  • We have developed a novel crystallization process, where the crystallization temperature is lowered compared to the conventional RTA process and the metal contamination is lowered compared to the conventional VIC process. A very-thin a-Si film was deposited and crystallized at $550^{\circ}C$ for 3 h by the VIC process and then a thick a-Si film was deposited and crystallized by the RTA process at $680^{\circ}C$ for 5 min using the VIC poly-Si layer as a crystallization seed layer. The RTA crystallized temperature could be lowered up to $50^{\circ}C$, compared to RTA process alone. The poly-Si film appeared a needle-like growth front and relatively well-arranged (111) orientation. In addition, the Ni concentration in the poly-Si film was lowered to $3{\times}10^{17}\;cm^{-3}$ and that at the poly-Si/$SiO_2$ interface was lowered to $5{\times}10^{19}\;cm^{-3}$. The reduction in metal contamination could be greatly helpful to achieve a low leakage current in poly-Si TFT, which is the critical parameter for commercialization of AMOLED.

  • PDF

LCD 연구 개발 동향

  • 이종천
    • 전자공학회지
    • /
    • 제29권6호
    • /
    • pp.76-80
    • /
    • 2002
  • 'Liquid Crystal의 상전이(相轉移)와 광학적 이방성(異方性)이 1888년과 1889년 F. Reinitzer와 O. Lehmann에 의해 Monatsch Chem.과 Z.Physikal.Chem.에 각각 보고된 후 부터 제2차 세계대전이 끝난 뒤인 1950년대 까지는 Liquid Crystal을 단지실험실에서의 기초학문 차원의 연구 대상으로만 다루어 왔다. 1963년 Williams가 Liquid Crystal Device로는 최초로 특허 출원을 하였으며, 1968년 RCA사의 Heilmeier등은 Nematic 액정(液晶)에 저주파(低周波) 전압(電壓)을 인가하면 투명한 액정이 혼탁(混濁)상태로 변화하는 '동적산란(動的散亂)'(Dynamic Scattering) 현상을 이용하여 최초의 DSM(Dynamic Scattering Mode) LCD(Liquid Crystal Display)를 발명하였다. 비록 150V 이상의 높은 구동전압과 과소비전력의 특성 때문에 실용화에는 실패하였지만 Guest-Host효과와 Memory효과 등을 발견하였다. 1970년대에 이르러 실온에서 안정되게 사용 가능한 액정물질들이 합성되고(H. Kelker에 의해 MBBA, G. Gray에 의한 Cyano-Biphenyl 액정의 합성), CMOS 트랜지스터의 발명, 투명도전막(ITO), 수은전지등의 주변기술들의 발전으로 인하여 LCD의 상품화가 본격적으로 이루어지게 되었다. 1971년에는 M. Shadt, W. Helfrich, J.L. Fergason등이 TN(Twisted Nematic) LCD를 발명하여 전자 계산기와 손목시계에 응용되었고, 1970년대 말에는 Sharp에서 Dot Matrix형의 휴대형 컴퓨터를 발매하였다. 