Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.16
no.12S
/
pp.1286-1291
/
2003
Quench behavior of resistive superconducting fault current limiters (SFCLS) with various pattern shapes was investigated. The pattern shapes employed were meander, bi-spiral, and spital shapes of identical line width, gap and margin. SFCLS were fabricated from YBCO thin films grown on two-inch diameter Al$_2$O$_3$ substrates under the same conditions. The total length of current limiting paths was the shortest at the spital shape due to its larger useless space. Inductance component of SFCLs with the spiral shape was around two times as high as those of other two shapes. This is not desirable since impedance characteristics of existing power systems can be changed. Resistance rise of current limiting elements was low at a spiral shape before the whole quench completion, which may act as a disadvantage for simultaneous quench in serial connection between current limiting elements, but the temperature tended to have similar values at higher voltages. On the other hand, hi-spital shape was severe at insulation level between current limiting lines. When these aspects were considered, we concluded that a meander shape was appropriate to design for a resistive SFCL based on thin films except the concentration of electric field at edge areas of strip lines.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2006.05a
/
pp.146-148
/
2006
The quench characteristics of flux-lock type high-Tc superconducting fault current limiters(SFCL) was investigated, $YBa_2Cu_3O_{7-x}$(YBCO) thin film was used as the current limiting elements of the flux-lock type SFCL. The quench characteristics of current limiting elements consisting of the flux-lock type SFCL was more improved than that of the resistive type SFCL.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2006.05a
/
pp.77-81
/
2006
We report the performance of a four-element, 11.67 GHz, high-Tc superconducting (HTS) microstrip antenna array with corporate feed network and circular polarization for direct broadcasting satellite (DBS) system. Our array antennas were designed and built on a 0.5 mm thick MgO substrate. To compare the superconducting antennas with normal conducting counterpart, One antenna pattern was fabricated from gold thin film, and a second pattern was fabricated from $YBa_2Cu_3O_{7-x}$ (YBCO) superconducting thin film. To improve the axial ratio of circularly polarized arrays, sequential rotation technique were used. Efficiency, radiation pattern, return loss and bandwidth were measured for both antennas at room temperature and at cryogenic temperature. The array produced good circular polarization, and the gain of the array at 77 K, relative to a copper array at room temperature was approximately 1.54 dB. The measured return loss of our HTS antenna array was 35.79 dB at the resonant frequency of 11.67 GHz and The total effective bandwidth was about 3.4 %. The results showed that high-temperature superconductors, when used in microstrip arrays, improved the efficiency of the HTS antenna array for circularly polarization.
Superconducting fault currents(SFCLs) are expected to improve not only reliability but also stability of power systems. The analysis on current limiting operations of the flux-lock type SFCL, which consists of a flux-lock reactor wound an iron core and a YBCO thin film, was compared the open-loop with the closed-loop iron core of the subtractive polarity winding. In the SFCL, operation characteristics could be controlled by adjusting the inductances and the winding directions of the coils, then magnetic field induced in the iron core. The current limiting characteristics under the same experimental conditions were generated regardless of the iron core conditions. We confirmed that capacity of the SFCL was increased effectively by the closed-loop iron core. However, the power burden of the system could be lowered by the open-loop iron core.
In this study, superconducting coil arrangements and cryostat concept design were conducted for the development of 13.2kV/630A bifilar winding type high temperature superconducting(HTS) fault current limiter(FCL) with YBCO coated conductor(CC) wire. The coil consists of several layers with unique non-inductive solenoid winding method. Six types of HTS coil arrangements were investigated for the optimal insulation design of HTS FCL. And, conceptual design of cryostat was conducted for the decrement of thermal invasion and the prevention of low voltage insulation breakdown in the LHe which is used as pressurization gas in sub-cooling condition of liquid nitrogen(LN2). As the results, it was found that the modified suspended type cryostat with horizontal coil arrangement is beneficial to the insulation design of 13.2kV level bifilar winding type HTS FCL.
