• 제목/요약/키워드: clad

검색결과 408건 처리시간 0.028초

Al 4343/3N03/4343 합금 3층 clad 재의 sagging 특성에 미치는 냉간압연조건의 영향 (Effect of cold rolling condition on sagging properties of Al 4343/3N03/4343 three-layer clad materials)

  • 김목순
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1999년도 춘계학술대회논문집
    • /
    • pp.157-160
    • /
    • 1999
  • Aluminum 4343(filler thickness ; 10${\mu}{\textrm}{m}$/Al 3N03(core 80${\mu}{\textrm}{m}$)/Al 4343(filler 10${\mu}{\textrm}{m}$) clad sheet which is recently developed as brazing sheet materials for automotive condensers was fabricated by castinglongrightarrowhot rollinglongrightarrowcold rollinglongrightarrowintermediate annealing(IA)longrightarrowfinal cold rolling(CR). and the effect of IA/CR conditions on microstructure and sagging resistance were investigated the sheet which were fabricated by optimum conditions (IA'ed at 42$0^{\circ}C$ followed by CR'ed to 20~45%) showed good sagging resistance because the core obtained a coarsely recrystallized grain structure during brazing and consequently inhibited filled alloy penetration into the core.

  • PDF

동복알루미늄의 내염특성 연구 (Study on Salt-Proof Characteristics of Copper Clad Aluminum)

  • 김진사;배덕권
    • 전기학회논문지
    • /
    • 제58권9호
    • /
    • pp.1764-1768
    • /
    • 2009
  • As the demand of electric power is increasing rapidly, the need of the compact and light electric power device is also increased. Copper clad aluminum (CCA) is newly proposed electrical conductor, because of its light-weight and low-cost characteristics, to replace the existing conductor made of copper. This paper presents the salt-proof characteristics of the copper clad aluminum (CCA) to certificate long time safe operation of the newly proposed electrical conductor. The two types of the CCA conductor were tested in the neutral salt spray tester. The experimental results of two types of the CCA with salt spray were presented in this paper. The results comprise resistance measured data, micro picture of the selected surface, and component measured data according to the elapsed time. The period of the experiment was 1,000 hours. There was no evidence to show the corrosion of CCA during the whole period of the experiments.

가요성 알루미늄피 케이블 (MCIF CABLE) 을 적용한 일체형 배선시스템 (IN-FLEX System Using Aluminum Clad Flex Cable (MCIF CABLE))

  • 구경완;전인석;문영재;이병용
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2007년도 춘계학술대회 논문집 전기설비전문위원
    • /
    • pp.58-60
    • /
    • 2007
  • This paper introduces the IN-FLEX system using aluminum clad flex cable, which is expected to alternate the conventional wiring method, such as, a steel pipe wiring method, and a synthetic resin pipe wiring method. The aluminum clad flex cable has a superior operation characteristics in heat dissipation property, in installation and maintenance facility, flammability, and appearance. Moreover, the IN-FLEX system adopted an easy connection mechanism which enable to reduce the time, hands and expense for the installation and maintenance of the system. Certification tests verifying the superior operation characteristics and reliability of the system using aluminum clad flex cable were carried with standard method in KOLAS certification institute.

  • PDF

(Ag-10 % Ni)/Cu 접점재의 냉간압연접합 (Cold Roll Bonding of (Ag-10% Ni)/Cu Clad Metals)

  • 김종헌;김성일;박상용
    • 소성∙가공
    • /
    • 제6권2호
    • /
    • pp.136-144
    • /
    • 1997
  • (Ag-10%Ni)/Cu clad metals for electric contact switch were fabricated by cold-roll bonding process. 2 or 3 passes of cold-rolling was carried out for each process to investigate the effect of the rolling passes on the bonding property. The effect of the annealing temperature of copper before the cold-roll bonding on the bond strength was also studied. The specimen bonded with copper annealed below 30$0^{\circ}C$ before roll bonding showed good bond strength. This is because high stored energy in copper promoted the short range diffusion and the grain refinement of copper by the static recrystallization increased the degree of the interfacial coherency. The maximum peel strength of clad metals bonded with Cu annealed below 30$0^{\circ}C$ was 120N.