이러한 단순 구동형의 TN LCD는 그래픽 정보를 표시하는 데에는 품질의 한계가 있어 1979년 영국의 Le Comber에 의해 a-Si TFT(amorphous Silicon Thin Film Transistor) LCD의 연구가 시작되었고, 1983년 T.J. Scheffer, J. Nehring, G. Waters에 의해 STN(Super Twisted Nematic) LCD가 창안되었고, 1980년 N. Clark, S. Lagerwall 및 1983년 K.Yossino에 의해 Ferroelectric LCD가 등장하여 LCD의 정보 표시량 증대에 크게 기여하였다. Color화의 진전은 1972년 A.G. Ficher의 셀 외부에 RGB(Red, Green, Blue) filter를 부착하는 방안과, 1981년 T. Uchida 등에 의한 셀 내부에 RGB filter를 부착하는 방법에 의해 상품화가 되었다. 1985년에는 J.L. Fergason에 의해 Polymer Dispersed LCD가 발명되었고, 1980년대 중반에 이르러 동화상(動畵像) 표시가 가능한 a-Si TFT LCD의 시제품(試製品) 개발이 이루어지고 1990년부터는 본격적인 양산 시대에 접어들게 되었다. 1990년대 초에는 STN LCD의 Color화 및 대형화(大型化) 고(高)품위화에 힘입어 Note-Book PC에 LCD가 본격적으로 적용이 되었고, 1990년대 후반에는TFT LCD의 표시품질 대비 가격경쟁력 확보로 인하여 Note-Book PC 시장을 독점하기에 이르렀다. 이후로는 TFT LCD의 대형화가 중요한 쟁점으로 부각되고 있고, 1995년 삼성전자는 당시 세계최대 크기의 22' TFT LCD를 개발하였다. 또한 LCD의 고정세(高情細)화를 위해 Poly Si TFT LCD의 개발이 이루어졌고, 디지타이져 일체형 LCD의 상품화가 그 응용의 폭을 넓혔으며, LCD의 대형화를 위해 1994년 Canon에 의해 14.8', 21' 등의 FLCD가 개발되었다. 대형화 방안으로 Tiled LCD 기술이 개발되고 있으며, 1995년에 Sharp에 의해 21' 두장의 Panel을 이어 붙인 28' TFT LCD가 전시되었고 1996년에는 21' 4장의 Panel을 이어 붙인 40'급 까지의 개발이 시도 되었으며 현재는 LCD의 특성향상과 생산설비의 성능개선과 안정적인 공정관리기술을 바탕으로 삼성전자에서 단패널 40' TFT LCD가 최근에 개발되었다. Projection용 디스플레이로는 Poly-Si TFT LCD를 이용하여 $25'{\sim}100'$사이의 배면투사형과 전면투사형 까지 개발되어 대형 TV시장을 주도하고 있다. 21세기 디지털방송 시대를 맞아 플라즈마디스플레이패널(PDP) TV, 액정표시장치 (LCD)TV, 강유전성액정(FLCD) TV 등 2005년에 약 1500만대 규모의 거대 시장을 형성할 것으로 예상되는 이른바 '벽걸이TV'로 불리는 차세대 초박형 TV 시장을 선점하기 위하여 세계 가전업계들이 양산에 총력을 기울이고 있다. 벽걸이TV 시장이 본격적으로 형성되더라도 PDP TV와 LCD TV가 직접적으로 시장에서 경쟁을 벌이는 일은 별로 없을 것으로 보인다. 향후 디지털TV 시장이 본격적으로 열리면 40인치 이하의 중대형 시장은 LCD TV가 주도하고 40인치 이상 대화면 시장은 PDP TV가 주도할 것으로 보는 시각이 지배적이기 때문이다. 그러나 이러한 직시형 중대형(重大型)디스플레이는 그 가격이 너무 높아서 현재의 브라운관 TV를 대체(代替)하기에는 시일이 많이 소요될 것으로 추정되고 있다. 그 대안(代案)으로는 비교적 저가격(低價格)이면서도 고품질의 디지털 화상구현이 가능한 고해상도 프로젝션 TV가 유력시되고 있다. 이러한 고해상도 프로젝션 TV용으로 DMD(Digital Micro-mirror Display), Poly-Si TFT LCD와 LCOS(Liquid Crystals on Silicon) 등의 상품화가 진행되고 있다. 인터넷과 정보통신 기술의 발달로 휴대형 디스플레이의 시장이 예상 외로 급성장하고 있으며, 요구되는 디스플레이의 품질도 단순한 문자표시에서 그치지 않고 고해상도의 그래픽 동화상 표시와 칼라 표시 및 3차원 화상표시까지 점차로 그 영역이 넓어지고 있다. <표 1>에서 보여주는 바와 같이 LCD의 시장규모는 적용분야 별로 지속적인 성장이 예상되며, 새로운 응용분야의 시장도 성장성을 어느 정도 예측할 수 있다. 따라서 LCD기술의 연구개발 방향은 크게 두가지로 분류할 수 있으며 첫째로는, 현재 양산되고 있는 LCD 상품의 경쟁력강화를 위하여 원가(原價) 절감(節減)과 표시품질을 향상시키는 것이며 둘째로는, 새로운 타입의 LCD를 개발하여 기존 상품을 대체하거나 새로운 시장을 창출하는 분야로 나눌 수 있다. 이와 같은 관점에서 현재 진행되고 있는 LCD기술개발은 다음과 같이 분류할 수 있다. 1) 원가 절감 2) 특성 향상 3) New Type LCD 개발.