The submicron $YBa_2Cu_3O_x$ powder was prepared by the sol-gel method. The particle size is distributed from 0.2 to 1.0 ${\mu}m$, which benefits to eliminate the micro-cracks formed in the $YBa_2Cu_3O_x$ films deposited by electrophoresis. The powder was single phase of $YBa_2Cu_3O_x$ examined by X-ray diffraction. In the sol-gel process the citrate gel was formed from citric acid and nitrate solution of $Y_2O_3$, $Ba(NO_3)_2$ and CuO. When pH values were adjusted to 6.4-6.7, $Ba(NO_3)_2$ could be dissolved in the citrate solution completely. Appropriate evaporative temperature of the sol-gel formation is discussed. Acetone is used as electrophoreticsolution, in which some water and iodine (0.2 g/1) and polyethylene glycol (2 vol. %) are added. The concentrations of $YBa_2Cu_3O_x$ powders is 20g/l. The thickness of deposited film could be more than 50 ${\mu}m$ in 3 minutes of depositing time. The most EPD films could be 90K zero resistance and the Jc values were over 1000A/cm2 (0 H, 77 K).
We fabricated resistive superconducting fault current limiters (SFCL) based on YBCO thin films grown on 2-inch diameter saphire substrates Two SFCLs with nearly identical properties were connected in series to investigate the simultaneous quench. There was a slight difference in the rate of voltage increase between two SFCL units when they were operated independently. This difference. however, resulted in significantly unbalanced power dissipation between the units. This imbalance was removed by connecting a shunt resistor to an SFCL in parallel. The appropriate values of the shunt resistances were $80{\Omega}$ at $75 V_{rms}$. $100{\Omega}$ at $100 V_{rms}$ and $110{\Omega}$ at $120 V_{rms}$, respectively. Increased power input at high voltages also reduced the initial imbalance in power dissipation. but with increase in film temperature to higher than 200 K.
Kim, Young Gon;Baek, Geonwoo;Han, Seunghak;Choi, Yojong;Kim, Junseong;Jeon, Haeryong;Ko, Tae Kuk
Progress in Superconductivity and Cryogenics
/
v.21
no.4
/
pp.48-52
/
2019
Recently, many studies have been reported on the magnetoresistance and Hall effect of REBCO thin films and bulk. The voltage interferes quench detection of high-temperature superconducting magnet and generates leakage current in no insulation high-temperature superconducting coil. Therefore, in this paper, experiments on magnetoresistance and Hall effect of commercial YBCO and GdBCO tapes have been carried out. As a result, anomalous voltages expected for the magnetoresistance and Hall effect of REBCO tapes were observed and analyzed. In addition, the voltage characteristics of REBCO have been identified, and the Hall coefficient are calculated for use in high magnetic field magnet applications.
The Transactions of The Korean Institute of Electrical Engineers
/
v.61
no.9
/
pp.1296-1299
/
2012
$YBa_2Cu_3O_{7-x}$ thin films were fabricated by the spin-coating method on $SiO_2$/Si substrate using an alkoxide-based sol-gel method. The structural and electrical properties were investigated for various 1st annealing temperature. Due to the formation of the polycrystalline single phase, synthesis temperature was observed at around $720^{\circ}C-800^{\circ}C$. $YBa_2Cu_3O_{7-x}$ thin films with the 1st annealing temperature of $450^{\circ}C{\sim}500^{\circ}C$ showed the single XRD patterns without the second phase, such as $YBa_2Cu_4O_8$. The thickness of films was approximately $0.23{\mu}m{\sim}0.27{\mu}m$. Aerage grain size, resistance and temperature coefficient of resistance (TCR) of $YBa_2Cu_3O_{7-x}$ thin films with the 1st annealing temperature of $500^{\circ}C$ were $0.27{\mu}m$, $59.7M{\Omega}$ and -3.7 %/K, respecvitely.
Park Chung-Ryul;Lim Sung-hun;Park Hyoung-Min;Lee Jong-Hwa;Ko Seokcheol;Choi Hyo-Sang;Han Byoung-Sung;Hyun Ok-Bae;Chung Dong-Chul
Proceedings of the KIEE Conference
/
summer
/
pp.1130-1132
/
2004
In this paper, we investigated the operational characteristics of the fault current limiting in the The flux-lock type high-Tc superconducting fault current limiter. The flux-lock type high-Tc superconducting fault current limiter was consisted of primary and secondary copper coils that flux was locked on iron core and YBCO thin film. The operational characteristic of a flux-lock type SFCL dependent on winding direction of coil 1 and coil 2, and the number of turns of coil 1 and coil 2, inductances of the coils, saturation in iron core, the properties of superconducting element etc. In this cases, we investigated the fault currents limiting characteristics of the flux-lock type SFCL when winding direction of coil 1 and coil 2 was subtractive polarity winding.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.