Electrooxidation of Zolpidem and its Voltammetric Quantification in Standard and Pharmaceutical Formulation using Pencil Graphite Electrode

  • Naeemy, A.;Sedighi, E.;Mohammadi, A.
    • Journal of Electrochemical Science and Technology
    • /
    • v.7 no.1
    • /
    • pp.68-75
    • /
    • 2016
  • In this study a new, simple, precise, accurate and economic electrochemical method was developed and validated for the voltammetric determination of zolpidem (ZP) using disposable pencil graphite (PG) electrode. The anodic oxidation of ZP on the surface of the PG electrode was examined in a britton robinson (BR) buffer. Square wave and cyclic voltammetry were used as electrochemical techniques in the potential range of 0-1.2 V in the pH 8 BR buffer. In cyclic voltammetry studies, the diffusion coefficient of ZP oxidation was found to be 3.6×10-6 cm2 s-1. On the other hand, the ZP has shown a well-defined irreversible anodic peak at 0.98 V in the square wave voltammetry mode. The PG electrode, primarily being graphite which has a large active surface area gives rise to increasing peak current with respect to ZP electrooxidation. PG electrode showed an electrocatalytic effect in anodic oxidation of ZP. A linear relationship between catalytic current response and ZP concentration was obtained over a concentration range of 10-30 μM with R.S.D. values ranging from 0.29-3.89. Limits of detection and quantitation were found to be 1 and 3 μM, respectively. Finally, the PG electrode was successfully used to determine ZP in standard and tablet dosage forms with a mean recovery of 100.69 %.

Cyclic voltammetry characteristics of $MnO_2$ electrode mixed with PVDF in sulfuric acid solution (PVDF로 혼합된 $MnO_2$ 전극의 황산 수용액중의 cyclic voltammetry 특성)

  • Kim, Bong-Seo;Lee, Dong-Yoon;Lee, Hee-Woong;Kim, Hyun-Sik;Lee, Hae-Yon;Chung, Won-Sub
    • Proceedings of the KIEE Conference
    • /
    • 2002.11a
    • /
    • pp.82-84
    • /
    • 2002
  • Dimensionally stable anode(DSA) can be used for the electrowinning of non-ferrous metal like as a Zn, and electrolysis of sea water. $MnO_2$ electrode satisfies the requirements of DSA, and has a good cycle life and a low overpotential for oxygen evolution. $MnO_2$ electrodes coated with DMF and PVDF based on Pb alloy produced at several compositions and dry temperatures. The viscosity of solvent used as a binder of $MnO_2$ powder increased with the increasing PVDF contents. When the ratio of PVDF to BMF with the 5 times dipping at the solution mixed with PVDF and DMF was 1/9, the coating thickness was $150{\mu}m$. When the ratio of PVDF to $MnO_2$ was lower than 1/6, the electrode didn't show any reaction irrespective of the concentrations of DMF. However, When the ratio of PVDF to $MnO_2$ was higher than 1/6, the electrode showed a constant current reactions and homogeneous cyclic voltammetry even though at a high cycle. The reason for the high current and homogeneous cyclic voltammetry is the good catalytic reactions of $MnO_2$ powder in electrode. The reactions of Pb electrode coated with $MnO_2$ and PVDF based on the pure Pb electrode.

  • PDF

Dynamics Study with DFT(Density Functional Theory) Calculation for Metal with a few Peripheral Electrons (범밀도함수론을 이용한 백금, 팔라듐, 니켈, 크롬과 수소반응성 연구)

  • Kim, Taewan;Park, Taesung;Jung, Yeonsung;Kang, Youngjin;Lee, Taeckhong
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.25 no.3
    • /
    • pp.234-239
    • /
    • 2014
  • To study catalytic activity and hydrogen embrittlement of Pd, Pt, Ni, and Cr in fuel cell electrode, we used density-functional theory. The calculation tools based electron density give much shorter calculation time and cheap costs. Maximum of bond overlap populations of each metal are 0.6539eV for Pd-H, 0.6711eV for Pt-H, 0.6323eV for Ni-H, 0.6152eV for Cr-H. Electron density of Cr has strongest in related metals, which shows strong localization of electron, implying anti hydrogen embrittlement behaviors.