  • PDF

Sol-gel deposited TiInO thin-films transistor with Ti effect

  • Kim, Jung-Hye;Son, Dae-Ho;Kim, Dae-Hwan;Kang, Jin-Kyu;Ha, Ki-Ryong
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2009년도 제38회 동계학술대회 초록집
    • /
    • pp.200-200
    • /
    • 2010
  • In recent times, metal oxide semiconductors thin films transistor (TFT), such as zinc and indium based oxide TFTs, have attracted considerable attention because of their several advantageous electrical and optical properties. There are many deposition methods for fabrication of ZnO-based materials such as chemical vapor deposition, RF/DC sputtering and pulsed laser deposition. However, these vacuum process require expensive equipment and result in high manufacturing costs. Also, the methods is difficult to fabricate various multicomponent oxide semiconductor. Recently, several groups report solution processed metal oxide TFTs for low cost and non vacuum process. In this study, we have newly developed solution-processed TFTs based on Ti-related multi-component transparent oxide, i. e., InTiO as the active layer. We propose new multicomponent oxide, Titanium indium oxide(TiInO), to fabricate the high performance TFT through the sol-gel method. We investigated the influence of relative compositions of Ti on the electrical properties. Indium nitrate hydrate [$In(NO^3).xH_2O$] and Titanium isobutoxide [$C_{16}H_{36}O_4Ti$] were dissolved in acetylacetone. Then monoethanolamine (MEA) and acetic acid ($CH_3COOH$) were added to the solution. The molar concentration of indium was kept as 0.1 mol concentration and the amount of Ti was varied according to weighting percent (0, 5, 10%). The complex solutions become clear and homogeneous after stirring for 24 hours. Heavily boron (p+) doped Si wafer with 100nm thermally grown $SiO_2$ serve as the gate and gate dielectric of the TFT, respectively. TiInO thin films were deposited using the sol-gel solution by the spin-coating method. After coating, the films annealed in a tube furnace at $500^{\circ}C$ for 1hour under oxygen ambient. The 5% Ti-doped InO TFT had a field-effect mobility $1.15cm^2/V{\cdot}S$, a threshold voltage of 4.73 V, an on/off current ratio grater than $10^7$, and a subthreshold slop of 0.49 V/dec. The 10% Ti-doped InO TFT had a field-effect mobility $1.03\;cm^2/V{\cdot}S$, a threshold voltage of 1.87 V, an on/off current ration grater than $10^7$, and a subthreshold slop of 0.67 V/dec.

  • PDF

$N_2$$SiH_4$ 가스를 사용하여 PECVD로 증착된 Silicon Nitride의 물성적 특성과 전기적 특성에 관한 연구 (Physical properties and electrical characteristic analysis of silicon nitride deposited by PECVD using $N_2$ and $SiH_4$ gases)

  • 고재경;김도영;박중현;박성현;김경해;이준신
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 춘계학술대회 논문집 유기절연재료 전자세라믹 방전플라즈마 일렉트렛트 및 응용기술
    • /
    • pp.83-87
    • /
    • 2002
  • Plasma enhanced chemical vapor deposited (PECVD) silicon nitride ($SiN_X$) is widely used as a gate dielectric material for the hydrogenated amorphous silicon(a-Si:H) thin film transistors (TFT's). We investigated $SiN_X$ films were deposited PECVD at low temperature ($300^{\circ}C$). The reaction gases were used pure nitrogen and a helium diluted of silane gas(20% $SiH_4$, 80% He). Experimental investigations were carried out with the variation of $N_2/SiH_4$ flow ratios from 3 to 50 and the rf power of 200 W. This article presents the $SiN_X$ gate dielectric studies in terms of deposition rate, hydrogen content, etch rate and C-V, leakage current density characteristics for the gate dielectric layer of thin film transistor applications. Electrical properties were analyzed through high frequency (1MHz) C-V and current-voltage (I-V) measurements. The thickness and the refractive index on the films were measured by ellipsometry and chemical bonds were determined by using an FT-IR equipment.