  • PDF

Ti/STS409L/Ti 냉연 클래드재의 접합계면특성에 미치는 후열처리의 영향 (Effect of Post Heat Treatment on Bonding Interfaces in Ti/STS409L/Ti Cold Rolled Clad Materials)

  • 배동수;김원중;엄성찬;박준형;이상필;김민중;강창룡
    • 소성∙가공
    • /
    • 제20권2호
    • /
    • pp.140-145
    • /
    • 2011
  • The aim of the present study is to derive optimized post heat treatment temperatures to get a proper formability for Ti/STS409L/Ti clad materials. These clad materials were fabricated by cold rolling followed by a post heat treatment process for 10 minutes at temperatures ranging from $500^{\circ}C$ to $850^{\circ}C$. The microstructure of the interface was observed using a Scanning Electron Microscope(SEM) and an Energy Dispersive X-ray Analyser(EDX) in order to investigate the effects of post heat treatment on the bonding properties of the Ti/STS409L/Ti clad materials. Diffusion bonding was observed at the interfaces with a diffusion layer thickness increasing with the post heat treatment temperature. The diffusion layer was composed of a type of(${\varepsilon}+{\zeta}$) intermetallic compound containing additional elements, namely, Fe, Ti and Ni. The micro Knoop hardness of the Ti/STS409L interfaces was found to increase with heat treatment up to $800^{\circ}C$ and then decrease for temperatures rising up to $850^{\circ}C$. The tensile strength was shown to decrease for heat treatment temperature increasing to $750^{\circ}C$ and then increase rapidly for temperature rising up to $850^{\circ}C$. A post heat treatment temperature range of $700{\sim}750^{\circ}C$ was found to optimize the formability of Ti/STS409L/Ti clad materials.

3층 Cu/Al/Cu 클래드재의 열처리온도에 따른 변형 및 파단거동 (Effect of Heat Treatment on the Deformation and Fracture Behaviors of 3-ply Cu/Al/Cu Clad Metal)

  • 김인규;하종수;홍순익
    • 대한금속재료학회지
    • /
    • 제50권12호
    • /
    • pp.939-948
    • /
    • 2012
  • A 3-ply clad metal consisting of aluminum and copper was fabricated by roll bonding process and the microstructures and mechanical properties of the roll-bonded and post-roll-bonding heat treated Cu/Al/Cu clad metal were investigated. A brittle interfacial reaction layer formed at the Cu/Al interfaces at and above $400^{\circ}C$. The thickness of the reaction layer increased from $12{\mu}m$ at $400^{\circ}C$ to $28{\mu}m$ at $500^{\circ}C$. The stress-strain curves demonstrated that the strength decreased and the ductility increased with heat treatment up to $400^{\circ}C$. The clad metal heat treated at $300^{\circ}C$ with no indication of a reaction layer exhibited an excellent combination of the strength and ductility and no delamination of layers up to final fracture in the tensile testing. Above $400^{\circ}C$, the ductility decreased rasxpidly with little change of strength, reflecting the brittle nature of the intermetallic interlayers. In Cu/Al/Cu clad heat treated above $400^{\circ}C$, periodic parallel cracks perpendicular to the stress axis were observed at the interfacial reaction layer. In-situ optical microscopic observation revealed that cracks were formed in the Cu layer due to the strain concentration in the vicinity of horizontal cracks in the intermetallic layer, promoting the premature fracture of Cu layer. Vertical cracks parallel to the stress axis were also formed at 15% strain at $500^{\circ}C$, leading to the delamination of the Cu and Al layers.

STS/Al/Cu 클래드재의 파괴거동 및 기계적 물성에 미치는 인장시험 온도의 영향 (Effect of Tension-Test Temperature on Fracture Behavior and Mechanical Properties in STS/Al/Cu Clad Materials)

  • 배동현;최영준;정원섭;배동수;조영래
    • 대한금속재료학회지
    • /
    • 제47권12호
    • /
    • pp.811-818
    • /
    • 2009
  • In order to meet increasingly complex and rigorous technical specifications, extensive effort has been devoted to fabricate clad materials with multi-layered metal plates. In this study, novel stainless steel/aluminum/copper (STS/Al/Cu) three-ply clad materials were fabricated by a hot rolling process for cookware applications. The effect of the testing temperature on the mechanical properties of the clad materials and on each component metal was investigated during the tensile tests. The interface properties of the clad materials were also examined by optical microscopy (OM) and an electron probe micro-analyzer (EPMA). The best mechanical and interfacial properties for a warm working process were found in a sample annealed at a temperature of $300^{\circ}C$. For the sample annealed at $400^{\circ}C$, the results of the tensile test indicated that interface delamination occurred only in the region of the Al/Cu interfaces. This was due to the formation of the thick and brittle intermetallic compound of $Al_2Cu$ in the Al/Cu interface. In contrast, no interface delamination was observed in the STS/Al interface, most likely due to its strong bond strength.