Improved Reduction of Carbon Monoxide by Highly Efficient Catalytic Shift for Fuel Cell Applications

  • Youn, M.J.;Chun, Y.N.
    • Environmental Engineering Research
    • /
    • v.13 no.4
    • /
    • pp.192-196
    • /
    • 2008
  • The generation of high purity hydrogen from reformed hydrocarbon fuels, or syngas, is essential for efficient operation of the fuel cell (PEMFC, Polymer Electrolyte Membrane Fuel Cell). Usually, major components of reformed gas are $H_2$, CO, $CO_2$ and $H_2O$. Especially a major component, CO poisons the electrode of fuel cells. The water gas shifter (WGS) that shifts CO to $CO_2$ and simultaneously produces $H_2$, was developed to a two stage catalytic conversion process involving a high temperature shifter (HTS) and a low temperature shifter (LTS). Also, experiments were carried out to reduce the carbon monoxide up to $3{\sim}4%$ in the HTS and lower than 5,000 ppm via the LTS.

A study of decomposition of sulfur oxides using Calcium hydroxide catalyst by plasma reactions (Ca(OH)2촉매를 이용한 플라즈마 반응에 의한 황산화물의 제거에 관한 연구)

  • Kim, Da Young;Woo, In Sung;Lee, Sun Hee;Kim, Do Hyeon;Kim, Byeong Cheol
    • Proceedings of the Safety Management and Science Conference
    • /
    • 2013.11a
    • /
    • pp.547-560
    • /
    • 2013
  • In this study, the air pollutant removal such as sulfur oxides was studied. A combination of the plasma discharge in the reactor by the reaction surface discharge reactor Calcium hydroxides catalytic reactor and air pollutants, hazardous gas SOx, changes in gas concentration, change in frequency, the thickness of the electrode, kinds of electrodes and the addition of simulated composite catalyst composed of a variety of gases, including decomposition experiments were performed by varying the process parameters. The experimental results showed the removal efficiency of 98% in the decomposition of sulfur oxides removal experiment when Calcium hydroxides catalysts and the tungsten(W) electrodes were used. It was increased 3% more than if you do not have the catalytic. If added to methane gas was added the removal efficiency increased decomposition.

  • PDF

Catalytic Effects of Barium Carbonate on the Anodic Performance of Solid Oxide Fuel Cells

  • Yoon, Sung-Eun;Ahn, Jae-Yeong;Park, Jong-Sung
    • Journal of the Korean Ceramic Society
    • /
    • v.52 no.5
    • /
    • pp.350-355
    • /
    • 2015
  • To develop ceramic composite anodes of solid oxide fuel cells without metal catalysts, a small amount of barium carbonate was added to an $(La_{0.8}Sr_{0.2})(Cr_{0.5}Mn_{0.5})O_3(LSCM)$ - YSZ ceramic composite anode and its catalytic effects on the electrode performance were investigated. A barium precursor solution with citric acid was used to synthesize the barium carbonate during ignition, while a barium precursor solution without citric acid was used to create hydrated barium hydroxide. The addition of barium carbonate to the ceramic composite anode caused stable fuel cell performance at 1073 K; this performance was higher than that of a fuel cell with $CeO_2$ catalyst; however, the addition of hydrated barium hydroxide to the ceramic composite anode caused poor stability of the fuel cell performance.

A study on the electrochemical reduction of carbon dioxide (전기화학환원에 의한 이산화탄소의 수소화 반응연구)

  • Sim, Kyu-Sung;Kim, Jong-Won;Kim, Yeon-Soon;Myeong, Kwang-Sik
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.9 no.1
    • /
    • pp.8-15
    • /
    • 1998
  • The catalytic hydrogenation of carbon dioxide has been studied for the fixation of carbon dioxide to mitigate global warming problems, but it needed hydrogen, which the price is still high. Recently, the electrochemical reduction of carbon dioxide has been drawn attractions because carbon dioxide could be converted to the valuable chemicals such as methane, ethane and alcohols electrochemically in the electrolyte solution using a catalytic electrode. This system is simple because the water electrolysis and hydrogenation take place at the same time using the surplus electricity at midnight. In this work, a continuous electrochemical reduction system was fabricated, which was composed of the reduction electrode (copper or perovskite type, $2{\times}2cm^2$), reference electrode(platinum, $2{\times}6cm^2$), standard electrode(Ag/AgCl), and potassium bicarbonate electrolyte solution saturated with carbon dioxide. The quality and quantity of the products and reduction current were analyzed, according to the electrolyte concentration and electrode type.

