A Electrical Characteristics of Disk-type Piezotransformer with Electrode Ratio of Driving and Generating Part (디스크형 압전변압기의 전극비에 따른 전기적 특성)

  • 이종필;채홍인;정수현;홍진웅
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.52 no.10
    • /
    • pp.458-463
    • /
    • 2003
  • In order to develope piezoelectric transformer for the ballast of fluorescent lamp, a new shape and electrode pattern of piezoelectric transformer has been investigated in this work. The composition of piezoelectric ceramics was 0.95Pb(Zr$_{0.51}$Ti$_{0.49}$)O$_3$+0.03Pb(Mn$_{1}$3/Nb$_{2}$3/)O$_3$+0.02Pb(Sb$_{1}$2/Nb$_{1}$2/)O$_3$. The sample prepared by this composition system showed the characteristics which has about 1200 of relative dielecric constant, 1100 of the mechanical quality factor, 0.53 of the electromechanical coupling coefficient, 320 pC/N of the piezoelectric constant d$_{33}$, 0.3 % of the dissipation factor. Diameter and thickness of disk-type piezoelectric transformer was 45 mm and 4 mm, respectively. The driving and generating electrode with their gap of 1mm were fabricated on the top surface. But the common electrode was fabricated on the whole bottom surface. The electrode surface ratio of driving and generating part on the top surface ranges from 1.4:1 to 3:1. We investigated the electrical characteristics with the variation of the electrode surface ratio of driving and generating part in the range of load resistance of 100 $\Omega$~70 k$\Omega$. The set-up voltage ratio of this piezoelectric transformer increases with increasing both the electrode surface of driving part and the load resistance. The set-up voltage ratio at no load resistance was more than 60 times. On the other hand, the efficiency decreases with increasing the electrode surface of driving part. In the case of the electrode surface of both 1.4:1 and 2:1, maximum efficiency showed above 97 % at load resistance of 2 k$\Omega$. However, in the case of the electrode surface of 3:1, maximum efficiency showed about 94 % at load resistance of 3 k$\Omega$.>.>.>.

A Study on the Mechanism with the Electrode Ratio of Driving and Generation Part of a Disk-Type Piezoelectric Transformer (디스크형 압전변압기의 전극 면적비에 따른 구동 메카니즘에 관한 연구)

  • Lee, Jong-Pil;Chae, Hong-In;Jin, Woong-Hong
    • Journal of the Korean Institute of Illuminating and Electrical Installation Engineers
    • /
    • v.19 no.5
    • /
    • pp.17-22
    • /
    • 2005
  • In this study, a disk-type piezoelectric transformer was fabricated. Its diameter was 50[mm] and thickness was 4.5[mm]. The driving and generating electrode with their gap of 1[mm] were fabricated on the top surface. But the common electrode was fabricated on the whole bottom surface. The electrode surface ratio of driving and generating part on the top surface was the range of 1.4:1 to 3:1. We investigated the electrical characteristics with the variation of its thickness and the electrode surface ratio of driving and generating part in the range of load resistance of 100${[\Omega]}\~70{[k\Omega]}$.. Form the experimental results, their influence on the set-up voltage ratio were investigated quantitively and qualitatively.

Improved Vertically-Aligned Nematic Mode for High Performance Displays

  • Jhun, Chul Gyu;Gwag, Jin Seog
    • Journal of the Optical Society of Korea
    • /
    • v.18 no.6
    • /
    • pp.783-787
    • /
    • 2014
  • This paper presents an improved vertical alignment nematic liquid crystal mode characterized by the protrusions or slits of the top substrate and additional stripe type common electrodes with polarity switching of the bottom substrate to improve multi-domain vertically aligned (MVA) and patterned vertically aligned (PVA) nematic modes. MVA and PVA modes have disadvantages such as an LC disclination in the vicinity of the middle region of electrodes between the top and bottom protrusions in MVA mode or the top and bottom slits in PVA mode. Therefore, the stripe type common electrode generating a horizontal electric field and the protrusion or slit producing some pretilt of liquid crystals (LCs) were used to improve the LC disclination, which influences the transmittance and response speed. The simulation results showed that the proposed VA mode has higher transmittance than the MVA and PVA modes. As a result, the proposed VA mode can improve the response speed and transmittance remarkably, which makes it useful for upgrading the LCD display quality.

Aluminum Based Oxide/Metal/Oxide Structures for the Application in Transparent Electrodes (알루미늄 기반 Oxide/Metal/Oxide 구조의 투명전극 적용성 기초 연구)

  • Kim, Daekyun;Choi, Dooho
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.31 no.7
    • /
    • pp.481-485
    • /
    • 2018
  • In this study, oxide/metal/oxide-type transparent electrodes based on Al and ZnO were investigated. Thin films of these materials were sputter-deposited at room temperature. To evaluate the thickness dependence of the oxide layers, the top and bottom ZnO layers were varied in the range of 5~80 nm and 2.5~20 nm, respectively. When the thicknesses of the top and bottom ZnO layers were fixed at 30 nm and 2.5 nm, a maximum transmitance of 66% and sheet resistance of $16.5{\Omega}/{\square}$ were achieved, which is significantly improved compared with the Al layer without top and bottom ZnO layers showing a maximum transmitance of 44.3% and sheet resistance of $44{\Omega}/{\square}$.

Electric properties of DLC Emitter (DLC Emitter 전기적 특성)

  • Lee, Sang-Heon
    • Proceedings of the KIEE Conference
    • /
    • 2009.07a
    • /
    • pp.1312_1313
    • /
    • 2009
  • In this study the fabrication technique of the planner field emission device structure with a DLC layer were studied. The bottom Mo electrode using electrochemical method on the DLC layer deposited using assist sputtering.