture. $DO_3{\leftrightarrow}B_2$ transition temperature of Fe-30at.%Al alloy was 520$^{\circ}C$, whereas the addition of 3Ti and 3Ti+0.5B comparably increased the temperature to 797 and 773$^{\circ}C$, respectively.

Brittle fracture analysis of the offset-crack DCDC specimen

  • Ayatollahi, M.R.;Bagherifard, S.
    • Structural Engineering and Mechanics
    • /
    • v.29 no.3
    • /
    • pp.301-310
    • /
    • 2008
  • Applications of fracture mechanics in the strength analysis of ceramic materials have been lately studied by many researchers. Various test specimens have been proposed in order to investigate the fracture resistance of cracked bodies under mixed mode conditions. Double Cleavage Drilled Compression (DCDC) specimen, with a hole offset from the centerline is a configuration that is frequently used in subcritical crack growth studies of ceramics and glasses. This specimen exhibits a strong crack path stability that is due to the strongly negative T-stress term. In this paper the maximum tensile stress (MTS) criterion is employed for investigating theoretically the initiation of brittle fracture in the DCDC specimen under mixed mode conditions. It is shown that the T-stress has a significant influence on the predicted fracture load and the crack initiation angle. The theoretical results suggest that brittle fracture in the DCDC specimen is controlled by a combination of the singular stresses (characterized by KI and KII) and the non-singular stress term, T-stress.

Structural, Electrochemical, DNA Binding and Cleavage Properties of Nickel(II) Complex [Ni(H2biim)2(H2O)2]2+ of 2,2'-Biimidazole

  • Jayamani, Arumugam;Thamilarasan, Vijayan;Ganesan, Venketasan;Sengottuvelan, Nallathambi
    • Bulletin of the Korean Chemical Society
    • /
    • v.34 no.12
    • /
    • pp.3695-3702
    • /
    • 2013
  • A nickel(II) complex $[Ni(H_2biim)_2(H_2O)_2](ClO_4)_2{\cdot}H_2O$ (1) of biimidazole ligand has been synthesized and characterized (Where $H_2biim$ = 2,2'-biimidazole). The single crystal X-ray diffraction of the complex shows a dimeric structure with six coordinated psudo-octahedral geometry. The cyclic voltammograms of complex exhibited one quasireversible reduction wave ($E_{pc}=-0.61V$) and an irreversible oxidation wave ($E_{pa}=1.28V$) in DMF solution. The interaction of the complex with Calf-Thymus DNA (CT-DNA) has been investigated by absorption and fluorescence spectroscopy. The complex is an avid DNA binder with a binding constant value of $1.03{\times}10^5M^{-1}$. The results suggest that the nickel(II) complex bind to CT-DNA via intercalative mode and can quench the fluorescence intensity of EB bind to CT-DNA with $K_{app}$ value of $3.2{\times}10^5M^{-1}$. The complex also shown efficient oxidative cleavage of supercoiled pBR322 DNA in the presence of hydrogen peroxide as oxidizing agent. The DNA cleavage by complex in presence of quenchers; viz. DMSO, KI, $NaN_3$ and EDTA reveals that hydroxyl radical or singlet oxygen mechanism is involved. The complex showed invitro antimicrobial activity against four bacteria and two fungi. The antimicrobial activity was nearer to that of standard drugs and greater than that of the free ligand.

The TRC Test for Cold Crack Susceptibility of Welded Zone for ABS EH32 Steel (인장구속 균열시험에 의한 ABS EH 32강 용접부 저온 균열 감수성 시험)

  • 정수원;박동환;김대헌
    • Journal of Welding and Joining
    • /
    • v.2 no.2
    • /
    • pp.62-69
    • /
    • 1984
  • In this study, cold crack susceptibility of high strength steel (ABS EH32 Steel) welded zone with shielded metal are welding was investigated by tensile restraint cracking test method. Effects of diffusible hydrogen content on root cracking, lower critical stress, crack initiation and fracture mode, hardness value distribution of welded zone and fractograph were mainly investigated. Following conclusions are made: 1. In the view of the lower critical stress level, wet electrode, containing much diffusible hydrogen content shows lower value than dried electrode. 2. Hardness value(Hv 5kg) in Heat Affected Zone of wet electrode is higher than that of dried electrode caused by hydrogen embrittlement. 3. In the case of wet electrode, root crack is initiated and propagated in Heat Affected Zone and then propagated to weld metal, but using of dried electrode, root crack is initiated in Heat Affected Zone and propagated to weld metal without propagating in HAZ. 4. For wet electrode, quasi-cleavage fracture mode is majorly observed on the fracture surface of HAZ and partially of weld metal due to hydrogen embrittlement.

