Browse > Article
http://dx.doi.org/10.1016/j.net.2020.01.020

Effects of temperature on the local fracture toughness behavior of Chinese SA508-III welded joint  

Li, Xiangqing (Institute of Process Equipment and Control Engineering, Zhejiang University of Technology)
Ding, Zhenyu (Institute of Process Equipment and Control Engineering, Zhejiang University of Technology)
Liu, Chang (Shanghai Nuclear Engineering Research and Design Institute)
Bao, Shiyi (Institute of Process Equipment and Control Engineering, Zhejiang University of Technology)
Qian, Hao (Shanghai Nuclear Engineering Research and Design Institute)
Xie, Yongcheng (Shanghai Nuclear Engineering Research and Design Institute)
Gao, Zengliang (Institute of Process Equipment and Control Engineering, Zhejiang University of Technology)
Publication Information
Nuclear Engineering and Technology / v.52, no.8, 2020 , pp. 1732-1741 More about this Journal
Abstract
The structural integrity of welded joints in the reactor pressure vessel (RPV) is directly related to the safety of nuclear power plants. The RPV is made from SA508-III steel in a pressurized water reactor. In this study, we investigated the effects of temperature on the tensile and fracture toughness properties of Chinese SA508-III welded joint in different sampling areas in order to provide reference data for structural integrity assessments of RPVs. The specimens used in tensile and fracture toughness tests were fabricated from the base metal (BM), weld metal (WM), and the heat-affected zone (HAZ) in the welded joint. The representative testing temperatures included the ambient temperature (20 ℃), upper shelf temperature (100 ℃), and service temperature (320 ℃). The results showed that temperature greatly affected the fracture toughness (JIC) values for the SA508-III welded joint. The JIC values for BM and HAZ both decreased remarkably from 20 ℃ to 320 ℃. The fracture morphologies showed that the BM and HAZ in the welded joint exhibited fully ductile fracture at 20 ℃, whereas partial cleavage fracture was mixed in ductile fracture mode at 100 ℃ and 320 ℃. The WM exhibited the ductile and cleavage fracture mixed mode at various temperatures, and the JIC values showed slight changes.
Keywords
Elevated temperature; Fracture toughness; Reactor pressure vessel steel; Unified J-integral resistance curve; Welded joint;
Citations & Related Records
Times Cited By KSCI : 3  (Citation Analysis)
연도 인용수 순위
1 J. Hohe, D. Siegele, E. Bechler, G. Nagel, Standard and customized correlation of crack resistance curves and Charpy upper shelf energy for German reactor pressure vessel steels, Int. J. Pres. Ves. Pip. 134 (2015) 101-111.   DOI
2 C. Prasad, P. Bhuyan, C. Kaithwas, R. Saha, S. Mandal, Mandal, Microstructure engineering by dispersing nano-spheroid cementite in ultrafine-grained ferrite and its implications on strength-ductility relationship in high carbon steel, Mater. Des. 139 (2017) 324-335.   DOI
3 B. Younise, A. Sedmak, M. Rakin, N. Gubeljak, B. Medjo, M. Burzic, M. Zrilic, Micromechanical analysis of mechanical heterogeneity effect on the ductile tearing of weldments, Mater. Des. 37 (2012) 193-201.   DOI
4 S.G. Park, K.H. Lee, K.D. Min, B.S. Lee, Influence of the thermodynamic parameters on the temper embrittlement of SA508 Gr.4N Ni-Cr-Mo low alloy steel with variation of Ni, Cr and Mn contents, J. Nucl. Mater. 426 (2012) 1-8.   DOI
5 K. Karthick, S. Malarvizhi, V. Balasubramanian, S.A. Krishnan, G. Sasikala, S.K. Albert, Tensile and impact toughness properties of various regions of dissimilar joints of nuclear grade steels, Nucl. Eng. Technol. 50 (2018) 116-125.   DOI
6 L.F. Dong, Y.X. Zhong, Q.X. Ma, C.L. Yuan, L.S. Ma, Manufacturing technology of heavy cylinder forgings, Forg. Stamping Technol. 3 (2007), 000.
7 M.C. Kim, S.G. Park, K.H. Lee, B.S. Lee, Comparison of fracture properties in SA508 Gr.3 and Gr.4N high strength low alloy steels for advanced pressure vessel materials, Int. J. Pres. Ves. Pip. 131 (2015) 60-66.   DOI
8 N. Irvine, J. Francis, Nuclear Welding: Potential and Challenges for Lasers, 50 Years of Laser Cutting, 2017, p. 20.
9 M. Kirk, G. Stevens, M.A. Erickson, S. Yin, A proposal for the maximum KIC for use in, ASME Code Flaw and Fracture Toughness Evaluations 1 (2011) 985-994.
10 B. Houssin, J.P. Chavaillard, C. Coudert, Influence of temperature on tearing resistance of welds for PWR vessels, Nucl. Eng. Des. 87 (1985) 73-81.   DOI
11 S. Kumar, P.K. Singh, K.N. Karn, V. Bhasin, Experimental investigation of local tensile and fracture resistance behaviour of dissimilar metal weld joint: SA508 Gr. 3 Cl. 1 and SA312 Type 304LN, Fatig. Fract. Eng. Mater. Struct. 40 (2017) 190-206.   DOI
12 J. Xing, D. Song, Y. Wu, HPR 1000: advanced pressurized water reactor with active and passive safety, Eng. Times 2 (2016) 79-87.