  • PDF

고희석 SiH4 가스를 이용하여 증착한 저온 PECVD 실리콘 질화물 박막의 기계적, 전기적 특성연구 (Characteristics of Low Temperature SiNx Films Deposited by Using Highly Diluted Silane in Nitrogen)

  • 노길선;금기수;홍완식
    • 대한금속재료학회지
    • /
    • 제50권8호
    • /
    • pp.613-618
    • /
    • 2012
  • We report on electrical and mechanical properties of silicon nitride ($SiN_x$) films deposited by a plasma enhanced chemical vapor deposition (PECVD) method at $200^{\circ}C$ from $SiH_4$ highly diluted in $N_2$. The films were also prepared from $SiH_4$ diluted in He for comparison. The $N_2$ dilution was also effective in improving adhesion of the $SiN_x$ films, fascilitating construction of thin film transistors (TFTs). Metal-insulator-semiconductor (MIS) and Metal-insulator-Metal (MIM) structures were used for capacitance-voltage (C-V) and current-voltage (I-V) measurements, respectively. The resistivity and breakdown field strength of the $SiN_x$ films from $N_2$-diluted $SiH_4$ were estimated to be $1{\times}10^{13}{\Omega}{\cdot}cm$, 7.4 MV/cm, respectively. The MIS device showed a hysteresis window and a flat band voltage shift of 3 V and 0.5 V, respectively. The TFTs fabricated by using these films showed a field-effect mobility of $0.16cm^2/Vs$, a threshold voltage of 3 V, a subthreshold slope of 1.2 V/dec, and an on/off ratio of > $10^6$.

Photofield-Effect in Amorphous InGaZnO TFTs

  • Fung, Tze-Ching;Chuang, Chiao-Shun;Mullins, Barry G.;Nomura, Kenji;Kamiya, Toshio;Shieh, Han-Ping David;Hosono, Hideo;Kanicki, Jerzy
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2008년도 International Meeting on Information Display
    • /
    • pp.1208-1211
    • /
    • 2008
  • We study the amorphous In-Ga-Zn-O thin-film transistors (TFTs) properties under monochromatic illumination ($\lambda=420nm$) with different intensity. TFT off-state drain current ($I_{DS_off}$) was found to increase with the light intensity while field effect mobility ($\mu_{eff}$) is almost unchanged; only small change was observed for sub-threshold swing (S). Due to photo-generated charge trapping, a negative threshold voltage ($V_{th}$) shift is also observed. The photofield-effect analysis suggests a highly efficient UV photocurrent conversion in a-IGZO TFT. Finally, a-IGZO mid-gap density-of-states (DOS) was extracted and is more than an order lower than reported value for a-Si:H, which can explain a good switching properties of the a-IGZO TFTs.

  • PDF

Poly-Silicon TFT's on Metal Foil Substrates for Flexible Displays

  • Hatalis, Miltiadis;Troccoli, M.;Chuang, T.;Jamshidi, A.;Reed, G.
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2005년도 International Meeting on Information Displayvol.I
    • /
    • pp.692-696
    • /
    • 2005
  • In an attempt to fabricate all inclusive display systems we are presenting a study on several elements that would be used as building blocks for all-on-board integrated applications on stainless steel foils. These systems would include in the same substrate all or many of the components needed to drive a flat panel OLED display. We are reporting results on both digital and analog circuits on stainless steel foils. Shift registers running at speeds greater than 1.0MHz are shown as well as oscillators operating at over 40MHz. Pixel circuits for driving organic light emitting diodes are presented. The device technology of choice is that based on poly-silicon TFT technology as it has the potential of producing circuits with good performance and considerable cost savings over the established processes on quartz or glass substrates (amorphous Silicon a-Si:H or silicon on Insulator SOI).