  • PDF

Effects of temperature on the local fracture toughness behavior of Chinese SA508-III welded joint

  • Li, Xiangqing;Ding, Zhenyu;Liu, Chang;Bao, Shiyi;Qian, Hao;Xie, Yongcheng;Gao, Zengliang
    • Nuclear Engineering and Technology
    • /
    • v.52 no.8
    • /
    • pp.1732-1741
    • /
    • 2020
  • The structural integrity of welded joints in the reactor pressure vessel (RPV) is directly related to the safety of nuclear power plants. The RPV is made from SA508-III steel in a pressurized water reactor. In this study, we investigated the effects of temperature on the tensile and fracture toughness properties of Chinese SA508-III welded joint in different sampling areas in order to provide reference data for structural integrity assessments of RPVs. The specimens used in tensile and fracture toughness tests were fabricated from the base metal (BM), weld metal (WM), and the heat-affected zone (HAZ) in the welded joint. The representative testing temperatures included the ambient temperature (20 ℃), upper shelf temperature (100 ℃), and service temperature (320 ℃). The results showed that temperature greatly affected the fracture toughness (JIC) values for the SA508-III welded joint. The JIC values for BM and HAZ both decreased remarkably from 20 ℃ to 320 ℃. The fracture morphologies showed that the BM and HAZ in the welded joint exhibited fully ductile fracture at 20 ℃, whereas partial cleavage fracture was mixed in ductile fracture mode at 100 ℃ and 320 ℃. The WM exhibited the ductile and cleavage fracture mixed mode at various temperatures, and the JIC values showed slight changes.

Mode of Action on EcoRI Restriction Endonuclease: EcoRI and EcoRI Variant N199H have Active Monomeric Forms

  • Kim, Jae-Jong;Koh, Suk-Hoon;Kim, Joong-Su;Lee, Dae-Sil
    • BMB Reports
    • /
    • v.31 no.2
    • /
    • pp.149-155
    • /
    • 1998
  • The N199H variant of the EcoRI endonuclease has about twice the catalytic activity of the wild-type. A comparison of their biochemical characteristics, using synthetic oligonucleotides 5'-dAAAACTTAAGAAAAAAAAAAA-3' (KA) and 5'-dTTTTTGAATTCTTTTTTTTTT-3' (KT), helps to define the cleavage reaction pathway of these enzymes. Both EcoRI and EcoRI variant N199H were found to cleave singlestranded KA or KT about three times faster than the double-stranded forms, although the KT oligonucleotide was more susceptible. Using the ssDNA substrate in kinetic analyses, lower $K_m$ values were obtained for the N199H variant than for the wild-type at low (50 mM), as well as high (200 mM), sodium chloride concentrations. This difference between the endonucleases is attributed to a grealter accessibility for tbe substrate by the variant, and also a higher affinity for the DNA backbone. It also appears that the relative activities of the two enzymes, particularly at high ionic strength, are proportional to their populations in the monomeric enzyme form. That is, according to gel filtration data, half of the N199H molecules exist as monomers in 200 mM NaCl, whereas those of the wild-type are mainly dimeric. Consequently, the Asp199 residue of the EcoRI endonuclease may be implicated in the protein-protein interaction leading to dimerization, as well as in coupling to DNA substrates. In summary, it is proposed that active monomeric endonuclease molecules, derived from the dimeric enzyme, recognize and form a complex with a single stranded form of the DNA substrate, which then undergoes nucleophilic substitution and cleavage.

  • PDF

Microstructures and Mechnical Properties of Ni-Al-Fe Ternary Alloys (Ni-Al-Fe 3 원계합금의 미세조직 및 기계적 특성)

  • Choi, Dap-Chun;Bae, Dae-Sung
    • Journal of Korea Foundry Society
    • /
    • v.24 no.6
    • /
    • pp.356-365
    • /
    • 2004
  • Mechanical properties and microstructures of the Ni-AI-Fe and Ni-AI-Fe-(B, Zr) alloys which containing $10{\sim}30at$.%Fe, 0.1at.%B and/or 0.1at.%Zr have been investigated. The experimental results showed that the microstructures of Ni25Al were changed from a single phase ${\gamma}$ to dual phase ${\gamma}$ and ${\beta}$ by addition of 27at.%Fe. Ni45Al, however, kept the single ${\beta}$ phase even though Fe was added upto 30at.%. The hardness of Ni25Al were increased from $H_RB$ 70 to $H_RC$ 39 by addition of 27at.%Fe. In the case of Ni45Al which have $H_RC$ 37, the hardness was decreased by lOat.%Fe addition, but increased with 30at.%Fe. The yield strength and ultimate compressive strength in the compressive test have showed a similar trend with the hardness change. The strain to fracture was 14% at maximum and achieved in Ni25Al-27at.%Fe and Ni25Al-27at.%Fe-0.1 at.%B alloys. The Ni45Al showed a relatively low strain to fracture as 4%. The impact absorption energy of Ni25Al increased from 0.74 kg-m to 1.81 kg-m by addition of 27at.%Fe. In case of Ni45Al, the addition of lOat.%Fe and lOat.%Fe with small amounts of Band Zr did not change significantly the impact absorption energy of 0.60 kg-m, whereas the addition of 30at.%Fe with small amounts of B and Zr increased it slightly. In fracture tests, both of two basic materials showed the same intergranular fracture but by adding Fe it changed to the cleavage fracture mode or co-existing of cleavage and intergranular fractures.