  • PDF

Synthesis of Pt-$MoO_3$ Electrode by Electrodeposition Method for Direct Methanol Fuel Cell (전기화학적 증착법에 의한 직접 메탄올 연료전지(DMFC)용 백금-삼산화몰리브테늄 전극제조)

  • Shin, Ju-Kyung;Jung, So-Mi;Baeck, Sung-Hyeon;Tak, Yong-Suk
    • Applied Chemistry for Engineering
    • /
    • v.21 no.4
    • /
    • pp.435-439
    • /
    • 2010
  • Pt-$MoO_3$ electrodes were fabricated on ITO-coated glass by electrodeposition method using 20 mM hydrogen hexachloroplatinate ($H_2PtCl_6$) and 10 mM Mo-peroxo electrolyte. Deposition order was varied, and catalytic activities of synthesized electrodes were compared with that of pure Pt electrode. Scanning Electron Microscopy (SEM) was utilized to examine surface morphology. The crystallinity of synthesized films was analyzed by X-ray Diffraction (XRD), and the oxidation state of both the platinum and molybdenum were determined by X-ray Photoelectron Spectroscopy (XPS) analyses. The catalytic activity and stability for methanol oxidation were measured using cyclic voltammetry (CV) and chronoamperometry (CA) in a mixture of 0.5 M $H_2SO_4$ and 0.5 M $CH_3OH$ aqueous solution. $MoO_3$ electrodeposited on the surface of Pt showed much higher catalytic acitivity and stability than pure Pt electrode due to the good contact between Pt and $MoO_3$.

Characterization of immobilized laccase and its catalytic activities (고정된 laccase의 특성 및 촉매효과)

  • Hyung Kyung Hee;Shin Woonsup
    • Journal of the Korean Electrochemical Society
    • /
    • v.2 no.1
    • /
    • pp.31-37
    • /
    • 1999
  • Copper-containig enzyme, laccase (Rhus vernicifera) was immobilized onto gold electrode using self-assembly technique and its surface properties and catalytic activities were examined. Laccase is an oxidoreductase capable to oxidize diphenols or diamines by 4-electron reduction of molecular oxygen without superoxide or peroxide intermediates. The electrode surface were modified by $\beta-mercaptopropionate$ to have a net negative charge in neutral solution and positively charged laccase (pI=9) was immobilized by electrostatic interaction. The successful immobilization was confirmed by cyclic voltammograms which showed typical surface-confined shapes and behaviors. The amount of charge to reduce the surface was similar to the charge calculated assuming the surface being covered by monolayer. The activity of the immobilized enzyme was tested by the capbility of oxidizing a substrate, ABTS (2,2-azine-bis-(3-ethylbenzthioline-6-sulfonic acid) and it was maintained for $2\~3$ days at $4^{\circ}C$. The immobilzed laccase showed about $10\~15\%$ activity compared to that in solution. The laccase-modified electrode showed the activity of elefoocatalytic reduction of oxygen in the presence of mediator, $Fe(CN)_6^{3-}$ The addtion of azide which is an inhibitor of laccase compeletly eliminated the catalytic current.

Degradation of Ferroelectric Properties of Pt/PZT/Pt Capacitors in Hydrogen-containing Environment

  • Kim, Dong-Chun;Lee, Won-Jong
    • Transactions on Electrical and Electronic Materials
    • /
    • v.6 no.5
    • /
    • pp.214-220
    • /
    • 2005
  • The ferroelectric properties of the $Pt/PZT(Pb(Zr,Ti)O_3)/Pt$ capacitors are severely degraded when they are annealed in hydrogen-containing environment. Hydrogen atoms created by the catalytic reaction of Pt top electrode during annealing in hydrogen ambient penetrate into PZT films and generate oxygen vacancies by the reduction of the PZT films, which is likely to cause the degradation. The degree of hydrogen-induced degradation and the direction of voltage shift in P-E curves of the pre-poled PZT capacitors after annealing in hydrogen ambient is dependent on the polarity of the pre-poling voltage. This implies that oxygen vacancies causing hydrogen induced degradation are generated by hydrogen ions having a polarity. The degraded ferroelectricity of the PZT capacitors can be effectively recovered by the shift of oxygen vacancies toward the Pt top electrode interface during post-annealing in oxygen environment with applying negative unipolar stressing.