• 제목/요약/키워드: chitosan-catechol polymer

검색결과 4건 처리시간 0.019초

키토산-카테콜 하이드로겔의 카테콜 함유량에 따른 유변학적 특성 분석 (Rheological Characteristics of Chitosan-Catechol Hydrogel attributed Catechol Content)

  • 방은지;고혜민
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2022년도 가을 학술논문 발표대회
    • /
    • pp.249-250
    • /
    • 2022
  • In this study, two types of chitosan-catechol polymers (a-CP and b-CP) were synthesized and mixed with polyvinyl alcohol (PVA) and sodium tetraborate decahydrate (Na2B4O7·10H2O) to form hydrogels. The characteristics of these polymers were tuned by varying the pH during their syntheses, and their structures were characterized using nuclear magnetic resonance spectroscopy and ultraviolet-visible spectroscopy. Rheological and self-healing properties of hydrogels were evaluated. As a result, the viscoelastic modulus was improved due to the increased functional group content, and the self-healing property was excellent regardless of the functional group content.

  • PDF

생체모방 폴리머의 구조 분석 및 폴리머 혼입율에 따른 시멘트 모르타르의 특성 변화 (Strength, Carbonation Resistance, and Chloride-Ion Penetrability of Cement Mortars Containing Catechol-Functionalized Chitosan Polymer)

  • 방은지;최세진;고혜민
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2022년도 봄 학술논문 발표대회
    • /
    • pp.253-254
    • /
    • 2022
  • In this study, catechol-functionalized chitosan (Cat-Chit), a well-known bioinspired polymer that imitates the basic structures and functions of living organisms and biological materials in nature, was synthesized and combined with cement mortar in various proportions. The compressive strength, tensile strength, drying shrinkage, accelerated carbonation depth, and chloride-ion penetrability of these mixes were then evaluated. In the ultraviolet-visible spectra, a maximum absorption peak appeared at 280 nm, corresponding to catechol conjugation. The sample containing 7.5% Cat-Chit polymer in water (CPW) exhibited the highest compressive strength, and its 28-day compressive strength was ~20.2% higher than that of a control sample with no added polymer. The tensile strength of the samples containing 5% or more CPW was ~2.3-11.5% higher than that of the control sample. Additionally, all the Cat-Chit polymer mixtures exhibited lower carbonation depths than compared to the control sample. The total charge passing through the samples decreased as the amount of CPW increased. Thus, incorporating this polymer effectively improved the mechanical properties, carbonation resistance, and chloride-ion penetration resistance of cement mortar.

  • PDF

혼합슬래그 잔골재 혼입율에 따른 생체모방 폴리머 혼입 모르타르의 유동성 및 공학적 특성 (Fluidity and engineering properties of mortar mixed with bioinspired polymer according to mixing ratio of mixed slag fine aggregate.)

  • 배성호;박사민;김대성;이재인;고혜민;최세진
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2022년도 봄 학술논문 발표대회
    • /
    • pp.259-260
    • /
    • 2022
  • In this study, as part of a study to solve the problem of aggregate supply and demand, blast furnace slag fine aggregate and ferronickel slag fine aggregate were used as substitutes for natural fine aggregate, and a bioinspired polymer, a catechol-functionalized chitosan, was used instead of the mixing water.

  • PDF

생체모방 폴리머 혼입율에 따른 모르타르의 강도 특성에 관한 실험적 연구 (An Experimental Study on the Strength Characteristics of Mortar according to the Incorporation Rate of Bioinspired Polymer)

  • 이재인;배성호;김채영;윤주호;고혜민;최세진
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2022년도 봄 학술논문 발표대회
    • /
    • pp.257-258
    • /
    • 2022
  • In this study, as a part of the study to alleviate the durability degradation due to low tensile performance and cracking of concrete, two kinds of catechol functional chitosan (Cat-Chit) were replaced at a ratio of 5, 10, 15, 20% as a mixed water substitute to evaluate the fluidility and strength characteristics of mortar.

  • PDF