  • PDF

Stability of Hydrogenated Amorphous Silicon TFT Driver

  • Bae, Byung-Seong;Choi, Jae-Won;Oh, Jae-Hwan;Kim, Kyu-Man;Jang, Jin
    • Journal of Information Display
    • /
    • 제6권1호
    • /
    • pp.12-16
    • /
    • 2005
  • Gate and data drivers are essential for driving active matrix display. In this study, we integrate drivers with a-Si:H to develop a compact, better reliability and cost effective display. We design and fabricate drivers with conventional a-Si:H thin film transistors (TFTs). The output voltages are investigated according to the input voltage, temperature and operation time. Based on these studies, we propose here a new driver to prevent gate line from the floated state. For the external coupled voltage fluctuation, the proposed driver shows better stability.

Direct deposition technique for poly-SiGe thin film achieving a mobility exceeding 20 $cm^2$/Vs with ~30 nm thick bottom-gate TFTs

  • Lim, Cheol-Hyun;Hoshino, Tatsuya;Hanna, Jun-Ichi
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2009년도 9th International Meeting on Information Display
    • /
    • pp.1028-1031
    • /
    • 2009
  • High quality poly-SiGe thin films were prepared on 6-inch substrates using Reactive-thermal CVD with $Si_2H_6$ and $GeF_4$ around at $500^{\circ}C$ directly. Its thickness uniformity was ~ 3% on the entire substrate area. N-channel mobility of ~30 nm thick bottom-gate TFTs exceeded 20 $cm^2$/Vs without any further crystallization.

  • PDF

대기압 플라즈마 정밀 Etching 기술 개발

  • 임찬주;김윤환;이상로;악흔
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2011년도 제40회 동계학술대회 초록집
    • /
    • pp.263-263
    • /
    • 2011
  • 본 연구에서는 DBD (Dielectric Barrier Discharge)방식의 상압 플라즈마를 이용하여 FPD (flat panel display) 공정에 사용되는 a-Si, Si3N4의 식각 공정 특성을 평가하였다. 사용된 DBD 반응기는 기존의 blank planar plate 형태의 Power가 인가되는 anode 부분과 Dielectric Barrier 사이 공간을 액상의 도전체로 채워 넣은 형태의 전극이 사용 하였으며, 인가 Power는 40kHz AC 최대인가 전압 15 kVp를 사용 하였다. 방전 가스는 N2, 반응가스로는 CDA (Clean Dry Air)와 NF3, 액상의 Etchant를 사용 하였으며 모든 공정은 In-line type으로 시편을 처리 하였다. NF3의 경우 30 mm/sec 이송속도 1회 처리 기준 a-Si 1300${\AA}$, Si3N4 1900${\AA}$의 식각 두께를 보였으며 a-Si : Si3N4 선택비는 N2, CDA의 조절을 통하여 최대 1:2에서 4:1 정도까지 변화가 가능하였다. 균일도는 G2 (370 mm${\times}$470 mm)의 경우 5.8 %의 균일도를 보이고 있다. 이외에도 NF3 공정의 경우 실제 TFT-LCD 공정 중 n+ channel (n+ a-Si:H)식각 공정에 적용하여 5.5 inch LCD panel feasibility를 확인 할 수 있었다. 액상 Etchant (HF수용액, NH4HF2)는 버블러를 사용하여 기화 시켜 플라즈마 소스를 통해 1차적으로 활성화 시키고 기존 DBD 반응기에 공급해 주는 형태로 평가를 진행하였다. 식각 특성은 30mm/sec 이송속도에서 a-Si $25{\AA}$ 정도로 가스 형태의 Etchant에 비해 매우 낮은 수준이나 Etching rate 향상을 위한 factor 파악 및 개선을 위한 연구를 진행 하였다.

  • PDF