13 J.W. Yang, S.Y. Li, M.L. Zhang, L.L. Wang, W.Y. Zhang, Welding Process and Welding Consumable of Generation III Nuclear Island Main Equipment, 2016, pp. 435-450.
14 A.F. Mark, J.A. Francis, H. Dai, M. Turski, P.R. Hurrell, S.K. Bate, J.R. Kornmeier, P.J. Withers, On the evolution of local material properties and residual stress in a three-pass SA508 steel weld, Acta Mater. 60 (2012) 3268-3278.   DOI
15 J.H. Liu, L. Wang, Y. Liu, X. Song, J. Luo, D. Yuan, Fracture toughness and fracture behavior of SA508-III steel at different temperatures, Int. J. Min. Met. Mater. 21 (2014) 1187-1195.   DOI
16 H.L. Ming, Z.M. Zhang, J.Q. Wang, E.H. Han, P.P. Wang, Z.Y. Sun, Microstructure of a safe-end dissimilar metal weld joint (SA508-52-316L) prepared by narrow-gap GTAW, Mater. Char. 123 (2017) 233-243.   DOI
17 H.T. Wang, G.Z. Wang, F.Z. Xuan, S.T. Tu, An experimental investigation of local fracture resistance and crack growth paths in a dissimilar metal welded joint, Mater. Des. 44 (2013) 179-189.   DOI
18 M.F. Yu, Y.J. Chao, Z. Luo, An assessment of mechanical properties of A508-3 steel used in Chinese nuclear reactor pressure vessels, J. Pressure Vessel Technol. 137 (2015), 031402.   DOI
19 J.H. Kim, E.P. Yoon, Notch position in the HAZ specimen of reactor pressure vessel steel, J. Nucl. Mater. 257 (1998) 303-308.   DOI
20 H.T. Wang, G.Z. Wang, F.Z. Xuan, S.T. Tu, Local mechanical properties of a dissimilar metal welded joint in nuclear power systems, Mater. Sci. Eng., A 568 (2013) 108-117.
21 J.W. Kim, K. Lee, J.S. Kim, T.S. Byun, Local mechanical properties of Alloy 82/182 dissimilar weld joint between SA508 Gr. 1a and F316 SS at RT and 320 C, J. Nucl. Mater. 384 (2009) 212-221.   DOI
22 B. Jeyaganesh, M.D. Callaghan, J.A. Francis, P.D. English, A. Vasileiou, M.J. Roy, W. Guo, N.M. Irvine, M.C. Smith, L. Li, A.H. Sherry, Overview of welding research under the new nuclear manufacturing, NNUMAN) Programme 6 (2014). V06BT06A076.
23 ASTM A508/A508M-2016, Standard Specification for Quenched and Tempered Vacuum-Treated Carbon and Alloy Steel Forgings for Pressure Vessels, United States: ASTM International, PA, 2016.
24 K.H. Lee, M.J. Jhung, M.C. Kim, B.S. Lee, Effects of temperature and PWHT on microstructures and mechanical properties of SA508 Gr.4N steel, Nucl. Eng. Technol. 46 (2014) 413-422.   DOI
25 ASTM E8/E8M-11, Standard Test Methods for Tension Testing of Metallic Materials, United States: ASTM International, PA, 2011.
26 ASTM E1820-13, Standard Test Method for Measurement of Fracture Toughness, United States: ASTM International, PA, 2013.
27 S. Kim, S.Y. Kang, S. Lee, J.H. Hong, Correlation of the microstructure and fracture toughness of the heat-affected zones of an SA508 steel, Metall. Mater. Trans. 31 (2000) 1107-1119.   DOI
28 G.F. Sun, Z.D. Wang, Y. Lu, R. Zhou, Z.H. Ni, Investigation on microstructure and mechanical properties of NV E690 steel joint by laser-MIG hybrid welding, Mater. Des. 127 (2017) 297-310.   DOI
29 H. Ming, Z. Zhang, J. Wang, E.H. Han, W. Ke, Microstructural characterization of an SA508-309L/308L-316L domestic dissimilar metal welded safe-end joint, Mater. Char. 97 (2014) 101-115.   DOI
30 H.L. Ming, R.L. Zhu, Z.M. Zhang, J.Q. Wang, E.H. Han, W. Ke, M.X. Su, Microstructure, local mechanical properties and stress corrosion cracking susceptibility of an SA508-52M-316LN safe-end dissimilar metal weld joint by GTAW, Mater. Sci. Eng., A 669 (2016) 279-290.
31 Y.T. Yang, C.H. Zhang, Z.N. Ding, C.H. Su, T.X. Yan, Y. Song, Y.G. Cheng, A correlation between micro- and nano-indentation on materials irradiated by high-energy heavy ions, J. Nucl. Mater. 498 (2018) 129-136.   DOI
32 S.G. Lee, S.S. Sohn, B. Kim, W.G. Kim, K.K. Um, S. Lee, Effects of martensiteaustenite constituent on crack initiation and propagation in inter-critical heat-affected zone of high-strength low-alloy (HSLA) steel, Mater. Sci. Eng., A 715 (2018) 332-339.